Development of a high temperature battery first quarterly technical report
High temperature battery development - zeolites, anode and cathode couples, and molten salts
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
High temperature battery development - zeolites, anode and cathode couples, and molten salts
To address the high cost, cobalt dependency, and resource constraints typical of conventional high-entropy oxide (HEO) anodes, this study reports the successful synthesis of two Co-free, six-component spinel-type HEOs(FeNiCrMnZnAl) 3 O 4 (HEO-Al) and (FeNiCrMnZnMg) 3 O 4 (HEO-Mg), via a sol-gel method. The distinct effects of Al 3+ and Mg 2+ incorporation on the electrochemical performance and lithium storage kinetics were systematically investigated. XRD, Raman, and TEM characterizations confirm that both materials possess a pure spinel phase, uniform particle size, and homogeneous elemental distribution. Notably, electrochemical evaluations reveal that HEO-Al delivers a superior reversible capacity of 480.7 mAh g −1 after 100 cycles at 0.1 A g −1 , and maintains 354.5 mAh g −1 after 1000 long-term cycles at 1 A g −1 , significantly outperforming HEO-Mg. Kinetic analysis indicates that HEO-Al exhibits lower charge transfer resistance, a higher Li + diffusion coefficient, and a pseudocapacitive contribution of up to 82%. Furthermore, these findings demonstrate that Al substitution effectively optimizes the structural stability and lithium storage kinetics of Co-free HEOs, providing a viable strategy for designing low-cost, highly stable HEO anode systems.
One promising method for reducing precious metal usage in proton exchange membrane water electrolysis is lowering iridium (Ir) loading at the anode. However, low-loading Ir catalysts often suffer from poor stability under high current densities. In this study, hydrogen (H2) crossover from the cathode to the anode is identified as a key degradation pathway. Temperature-programmed reduction confirms the reduction of IrO2 at 80 °C in a hydrogen environment, highlighting the vulnerability of IrO2-based catalysts to H2 exposure. To mitigate this effect, palladium (Pd) is introduced as an anode additive, acting as an H2 oxidation catalyst and mitigating IrO2 reduction. This protective role is verified by inductively coupled plasma optical emission spectroscopy and in situ X-ray absorption spectroscopy, showing significantly suppressed Ir dissolution at 80 °C under H2 flow when an O-covered Pd surface is present at oxygen evolution reaction potentials. Results from the current study identify a new strategy in improving activity and durability of catalysts in electrolyzers.
High energy anode and cathode development, electrolyte encapsulation, tape activation, and parasitic operation techniques for dry tape battery concept
High energy anode and cathode for dry tape battery - incapsulation of electrolyte - manufacturing and testing of device
Cell discharge measurements for dry tape battery couple - anode and cathode development in aqueous and nonaqueous electrolytes
Conventional solid electrolyte interphases (SEIs) strongly adhere to micro-silicon (µ-Si) and crack under volume changes, causing poor cycling performance. Nano-silicon improves cycling performance but remains costly with limited calendar life. Here potentiostatic ageing tests demonstrate that both calendar and cycle ageing are governed by SEI cracking and dissolution with different relative contributions. When the system is not dominated by SEI dissolution, the relative calendar life of Si anodes could correlates positively with their cycle life. LiF-rich SEI that enables long cycle life in µ-Si is therefore expected to enhance calendar life as well. Using this framework, we screened electrolytes, SEIs and electrodes and validated them with full-cell storage. LiF-rich SEI minimizes cracking and dissolution, enabling μ-Si to achieve excellent calendar life, whereas nano-silicon suffers from SEI dissolution and needs reduced electrolyte–electrode contact for better calendar life. This work clarifies calendar-ageing behaviour and accelerates electrolytes and SEI development for long-life Si anodes.
