At least 37 records · Page 2

Reducing warpage in a hybrid large-scale additive manufacturing and compression molding process

In recent years, a hybrid manufacturing process, developed by combining extrusion-based large-scale additive manufacturing (AM) and compression molding (CM) techniques, has shown promising outcomes for producing structurally functional parts. The process can be used with both short fiber-reinforced composites and neat polymers and hence, even multi-material parts can be manufactured easily. This process offers the advantages of structural enhancement by having a desired fiber orientation using a large-scale AM process, as well as rapid manufacturing capability using a CM process. In the large-scale AM process, the alignment of fibers in the deposition direction enables significant improvement in the mechanical properties of the manufactured parts. However, the anisotropy resulting from the directional arrangement of fibers also introduces challenges related to warpage in the produced parts. This study aims to identify the causes of warpage and propose strategies to mitigate it. The research involves the use of preforms manufactured through the large-scale AM, which are then combined with the neat resin for CM manufacturing. A finite element-based numerical simulation model is developed, employing a sequentially coupled thermomechanical approach. Through a parametric study using the simulation models, optimization of printing direction and preform geometry is performed to minimize warpage. This contributes to the advancement and wider adoption of AM/CM hybrid manufacturing to produce structurally functional parts.

Jo, Eonyeon↗

Macro-level mechanical interlocking: A rapid joining approach for additively manufactured compression molded composite panels

Composite joining typically involves multiple steps, such as drilling and surface treatment, as part of the manufacturing process, which leads to low throughput and long cycle times. In the present study, we demonstrated a macro-level mechanical interlocking (MI) based, rapid joining technique to assemble additively manufactured compression molded (AMCM) panels, enabling the production of parts larger than the mold dimensions. Composite panels made of 20 wt% short carbon fiber reinforced acrylonitrile butadiene styrene (CF/ABS) were joined using MI features of various geometries, namely tree (TR), dovetail (Dov), rectangle 2 (Rect2), and rectangle 1 (Rect1), and their in-plane strength was evaluated. The resultant strength of the tested MI joints reached up to 74 % of the baseline tensile strength (i.e., the ‘no joint’ case). Observations from optical and scanning electron microscopy revealed inadequate polymer diffusion between the adherends, indicating that the joint strength was primarily derived from mechanical interlocking. Additionally, the fracture surfaces exhibited stress-whitening marks, which were characterized using differential scanning calorimetry (DSC). The increase in melting enthalpy suggested local stretching of polymer chains due to MI. Finite element analysis (FEA) indicated that the Rect1 MI feature, which generated the lowest stress concentration, outperformed the others in terms of joint strength, achieving 42 MPa. As a demonstration of the MI joining method, a battery box tray measuring 108 cm × 34 cm using a mold with an effective dimension of 36 cm × 34 cm successfully manufactured, resulting in a part with an area three times larger than the mold. In conclusion, this study presents a promising approach to improving composite joining techniques while minimizing production complexities.

In-plane joining↗

HYBRID COMPOSITES VIA CO-EXTRUSION ADDITIVE MANUFACTURING-COMPRESSION MOLDING FOR PERFORMANCE OPTIMIZATION

The growing demand for hybrid polymer composites with multifunctional properties has led to the development of various hybridization techniques, such as multi-material compounding and controlled laminate stacking sequence. In this study, a novel hybrid manufacturing approach was used by integrating a multiplexing extrusion system (MExS) based on additive manufacturing with subsequent compression molding process. This technique enabled the co-extrusion of different materials during the additive manufacturing process to fabricate composites with tailored performance. The developed hybrid composite featured a skin layer of glass fiberreinforced polycarbonate (PC/GF) encapsulating a carbon fiber-reinforced acrylonitrile butadiene styrene (CF/ABS) core. The structure was engineered to promote improved thermal and impact resistance at the surface, supported by a stiff core for enhanced overall mechanical integrity. Mechanical, thermal and morphological properties of the hybrid composites were investigated to understand trade-offs in performance compared to a single-material system. The results demonstrate that this approach enables the production of multifunctional composites suitable for applications such as automotive body panels and protective housings, where a balance of weight, mechanical strength, and thermal performance is essential.

