Search NASA⌕ Search

SEARCH · Search NASA

Results for “LSCF”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Core-Shell Heterostructures as Functional Materials for Solid Oxide Fuel Cell (SOFC) Electrodes

The principal objective of this project was to synthesize core-shell heterostructures for solid oxide fuel cell cathodes using a molten salt solvent. In doing so, the main goals were split into a) to elucidate and understand the influence of molten salt chemistries to expeditiously synthesize perovskite type oxides for solid oxide fuel cells, b) provide a chemical framework for future molten salt syntheses of energy relevant ceramic materials, c) demonstrate and investigate the required parameters for the optimal core-shell synthesis and yield of La 0.6 Sr 0.4 Co 0.2 Fe 0.8 O 3 (LSCF) – La 0.8 Sr 0.2 MnO 3 (shell), and d) demonstrate improved cathode performance of core-shell LSCF-LSM compared to an LSCF cathode on symmetric cells. The results clearly show that a) the influence of the molten salt cation outweighs the anion in regards to product stoichiometry, b) molten salts should be tailored to balance cationic and anionic acidity for high product yield, c) high yield of core-shell nanoparticles can be achieved by optimal mass ratio between core to shell, dwell time in the salt, size ratio between core to shell, and mass ratio between overall powder to salt, and d) the core-shell LSCF-LSM cathodes have lower polarization resistances than LSCF at higher temperatures. More work is required to optimize core-shell cathode performance at lower temperatures. However, this work thus provided justification for using the molten salt synthesis for SOFC cathodes and provided insights into future material modifications for improved performance.

08 HYDROGEN↗

Computationally Guided Design of Multiple Impurities Tolerant Electrode (Final Report)

The current project was based on a combined experimental and computational approach, which can help recommend better cathode materials under multiple impurities conditions. The PI will mainly take in charge of experimental and computational thermodynamics of the selected cathode materials for the SOFC applications under multiple impurities. While the co-PI will run the electrochemical tests of the cathodes recommended and eventually the long-term degradation tests. At the end of the project, a multiple tolerant cathode material based on the combined experimental and computational approach will be recommended and the reliability of the commonly used accelerated testing will be evaluated. It will address multiple impurities poisoning effect of SO2, CO2, Cr and H2O on the LSM, LSCF and LNO cathodes by identifying the formation of the detrimental secondary phases by XRD, SEM and TEM techniques. And further recommended cathode material will be subjected to electrochemical testing and the most promising ones will be applied to long-term tests. The hybrid approach the PI proposed will not only be applied to the design of multiple impurities tolerant cathodes but will also be considered in the future oxygen electrode applications in SOECs or reversible SOCs. This hybrid computational and experimental approach includes four sections: 1) Investigation of single impurity poisoning on LSM, LSCF and LNO cathodes in the presence of SO2, CO2, Cr. In this section, LSM, LSCF cathodes from FuelCellMaterials and LNO cathodes from Sol-Gel synthesis will be heat-treated in the above single impurity. And the formation of the secondary phases as well as the corresponding simulations will be cross compared, which shows good agreement between each other. Meanwhile, the accelerated testing approach will be evaluated in these systems compared with the previous published work to understand the reliability of the approach. 2) Investigation of multiple impurities poisoning on LSM, LSCF and LNO cathodes in the presence of Cr+H2O, SO2+Cr and SO2+Cr+H2O conditions. We have also applied these 3 candidate cathodes under these multiple impurities’ conditions and the long-term degradation mechanism of the multiple impurities will be understood with the help of the combined experimental and computational approach. Meanwhile, the synergistic effect of those impurities will be compared with the individual ones in the same cathode system to further reveal the actual operating conditions. 3) Electrochemical testing and polarization of the recommended cathode. We have demonstrated very low polarization resistance in LSCF (core)-LSM (shell) electrodes using MSD process and analyzed impedance spectra using DRT analysis and confirming that the low polarization resistance in LSM infiltrated MSD cells is due to reduction in polarization resistance associated with O2-adsorption process. 4). Long-term degradation testing. We have developed a versatile MSD-based process to deposit various continuous coatings onto porous scaffolds and established baseline for longer term Cr-impurity testing in future projects.

