Long-Term Effects of Humidity on Stainless Steel Pitting in Sea Salt Exposures

Ground 304 stainless steel (SS) samples were exposed to sea salt particles at 35 °C and two relative humidity (RH) levels for durations ranging from 1 week to 2 years. For all exposure times, pit number density and total pit volume at 40% RH were observed to be considerably greater than those at 76% RH. Statistical analysis of distributions of pit populations for both RH conditions showed that pit number density and total pit volume increased rapidly at first but slowed as exposure time increased. Cross-hatched features were observed in the 40% RH pits while ellipsoidal, faceted pits were observed at 76% RH. Optical profilometry indicated that most pits were not hemispherical. X-ray tomography provided evidence of undercutting and fissures. Piecewise curve fitting modeled the 40% RH data closely, predicting that corrosion damage would eventually plateau. However, a similar treatment of the 76% RH data suggested that corrosion damage would continuously increase, which implied that the piecewise power-law fit was limited in its ability to model atmospheric corrosion generally. Based on these observations, the operative mechanisms determining long-term corrosion behavior were hypothesized to be different depending on the RH of exposure.

36 MATERIALS SCIENCE↗

Phase Field Modeling of Crystallographic Corrosion Pits

The modeling of corrosion to understand and predict corrosion behavior is a topical issue. Here, a 3D phase field model is developed to simulate the pit morphology, primarily focusing on crystallographic pits. A crystallographic function is employed to incorporate different corrosion rates for different crystallographic planes. The model is benchmarked and validated against an analytical solution for a simple case. 3D crystallographic pits in a single crystal are simulated and the effect of substrate orientation on the pit morphology is studied. The crystallographic pit morphology changes significantly with the substrate orientation and these morphologies have a symmetry consistent with the substrate orientation. This first 3D phase field model of crystallographic pits will help in predicting the intricate shapes of pits, thereby, pushing the frontiers of pitting corrosion modeling.

36 MATERIALS SCIENCE↗

Influence of Realistic, Cyclic Atmospheric Cycles on the Pitting Corrosion of Austenitic Stainless Steels

Pitting corrosion was evaluated on stainless steels 304H, 304, and 316L the surfaces of which had ASTM seawater printed on them as a function of surface roughness after exposure to an exemplar realistic atmospheric diurnal cycle for up to one year. Methods to evaluate pitting damage included optical imaging, scanning electron microscopy imaging, profilometry analysis, and polarization scans. The developed cyclic exposure environment did not significantly influence pitting morphology nor depth in comparison to prior static exposure environments. Cross-hatching was observed in a majority of pits for all material compositions with the roughest surface finish (#4 finish) and in all surface finishes for the 304H composition. Evidence is provided that cross-hatched pit morphologies are caused by slip bands produced during the grinding process for the #4 finish or by material processing. Additionally, micro-cracking was observed in pits formed on samples with the #4 surface finish and was greatly reduced or absent for pits formed on samples with smooth surface finishes. This suggests that both a low RH leading to an MgCl 2 -dominated environment and a rough surface containing significant residual stress are necessary for micro-cracking. Finally, the use of various characterization techniques and cross sectioning was employed to both qualitatively and quantitatively assess pitting damage across all SS compositions and surface finishes.

36 MATERIALS SCIENCE↗

Quantitative assessment of environmental phenomena on maximum pit size predictions in marine environments