Wasti, Sanjita [ORNL]↗

Siloxane-modified polycarbosilane flexible Prepregs for fabrication of ceramic matrix composites via compression molding and PIP densification

For this work, the development of ceramic matrix composites (CMCs) using 5 harness satin carbon fiber fabric impregnated with commercial polycarbosilane precursor plasticized by siloxane copolymer was investigated aiming to improve wetting behavior and shape conformability. The polycarbosilane precursor and polysiloxane plasticizer were mixed at varying weight ratios to obtain flexible preceramic resin prepreg cloths. 13 plies of preceramic polymer prepreg cloths were stacked in 0/90° layup and cured by compression molding, followed by densified via PIP process. The CMCs were densified with eight PIP cycles followed by final crystallization at 1600 °C. The CMCs made with 10 wt% polysiloxane loading showed lower viscosity of the prepreg resin as well as higher strength and displacement to failure compared to those fabricated from unplasticized polycarbosilane prepolymer. In contrast, at higher concentration of plasticizer, viscosity of the prepreg resin increased, and the CMC became more brittle; however, it exhibited considerably higher thermal conductivity.

Carbosilane↗

Large-scale additive manufacturing tooling for extrusion-compression molds

Carbon fiber reinforced polymer composites (CFPC) have been used in additive manufacturing (AM) due to both the high-strength-to-weight and superior-stiffness-to-weight ratios. CF AM is being considered for tooling applications. In AM, CFPCs are usually aligned along the deposition direction; however, it results in anisotropic thermal properties which affect the heat transfer and warpage of the final part. In this study, three male molds with different infill patterns were produced via the material extrusion additive manufacturing (EDF-AM) process. These include (a) 0°: infill pattern along the printing direction; (b) 90°: infill pattern perpendicular to the printing direction; and (c) 0°/90°: alternate layers along and perpendicular directions. The effect of the infill pattern on thermal conductivity was analyzed and observed that 0° infill (surface temperature: 79.2°C) had the highest conductivity; and 90° infill (surface temperature: 66.4°C) had the least.

36 MATERIALS SCIENCE↗

The use of digital thread for reconstruction of local fiber orientation in a compression molded pin bracket via deep learning

A deep convolutional neural network (DCNN) was used for microstructure reconstruction using artificial intelligence (MR-AI) by predicting local average fiber orientation distributions (FOD) in a 3D prepreg platelet molded composite (PPMC) pin bracket. To train the MR-AI model, surface strain fields from residual stresses simulated in PPMC plates were used as the input to the DCNN. A training dataset included PPMC plates with various degrees of global fiber alignment, based on the information obtained from high-fidelity flow simulation of a pin bracket. Further, the MR-AI model was then deployed to analyze FOD in the 3D pin bracket by conducting thermo-elastic residual stress analysis. Initially, the MR-AI model was established entirely on the synthetic simulation data. Then, a μCT scan of a physically molded pin bracket was used to create a finite element model that provided data for additional validation of the DCNN model. For the μCT scan finite element pin bracket the MR-AI model predicted the distribution of fiber orientation tensor components with MAE of 0.10 indicating a global prediction error of 10%. For the flow simulated pin bracket, the MR-AI model predicted the distribution of fiber orientation tensor components with a global prediction error of 11%. The MR-AI model showed the ability to predict regions of varying alignment in the base and flange of the pin bracket. The proposed MR-AI methodology allows for rapid prediction of FOD in geometrically complex parts and offers a promising path to detecting unique fiber orientation states in molded components.

