At least 37 records · Page 2

High spatial resolution thermal conductivity mapping of SiC/SiC composites

Herein, silicon carbide (SiC) ceramic matrix composites are being investigated as a new generation of fuel cladding materials due to its higher accident tolerance compared to Zircaloy. Characterization of the thermal conductivity of SiC constituents and their interfaces and interphases in SiC/SiC composites is needed as inputs to models of cladding performance. We used time-domain thermoreflectance (TDTR) to map the thermal conductivity with a spatial resolution of 2 µm. The SiC/SiC composite is comprised of Hi-Nicalon Type S fibers in a matrix made by chemical vapor infiltration (CVI matrix). The interphase material is a pyrolytic carbon/SiC multilayer. We report thermal conductivity maps of the SiC fiber and SiC matrix at temperatures of 25 °C, 90 °C, 164 °C, and 250 °C. The fiber has a uniform and isotropic thermal conductivity of 22 W m -1 K -1 at 25 °C; the thermal conductivity of fiber is approximately independent of temperature. The matrix thermal conductivity is not uniform and varies from 50 to 120 W m -1 K -1 at 25 °C; the thermal conductivity of the matrix scales approximately with the inverse of the square root of temperature, i.e., ∝ 1/T 1/2 . The thermal conductivity of the interphase at room temperature is 6 W m -1 K -1 . The calculated spatially averaged thermal conductivity of this SiC/SiC composite at 1000°C is 29 W m -1 K -1 .

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Qualitative and quantitative analysis of neutron irradiation effects in SiC/SiC composites using X-ray computed tomography

Silicon carbide fiber-reinforced silicon carbide matrix (SiC/SiC) composites are candidate materials for cladding of light water reactor (LWR) fuels. Loss of fission product gas retention due to the formation of microcrack networks is considered a potential failure mechanism for SiC/SiC-cladded fuels. In this work, a variety of SiC/SiC composite tubes were irradiated with and without an LWR-relevant radial heat flux in the High Flux Isotope Reactor, followed by detailed characterization with X-ray computed tomography (XCT). This first set of XCT data for neutron-irradiated samples confirmed that the internal stresses arising from a combination of temperature gradients and irradiation-induced swelling act as the primary driver for cracking. Consequently, while the observed cracking patterns varied depending on the tube architectures, the sharp edges of relatively large pores were found to be the common stress concentrator. These findings are useful to help improve the design and manufacturing of SiC/SiC fuel claddings for reduced failure probability.

42 ENGINEERING↗

Experimental investigation of probabilistic failure of SiC/SiC composite tubes under multiaxial loading

This paper presents an experimental investigation of the failure behavior of SiC fiber-reinforced SiC matrix (SiC/SiC) composite tubes under multiaxial loading. A new testing apparatus is designed to independently apply axial stress and internal pressure to SiC/SiC tubes. Acoustic emission (AE) is used to monitor the damage growth in the specimen. Based on the measured stress–strain response, a strain-based criterion is proposed to determine the proportional limit stress (PLS). The proposed strain-based criterion is compared with the PLS determined by the AE measurement. The PLS is determined for different loading ratios to form a multiaxial failure surface. By testing multiple replicates, the statistical variations of the PLS are determined. In conclusion, based on the experimental results, a mathematical model is developed to characterize the probability distribution of the PLS of SiC/SiC composites under multiaxial loading.

36 MATERIALS SCIENCE↗

Effects of high-dose neutron irradiation at light-water reactor relevant temperature on the mechanical properties of SiC/SiC composites

For this study, the neutron dose-dependent evolutions and the underlying mechanisms of properties of SiC fiber-reinforced SiC matrix (SiC/SiC) composites at a temperature relevant to light-water reactors (∼600 K) were investigated and analyzed. Chemical vapor infiltrated (CVI) SiC/SiC composites reinforced with Hi-Nicalon Type S or Tyranno SA3 fiber were neutron-irradiated to doses up to 30 dpa. The irradiated composites retained their flexural strengths. The thermal diffusivity and dimensional changes were mostly retained from 2.0 to 30.2 dpa. Discrepancies in irradiation responses among CVI SiC/SiC composites from different sources were found. Additional microstructural analysis using Raman spectroscopy and numerical analysis on irradiation effect on residual stress were used to explain how the microstructural variables, especially of carbon interphases, affect the mechanical properties in the 30–40 dpa dose range.