Maximum pit sizes were predicted for dilute and concentrated NaCl and MgCl 2 solutions as well as sea-salt brine solutions corresponding to 40% relative humidity (RH) (MgCl 2 -rich) and 76% RH (NaCl-rich) at 25 °C. A quantitative method was developed to capture the effects of various cathode evolution phenomena including precipitation and dehydration reactions. Additionally, the sensitivity of the model to input parameters was explored. Despite one's intuition, the highest chloride concentration (roughly 10.3 M Cl – ) did not produce the largest predicted pit size as the ohmic drop was more severe in concentrated MgCl 2 solutions. Therefore, the largest predicted pits were calculated for saturated NaCl (roughly 5 M Cl – ). Next, it was determined that pit size predictions are most sensitive to model input parameters for concentrated brines. However, when the effects of cathodic reactions on brine chemistry are considered, the sensitivity to input parameters is decreased. Although there was not one main input parameter that influenced pit size predictions, two main categories were identified. Under similar chloride concentrations (similar RH), the water layer thickness (WL), and pit stability product, (i · x) sf , are the most influential factors. When varying chloride concentrations (RH), changes in WL, the brine specific cathodic kinetics on the external surface (captured in the equivalent current density (i eq )), and conductivity (k o ) are the most influential parameters. Finally, it was noted that dehydration reactions coupled with precipitation in the cathode will have the largest effect on predicted pit size, and cause the most significant inhibition of corrosion damage.

54 ENVIRONMENTAL SCIENCES↗

Effect of varying threading dislocation densities on the optical properties of InGaN/GaN quantum wells with intentionally created V-shaped pits

The effect of varying threading dislocation densities on the internal quantum efficiencies (IQEs) of InGaN quantum wells (QWs), with and without intentionally created “V-pits,” is reported here. InGaN QW samples grown on GaN-on-sapphire templates with threading dislocation densities of <1 × 108 and <1 × 109 cm−2 are compared, with and without GaN/InGaN superlattice (SL) layers incorporated to intentionally open up the threading dislocation cores and form large-size “V-pits.” The formation of “V-pits” is confirmed by cross-sectional transmission electron microscopy to initiate from threading dislocations in the SL layers. The densities of the pits are confirmed by plan-view SEM to agree with the substrate threading dislocation densities. The experimental room temperature IQEs of the “V-pit” QW samples are enhanced to 15% ± 1% compared to 6% ± 2% for conventional QW samples. Both conventional and “V-pit” samples show insensitivity to the magnitude of the dislocation densities with respect to IQE performance, while the “V-pit” samples show shifts in the peak emission wavelengths compared to the conventional samples, attributed to strain modulation. This study provides additional understanding of the causes of the observed insensitivity of the IQEs to different threading dislocation densities.

Engineering↗

Research on Deformation Law of Deep Foundation Pit of Station in Core Region of Saturated Soft Loess Based on Monitoring

Saturated soft loess has a large pore structure, high compressibility, low strength, fluid plastic state, and poor engineering properties. It is still one of the key problems that engineering needs to solve. In order to study the influence of deep foundation pit excavation in the saturated soft loess area on the deformation of foundation pits, the deformation laws of ground settlement, enclosure structure, and supporting axial force were clarified based on the field tests on the deformation characteristics of deep foundation pits in areas with the high-water level in saturated soft loess, combined with geological conditions and on-site construction procedures. The results indicate the following: water supply and construction process were found to be the main factor in changing the surface settlement curve of deep foundation pits in saturated soft loess; increasing the construction speed of the pit bottom floor, inverted braces, floor frame beams, and sidewall frame beams to close the structure, which is conducive to restraining the deformation of the continuous underground wall and foundation pits in similar areas. In the initial stage of support layout, the axial force of steel support tends to increase too fast or even exceed the standard control value. Therefore, a reasonable preadding axial force is an effective means to control the deformation of the continuous underground wall and the axial force of the steel support. The current research results may provide a reference for constructing deep foundation pits in similar areas.

