Search NASA⌕ Search

SEARCH · Search NASA

Results for “anode free batteries”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 37 records · Page 2

Fast and Simple Ag/Cu Ion Exchange on Cu Foil for Anode-Free Lithium-Metal Batteries

Lithium-metal batteries with zero excess lithium on the anode side paired with a fully lithiated cathode are regarded as a form of the highest energy-density configuration. Unfortunately, the continuous lithium loss over cycling from a limited amount of lithium reservoir significantly degrades the overall cell performance in the anode-free system. To mitigate the deterioration, modifying the current collector for enhanced lithium cycling is an indispensable route. Here, we apply a Ag/Cu ion exchange to precipitate micro-sized Ag particles on the Cu current collector to enhance the lithium reversibility via (de)alloying process. Further, we show a smoother morphology of lithium upon alloying, which leads to a lowered nucleation potential as well as increased average Coulombic efficiency in Li||Cu cells regardless of electrolyte formulation. The preferred lithium adsorption on Ag and AgLi over Cu is demonstrated with density functional theory calculations, which supports that Li is forming a gamma-phase alloy in the last stage rather than being deposited beneath the alloy. Lastly, this simple Cu foil modification enhances lithium reversibility and reduces its nucleation barrier, thus mitigating the capacity fade of a Cu||LiFePO 4 with reduced polarization.

25 ENERGY STORAGE↗

Regulating the growth of aluminum electrodeposits: towards anode-free Al batteries

The high earth abundance and large specific capacity of aluminum on either a volume (8040 mA h cm -3 ) or mass (2980 mA h g -1 ) basis continues to drive interest in electrochemical cells that utilize metallic Al as the anode. At practical anode capacities, uneven and non-planar deposition of Al during battery recharge combined with the high Young's modulus (EAl = 70 Ga) of the metal limits the electrode lifetime in all known electrolytes. Here we study the effect of a thin, textured coating composed of two-dimensional gold nanosheets with strong diffraction from (111) facets and low lattice mismatch for Al, as a substrate for regulating the Al electrodeposit morphology. We report that these coatings are not only effective in preventing Al deposition in non-planar morphologies, but have a large beneficial effect on the reversibility of Al electrodes. In Al plating/stripping studies, the textured Au coatings sustain stable cell operations for 500 cycles or more with a high coulombic efficiency of over 99%. Full cell Al batteries composed of the Au nanosheets as the anode substrate and graphene as the cathode are reported to exhibit capacity retention of 80% after 1000 charge–discharge cycles, and 74% at the 2000th cycle, exceeding the lifetimes (~200 cycles) of comparable Al batteries in which a standard stainless steel material is used as the anode substrate. Our results demonstrate that through rational design of the substrate for Al deposition, both the electrodeposit morphology and cycle life of Al-based batteries can be markedly improved.

25 ENERGY STORAGE↗

High-efficiency, anode-free lithium–metal batteries with a close-packed homogeneous lithium morphology

Anode-free lithium–metal batteries (LMBs) are ideal candidates for high-capacity energy storage as they eliminate the need for a conventional graphite electrode or excess lithium–metal anode. Current anode-free LMBs suffer from low Coulombic efficiency (CE) due to poor lithium stripping efficiency. Advanced electrolyte development is a promising route to maximize lithium plating and stripping CE and minimize capacity fade. However, a poor understanding of the mechanisms by which advanced electrolytes improve performance hampers progress in the practical development of anode-free LMBs. Here, we use synchrotron techniques and other tools to analyze the influence of three commercially available electrolytes on the composition, heterogeneity, kinetics, morphology, and electrochemistry of anode-free LMBs. Advanced electrolytes improve the electrochemical performance of anode-free LMBs by forming much denser and better-packed Li morphologies on a Cu current collector than on the conventional electrolyte. Li plates uniformly over the electrode area with the advanced electrolytes rather than in a few active sites. Inactive crystalline Li with heterogeneous distribution dominates the capacity degradation of anode-free cells, especially with the conventional electrolyte, indicating that reducing the amount of “dead” crystalline Li will significantly improve the cycling stability of anode-free cells. Finally, the understanding of the Li plating and stripping process obtained from this work will accelerate the development of anode-free LMBs with high efficiency.