The growing demand for sodium-ion batteries (SIBs) in grid storage underscores the need for electrode materials that balance performance and cost, including sustainable and robust carbon sources. The equitable and abundant distribution of materials for SIBs, along with their superior low-temperature performance, safety, and fast-charging capability, further distinguishes them from lithium-ion batteries (LIBs). Hard carbon (HC) is the state-of-the-art anode for SIBs, but current commercial HC production is localized mostly to one region of the world, raising concerns about supply chain vulnerability, critical material dependency, and environmental aspects. Here, the first demonstration of humins, an abundant biorefinery byproduct, as a precursor for HC anodes for sodium-ion storage is reported. Humins were carbonized at 1100 degrees C-1300 degrees C, and the resulting materials were subjected to comprehensive materials and electrochemical characterization. Among the temperatures studied, humins-derived hard carbon synthesized at 1200 degrees C delivers an initial reversible capacity 270mA h g-1 , with stable cycling performance up to 500 cycles and excellent rate capability, representing the optimal performance. This study establishes humins as a promising and low-cost carbon source that provides a route to mitigate supply chain risks and valorizes an underutilized biorefinery waste stream for high-performance SIB anodes.
High energy density primary battery development - anode-electrolyte, cupric fluoride cathode, and chemical stability tests
High energy density primary battery development - electrochemical half-cell screening of anode- electrolyte combinations, cell discharge, and potential studies
Lithium anodes, inorganic and organic cathodes, vacuum-distilled solvents, and methods for sintering cupric fluoride on lightweight metal substrates - development of high energy battery
Traditional design principles for heterogeneous catalysis guide the use of catalytic particles with mesosized (∼2–50 nm) pores to increase the number of surface-active sites by way of an increased surface area. However, the entry of long-chain polymers into such pores may be significantly limited by the size and entanglement of polymers in the melt state, thereby decreasing the number of accessible sites. Assessment of catalyst performance from traditional reactor-based studies averages over intrapore reaction events as well as reactions on the surface of a particle, resulting in an inability to distinguish between differences in site accessibility and activity. Techniques that assess the intrapore performance can inform the design of future heterogeneous catalysts for polymer upcycling. In this work, we demonstrate the use of broadband dielectric spectroscopy to monitor depolymerization of a polymer melt within mesopores via changes in the segmental relaxation time scale of amorphous polymer chains. In particular, we highlight the use of an anodic aluminum oxide (AAO) membrane as a readily available model for catalyst pores with a well-characterized pore morphology. The decrease in the segmental relaxation (α-relaxation) time of the melt with increasing chain scission emerges as a measure of the extent of polymer deconstruction inside mesopores. To demonstrate the utility of this technique, we demonstrate the decomposition of two commercial poly(propylene carbonate) polymers with different decomposition rates within mesopores. As the polymers depolymerize, their segmental relaxation time decreases as the molecular weight decreases (as predicted by the Fox–Flory equation). The BDS-measured change in segmental relaxation time mirrors the expected trend based on change in molecular weight measured by size exclusion chromatography.
We report a purely mechanical “cold-compression flow” method for fabricating Zn, Sn, and In substrates with tunable crystallographic textures. Using textured Zn as a model system, we investigate Zn electrocrystallization and demonstrate correlated growth of crystalline films with correlation lengths from tens to hundreds of micrometers. At 5 milliamperes per square centimeter (mA/cm 2 ), capacities between 20 and 82 milliampere hours per square centimeter (mA·hour/cm 2 ) are achieved depending on substrate texture level. At higher currents (40 mA/cm 2 ), capacities reach up to 604 mA·hour/cm 2 . Rotating disk electrode studies show that dominantly (002) textured Zn substrates exhibit enhanced corrosion resistance and reduced interphase passivation. We introduce an effective Damköhler number (Da*) to concisely describe morphological evolution during electrocrystallization across substrates with different textures. High-texture (002) Zn substrates substantially enhance performance in high-capacity (~20 mA·hour/cm 2 ) symmetric Zn||Zn cells and full cells (Zn||δ-MnO 2 and Zn||I 2 ), enabling fast-charging and prolonged energy storage in coin and pouch rechargeable Zn battery formats.