Wang, Xueyan↗

Pit Technologies at a Glance

The National Nuclear Security Administration has tasked Los Alamos National Laboratory (LANL) with important national security work: to develop a plutonium pit manufacturing capability and deliver a minimum of 30 plutonium pits per year in the years ahead. A pit is a hollow sphere of plutonium that, when uniformly compressed by explosives inside a warhead or bomb, causes a nuclear explosion. New pits are needed to maintain the nation’s nuclear stockpile and are a key component of nuclear deterrence and world peace. LANL’s Pit Technologies (PT) division manufactures these pits safely and securely. The work takes place in the Plutonium Facility (PF-4), the nation’s most modern plutonium science and manufacturing facility. LANL is currently the only place in the country with the capability to manufacture plutonium pits.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Refinement of Pitting Factor Basis to Evaluate Minimum Nitrite Requirement in Dilute Waste Chemistries

Considering that chloride concentrations are an order of magnitude lower at SRS than the maximum chloride previously tested to evaluate pitting susceptibility of carbon steel, it has been proposed that the Pitting Factor methodology be refined to determine if a reduction in the minimum nitrite requirement is warranted in more dilute solutions and those with chloride concentrations more indicative of waste tank chemistries at SRS. Through the use of cyclic potentiodynamic polarization, the susceptibility of A537 carbon steel to pitting corrosion was evaluated. The Pitting Factor was shown to accurately predict pitting susceptibility throughout the chemistry envelope evaluated. In addition, it was shown that nitrite is not required for inhibition of pitting corrosion in tank conditions with chloride concentrations observed at SRS and up to 4 M nitrate. Based upon these findings, new control limits were proposed that removed the minimum nitrite requirement within the chemistry envelope evaluated up to 50 °C.

36 MATERIALS SCIENCE↗

Repassivation underneath salt film on stainless steel pits

The repassivation temperature (Trp) of one-dimensional artificial pits made from 316L stainless steel was investigated in 3.5 wt.% NaCl by downward temperature scanning. For a given pit depth, T rp exhibited an unexpected “S” dependence on applied potential. Further analysis shows that this relationship is derived from repassivation underneath the salt film, which is different from repassivation that occurs when the concentration of metal cations at the pit surface decreases below a critical value. This indicates that there exists a reversal in the effect of the salt film on pit growth stability, which depends on temperature, applied potential, and pit depth.

36 MATERIALS SCIENCE↗

Pits 101: The four types of nuclear weapons modernization activities

We learned why we don’t need plutonium to make new pits in an earlier edition of Pits 101, but why do we need new pits from a national security standpoint? A plutonium pit, or the core of a nuclear weapon, is like a weapon’s battery. The pits that Los Alamos will make in coming years will be like new batteries for nuclear weapons in the existing stockpile. Pit production is mandated in order to meet Department of Defense (DOD) requirements by our primary customer, the National Nuclear Security Administration (NNSA), which is a semi-autonomous agency within the Department of Energy. NNSA’s mission is to “deliver safe, secure, reliable warheads for an effective nuclear deterrent.” As Marv Adams, head of NNSA Defense Programs, describes, it’s a mission that is simple to state, but challenging to deliver.

45 MILITARY TECHNOLOGY, WEAPONRY, AND NATIONAL DEF↗

Evaluation of Applied Stress on Atmospheric Corrosion and Pitting Characteristics in 304L Stainless Steel

For this study, the effects of applied stress, ranging from tensile to compressive, on the atmospheric pitting corrosion behavior of 304L stainless steel (SS304L) were analyzed through accelerated atmospheric laboratory exposures and microelectrochemical cell analysis. After exposing the lateral surface of a SS304L four-point bend specimen to artificial seawater at 50°C and 35% relative humidity for 50 d, pitting characteristics were determined using optical profilometry and scanning electron microscopy. The SS304L microstructure was analyzed using electron backscatter diffraction. Additionally, localized electrochemical measurements were performed on a similar, unexposed, SS304L four-point bend bar to determine the effects of applied stress on corrosion susceptibility. Under the applied loads and the environment tested, the observed pitting characteristics showed no correlation with the applied stress (from 250 MPa to -250 MPa). Pitting depth, surface area, roundness, and distribution were found to be independent of location on the sample or applied stress. The lack of correlation between pitting statistics and applied stress was more likely due to the aggressive exposure environment, with a sea salt loading of 4 g/m 2 chloride. The pitting characteristics observed were instead governed by the available cathode current and salt distribution, which are a function of sea salt loading, as well as pre-existing underlying microstructure. In microelectrochemical cell experiments performed in Cl - environments comparable to the atmospheric exposure and in environments containing orders of magnitude lower Cl - concentrations, effects of the applied stress on corrosion susceptibility were only apparent in open-circuit potential in low Cl - concentration solutions. Cl - concentration governed the current density and transpassive dissolution potential.