36 MATERIALS SCIENCE↗

Sulfur Poisoning and Performance Recovery of SOFC Air Electrodes

The sulfur poisoning and performance recovery of the state-of-the-art SOFC cathodes (La 0 . 80 Sr 0 . 20 ) 0 . 95 MnO 3 ± δ (LSM) and (La 0 . 60 Sr 0 . 40 ) 0 . 95 Co 0 . 20 Fe 0 . 80 O 3 – δ (LSCF), have been studied. Electrochemical impedance spectroscopy measurements of LSCF|GDC and LSM|YSZ half-cells are carried out in alternating atmospheres of air and SO 2 –air at 700°C for hundreds of hours. In the presence of SO 2 , the electrochemical performance of both the cells decays with ohmic and non-ohmic losses, owing to the absorption and chemical interaction of SO 2 with the electrodes. In LSCF, the SrO segregated on the surface tends to absorb and react with SO 2 , forming SrSO 4 followed by the exsolution of Co-Fe. As for LSM, SO 2 is absorbed onto the Sr-rich areas of LSM, including the active reaction sites near the TPBs, leading to Sr exsolution and SrSO 4 formation, leaving a Sr-deficient LSM. During the subsequent exposure to air, the performance of the sulfur-contaminated LSM is almost restored. The LSM particles, exposed to alternating atmospheres of air and SO 2 -air during the electrochemical tests, show a relatively clean surface with sparsely distributed SrSO 4 particles, indicating a high stability against sulfur poisoning. It is suggested that the loosely adsorbed SO 2 at the TPBs is readily swept away by the SO 2 -free air flow, recovering its ORR activity, whereas the Sr-deficient LSM due to Sr-exsolution stays modified, contributing to the incomplete performance restoration. Unlike the case of LSM, the performance of the sulfur-poisoned LSCF partially recovers during the subsequent exposure to air. Correspondingly, the LSCF particles have a modified morphology covered with numerous nanoparticles, mostly SrSO 4 , showing the irreversible aspect of the sulfur poisoning. The morphology modification is not concentrated near the electrode/electrolyte interface but over the entire cathode, indicating that the degree of recovery from sulfur poisoning is closely related to the presence of SrO and chemical activity of Sr in the electrodes at the solid-gas interface. These results also show the potential application of LSM for a sulfur sensor available in high-temperature harsh conditions.

25 ENERGY STORAGE↗

Understanding (La,Sr)(Co,Fe)O$_{3-δ}$ Phase Instability within SOECs Using a Combined Experimental and Atomistic Modeling Approach

Understanding the onset of degradation in the air electrode within solid oxide electrolysis cells (SOECs), and the subsequent impact on cell performance, is a critical step in mitigating the performance losses and stability issues of SOECs. In an effort to identify early onset degradation phenomena, SOECs were characterized as fabricated and after testing potentiostatically at 1.3 V for 1000 h at 750 °C. SOEC air electrodes composed of a 1:1 composite of La 0.6 Sr 0.4 Co 0.2 Fe 0.8 O 3–δ (6428-LSCF) and Gd 0.1 Ce 0.9 O 1.95 (GDC) were studied using synchrotron X-ray diffraction (XRD), scanning transmission electron microscopy coupled with energy dispersive X-ray spectroscopy (STEM-EDS), and X-ray absorption near-edge spectroscopy (XANES) to evaluate the changes in the air electrode structurally and chemically. These techniques show the migration of Sr species from the air electrode through pores in the GDC barrier layer, progressing to the electrolyte boundary, where it accumulates and reacts with (Zr 0.84 Y 0.16 )O 2–δ (YSZ) to form SrZrO 3 . Microscopy results are paired with atomistic simulations to better understand the relationship between the thermodynamic instability of 6428-LSCF and cell fabrication/testing conditions. First-principles calculations reveal that LSCF-6428 is not stable during cell manufacturing and testing conditions, which supports the experimental identification of secondary phases in both as-fabricated and tested cells. Together, these results demonstrate that the challenging environments encountered by SOECs during cell manufacturing and operation lead to instabilities of the target 6428-LSCF anode material and underscore the need for more durable, high-performing SOEC components.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

An Efficient Bifunctional Air Electrode for Reversible Protonic Ceramic Electrochemical Cells