25 ENERGY STORAGE↗

Time-Evolved Hetero-Alkali Interphases Enable Long-Life Sulfide-Based Anode-Free Solid-State Batteries

Sulfide-based anode-free solid-state batteries (AFSSBs) offer compelling advantages in terms of energy density and safety, yet their practical implementation is severely hindered by undesirable interfacial reactions between sulfide solid electrolytes (SEs) and freshly plated lithium (Li), as well as non-uniform Li plating/stripping behavior. Herein, an effective interfacial stabilization strategy by incorporating sodium bis(fluorosulfonyl)imide (NaFSI) additive into the Li5.4PS4.4Cl1.6 (LPSC) is investigated. Unlike conventional Li-based additives that form static passivation layers, NaFSI introduces a transient hetero-alkali chemistry that kinetically governs interphase evolution during fresh Li plating. NaFSI induces a timesequenced interphase evolution: an initial NaF/LiF-rich layer that suppresses early sulfide reduction, followed by a LiF/Li3N-rich layer that optimizes Li⁺ transport during repeated anode-free cycling. This evolved robust and fast ion conducting layer mitigates interfacial impedance growth, enhances Li + transport kinetics, and suppresses localized Li growth and filamentary shorting. As a result, the anode-free full cell with NaFSI modified LPSC as the interlayer exhibits an excellent cycling stability over 500 cycles at 0.2 C with a capacity retention of 77.6%, whereas the cell with bare LPSC suffers from rapid capacity decay after 100 cycles, retaining only 32.1% of its initial capacity. This work establishes dynamic heteroalkali additive chemistry as a general strategy to kinetically program solid-solid interphases, guiding the interface design in anode-free solid-state batteries.

25 ENERGY STORAGE↗

Particle Tracking Methods for Battery Precipitation Reactions

Precipitation and deposition reactions at solid–liquid interfaces play a key role in a number of battery chemistries, including Li-ion, so-called “anode free” batteries, zinc-based battery chemistries, and lithium–sulfur, among others. Although models with heterogeneous nucleation and growth phenomena are present in the literature, papers have not to date provided much detail on the numerical algorithms used to track the temporal evolution of the particle size distribution of deposits on electrode surfaces. In this paper we examine several approaches to discretize and track the particle size distribution, demonstrating that common approaches lead to anomalous flattening of the particle size distribution. We conclude by presenting an algorithm that preserves the appropriate particle size distribution during particle growth.

Algorithms↗

Non-fluorinated electrolyte for high-voltage anode-free sodium metal battery

Abundant sodium (Na) batteries are a sustainable alternative to resource-constrained lithium-ion batteries, offering huge cost advantages. However, developing high-voltage anode-free sodium metal batteries (SMBs) to narrow the energy density gap with lithium-ion batteries is hindered by a critical challenge: existing electrolytes cannot simultaneously achieve ultra-high Na coulombic efficiency and anodic stability. Here, in this study, we present a rationally designed non-fluorinated electrolyte (1.0 M NaPF 6 in 1,2-diethoxyethane/1,2-di-tert-butoxyethane) to address this key limitation, achieving Na coulombic efficiency of >99.95% and anodic stability of >4.8 V. For coin cells (2.0 mAh cm −2 , N/P = 1.7), our electrolyte design enables 4.0 V Na | |Na 3 V 2 (PO 4 ) 3 (NVP) at 5 C and 4.3 V Na | |NaNi 0.6 Mn 0.2 Co 0.2 O 2 (NMC622) at 0.3 C for 5,000 and 500 cycles with a capacity retention >80%. Remarkably, the 50 mAh anode-free pouch cells 4.0 V Al | |NVP and 4.3 V Al | |NMC622 also achieve 500 and 300 cycles (retention >75%) with a specific energy of >360 Wh kg (electrode) −1 . This work focuses on electrolyte optimization and conceptual advances, whereas critical aspects such as safety, large-scale manufacturability and practical feasibility of SMBs require further investigation. The electrolyte design using non-fluorinated solvents enhances the anodic stability without sacrificing Na efficiency, laying groundwork for advancing low-cost, high-energy SMBs and supporting the transition to sustainable battery technologies.