36 MATERIALS SCIENCE↗

Corrosion and repassivation of Super 13Cr stainless steel in artificial 1D pit electrodes at elevated temperature

Repassivation behavior of Super 13Cr martensitic stainless steel was investigated using a one-dimensional artificial pit electrode in deaerated NaCl solutions at 85 °C. Critical potentials for pit repassivation (E crit ) were measured by downward potential scans. E crit and the final current density (i f ) at the end of the scan can be correlated to the pit repassivation, showing that repassivation is more probable with smaller i f and higher E crit . Pit repassivation at a constant potential was correlated with if and average current density (i avg ). A combination of lower i f and i avg suggests a higher probability for pit repassivation.

36 MATERIALS SCIENCE↗

Efficient screening of rare large pit anomalies on polished surfaces using a minimalist sampling scheme

Lawrence Livermore National Laboratory (LLNL) has made significant strides in generating clean energy through its inertial confinement fusion (ICF) experiments. These experiments rely on high-density carbon (HDC) coated shells to encapsulate the fusion fuel. The success of these experiments is heavily dependent on the surface quality of these shells, as even minor imperfections, such as deep pits, can negatively impact fusion yield. Ensuring the required smoothness involves an extensive surface-finishing process that spans approximately 20 stages, making it both time-intensive and resource-demanding. A critical challenge in this process is the need for high-resolution scans to detect rare deep pits, which can be costly and impractical if performed on every shell. This highlights the necessity of developing more efficient scanning methods to optimize time and cost without compromising accuracy. To address these challenges, we introduce a novel approach that employs the multivariate Dvoretzky–Kiefer–Wolfowitz (DKW) inequality to provide a probabilistic upper bound on the error in estimating pit distribution characteristics via a Kernel Density Estimator (KDE). This error bound enables efficient and reliable estimation of pit distribution characteristics at a specified statistical confidence level using a minimal number of surface scans. The integrated DKW-KDE approach was validated through surface-finishing experiments across two batches of HDC-coated shells, demonstrating consistent and robust performance across multiple stages of the surface-finishing experiments. The validation studies suggest that the integrated DKW-KDE approach achieves comparable accuracy in estimating the risk of deleterious large pits with six scans, thus conserving time and resources. Further evaluations show that performance remains consistent across batches and over multiple polishing stages. In conclusion, based on these findings, one can leverage the minimal-scan insights to strategically improve the bottleneck inspection process, thus enhancing the productivity and quality of shell polishing and similar challenging manufacturing processes.

Inertial confinement fusion↗

Critical role of slags in pitting corrosion of additively manufactured stainless steel in simulated seawater

Abstract Pitting corrosion in seawater is one of the most difficult forms of corrosion to identify and control. A workhorse material for marine applications, 316L stainless steel (316L SS) is known to balance resistance to pitting with good mechanical properties. The advent of additive manufacturing (AM), particularly laser powder bed fusion (LPBF), has prompted numerous microstructural and mechanical investigations of LPBF 316L SS; however, the origins of pitting corrosion on as-built surfaces is unknown, despite their utmost importance for certification of LPBF 316L SS prior to fielding. Here, we show that Mn-rich silicate slags are responsible for pitting of the as-built LPBF material in sodium chloride due to their introduction of deleterious defects such as cracks or surface oxide heterogeneities. In addition, we explain how slags are formed in the liquid metal and deposited at the as-built surfaces using high-fidelity melt pool simulations. Our work uncovers how LPBF changes surface oxides due to rapid solidification and high-temperature oxidation, leading to fundamentally different pitting corrosion mechanisms.