Anode-less solid-state lithium-sulfur batteries (SSLSBs) with lithium sulfide (Li 2 S) as the cathode promise a high energy density and ease of manufacturing. However, Li 2 S is plagued by poor conductivity, sluggish activation kinetics, and a poor cycle life. Here, in this study, we report an FeCl 3 -activated Li 2 S (FLS) cathode with solid-state polysulfide intermediates generated through a redox reaction between FeCl 3 and Li 2 S. This strategy is shown to boost the electrical conductivity of Li 2 S by 7 orders of magnitude and lower the activation barrier. During cycling, Fe plays a significant role in stabilizing the highly active polysulfide species, contributing to the exceptional electrochemical performance. The FLS cathode achieves 80% capacity retention over 500 cycles with >99% Li 2 S utilization. Furthermore, a Li-metal-free (anode-less) full cell retained over 80% of its initial capacity after 240 cycles. This work underscores the promise of leveraging Fe-stabilized polysulfides in enabling high-energy, long-lasting, solid-state Li-S batteries.
Addressing sustainable energy storage remains crucial for transitioning to renewable sources. While Li‐ion batteries have made significant contributions, enhancing their capacity through alternative materials remains a key challenge. Micro‐sized silicon is a promising anode material due to its tenfold higher theoretical capacity compared to conventional graphite. However, its substantial volumetric expansion during cycling impedes practical application due to mechanical failure and rapid capacity fading. A novel approach is proposed to mitigate this issue by incorporating trace amounts of aluminum into the micro‐sized silicon electrode using ball milling. Density functional theory (DFT) is employed to establish a theoretical framework elucidating how grain boundary sliding, a key mechanism involved in preventing mechanical failure is facilitated by the presence of trace aluminum at grain boundaries. This, in turn, reduces stress accumulation within the material, reducing the likelihood of failure. To validate the theoretical predictions, capacity retention experiments are conducted on undoped and Al‐doped micro‐sized silicon samples. In conclusion, the results demonstrate significantly reduced capacity fading in the doped sample, corroborating the theoretical framework and showcasing the potential of aluminum doping for improved Li‐ion battery performance.
Abstract Lithium‐metal batteries (LMB) employing cobalt‐free layered‐oxide cathodes are a sustainable path forward to achieving high energy densities, but these cathodes exhibit substantial transition‐metal dissolution during high‐voltage cycling. While transition‐metal crossover is recognized to disrupt solid‐electrolyte interphase (SEI) formation on graphite anodes, experimental evidence is necessary to demonstrate this for lithium‐metal anodes. In this work, advanced high‐resolution 3D chemical analysis is conducted with time‐of‐flight secondary‐ion mass spectrometry (TOF‐SIMS) to establish spatial correlations between the transition metals and electrolyte decomposition products found on cycled lithium‐metal anodes. Insights into the localization of various chemistries linked to crucial processes that define LMB performance, such as lithium deposition, SEI growth, and transition‐metal deposition are deduced from a precise elemental and spatial analysis of the SEI. Heterogenous transition‐metal deposition is found to perpetuate both heterogeneous SEI growth and lithium deposition on lithium‐metal anodes. These correlations are confirmed across various lithium‐metal anodes that are cycled with different cobalt‐free cathodes and electrolytes. An advanced electrolyte that is stable to higher voltages is shown to minimize transition‐metal crossover and its effects on lithium‐metal anodes. Overall, these results highlight the importance of maintaining uniform SEI coverage on lithium‐metal anodes, which is disrupted by transition‐metal crossover during operation at high voltages.
This manuscript contributes a Viewpoint article to ACS Sustainable Resource Management and discusses the graphite supply chain, growing mismatch between graphite demand and global manufacturing capacity, current graphite manufacturing technologies, and different feedstocks.
Abstract Anion chemistry in electrolytes can greatly dictate the nature and quality of passivation layers on both cathode and anode surfaces. This will be more significant when it comes to highly reactive Li‐metal anode and aggressive high‐nickel cathodes. Herein, a competitive bi‐anion activity is found in electrolytes with the co‐existence of two anions, which leads to a controlled Li‐salt decomposition kinetics and entirely favorable interphasial chemistry on both Li‐metal anode and ultrahigh‐nickel cathode. The proposed bi‐anion localized high‐concentration electrolytes are demonstrated to exhibit superior electrochemical compatibility toward Li metal and long‐term cycling stabilities under both 4.4 and 4.6 V in Li‐metal batteries with ultrahigh‐nickel cathode. This study sheds fresh light on dendrite‐free Li‐metal anodes and provides guidance to achieve high‐energy‐density batteries.