One of the main bottlenecks that limits the performance of reversible protonic ceramic electrochemical cells (R-PCECs) is the sluggish kinetics of the oxygen reduction and evolution reactions (ORR and OER). Here, the significantly enhanced ORR and OER kinetics and stability of a conventional La 0.6 Sr 0.4 Co 0.2 Fe 0.8 O 3-δ (LSCF) air electrode by an efficient catalyst coating of barium cobaltite (BCO) is reported. The polarization resistance of a BCO-coated LSCF air electrode at 600 oC is 0.16 Ω cm 2 , about 30% of that of the bare LSCF air electrode under the same conditions. Further, a R-PCEC with the BCO-coated LSCF air electrode shows exceptional performance in both fuel cell (maximum power density of 1.16 W cm -2 at 600 ºC) and electrolysis (current density of 1.80 A cm -2 at 600 ºC at 1.3 V) modes. Finally, the performance enhancement is attributed mainly to the facilitated rate of oxygen surface exchange.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Highly Active and Durable Air Electrodes for Reversible Protonic Ceramic Electrochemical Cells Enabled by an Efficient Bifunctional Catalyst

The commercialization of reversible protonic ceramic electrochemical cells is hindered by the lack of highly active and durable air electrodes exposed to high concentration of steam under operating conditions. We report findings that dramatically enhance the electrocatalytic activity and stability of a conventional (La 0.6 Sr 0.4 ) 0.95 Co 0.2 Fe 0.8 O 3-δ (LSCF) air electrode by a multiphase catalyst coating composed of a conformal Pr 1-x Ba x CoO 3-δ thin film and exsolved BaCoO 3-δ nanoparticles, are reported. At 600 °C, the catalyst coating decreases the polarization resistance of the LSCF air electrode by a factor of 25 (from 1.09 to 0.043 Ω cm 2 ) in air and the degradation rate by two orders of magnitude (from 1.0 × 10 -2 to 1.8 × 10 -4 Ω cm2 h -1 in humidified air with 30 vol% H2O). Further, a single cell with the catalyst-coated LSCF air electrode at 600 °C demonstrates a high peak power density of 1.04 W cm -2 in the fuel cell mode and a high current density of 1.82 A cm -2 at 1.3 V in the electrolysis mode. The significantly enhanced performance of the LSCF air electrode is attributed mainly to the high rate of surface oxygen exchange, fast surface proton diffusion, and the rapid H 2 O and O 2 dissociation on the catalysts.

36 MATERIALS SCIENCE↗

Modeling Electrokinetics of Oxygen Electrodes in Solid Oxide Electrolyzer Cells

A microscale model is presented in this study to simulate electrode kinetics of the oxygen electrode in a solid oxide electrolyzer cell (SOEC). Two mixed ionic/electronic conducting structures are examined for the oxygen producing electrode in this work: single layer porous lanthanum strontium cobalt ferrite (LSCF), and bilayer LSCF/SCT (strontium cobalt tantalum oxide) structures. A yttrium-stabilized zirconia (YSZ) electrolyte separates the hydrogen and oxygen electrodes, as well as a gadolinium doped-ceria (GDC) buffer layer on the oxygen electrode side. Electrochemical reactions occurring at the two-phase boundaries (2PBs) and three-phase boundaries (3PBs) of single-layer LSCF and bilayer LSCF/SCT oxygen electrodes are modeled under various SOEC voltages with lattice oxygen stoichiometry as the key output. The results reveal that there exists a competition in electrode kinetics between 2PBs and 3PBs, but 3PBs are the primary reactive sites for single-layer LSCF oxygen electrode under high voltages. These locations experience the greatest oxygen stoichiometry variations and are therefore the most likely locations for dimensional changes. By applying an active SCT layer over LSCF, the 2PBs become activated to compete with the 3PBs, thus alleviating oxygen stoichiometry variations and reducing the likelihood of dimensional change. This strategy could reduce lattice structural expansion, proving to be valuable for electrode-electrolyte delamination prevention and will be the focus of future work.

30 DIRECT ENERGY CONVERSION↗

A Facile, One-Step Synthesis for Core–Shell Perovskite Materials via Molten Salt

Core–shell La 0.6 Sr 0.4 Co 0.2 Fe 0.8 O 3 (LSCF)–La 0.8 Sr 0.2 MnO 3 (LSM) heterostructure crystalline materials have been synthesized in a simple, one-step feeding method via a KNO 3 molten salt solvent. Two-phase perovskite composites can be synthesized in times as short as 10 minutes and is demonstrated for the first time in a molten salt. Further, a combination of X-ray diffraction and S/TEM energy dispersive X-ray spectroscopy has been utilized to confirm the formation of an LSM shell on LSCF cores in all samples when adjusting dwell time, core size, weight ratio between core and shell precursors, and weight ratio of powder to salt. Specifically, decreasing the LSCF core size increases core–shell yield. Smaller cores introduce a greater density of facets on the crystal surface and provide more favorable sites for LSM heterogeneous nucleation.