42 ENGINEERING↗

Dimensional stability of low-cost thermoplastic composite molds

This report addresses a key question for using additively manufactured tooling from carbon fiber reinforced thermoplastic composites. How does the distortion of the molded part change with the print orientation used in the manufacture of tooling? The objective of this research was to discuss the distortion of parts molded with such tooling, in relation to the deflections in the tooling during the compression molding process. This was achieved through both model simulations and experimental molding runs. A vertical orientation was used in printing the mold with a distinctly non-planar surface: this orientation allowed for higher performance along the press closing direction -- higher thermal conductivity, higher stiffness, and lower coefficient of thermal expansion. Epoxy-carbon fiber twill weave fabric prepreg was then compression molded in this mold. The thermomechanical properties of the tooling material and the molded part were measured and used in simulation of mold deformation as well as part distortion. The thermomechanical anisotropy of the mold is quite different from that of the molded part because in the mold, the stiffest direction is the z-axis, while in the molded thermoset part, the z-axis is the weakest direction. The connection between mold deformation during the compression molding process and the final part distortion can be seen from the simulation results. The simulation results for the case where the mold was four times as stiff as the part along the press closing direction compared well with experiment. When the mold stiffness was lowered in relation to the part stiffness, the mold deformation during the compression molding increased; but this led to a smaller extent of part distortion.

36 MATERIALS SCIENCE↗

Multi-Process Tooling

Decisions made early in the automotive design process influence material selection, which in turn dictates process selection and tool design. Because of tool build time and cost of tooling, the original path is not easily altered, even if there is compelling evidence that another material or process would be beneficial. This project focused on tool design that is agile enough to allow its use in multiple processes—injection, injection compression, and extrusion-compression. This tool design allows for the manufacture of components with the most efficient process or materials, without building multiple, single-process tools. The primary purpose of the Multi-Process Tool project was to physically demonstrate that a single, well-designed tool could be used to manufacture parts with a variety of materials that require different processes. A multi-process tool would be beneficial to providing data for any changes to the process since materials and processes can be interchanged without incurring additional tool cost(s). Battery tray parts, (representative of a multi-process tool, were successfully manufactured using various types of materials, such as fiber reinforced (carbon fiber and/or glass fibers, recycled carbon fibers), amorphous (PP, TPU), semi-crystalline (PA6, PA66), and crystalline (thermoset epoxy resin) polymers. Processing of the parts was achieved by injection molding, compression molding, compression overmolding, and injection overmolding. Specimens extracted from various locations on the battery tray parts were evaluated for mechanical properties (flexure and interlaminar shear strength properties). The results show that the tool can be used to produce parts from a wide range of materials and processes with no degradation of the physical or cosmetic properties.

42 ENGINEERING↗

Biodegradable High-Molecular-Weight Poly(pentylene adipate- co -terephthalate): Synthesis, Thermo-Mechanical Properties, Microstructures, and Biodegradation

Poly(pentylene adipate-co-terephthalate) (PPAT) is a promising biobased and biodegradable polymer that can replace polyethylene in flexible packaging films where biodegradability is desired. High-molecular-weight (100K–145 KDa) aliphatic–aromatic polyester PPAT was successfully synthesized, and the effects of reaction conditions on molecular weight were reported. PPAT polyesters were characterized for polymer compositions, number-average unit length, thermal transitions, and rheological properties. PPAT compression-molded films were characterized for crystallinity and tensile properties to correlate micro- and macroproperties. PPAT compression-molded films exhibited up to a 76% higher tensile modulus than compression-molded films from poly(butylene adipate-co-terephthalate) (PBAT), making PPAT films potentially comparable with compression-molded films from linear low-density polyethylene (LLDPE). Finally, PPAT is biodegradable in soil and freshwater environments with estimated 90% biodegradation times of 504–580 and 604–845 days, respectively, while PBAT takes 971 days in soil and 395 days in freshwater.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

High-performance molded composites using additively manufactured preforms with controlled fiber and pore morphology