Continuous fiber-reinforced ceramic matrix composi↗

Irradiation Vehicles for Evaluating SiC/SiC Cladding Bowing Under Neutron Flux Gradients

Silicon carbide fiber–reinforced silicon carbide matrix (SiC/SiC) composites are among the most promising candidates for long term accident-tolerant nuclear fuel cladding. A key challenge related to their deployment is lateral bowing caused by differential radiation-induced swelling under dose or temperature gradients, which could obstruct coolant flow or interfere with control rod/blade movements. Although previous modeling efforts have predicted bowing behavior in light-water reactor (LWR) environments, experimental validation remains limited, especially at prototypic LWR temperatures. This study addresses that gap by irradiating six reduced-length SiC/SiC cladding tubes (~600 mm) in the High Flux Isotope Reactor (HFIR) at ~300°C, which is representative of LWR conditions. The tubes will be housed in a sealed vessel with an inert gas gap to maintain target temperatures and prevent direct coolant contact. Arranged in three pairs, each set will receive a different radiation dose (low, medium, high), with the central pair receiving ~0.1 displacements per atom (dpa)—the expected dose for peak bowing. The experiment will determine the dose-dependent bowing behavior and validate predictive finite element models. In this work, the tubes are freely suspended from pins to allow for unconstrained bowing; however, we present a concept for introducing localized constraints to represent grid spacer effects. Post-irradiation examination will include swelling measurements and profilometry to assess bowing and compare the results with model predictions. This work aims to confirm the conditions under which maximum bowing occurs so as to improve the reliability of SiC/SiC performance models in nuclear applications.

Russell, Nick [ORNL] (ORCID:0000000296099820)↗

Durability Evaluation of a Thin Film Sensor System With Enhanced Lead Wire Attachments on SiC/SiC Ceramic Matrix Composites

An advanced thin film sensor system instrumented on silicon carbide (SiC) fiber reinforced SiC matrix ceramic matrix composites (SiC/SiC CMCs), was evaluated in a Mach 0.3 burner rig in order to determine its durability to monitor material/component surface temperature in harsh environments. The sensor system included thermocouples in a thin film form (5 microns thick), fine lead wires (75 microns diameter), and the bonds between these wires and the thin films. Other critical components of the overall system were the heavy, swaged lead wire cable (500 microns diameter) that contained the fine lead wires and was connected to the temperature readout, and ceramic attachments which were bonded onto the CMCs for the purpose of securing the lead wire cables, The newly developed ceramic attachment features a combination of hoops made of monolithic SiC or SiC/SiC CMC (which are joined to the test article) and high temperature ceramic cement. Two instrumented CMC panels were tested in a burner rig for a total of 40 cycles to 1150 C (2100 F). A cycle consisted of rapid heating to 1150 C (2100 F), a 5 minute hold at 1150 C (2100 F), and then cooling down to room temperature in 2 minutes. The thin film sensor systems provided repeatable temperature measurements for a maximum of 25 thermal cycles. Two of the monolithic SiC hoops debonded during the sensor fabrication process and two of the SiC/SiC CMC hoops failed during testing. The hoops filled with ceramic cement, however, showed no sign of detachment after 40 thermal cycle test. The primary failure mechanism of this sensor system was the loss of the fine lead wire-to-thin film connection, which either due to detachment of the fine lead wires from the thin film thermocouples or breakage of the fine wire.

Lei, Jih-Fen↗

Progress in SiC/SiC Ceramic Composite Development for Gas Turbine Hot-Section Components under NASA EPM and UEET Programs