36 MATERIALS SCIENCE↗

Degradation & Performance Studies of ALD-Stabilized Nano-Composite SOFC Cathodes

This work showed, definitively, for the first time, that zirconia Atomic Layer Deposited (ALD) overcoats improve the stability of Solid Oxide Fuel Cell (SOFC) cathodes by chemically gettering interfacial Sr that has segregated out of lanthanum strontium cobalt iron oxide (LSCF). The optimum ALD ZrO 2 overcoat thickness was found to be ≥5 nm and <10 nm. Gadolinium doped ceria (GDC) pre-infiltration was also shown, for the first time, to improve SOFC cathode stability through the chemical getting of Sr at the LSCF-backbone and LSCF-gas interfaces. Due to the fact that it can be performed easily in air on large-area electrodes, GDC pre-infiltration is likely more commercially viable than ALD ZrO 2 overcoating as an interfacial Sr gettering technique. Combining ZrO 2 overcoating with GDC pre-infiltration was not successful because the GDC nano-particles gettered the ZrO 2 overcoat instead of the interfacial Sr.

30 DIRECT ENERGY CONVERSION↗

Unconventional Highly Active and Stable Oxygen Reduction Catalysts Informed by Computational Design Strategies

Abstract Discovering and engineering new materials with fast oxygen surface exchange kinetics and robust long‐term stability is essential for the large‐scale, economically viable commercialization of solid oxide fuel cell (SOFC) technology. The perovskite catalyst material BaFe 0.125 Co 0.125 Zr 0.75 O 3 (BFCZ75), predicted to be promising from recent density functional theory (DFT) calculations and unconventional due to its extremely high Zr content and low electronic conductivity, exhibits oxygen reduction reaction surface exchange rates on par with Ba 0.5 Sr 0.5 Co 0.8 Fe 0.2 O 3 (BSCF) and excellent stability at typical operating temperatures. New composite electrodes are engineered by integrating BFCZ75 with commercial electrode materials La 1– x Sr x MnO 3 (LSM) and La 1– x Sr x Co y Fe 1– y O 3 (LSCF) and achieve high performance as measured by low area specific resistance (ASR) values, with the LSCF/BFCZ75 ASR values comparable to top performing noncomposite electrode materials such as SrCo 0.8 Sc 0.2 O 3– δ , BaNb 0.05 Fe 0.95 O 3– δ and BaCo 0.7 Fe 0.22 Y 0.08 O 3– δ . The use of BFCZ75 as a composite with LSCF achieving low ASR values shows that BFCZ75 is highly active and can easily integrate into existing SOFC material supply chains, lowering the barrier for potential commercial application of new electrode materials. Finally, these findings point to a broader unexplored class of perovskite materials with high fractions of redox inactive species (e.g., Zr, Nb, and Ta) that may unlock new pathways to realizing improved commercial SOFCs.

Jacobs, Ryan↗

Long term durability test and post mortem for metal-supported solid oxide electrolysis cells

Hydrogen is a renewable energy carrier, and electrolysis to split water is the most environmentally friendly method to produce hydrogen. This work reports long-term durability and degradation mode analysis for metal-supported solid oxide electrolysis cells (MS-SOECs). Catalyst screening showed that MS-SOECs with composite electrode catalysts (samarium-doped ceria-nickel [SDC-Ni] serving as a fuel electrode catalyst, and praseodymium oxide [PrO x ]-SDC or La 0.6 Sr 0.4 Co 0.2 Fe 0.8 O 3 [LSCF]-SDC serving as an air electrode catalyst) exhibit the highest electrochemical performance at 700 °C. The degradation rate of cells with LSCF-SDC as the air electrode catalyst was as low as 1.3%/100 h in long term durability tests at a current density of 0.33 A cm -2 , in contrast to rapid degradation observed for a cell with a PrO x -SDC air electrode. Furthermore, post-mortem analysis reveals the degradation is dependent on the primary modes of fuel electrode catalyst coarsening and Cr poisoning on the air electrode catalyst, as well as secondary modes of oxidation of the metal support and local elemental accumulation of Ni. Other degradation modes reported in conventional anode-supported SOECs, such as Ni migration, foreign element contamination, delamination of the cell, and nano-voids on the electrolyte, are not observed in the present MS-SOECs.