Here, large-scale multimaterial preforms produced by additive manufacturing (AM) underwent compression molding (CM) to produce high-performance thermoplastic composites reinforced with short carbon fibers. AM and CM techniques were integrated to control the fiber orientation (microstructure) and to reduce void content for the improved mechanical performance of the composite. The new integrated manufacturing technique is termed “additive manufacturing-compression molding” (AM-CM). For the present study, the most common materials were used for large-scale printing, i.e., acrylonitrile butadiene styrene (ABS), carbon fiber (CF)–filled ABS (CF/ABS) and glass fiber (GF)–filled ABS (GF/ABS). Three different manufacturing processes; (a) AM (b) extrusion compression molding (ECM), and (c) AM-CM were used to prepare four different panel configurations: (1) neat ABS, (2) CF/ABS, (3) overmold (CF/ABS over neat ABS), and (4) sandwich (neat ABS between two CF/ABS layers). The mechanical properties (tensile and flexural strength and modulus, and Izod impact energy) of samples prepared via all three manufacturing processes were compared. X-ray microcomputer tomography was employed to evaluate the fiber orientation distribution and the volumetric porosity content. The preform maintained high fiber alignment (≈ 82% of fibers within the range of 0–20° in the deposition direction), and the volumetric porosity was reduced by 50% from 3.79% to 1.91% after compression. The alignment of long pores along the deposition direction was also observed. The mechanical properties are discussed with correlation to the fiber alignment and void content in the samples. CF/ABS samples prepared by AM-CM showed significant improvement of 11.15%, 35.27%, 28.6%, and 74.3% in the tensile strength, tensile modulus, flexural strength, and flexural modulus, respectively, when compared with samples prepared by ECM. Unique aspects of this study are the demonstration of large-scale multimaterial AM and the use of multimaterials as preforms to make high-performance composites.

36 MATERIALS SCIENCE↗

Blending Polyurethane Thermosets Using Dynamic Urethane Exchange

Recycling crosslinked polyurethanes (PUs) is accomplished through mechanical or chemical processes that are energy-intensive or produce plastics of lesser value. Polymer recycling processes are notably intolerant of polymer mixtures, yet the ability to reprocess and compatibilize two or more crosslinked PUs together will make this process more amenable to mixed waste streams while offering an opportunity to tune the properties of the recycled polymer products. Here, we blend a rigid polyester PU and a soft polyether PU using twin-screw extrusion to yield materials with tunable mechanical properties based on the feed composition. Their material properties were compared to those of compression-molded reprocessed blends and blends where the monomers were mixed prior to synthesis. The extruded materials showed similar mechanical and thermal properties to newly prepared blends and had higher-value mechanical properties compared to the samples reprocessed via compression molding. The morphologies of the blends were observed using phase imaging via atomic force microscopy to show that there is less phase separation in the extruded materials compared to compression-molded blends. The mechanical properties of these materials were tunable from soft to elastomeric to rigid based on the feed composition, and this tunability was demonstrated through four consecutive reprocessing cycles, through which the mechanical properties were steadily varied from rigid to soft by incorporating increasing amounts of soft polyether PU material. Here, this blending method for reprocessing mixed waste compatibilizes different PUs and provides a means to tune the mechanical properties of a PU product, even if starting from waste streams of varying compositions. As such, this process represents an intriguing new approach for polymer reprocessing.

Extrusion↗

RapidClave® Technology Demonstrations – II Hat Stiffener

This project sought to evaluate the cost and performance of both polymeric and metallic tooling for use with the RapidClave® composite process. Teijin’s rapid cure carbon/epoxy prepreg, Q183, was selected to fabricate demonstration components, of aerospace design, which currently are fabricated via compression molding using matched steel tooling. The ability to fabricate components using this prepreg in the RapidClave®, and using low cost single sided tooling, could significantly reduce the cost of part manufacture and shorten production lead times for tooling fabrication. The component demonstration article was a “hat stiffener” geometry typically used to reinforce fuselage or wing skins of an aircraft. A rapid preforming process was demonstrated and rapid process cycle times similar to compression molding were achieved by placing the preform on hot tooling, thus avoiding the time and energy associated with typical thermal cycling. A 90% reduction in tooling cost was achieved through the use of single sided aluminum or polymeric additive tooling when compared to compression molding matched steel tooling. In addition to rapid cycle times, RapidClave® offers the ability to change out tooling in minutes such that multiple part geometries can be fabricated in one shift.