25 ENERGY STORAGE↗

Accelerated Short Circuiting in Anode-Free Solid-State Batteries Driven by Local Lithium Depletion

“Anode-free” solid-state batteries (SSBs), which have no anode active material, can exhibit extremely high energy density (≈1500 Wh L -1 ). However, there is a lack of understanding of the lithium plating/stripping mechanisms at initially lithium-free solid-state electrolyte (SSE) interfaces because excess lithium metal is often used. Here, it is demonstrated that commercially relevant quantities of lithium (>5 mAh cm -2 ) can be reliably plated at moderate current densities (1 mA cm -2 ) using the sulfide SSE Li 6 PS 5 Cl. Investigations of lithium plating/stripping mechanisms, in conjunction with cryo-ocused ion beam (FIB) imaging, synchrotron tomography, and phase-field modeling, reveal that the cycling stability of these cells is fundamentally limited by the nonuniform presence of lithium during stripping. Local lithium depletion causes isolated lithium regions toward the end of stripping, decreasing electrochemically active area and resulting in high local current densities and void formation. This accelerates subsequent filament growth and short circuiting compared to lithium-excess cells. Despite this degradation mode, here it is shown that anode-free cells exhibit comparable Coulombic efficiency to lithium-excess cells, and improved resistance to short circuiting is achieved by avoiding local lithium depletion through retention of thicker lithium at the interface. These new insights provide a foundation for engineering future high-energy anode-free SSBs.

25 ENERGY STORAGE↗

Control of Two Solid Electrolyte Interphases at the Negative Electrode of an Anode‐Free All Solid‐State Battery based on Argyrodite Electrolyte

Abstract Anode‐free all solid‐state batteries (AF‐ASSBs) employ “empty” current collector with three active interfaces that determine electrochemical stability; lithium metal – Solid electrolyte (SE) interphase (SEI‐1), lithium – current collector interface, and collector – SE interphase (SEI‐2). Argyrodite Li 6 PS 5 Cl (LPSCl) solid electrolyte (SE) displays SEI‐2 containing copper sulfides, formed even at open circuit. Bilayer of 140 nm magnesium/30 nm tungsten (Mg/W‐Cu) controls the three interfaces and allows for state‐of‐the‐art electrochemical performance in half‐cells and fullcells. AF‐ASSB with NMC811 cathode achieves 150 cycles with Coulombic efficiency (CE) above 99.8%. With high mass‐loading cathode (8.6 mAh cm −2 ), AF‐ASSB retains 86.5% capacity after 45 cycles at 0.2C. During electrodeposition of Li, gradient Li‐Mg solid solution is formed, which reverses upon electrodissolution. This promotes conformal wetting/dewetting by Li and stabilizes SEI‐1 by lowering thermodynamic driving force for SE reduction. Inert refractory W underlayer is required to prevent ongoing formation of SEI‐2 that also drives electrochemical degradation. Inert Mo and Nb layers likewise protect Cu from corroding, while Li‐alloying layers (Mg, Sn) are less effective due to ongoing volume changes and associated pulverization. Mechanistic explanation for observed Li segregation within alloying Li x Mg layer is provided through mesoscale modelling, considering opposing roles of diffusivity differences and interfacial stresses.

Wang, Yixian [Materials Science and Engineering Pr↗

Floatable Protective Layers: a Strategy to Minimize Solid Electrolyte Interphase Growth and Maximize the Lithium Utilization

Abstract Maximizing lithium (Li) utilization is crucial for enhancing the long‐term stability of Li‐based batteries. In anode‐free Li batteries (AFLBs), although the initial formation of solid electrolyte interphase (SEI) is beneficial on limiting further reaction between Li and electrolyte, large volume change of Li metal anode (LMA) during cycling often leads to continuous breakdown and re‐formation of SEI and formation of inactive Li, hindering its efficiency. In this study, a novel strategy is presented to protect Li metal by applying a floatable protection layer (FPL) on a copper substrate, enabling large Li particles to be primarily deposited below FPL, but SEI to be primarily formed above FPL. This approach effectively minimizes the direct contact between electrolyte and freshly deposited Li, therefore mitigating the continuous side reactions and early failure of AFLBs. As a result, Li consumption is minimized, and the overall stability of the battery is significantly enhanced. Further development of this approach can also be used to improve the performance of other Li‐based batteries for large‐scale applications.

