Search NASA⌕ Search

SEARCH · Search NASA

Results for “Kovar”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

A parylene coating process for hybrid circuits

The parylene coating process developed during this program consists of (1) obtaining a hybrid cover with a hole in it, (2) sealing of the circuit with a hole in the cover, (3) parylene coating through the hole with the external leads protected from parylene by appropriate fixturing, and (4) sealing of the hole by soldering a pretinned kovar tab. Development of the above process required optimization of the parylene coater parameters to obtain a uniform consistent coating which could offer adequate protection to the circuits, fixture design for packages of various types, determination of the size of the deposition hole, and the amount of dimer charge per run, a process to hermetically seal the deposition holes and establishment of quality control techniques or acceptance criteria for the deposited film.

Source record↗

Device/packaging reliability problems of solid-state devices for space applications

This paper presents data that has been generated within NASA, especially the Marshall Space Flight Center, concerning several failure mechanisms that have occurred with microelectronic packages. The types of packages that will be discussed are primarily flat packs with 14-24 exit leads that are composed of Kovar electro-deposited nickel and finally gold plated.

Villella, F.↗

Investigation of package sealing using organic adhesives

A systematic study was performed to evaluate the suitability of adhesives for sealing hybrid packages. Selected adhesives were screened on the basis of their ability to seal gold-plated Kovar butterfly-type packages that retain their seal integrity after individual exposures to increasingly severe temperature-humidity environments. Tests were also run using thermal shock, temperature cycling, mechanical shock and temperature aging. The four best adhesives were determined and further tested in a 60 C/98% RH environment and continuously monitored in regard to moisture content. Results are given, however, none of the tested adhesives passed all the tests.

Perkins, K. L.↗

A hermetic sealing process for large irregularly shaped hybrid microcircuit enclosures

A system for sealing vacuum baked hybrids in a dry inert atmosphere using an overlapping spot resistance weld is described. A unique electrode configuration and fixturing that permits sealing of large and irregularly shaped gold plated Kovar packages to the hermeticity requirements of MIL-STD-883 was discussed. Metallurgical considerations and comparisons to laser sealing were made. Problems encountered during the development and optimization of the process were highlighted. Solutions to plating, fixturing, warpage, weld splatter and cracked bead problems are presented.

Stahler, M. R.↗

Development of low cost, high reliability sealing techniques for hybrid microcircuit packages. Phase 2, supplement 1: Moisture permeation of adhesive-sealed hybrid microcircuit packages

The susceptibility of adhesive-sealed ceramic packages to moisture permeation was investigated. The two adhesives, Ablebond 789-1 and Epo-Tek H77, were evaluated as package sealants. These adhesives were previously selected as the most promising candidates for this application from a group of ten adhesives. Ceramic packages sealed with these adhesives were exposed to temperature-humidity conditions of 25 C/98 percent RH, 50 C/60 percent RH, 50 C/98 percent RH, and 85 C/85 percent RH and their moisture contents using were monitored solid state moisture sensors sealed inside them. Five packages were tested at each of these exposures - two ceramic packages sealed with each of the two adhesives and one seam-sealed gold-plated Kovar package. This latter package was included to serve as a control. The results showed that the adhesive-sealed packages were not hermetic to moisture. The rates at which moisture entered the packages increased with the severity of the exposure environments (i.e., higher temperatures and higher moisture vapor pressures) with greater dependence on temperature than on moisture vapor pressure.

Perkins, K. L.↗

Investigation into the effect of plasma pretreatment on the adhesion of parylene to various substrates

A procedure is described for using argon and oxygen plasmas to promote adhesion of parylene coatings upon many difficult-to-bond substrates. Substrates investigated were gold, nickel, kovar, teflon (FEP), kapton, silicon, tantalum, titanium, and tungsten. Without plasma treatment, 180 deg peel tests yield a few g/cm (oz/in) strengths. With dc plasma treatment in the deposition chamber, followed by coating, peel strengths are increased by one to two orders of magnitude.