The successful application of ceramic matrix composites as hot-section components in advanced gas turbine engines will require the development of constituent materials and processes that can provide the material systems with the key thermostructural properties required for long-term component service. Much initial progress in identifying these materials and processes was made under the former NASA Enabling Propulsion Materials Program using stoichiometric Sylramic (trademark) silicon-carbide (SiC) fibers, 2D (two dimensional)-woven fiber architectures, chemically vapor-infiltrated (CVI) BN fiber coatings (interphases), and SiC-based matrices containing CVI SiC interphase over-coatings, slurry-infiltrated SiC particulate, and melt-infiltrated (MI) silicon. The objective of this paper is to discuss the property benefits of this SiC/SiC composite system for high-temperature engine components and to elaborate on further progress in SiC/SiC development made under the new NASA Ultra Efficient Engine Technology Program. This progress stems from the recent development of advanced constituent materials and manufacturing processes, including specific treatments at NASA that improve the creep, rupture, and environmental resistance of the Sylramic fiber as well as the thermal conductivity and creep resistance of the CVI SiC over-coatings. Also discussed are recent observations concerning the detrimental effects of inadvertent carbon in the fiber-BN interfacial region and the beneficial effects of certain 2D-architectures for thin-walled SiC/SiC panels.

DiCarlo, J. A.↗

Advanced Environmental Barrier Coatings Developed for SiC/SiC Composite Vanes

Ceramic components exhibit superior high-temperature strength and durability over conventional component materials in use today, signifying the potential to revolutionize gas turbine engine component technology. Silicon-carbide fiber-reinforced silicon carbide ceramic matrix composites (SiC/SiC CMCs) are prime candidates for the ceramic hotsection components of next-generation gas turbine engines. A key barrier to the realization of SiC/SiC CMC hot-section components is the environmental degradation of SiC/SiC CMCs in combustion environments. This is in the form of surface recession due to the volatilization of silica scale by water vapor. An external environmental barrier coating (EBC) is a logical approach to achieve protection and long-term durability.

Lee, Kang N.↗

Advanced Woven SiC/SiC Composites for High Temperature Applications

The temperature, stress, and environmental conditions of many gas turbine, hypersonic, and even nuclear applications make the use of woven SiC/SiC composites an attractive enabling material system. The development in SiC/SiC composites over the past few years has resulted in significant advances in high temperature performance so that now these materials are being pursued for several turbine airfoil and reusable hypersonic applications. The keys to maximizing stress capability and maximizing temperature capability will be outlined for SiC/SiC. These include the type of SiC fiber, the fiber-architecture, and the matrix processing approach which leads to a variety of matrix compositions and structure. It will also be shown that a range of mechanical, thermal, and permeability properties can be attained and tailored depending on the needs of an application. Finally, some of the remaining challenges will be discussed in order for the use of these composite systems to be fully realized.

Morscher, Gregory N.↗

Creep Behavior of Hafnia and Ytterbium Silicate Environmental Barrier Coating Systems on SiC/SiC Ceramic Matrix Composites

Environmental barrier coatings will play a crucial role in future advanced gas turbine engines because of their ability to significantly extend the temperature capability and stability of SiC/SiC ceramic matrix composite (CMC) engine components, thus improving the engine performance. In order to develop high performance, robust coating systems for engine components, appropriate test approaches simulating operating temperature gradient and stress environments for evaluating the critical coating properties must be established. In this paper, thermal gradient mechanical testing approaches for evaluating creep and fatigue behavior of environmental barrier coated SiC/SiC CMC systems will be described. The creep and fatigue behavior of Hafnia and ytterbium silicate environmental barrier coatings on SiC/SiC CMC systems will be reported in simulated environmental exposure conditions. The coating failure mechanisms will also be discussed under the heat flux and stress conditions.

Zhu, Dongming↗

Advanced Environmental Barrier Coating Development for SiC/SiC Ceramic Matrix Composites: NASA's Perspectives

This presentation reviews NASA environmental barrier coating (EBC) system development programs and the coating materials evolutions for protecting the SiC/SiC Ceramic Matrix Composites in order to meet the next generation engine performance requirements. The presentation focuses on several generations of NASA EBC systems, EBC-CMC component system technologies for SiC/SiC ceramic matrix composite combustors and turbine airfoils, highlighting the temperature capability and durability improvements in simulated engine high heat flux, high pressure, high velocity, and with mechanical creep and fatigue loading conditions. The current EBC development emphasis is placed on advanced NASA 2700F candidate environmental barrier coating systems for SiC/SiC CMCs, their performance benefits and design limitations in long-term operation and combustion environments. Major technical barriers in developing environmental barrier coating systems, the coating integrations with next generation CMCs having the improved environmental stability, erosion-impact resistance, and long-term fatigue-environment system durability performance are described. The research and development opportunities for advanced turbine airfoil environmental barrier coating systems by utilizing improved compositions, state-of-the-art processing methods, and simulated environment testing and durability modeling are discussed.