25 ENERGY STORAGE↗

Volatilized Molten Salts: An Alternative Avenue for Synthesizing Single-Phase Perovskites

Single phase La 0.8 Sr 0.2 MnO 3 (LSM) and core-shell La 0.6 Sr 0.4 Co 0.2 Fe 0.8 O 3 (LSCF)-LSM have been synthesized using a volatilized mol-ten salt synthesis (vMSS) method for the first time with a LiCl-KCl eutectic. While deleterious to LSM formation when the MSS takes place in the liquid phase, LiCl-KCl eutectic successfully facilitates LSM formation when volatilized. Specifically, KCl evaporates before LiCl and promotes formation of LSM via the gaseous phase. As time progresses, LiCl volatilizes and contributes negatively to Sr retention in the perovskite phase in accordance with Lux-Flood chemistry and to product phase purity. The vMSS is therefore a way to obviate the more immediate restrictions of Lux-Flood chemistry in the liquid phase. LiCl-KCl eutectic can also be used to successfully synthesis core-shell LSCF-LSM nanoparticles in times as short as 1 hour at 600 °C. These results demonstrate the surprising versatility and flexibility of the MSS method to synthesize numerous potential energy relevant materials with greater ease than previously thought.

36 MATERIALS SCIENCE↗

Boosting solid oxide fuel cell performance via electrolyte thickness reduction and cathode infiltration

Increasing the power density and reducing the operating temperature of solid oxide fuel cells (SOFCs) is important for improving commercial viability. Here we discuss two strategies for achieving such improvements in Ni–YSZ supported SOFCs – electrolyte thickness reduction and cathode infiltration. Microstructural and electrochemical results are presented showing the effect of reducing YSZ/GDC electrolyte thickness from 8 to 2.5 μm, and the effect of PrO x infiltration into the LSCF–GDC cathode. Both of these measures are effective, particularly at lower temperatures, leading to an increase in the maximum power density at 650 °C from 0.4 to 0.95 W cm –2 , for example. Electrochemical impedance spectroscopy utilizing subtractive analysis shows that PrO x enhances the cathode charge transfer process. Reducing the electrolyte thickness reduces not only the cell ohmic resistance but also the electrode polarization resistance. Furthermore, the latter effect appears to be an artifact associated with a slight increase in the steam partial pressure at the anode due to minor gas leakage across the thinner electrolyte.

25 ENERGY STORAGE↗

Effects of surface chemical potentials on cation segregation

Surface cation segregation on perovskite-type electrodes is one of the major issues limiting the durability of high-temperature solid-oxide electrochemical cells, and this process is strongly dependent on temperature, the external gas-environment, and impurities in air, such as CO 2 . Here cation segregation on La 0.6 Sr 0.4 Co 0.2 Fe 0.8 O 3-δ (LSCF) is systematically evaluated under a set of chemical potentials to determine the origin of surface segregation and the dominant factors that govern the segregation process. Temperature is the main driving force for surface strontium segregation as the thermodynamic stability of each phase varies, and the SrO particles appear primarily in a specific operating window. In addition to the required thermal energy, the presence of gaseous oxygen-containing molecules as reactants help drive the precipitation of SrO. Oxygen partial pressure (pO 2 ) controls the defect chemistry of LSCF, leading to promotion or suppression of surface segregation. The presence of CO 2 promotes the nucleation process and suppresses the surface migration step, significantly altering the surface morphology. We also show that A-site deficiency can limit the SrO segregation in certain conditions but shows no effect in others. This study reveals the impact of gas–solid interactions on surface segregation and highlights the subtle relationship between multiple segregation driving forces.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Crack Growth Rate at Oxygen Electrode/Electrolyte Interface in Solid Oxide Electrolysis Cells Predicted by Experiment Coupled Multiphysics Modeling