36 MATERIALS SCIENCE↗

Enhanced Interfacial Strength in Carbon Fiber Composites via Mussel‐Inspired Sizing Polymers

Composite materials possess a high strength-to-weight ratio. A key determinant of their mechanical performance is the interfacial strength between the fibers and the matrix. Sizing agents are commonly used to improve this interface by promoting better adhesion, though optimizing this interaction remains a significant challenge. Here, this study evaluates the use of poly(catechol-styrene) (PCS), a mussel-inspired sizing agent, to enhance fiber–matrix bonding in carbon fiber composites. Woven carbon fiber laminates were dip-coated with varying concentrations of PCS (0.05 and 0.1 wt%) and subsequently fabricated using vacuum-assisted resin transfer molding followed by compression molding. Interlaminar shear strength (ILSS) tests showed improvements of 4% and 8% for the 0.05% and 0.1% PCS treatments, respectively. These results indicate that PCS is effective in reinforcing interfacial adhesion, thereby improving the mechanical integrity of carbon fiber-reinforced composites.

Carbon fiber composites↗

Effect of fiber sizing and glass fiber laminate hybridization on vibration damping and mechanical properties of banana fiber reinforced polypropylene composites

Modern automotive applications demand lightweight, multifunctional materials to reach mileage goals and natural fiber reinforced composites (NFRCs) are one of the classes of materials proposed as a solution. NFRCs exhibit good vibration damping properties and have low density, but are often limited by processing challenges, poor-fiber matrix compatibility and variable performance. Herein, we investigate non-woven wet-lay of comingled banana fiber (BF), recycled glass fiber (rGF), and polypropylene (PP) fibers to in situ sizing and preparation of composite feedstocks for compression molding. BF and rGF hybrids were prepared by stacking rGF layers during compression molding to produce composites with various fiber ratios. The effect of fiber content, in-situ sizing and ratio of BF to rGF on tensile, flexural and vibration damping performance are investigated. Key results are the significant increase in tensile strength by in situ sizing (40 % sized at 60 wt% BF) and in flexural modulus (+58 % sized at 60 wt% BF) and flexural strength (+41 % sized 60 wt% BF) compared to the unsized equivalent. For BF-rGF hybrid composites with40 wt% total fiber content, flexural strength and modulus were improved by 51 % and 231 % respectively for a 1:1 ratio BF:rGF compared to BF reinforced system. Lastly, identifying the cross-over point where damping and stiffness are optimized for a hybrid composite. These findings demonstrate that these composites can be used as alternative to synthetic fiber or mineral filled composites in automotive applications, particularly where weight reduction, vibration damping and stiffness are desired.