Riley, T.↗

Investigation into the effect of plasma pretreatment on the adhesion of parylene to various substrates

An experimental effort has been undertaken to examine the effect of plasma pretreatment of various substrate materials coated with a polymer in the parylene family. This report describes the procedure and discusses initial data which indicate using plasmas of argon and oxygen to promote adhesion of parylene coatings upon many difficult-to-bond substrates. Substrates investigated were gold, nickel, kovar, teflon (FEP), kapton, silicon, tantalum, titanium, and tungsten. Without plasma treatment, 180 deg peel tests yield a few g/cm (oz/in) strengths. With dc plasma treatment in the deposition chamber, followed by coating, peel strengths are increased by one to two orders of magnitude.

Riley, T.↗

Low-Cost Alternatives in Hybrid Microcircuit Packaging

Adhesive sealing, nickel plating, and multiwire boards evaluated. Based on study involving fully developed hardware, report considers adhesive packaging instead of seam welding, nickel-plated Kovar (commercial Fe/NI/Co alloy) packages instead of gold plates ones, and multiwire circuit boards instead of multilayer boards as alternatives for reducing cost of hardware without reducing reliability.

Caruso, S. V.↗

Method for forming hermetic seals

The firmly adherent film of bondable metal, such as silver, is applied to the surface of glass or other substrate by decomposing a layer of solution of a thermally decomposable metallo-organic deposition (MOD) compound such as silver neodecanoate in xylene. The MOD compound thermally decomposes into metal and gaseous by-products. Sealing is accomplished by depositing a layer of bonding metal, such as solder or a brazing alloy, on the metal film and then forming an assembly with another high melting point metal surface such as a layer of Kovar. When the assembly is heated above the temperature of the solder, the solder flows, wets the adjacent surfaces and forms a hermetic seal between the metal film and metal surface when the assembly cools.

Gallagher, Brian D.↗

Tool For Tinning Integrated-Circuit Leads

As many as eight flatpacks held. Tool made of fiberglass boards. Clamps row of flatpacks by their leads so leads on opposite side of packages dipped. After dipping, nuts on boards loosened, flatpacks turned around, nuts retightened, and untinned leads dipped. Strips of magnetic material grip leads of flatpacks (made of Kovar, magnetic iron/nickel/cobalt alloy) while boards repositioned. Micrometerlike screw used to adjust exposed width of magnetic strip to suit dimensions of flatpacks. Holds flatpack integrated circuits so leads tinned. Accommodates several flatpacks for simultaneous dipping of leads in molten solder. Adjusts to accept flatpacks in range of sizes.

Prosser, Gregory N.↗

Development of the RAIDS extreme ultraviolet wedge and strip detector

In the next few years the Remote Atmospheric and Ionospheric Detector System (RAIDS) package will be flown on a Tiros spacecraft. The EUV spectrometer experiment contains a position-sensitive detector based on wedge and strip anode technology. A detector design has been implemented in brazed alumina and kovar to provide a rugged bakeable housing and anode. A stack of three 80:1 microchannel plates is operated at 3500-4100 V. to achieve a gain of about 10 to the 7th. The top MCP is to be coated with MgF for increased quantum efficiency in the range of 50-115 nm. A summary of fabrication techniques and detector performance characteristics is presented.

Kayser, D. C.↗

Hydrogen Effects on GaAs, Status and Progress

It has been observed that GaAs devices in hermetically sealed packages when exposed to temperatures as low as 125oC can exhibit unacceptable degradation in both RF and DC characteristics. The source of the problem was found to be hydrogen that has been absorbed in the package's metals (Kovar, plating, etc.) and converted into atomic hydrogen within the Pt metallization of the gate structure. Subsequently, atomic hydrogen diffuses into the channel region of the FET structure and neutralizes the Si donors, resulting in a degradation of the device characteristics. Most of the data indicates the onslaught of the problem to occur after 500 hours at 125oC. This onslaught has been observed to be dependent on the thickness and processing conditions of the passivation layer, the sealing environment, and the amount of Pt or Pd in the gate structure of the device.