Solid oxide electrolysis cell (SOEC) is a very efficient hydrogen production technology, but the cell degradation is a serious limiting factor for its long-term implementation. Oxygen electrode (OE) delamination is reported to be the critical degradation mechanism. In this study, we present a methodology to understand the delamination failure of the OE due to chemical stress in a better perspective. Several OE configurations were tested: baseline strontium-doped lanthanum cobalt iron oxide (LSCF) single layer design and tantalum-doped strontium cobalt oxide (SCT) - LSCF bilayer designs with different SCT loadings. An electro-chemo-mechanical model is developed to associate the electrochemical behavior of the cell with solid mechanics for calculating crack growth of the cell during long term test. The bilayer configuration with SCT 20 wt% has better performance as it survived in the long-term life test with the least crack length. This study implies that an additional nano-coating of SCT over the OE have improved the species transport and oxygen evolution with reduced chemical stress. As the operating current density decreases, it takes longer time for the cell to reach the delamination with the same critical crack length of 6.5 μ m (∼93% of the electrode/electrolyte interface length). Finally, it was concluded that chemical stress plays a significant role in interface delamination failure, however it may not be the only source of stresses at the interface.

08 HYDROGEN↗

Development of Chromium and Sulfur Getter for Solid Oxide Fuel Cell (SOFC) System

Under the “real world” SOFC operating conditions, gaseous Cr and S species coexist in air stream. The combined Cr and S effect on the electrochemical poisoning of candidate LSM and LSCF electrodes has been investigated. Electrochemical and structural analysis revealed that the combined Cr and S interactions with the LSCF electrode remains significantly different from those of the individual Cr and S interactions. S reacts with the surface SrO accompanied by morphological changes whereas the hexavalent gaseous Cr species mainly deposit at the LSCF/GDC interface as is the case with Cr-only poisoning. For LSM electrode, the combined interactions of Cr and S remains similar to the sum of individual Cr and S effects as SO 2 reacts with Sr-rich regions of the bulk LSM, while Cr deposits at the electrochemically active sites. The use of getter, consisting of alkaline earth and transition metal oxides, has been proposed as a cost-effective approach to mitigate electrode poisoning. SrMnO 3 (SMO) is suggested as a robust getter material for the co-capture of airborne gaseous S and Cr species entering high-temperature electrochemical systems. The honeycomb getter forms, covered with SMO nanoparticles, were fabricated using dip coating. The SMO getter successfully maintained the electrochemical activity of LSM under the presence of gaseous Cr and S species, validating the efficacy of the getter. Post-test characterization revealed that the absorption of S and Cr contaminants led to the elongation of granular SMO particles, forming SrO nanorods and SrCrO 4 whiskers leaving Mn oxides underneath where inward-migrating Cr reside, indicating the high mutual affinity of Sr and Mn. The growth of reaction products during the long term exposure favors continued absorption of incoming S and Cr contaminants. The Mn 2 O 9 dimers, existing on the surface, are considered to help absorb S and Cr impurities, along with the Sr-terminated surface. The SMO getter also displays robust stability in humid environments at high temperatures without phase transformation or hydrolysis, fulfilling the requirement for operation in high-temperature electrochemical systems.

30 DIRECT ENERGY CONVERSION↗

Chromium Tolerant, Highly Active and Stable Electrocatalytic Internal Surface Coating for Cathode of Commercial SOFCs (Final Report)