Lim, Hyung‐Seok [Energy and Environment Directorat↗

Current‐Dependent Lithium Metal Growth Modes in “Anode‐Free” Solid‐State Batteries at the Cu|LLZO Interface

Abstract Controlling the lithium growth morphology in lithium reservoir‐free cells (RFCs), so‐called “anode‐free” solid‐state batteries, is of key interest to ensure stable battery operation. Despite several benefits of RFCs like improved energy density and easier fabrication, issues during the charging of the cell hinder the transition from lithium metal batteries with a lithium reservoir layer to RFCs. In RFCs, the lithium metal anode is plated during the first charging step at the interface between a metal current collector and the solid electrolyte, which is prone to highly heterogeneous growth instead of the desired homogeneous film‐like growth. Herein, the lithium morphology during the first charging step in RFCs is explored as a function of current density and current collector thickness. Using operando scanning electron microscopy, an increase in the lithium particle density is observed with increasing current density at the Cu|Li 6.25 Al 0.25 La 3 Zr 2 O 12 interface. This observation is then applied to improve the area coverage of lithium by pulsed plating. It is also shown that thin current collectors ( d = 100 nm) are unsuited for RFCs, as lithium whiskers penetrate them, resulting in highly heterogeneous interfaces. This suggests the use of thicker metal layers (several µm) to mitigate whisker penetration and facilitate homogeneous lithium plating.

25 ENERGY STORAGE↗

Visualizing diverse lithium growth and stripping behaviors in anode-free solid-state batteries with operando X-ray tomography

Anode-free solid-state batteries (SSBs), which eliminate the need for lithium metal use during cell assembly, have the potential to enable high energy densities and simplified manufacturing. However, the factors that control lithium growth/stripping at the anode current collector are not well understood. Here, we use operando X-ray microcomputed tomography to comprehensively image and quantify lithium deposition and stripping under various conditions in three different Li|Li 6 PS 5 Cl|current collector cells, revealing diverse behavior that depends on interface morphology, cell resistance, and solid-state electrolyte (SSE) microstructure. A cell with high resistance exhibits extensive lithium filament growth across the entire current collector interface, with filaments that grow around pre-existing pores in the SSE rather than lithium filling these pores. Lithium filament formation is partially reversible, with the cracks shrinking as lithium metal is stripped. Uniform lithium deposition is achievable at low current densities in low-resistance cells, whereas higher current densities in these cells cause an increase in interfacial roughness, which is correlated with subsequent filamentary growth at the edges of the cell. These results provide insight into filamentary vs. planar lithium growth and highlight that the evolution of lithium is sensitively dependent on SSE microstructure and electrochemical processes.

25 ENERGY STORAGE↗

Texture Evolution of Plated Lithium in Anode-Free Solid-State Batteries

Here, this study investigates lithium plating texture in anode-free solid-state batteries using synchrotron-based X-ray diffraction. Conventional methods are limited by lithium’s low electron density and softness, which hinders direct interrogation in anode-free solid-state batteries. Results reveal that lithium plating texture is influenced by temperature and current density. Under mild conditions, lithium exhibited a ⟨110⟩ fiber texture. However, higher current densities and elevated temperatures led to a more randomized orientation, suggesting a dependence on plating conditions. The results highlight how the operating and processing conditions for lithium metal can influence the texture of lithium metal and reversible operation.

36 MATERIALS SCIENCE↗

An Anode-Free Zn–MnO 2 Battery

Aqueous Zn-based batteries are attractive because of the low cost and high theoretical capacity of the Zn metal anode. However, the Zn-based batteries developed so far utilize an excess amount of Zn (i.e., thick Zn metal anode), which decreases the energy density of the whole battery. In this study, we demonstrate an anode-free design (i.e., zero-excess Zn), which is enabled by employing a nanocarbon nucleation layer. Electrochemical studies show that this design allows for uniform Zn electrodeposition with high efficiency and stability over a range of current densities and plating capacities. Using this anode-free configuration, we showcase a Zn–MnO 2 battery prototype, showing 68.2% capacity retention after 80 cycles. Our anode-free design opens a new direction for implementing aqueous Zn-based batteries in energy storage systems.