Hydrogen GaAs↗

Hydrogen Effects on GaAs Device Reliability

GaAs and InP devices in hermetically sealed packages have been observed to exhibit unacceptable degradation in both RF and DC characteristics. This degradation has been observed to occur at temperatures as low as 125oC. The source of the degradation has been linked to hydrogen gas that has been absorbed in the package's metals (Kovar, plating, etc.) and converted into atomic hydrogen within the Pt or Pd metallization of the gate structure. Subsequently, atomic hydrogen diffuses into the channel region of the FET structure and neutralizes the Si donors, resulting in a degradation of the device characteristics.

Gallium Arsenide↗

Development and Characterization of the Bonding and Integration Technologies Needed for Fabricating Silicon Carbide Based Injector Components

Advanced ceramic bonding and integration technologies play a critical role in the fabrication and application of silicon carbide based components for a number of aerospace and ground based applications. One such application is a lean direct injector for a turbine engine to achieve low NOx emissions. Ceramic to ceramic diffusion bonding and ceramic to metal brazing technologies are being developed for this injector application. For the diffusion bonding technology, titanium interlayers (coatings and foils) were used to aid in the joining of silicon carbide (SiC) substrates. The influence of such variables as surface finish, interlayer thickness, and processing time were investigated. Electron microprobe analysis was used to identify the reaction formed phases. In the diffusion bonds, an intermediate phase, Ti5Si3Cx, formed that is thermally incompatible in its thermal expansion and caused thermal stresses and cracking during the processing cool-down. Thinner interlayers of pure titanium and/or longer processing times resulted in an optimized microstructure. Tensile tests on the joined materials resulted in strengths of 13-28 MPa depending on the SiC substrate material. Nondestructive evaluation using ultrasonic immersion showed well formed bonds. For the joining technology of brazing Kovar fuel tubes to silicon carbide, preliminary development of the joining approach has begun. Various technical issues and requirements for the injector application are addressed.

Halbig,Michael C.↗

Bonding and Integration Technologies for Silicon Carbide Based Injector Components

Advanced ceramic bonding and integration technologies play a critical role in the fabrication and application of silicon carbide based components for a number of aerospace and ground based applications. One such application is a lean direct injector for a turbine engine to achieve low NOx emissions. Ceramic to ceramic diffusion bonding and ceramic to metal brazing technologies are being developed for this injector application. For the diffusion bonding, titanium interlayers (PVD and foils) were used to aid in the joining of silicon carbide (SiC) substrates. The influence of such variables as surface finish, interlayer thickness (10, 20, and 50 microns), processing time and temperature, and cooling rates were investigated. Microprobe analysis was used to identify the phases in the bonded region. For bonds that were not fully reacted an intermediate phase, Ti5Si3Cx, formed that is thermally incompatible in its thermal expansion and caused thermal stresses and cracking during the processing cool-down. Thinner titanium interlayers and/or longer processing times resulted in stable and compatible phases that did not contribute to microcracking and resulted in an optimized microstructure. Tensile tests on the joined materials resulted in strengths of 13-28 MPa depending on the SiC substrate material. Non-destructive evaluation using ultrasonic immersion showed well formed bonds. For the joining technology of brazing Kovar fuel tubes to silicon carbide, preliminary development of the joining approach has begun. Various technical issues and requirements for the injector application are addressed.

Halbig, Michael C.↗

Alignment and Integration of Lightweight Mirror Segments

The optics for the International X-Ray Observatory (IXO) require alignment and integration of about fourteen thousand thin mirror segments to achieve the mission goal of 3.0 square meters of effective area at 1.25 keV with an angular resolution of five arc-seconds. These mirror segments are 0.4 mm thick, and 200 to 400 mm in size, which makes it difficult not to impart distortion at the sub-arc-second level. This paper outlines the precise alignment, permanent bonding, and verification testing techniques developed at NASA's Goddard Space Flight Center (GSFC). Improvements in alignment include new hardware and automation software. Improvements in bonding include two module new simulators to bond mirrors into, a glass housing for proving single pair bonding, and a Kovar module for bonding multiple pairs of mirrors. Three separate bonding trials were x-ray tested producing results meeting the requirement of sub ten arc-second alignment. This paper will highlight these recent advances in alignment, testing, and bonding techniques and the exciting developments in thin x-ray optic technology development.

Evans, Tyler↗