This project is aimed to develop a chromium (Cr) tolerant, highly active, and stable coating layer on the internal surfaces of the porous composite cathode from commercially available SOFCs. Such coating layer was developed using the additive manufacturing process of Atomic Layer Deposition (ALD) and has been applied on the cathode consisting of either an electronic conductor of LaxSr 1-x MnyO 3-δ (LSM) or mixed ionic and electronic conducting La x Sr 1-x Co y Fe 1-y O 3-δ (LSCF). PI's work has demonstrated that the internal surface of cathode from the commercial cells, can be further tailored using ALD coating to dramatically enhance the cell performance. For instance, ALD layer consisting heterostructured nano composite of nano-Pt and nano-(Mn 0.8 Co 0.2 ) 3 O 4 oxide on the internal surface of porous LSM/YSZ cathode from SOFCs, has resulted in the large reduction of the cell polarizations resistance by up to 53%, and enormous increase of power density over 370%. For the cells with LSCF/Sm 2 O 3 doped CeO 2 (SDC) cathode, the conformal layer of nano-composite consisting of superjacent CoOx and subjacent minimum amount of Pt nano-grains has resulted in the power density enhancement by 126% for the large scale industry tubular cells at 750°C, and both the performance enhancement and nanostructure of the ALD layer are stable over ~ 2000 h continuous operation performed at industry test station. In the meanwhile, those ALD coating layer developed by PI's work is also inherently Cr-tolerant, and could act as physical barrier for preventing Cr diffusion into the cathode backbone, so as to mitigate the Cr poisoning effect on the cathode. In this project, the impact of Cr on the performance of those ALD coated commercial cells has been evaluated. Based on evolution of the cell performance, the ALD coating layer chemistry and ALD coating layer thickness has been optimized to maximize the overall Cr tolerance, cell power density and cell longevity. Different ALD coating has been applied onto the internal surface of LSM/YSZ and LSCF/SDC backbone respectively. The architecture/scaffold structures on the internal surface of different cathode, designed by this project, was catalogued and analyzed using High Resolution Transmission Electron Microscopy (HRTEM), and cell power/durability performance are assured via comprehensive electrochemical performance testing in the industry operation relevant conditions. The impact of the electrochemical operation current density, the water humidity, the cell operation temperature, and cell operation duration on the Cr tolerance of ALD coated cells has been systematically investigated. There is completely different nanostructure degradation mechanisms between LSM and LSCF cells induced by Cr contamination. For the LSCF/SDC baseline cell, With the Cr source, there is no apparent Sr surface segregation phase even for the baseline cell operated for 3000 h at 750 °C. With the Cr source, there is significant amorphous (SrCr)Ox phase accumulated in the original pore region. For the commercial baseline cells, Cr contaminants on the LSM electrode severely impacted the entire cell's electrochemical performance and nanostructure degradation. Those degradations include (1). Peak power density loss of 64 % after 109 h of operation. The dramatic increase in Rp (2). They are cracking at LSM/SSZ interface, LSM grains. SSZ remains intact but with (CrMn)Ox. By contrast, ALD coating (MnCo)Ox/Pt dramatically improves the Cr resistance, as follows (1). ALD-coated cell with a power density is 280-380 % of the baseline cell, depending on the ALD layer thickness. (2). For a cell with a 20 nm thick ALD layer, there is a large performance enhancement (> 200 % power density) induced by ALD coating of Cr-tolerant Mn 0.8 Co 0.2 Ox. (3). For a cell with a 20 nm thick ALD layer, after 168 h at 750 °C power density of the ALD-coated cell is ~ 600% of that baseline cell upon operation with Cr contamination for 109 h. The ALD coating on the internal surface of cathode developed by this project integrated multi-functions. Those multi-functions include (1). Dramatically improving the cell power density for the commercial cells; (2). Dramatically improving contamination resistance of the cathode, for being an excellent protection coating layer sealing off Cr contamination. (3). Dramatically increasing the cell longevity by potentially preventing the microstructure evolution and grain coarsening of the cathode. Overall, this project will provide a simple solution to simultaneously enhance power density and increase the reliability, robustness, and endurance of commercial SOFCs, over the entire operating temperature range of 650-800 °C. For the inherently functional SOFC, the ALD coating of LSM based cathode mitigate the Cr-contamination. Power density of ALD-coated cell is ~ 600% of that baseline cell upon operation with Cr contamination. In addition to SOFCs, the novel on-demand design approach and creation of multifunctional heterogeneous architecture on the electrode surface presented in this work opens further research for their application in other types of fuel cells, batteries, and sensors for which electrochemical reactions on the surface are similarly critical.

36 MATERIALS SCIENCE↗

Cation Migration and LSCF/SDC Decomposition Related to Long-Term Operation Mode as Revealed by Electron Microscopy

This study utilized energy dispersive spectroscopy (EDS) in a scanning electron microscope (SEM) and a scanning transmission electron microscope (STEM) in order to track cation migration and related particle decomposition for air electrode components of solid oxide cells. The influence of a Sm-doped ceria (SDC) barrier layers was assessed for three operation modes (fuel cell, electrolysis, reversible) over long time periods (1000-1500 hours). Composition profiles across air electrode/electrolyte interfaces indicated negligible accumulation of La/Sr cations to the yttria-stabilized zirconia (YSZ) electrolyte during operation. Instead, air electrode particles composed of SDC and/or La-Sr-Co-Fe-oxides (LSCF) exhibited decomposition by Sr evaporation and Sm migration to LSCF particle edges.

Picard, Yoosuf↗