25 ENERGY STORAGE↗

The Microscopic Mechanism of Lithiation and Delithiation in the Ag/C Buffer Layer for Anode‐Free Solid‐State Batteries

Abstract Lithium metal solid‐state batteries (LMSSBs) have demonstrated their high energy density and cycling performance at high current densities in an anode‐free architecture, featuring a thin Ag/C composite buffer layer (BL) between the current collector (CC) and the solid electrolyte (SE). This study explains the microscopic mechanism of the Ag/C BL by using first‐principles atomistic and continuum modeling. It is shown that Ag effectively acts as a homogeneous solid‐solution beyond AgLi 2.32 and maintains a positive potential even at AgLi 25 during lithiation. Key factors underlying the working of the Ag/C BL include lower interfacial resistance at the BL/CC interface than at the BL/SE interface, leading to predominant Li deposition on BL/CC, and substantial Ag–Li volume expansion during lithiation. This, combined with stronger BL/SE adhesion, causes BL/SE separation and Ag–Li extrusion toward the CC side. During delithiation, Ag re‐precipitates as nanoparticles uniformly on the CC, with its positive lithiation potential homogenizing Li currents in subsequent cycles. Other metals are less effective due to their relatively large overpotential, premature lithiation termination, and limited volume expansions hindering movement toward the CC. The study aids the BL design, focusing on metal choice and optimization material and microstructural properties, such as the Li‐ion conductivity and interfacial resistance.

25 ENERGY STORAGE↗

Sulfide-Based Anode-Free Solid-State Batteries: Key Challenges and Emerging Solutions

Sulfide-based anode-free solid-state batteries (AFSSBs) have emerged as a transformative technology for next-generation energy storage, offering compelling advantages in energy density, safety, and manufacturing scalability. However, these batteries face significant challenges, particularly rapid capacity degradation that currently limits their practical implementation. This comprehensive review critically examines three fundamental issues affecting AFSSBs: nonuniform lithium nucleation on bare current collectors, unstable interfaces between plated lithium and sulfide electrolytes, and formation of interfacial voids during cycling. We systematically evaluate recent strategic advances in addressing these challenges, including metal seed coatings, conversion reaction-based compounds, and carbon-based interlayers. The review also analyzes the crucial role of advanced characterization techniques, from cryo-FIB-SEM to operando methods, in understanding failure mechanisms and validating improvement strategies. Finally, we present a forward-looking perspective on research directions necessary for commercialization. This work provides a thorough framework for understanding and advancing sulfide-based AFSSBs toward practical applications in next-generation energy storage systems.

25 ENERGY STORAGE↗

Dynamic Molecular Investigation of the Solid-Electrolyte Interphase of an Anode-Free Lithium Metal Battery Using In Situ Liquid SIMS and Cryo-TEM

Solid electrolyte interphase (SEI) has been widely perceived to play a critical role in the stable cycling of rechargeable batteries. However, associated with the fragile and air-sensitive nature of the SEI layer, delineation of the formation process and the nature of SEI remains a big challenge. Here, we use in situ liquid time-of-flight secondary ion mass spectroscopy (TOF-SIMS), cryo- transmission electron microscope (TEM) and density functional theory (DFT) calculation to delineate molecular process on the formation of SEI layer under the dynamic operating condition. We discover that the onset potential for SEI layer formation and the thickness of the SEI show dependence on the solvation shell structure. Using LiCoO 2 as a cathode and Cu film as an anode, the SEI is noticed to start to form at around 2.0 V and reach its final thickness (irreversible part, ~ 40-50 nm) at about 3.0 V in the 1 M LiPF 6 –EC/DMC electrolyte, while for the case of 1 M LiFSI–DME, the SEI starts to form at around 1.5 V and reaches its final thickness (~ 20 nm) at about 2.0 V. The in situ TOF-SIMS clearly indicates the outer SEI layer formation and dissipation upon charging and discharging, implying a continued evolution of electrolyte structure with extended cycling. In conclusion, the present work establishes a direct correlation between the molecular signature of SEI layer with solvation feature of electrolytes in lithium batteries, providing insights for tailoring SEI layer toward improved electrochemical properties of lithium batteries.

25 ENERGY STORAGE↗