Banana fiber↗

Low-Cost Preform and Molding Processes

The entry cost for prototyping a composite component for manufacture using automated, high rate processes is prohibitively expensive in many cases, especially for small business, where tooling costs may be several $100k. Discussions with industry also indicate that many small companies, tier 1 and 2 suppliers, have an interest to mold composite parts but do not want to deal with the capital cost, material handling issues, and labor associated with dry fiber preforming operations. While the molders may locate near the end user for logistics reasons, it may be more cost effective for the performer to remain regional and invest in capital equipment to support preform automation, thus keeping costs to a minimum. This project was designed to explore and demonstrate several options to meet these industry needs. Dry fiber preforming approaches were evaluated which allow for low pressure resin infusion, single sided tooling options such a vacuum assisted resin transfer molding (VARTM) or low pressure resin transfer molding (RTM-light). Unlike sheet molding compound, SMC compression molding where typical molding pressures of 1000 psi are required to push material into the desired location; positioning of a dry fiber preform into the desired location on the tool allows for low molding pressures of 10-50 psi. Lower molding pressures allow for use of low cost, additive fabrication of polymeric tooling. Polymeric tooling is suitable for rapid part prototyping and limited production. Dry fiber preforming approaches evaluated included use of commercial chopped strand mat, robotic chopper gun deposition, and continuous fiber preform augmentation using tailored fiber placement (TFP). Use of chopped strand mat does not require a robotic deposition method, however a cutting table is generally required and there is typically 20-30% scrap generation. While various fiber areal weights are available, the preform is not readily optimized for minimal fiber use or weight savings. In contrast, a robotic chopper gun approach allows for localized deposition where fiber is required to meet structural requirements. The robotic method is highly automated and minimizes fiber scrap, however the capital cost of the equipment and engineering labor for programming can result in higher preform cost compared to chopped strand mat in certain cases depending on preform complexity. Dry fiber preforming using the robotic chopper gun method allows for creation of three dimensional forms. This approach may be ideal for molding in-house, or if the preforms stack together densely to allow for efficient shipping. Applications evaluated for this program considered trade-off between fabrication of a fully 3D preform versus production of a flat preform which is designed to readily drape into the final desired shape. Such a preform design greatly simplifies robotic programming and requires no specialized tooling. The flat preforms are easily stacked and shipped to the final molding location. Flat preforms are much easier to augment with TFP continuous fiber to provide local reinforcement. The demonstration and evaluation of these preforming and tooling methods were completed on three component applications. The first application was a battery box cover for an electric vehicle which was highly three dimensional. The second demonstrator article was comprised of complex contours and was used to demonstrate the use of TFP and RTM-light molding process. The third demonstration article was the roof of an operator’s cab for large construction equipment. The roof is relatively flat however it is comprised of complex changes in thickness which clearly demonstrate the advantage of robotic chopper gun approach as compared to using numerous preform layers of chopped strand mat. The cost trades for the various preforming methods are summarized to help guide the reader as to preforming method considerations. Finally, these demonstrations all used glass fiber roving. A fourth, exploratory task was added to evaluate the ability to make preforms using Zoltek’s carbon fiber split tow roving. We were able to adapt the chopper gun to make flat preforms for laminate testing, but further development effort would be required to make suitable preforms.

36 MATERIALS SCIENCE↗

Mechanical Characterization of High-Temperature Carbon Fiber-Polyphenylene Sulfide Composites for Large Area Extrusion Deposition Additive Manufacturing

Additive manufacturing (AM) is evolving from rapid prototyping to production of structural components. The widespread application of AM demands a high level of mechanical performance from these components, and it is therefore essential to improve feedstock material in order to meet these mechanical expectations. However, compared to traditional manufacturing techniques, the mechanical properties of AM materials and their resulting components are not well understood. In this study, we investigated the processability, microstructure, and mechanical performance of twin-screw compounded short carbon fiber reinforced polyphenylene sulfide (PPS) pellets as a feedstock material for big area AM (BAAM). The performance of the AM components was compared to that of traditional processing methods, namely injection molding (IM) and extrusion-compression molding (ECM). It was found that the AM composites exhibited 118% lower tensile strength and 55% lower tensile modulus when compared to traditional injection molding composite specimens; however, AM composites exhibited comparable properties to ECM composites. This response was attributed to highly aligned fibers in IM and AM samples. However, the AM composites contained porosity (15.5% volume), which reduced their mechanical properties in comparison to ECM composites. Finally, the IM process showed the maximum amount of fiber attrition with minimum porosity (0.007% volume), while the ECM process exhibited the least fiber attrition with 4.3% volume porosity.