Ceramic Matrix Composites↗

InSitu SEM Investigation of Microstructural Damage Evolution and Strain Relaxation in a Melt Infiltrated SiC/SiC Composite

With CMC components poised to complete flight certification in turbine engines on commercial aircraft within the near future, there are many efforts within the aerospace community to model the mechanical and environmental degradation of CMCs. Direct observations of damage evolution are needed to support these modeling efforts and provide quantitative measures of damage parameters used in the various models. This study was performed to characterize the damage evolution during tensile loading of a melt infiltrated (MI) silicon carbide reinforced silicon carbide (SiC/SiC) composite. A SiC/SiC tensile coupon was loaded to a maximum global stress of 30 ksi in a tensile fixture within an SEM while observations were made at 5 ksi increments. Both traditional image analysis and DIC (digital image correlation) were used to quantify damage evolution. With the DIC analysis, microscale damage was observed at the fiber-matrix interfaces at stresses as low as 5 ksi. First matrix cracking took place between 20 and 25 ksi, accompanied by an observable relaxation in strain near matrix cracks. Matrix crack opening measurements at the maximum load ranged from 200 nm to 1.5 m. Crack opening along the fiber-matrix interface was also characterized as a function of load and angular position relative to the loading axis. This characterization was funded by NASA GRC and was performed to support NASA GRC modeling of SiC/SiC environmental degradation

testing↗

Development and Property Evaluation of Selected HfO2-Silicon and Rare Earth-Silicon Based Bond Coats and Environmental Barrier Coating Systems for SiC/SiC Ceramic Matrix Composites

Ceramic environmental barrier coatings (EBC) and SiC/SiC ceramic matrix composites (CMCs) will play a crucial role in future aircraft propulsion systems because of their ability to significantly increase engine operating temperatures, improve component durability, reduce engine weight and cooling requirements. Advanced EBC systems for SiC/SiC CMC turbine and combustor hot section components are currently being developed to meet future turbine engine emission and performance goals. One of the significant material development challenges for the high temperature CMC components is to develop prime-reliant, high strength and high temperature capable environmental barrier coating bond coat systems, since the current silicon bond coat cannot meet the advanced EBC-CMC temperature and stability requirements. In this paper, advanced NASA HfO2-Si and rare earth Si based EBC bond coat EBC systems for SiC/SiC CMC combustor and turbine airfoil applications are investigated. High temperature properties of the advanced EBC systems, including the strength, fracture toughness, creep and oxidation resistance have been studied and summarized. The advanced NASA EBC systems showed some promise to achieve 1500C temperature capability, helping enable next generation turbine engines with significantly improved engine component temperature capability and durability.

Oxidation and cyclic durability↗

Combined Thermomechanical and Environmental Durability of Environmental Barrier Coating Systems on SiC/SiC Ceramic Matrix Composites

Environmental barrier coatings (EBCs) and SiC/SiC ceramic matrix composites (CMCs) will play a crucial role in next generation turbine engines for hot-section component applications. The development of prime-reliant environmental barrier coatings is essential to the EBC-CMC system durability, ensuring the successful implementations of the high temperature and lightweight engine component technologies for engine applications.This paper will emphasize recent NASA environmental barrier coating and CMC developments for SiC/SiC turbine airfoil components, utilizing advanced coating compositions and processing methods. The emphasis has been particularly placed on thermomechanical and environment durability evaluations of EBC-CMC systems. We have also addressed the integration of the EBCs with advanced SiC/SiC CMCs, and studied the effects of combustion environments and Calcium-Magnesium-Alumino-Silicate (CMAS) deposits on the durability of the EBC-CMC systems under thermal gradient and mechanical loading conditions. Advanced environmental barrier coating systems, including multicomponent rare earth silicate EBCs and HfO2-Si based bond coats, will be discussed for the performance improvements to achieve better temperature capability and CMAS resistance for future engine operating conditions.