36 MATERIALS SCIENCE↗

Pit growth kinetics in aluminum: effects of salt loading and relative humidity

Abstract The growth kinetics of localized corrosion, e.g. pits, in corrosive environments often controls the service life of metallic components. Yet, our understanding of these kinetics is largely based on coupon-level, e.g. mass-loss, studies which provide limited insights into the evolution of individual damage events. It is critical to relate observed cumulative loss trends, such as links between changing humidity and mass loss rates, to the growth kinetics of individual pits. Towards this goal, we leverage in-situ X-ray computed tomography to measure the growth rates of over sixty pits in aluminum in four different humid, chloride environments over ≈3 days of exposure. Pit growth rates and final volumes increased with increasing droplet volume, which was observed to increase with increasing humidity and salt loading. Two factors, droplet spreading and oxide jacking, dramatically increased pit growth rates and final volumes.

Noell, Philip J. (ORCID:0000000346998999)↗

Mitigation of Pitting on Nitrogen-Doped Niobium Surfaces through Two-Step Electropolishing

Surface processing of niobium superconducting RF cavities used in particle accelerators is crucial for determining their performance. The nitrogen (N)-doping method, developed at Fermilab, enhances the cavities’ quality factor by doping the cavity’s interior surface with N atoms at 800 °C. After N-doping, electropolishing (EP) is employed to remove the niobium nitride phases and attain the desired concentration of interstitial N atoms. This study explores the effects of EP conditions on N-doped niobium samples. The samples were electropolished at 5 to 40 °C and voltages between 3 and 22 V. Different EP voltage ranges produced two types of pits, classified based on their sizes. Larger pits, linked to higher voltages, are also affected by the reaction rate. Pitting could be reduced at a lower temperature and adequate EP voltage. However, to effectively minimize gas evolution forming large-sized pitting, peeling off the top nitride layer before EP might be beneficial. This was achieved through precise low-voltage etching, forming a two-step EP process. The process involves removing the top 100–200 nm layer at a low voltage, followed by standard EP to remove the required material. This two-step EP process effectively mitigated the pitting risk associated with gas evolution on N-doped surfaces.

43 PARTICLE ACCELERATORS↗

Pit depth analysis using automated software for three containers with complete imaging

The 3013 surveillance program is tasked with ensuring the long term safety of plutonium storage in 3013-compliant containers. One component of this task is to understand corrosion features found on the interior sidewall of the inner container closure weld region (ICCWR). To this end, three containers were selected to have laser confocal microscope (LCM) 20X imaging of the entire ICCWR. This report describes the analysis of the LCM pit depth data using the automated corrosion analysis software. The analysis included determining maximum pit depths and distributions of pit depths, volumes, and diameters for all pit features identified on the three containers. Results provided insight into possible corrosion mechanisms and were consistent with previous pit growth model predictions.

36 MATERIALS SCIENCE↗

Automated Image Segmentation and Processing Pipeline Applied to X–Ray Computed Tomography Studies of Pitting Corrosion in Aluminum Wires

Understanding pitting corrosion is critical, yet its kinetics and morphology remain challenging to study from X-ray computed tomography (XCT) due to manual segmentation barriers. To address this, an automated pipeline leveraging deep learning for efficient large-scale XCT analysis is developed, revealing new corrosion insights. The pipeline enables pit segmentation, 3D reconstruction, statistical characterization, and a topological transformation for visualization. Here, the pipeline is applied to 87 648 XCT images capturing commercial purity aluminum (1100 Al) wire exposed to sodium chloride (NaCl) salt particles over a period of 122 h. The pipeline achieves complete feature extraction and statistical quantification across the entire XCT dataset, leveraging distributed computing environment for high efficiency. Global growth kinetics such as high-level stepwise sigmoidal volume loss patterns and granular individual pit developments are both captured for 36 detected pits. By combining automation, computer vision, and extensive XCT datasets, this research accelerates precise corrosion assessment to enable materials science discoveries at scale.

36 MATERIALS SCIENCE↗