Ceramic Matrix Composites↗

Modeling of Time-Dependent Strength Degradation of SiC/SiC Ceramic Matrix Composites via MAC/GMC Computer Code

Silicon carbide fiber reinforced silicon carbide (SiC/SiC) ceramic matrix composites (CMCs) display time-dependent strength degradation at intermediate temperatures (600 to 900 degrees Centigrade). This is generally believed to be an oxidation induced phenomenon. The understanding of the effect of temperature with environment (oxidation) is key towards development of SiC/SiC CMCs with a reliable load carrying capacity. Various theories have been proposed to explain the strength degradation. One suggests that the boron nitride (BN) coating deposited on the fibers oxidizes causing fusion of fibers. Another theory proposes that the SiC fibers are oxidized forming a silica scale leading to premature fiber failure. A more recent theory suggests that SiC fiber strength is intrinsically time-dependent due to slow crack growth of flaws in the fibers. An empirical model, termed as a "fiber classic model," which is based on a standard slow crack growth type power-law, has been implemented within NASA's micromechanics-based MAC/GMC computer code as a user routine. Model parameters for this "classic model" were calibrated from stress-rupture data of Hi-Nicalon (TM) monofilaments using the maximum likelihood estimation (MLE) technique. This new capability in the MAC/GMC computer code was then used to predict the stress-rupture behavior of Hi-Nicalon (TM) tows as well as 2-D SiC/SiC composites reinforced with Hi-Nicalon (TM) fibers. Results demonstrate that the MAC/GMC with this new capability successfully predicts the time-to-failure vs. applied stress within the intermediate temperature range at various scales as well as laminated composites in an oxidizing environment.

Environmental degradation↗

In-Plane Tensile Properties, Creep Behavior and Failure Mechanisms of CVI and PIP SiC/SiC Composites at Temperatures to 1,650⁰C in Air

The in-plane tensile and creep properties of 2D woven CVI and PIP SiC/SiC composites with SylramicTM-iBN SiC fibers were measured at temperatures to 16500C in air and the data compared with the literature. Batch-to-batch variations in the tensile and creep properties, influence of thermal treatment on creep, creep parameters, damage mechanisms and failure modes for these composites were studied. Under the tested conditions, the CVI SiC/SiC composites exhibited both matrix and fiber dominated creep depending on stress, whereas the PIP SiC/SiC composites displayed only fiber dominated creep. Creep durability in both composite systems is controlled by the most creep resistant phase as well as oxidation of the fibers via cracked matrix. The Larson-Miller parameter and Monkman-Grant relationship were used wherever applicable for analyzing and predicting creep durability.

SiC-SiC Composites, CVI, PIP, Creep, In-plane tens↗

Anisotropic thermal diffusivity and conductivity in SiC/SiC tubes studied by infrared imaging and X-ray computed tomography

Traditional flash diffusivity evaluation of thermal diffusivity/conductivity of composite tubes require machining of specimens. For a thin-wall tube, this method can only be used to obtain through-thickness transport property. A novel method to evaluate anisotropic thermal diffusivity in a composite tube has been developed. Braided SiC/SiC composite tubes were subjected to a xenon flash heating pulse. A high-speed, high-sensitivity infrared camera was used to measure surface temperature changes as a function of time and nondestructively detect subsurface defects/damages, such as macroscopic pores. Standard reference material (Pyroceram 9606) and curved SiC/SiC composite tube specimens were used to validate thermal diffusivity obtained from infrared imaging. Unlike the traditional method, there is no need prepare special specimens, and thermal diffusivity values in three orientations are obtained after a single flash. A finite element analysis model based on x-ray computed tomography scans was developed to simulate the heat transfer. In conclusion, this technique is significant in assessing thermal conductivity and inspecting the health of ceramic tubes during and after service.

36 MATERIALS SCIENCE↗

Evaluation of CVI SiC/SiC Composites for High Temperature Applications

Silicon carbide fiber reinforced silicon carbide (SiC/SiC) composites are candidate materials for various high temperature turbine engine applications because of their high specific strength and good creep resistance at temperatures of 1400 C (2552 F) and higher. Chemical vapor infiltration (CVI) SiC/SiC ceramic matrix composites (CMC) incorporating Sylramic-iBN SiC fiber were evaluated via fast fracture tensile tests (acoustic emission damage characterization to assess cracking behavior), tensile creep testing, and microscopy. The results of this testing and observed material behavior degradation mechanisms are reviewed.

testing↗