Search NASA⌕ Search

SEARCH · Search NASA

Results for “Fuel Cladding”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 361 records · Page 20

Tensile properties of the neutron irradiated HT-9 ACO-3 duct

HT-9, a ferritic-Martensitic steel, has attracted significant interest as a structural and cladding material for a variety of high dose nuclear component applications. This study examines the tensile properties of a HT-9 fuel assembly duct from the fast flux test facility, FFTF. The duct, from the Advanced Core Oxide-3 (ACO-3) irradiation test, was subjected to fast neutron irradiation exposure ranging from 3 dpa above the core top to nearly 155 dpa near the core mid-plane, spanning a temperature range from 382 °C at the lower end to 504 °C at the top. Due to the combination of thermal and neutron flux gradients along the core height. This yields a variety of irradiation damage processes which depend on core location. Tensile properties of specimens extracted at different positions along the height of the irradiated duct were measured at 25 °C, 200 °C and near their in-core irradiation temperature. The results show temperature has a greater impact than dose on post-irradiation strength and ductility. Two irradiation temperature regimes were determined, below irradiation temperatures of 420 °C irradiation hardening increases as irradiation temperature decreases, and above that temperature relatively minor changes are observed in tensile properties. These results are discussed in terms of expected microstructural changes, indicating that dislocation content is a strong contributor in these findings.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Long-Length SiC/SiC Tube Irradiation Experiment at LWR Temperatures Inserted into HFIR

This report describes the pre-irradiation characterization and successful assembly of a High Flux Isotope Reactor (HFIR) irradiation experiment designed to assess radiation-induced lateral bowing of silicon carbide fiber–reinforced, silicon carbide matrix composite (SiC/SiC) components under a radial fast neutron flux gradient at representative light-water reactor (LWR) temperatures of approximately 300 °C. The over-arching goal of this work is to validate thermomechanical models of SiC/SiC composite fuel assembly distortion used to predict the extent of lateral bowing and dose at which bowing reaches a maximum value. Ultimately, these models are used to ensure that fuel assembly distortion does not block coolant channels, interfere with control rod/blade movements, and/or impact local reactivity. The experiment contains six cladding tube specimens that are approximately 558.5 mm long with representative pressurized water reactor (PWR) outer and inner diameters of 9.5 mm and 7.5 mm, respectively. The specimens were thoroughly characterized prior to irradiation using traditional dimensional inspection and surface profilometry so that these measurements can later be compared with similar measurements that will be made post-irradiation to determine radiation-induced deformations. Furthermore, fine engraving markers were inscribed along the outer surfaces of the specimen and mapped using analytic photography and a three-dimensional stage. This technique allowed for accurate measurements of the marker spacings, which can be compared with similar measurements that will be made post-irradiation to provide local radiation-induced strain mapping. A light curtain optical micrometer was also employed to measure the pre-irradiation bowing of each specimen. The experiment was successfully assembled and inserted into position VXF-19 for HFIR cycle 516, which began May 12, 2026. The experiment will be removed after cycle 519, which is currently scheduled to end in December 2026.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

International fuel performance study of fresh fuel experiments for PCMI effects during RIA experiments

This paper presents the results of High-burnup Experiments for Reactivity-initiated Accident (HERA) Modeling & Simulation (M&S) exercise. The HERA project under the Nuclear Energy Agency (NEA) Second Framework for Irradiation Experiments (FIDES-II) program is focused on studying Light Water Reactor (LWR) fuel behavior during Reactivity-Initiated Accident (RIA) conditions. The Part I M&S cases are based on a series of tests in the Transient Reactor Test (TREAT) facility in the United States and the Nuclear Safety Research Reactor (NSRR) in Japan. The purpose of this work is to evaluate the test design to accomplish its goals in establishing clearer understanding of the effects of power pulse width during RIA conditions. Further, the blind predictions using various computational tools have been performed and compared amongst to interpret the behaviors of high burnup fuels during RIA. While many international participants evaluate the thermal–mechanical behavior of fuel rod under different conditions, a considerable scatter of outputs comes out for the cases due to the disparity between codes in predicting mechanical behaviors. In general, however, the results of thermal–mechanical analysis elaborate that nominal design conditions the shorter pulse width tests in NSRR should cause cladding failures while the TREAT tests appear to have more split prediction of failure or not. Furthermore, the sensitivity analysis varying key testing parameters reveals the considerable effect of power pulse width and total energy deposition on prediction of fuel rod failure.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

A LOCA Analysis Tool: Coupling RELAP5-3D to BISON

Experimental evidence illustrates that at burnups slightly above the current regulatory limit of a rod-averaged burnup of 62 MWd/kgU, the ceramic UO 2 inside light-water reactor fuel rods becomes susceptible to a phenomenon known as fuel fragmentation, relocation, and dispersal (FFRD) during a loss of coolant accident (LOCA) transient. The severity of FFRD is strongly influenced by the zirconium-based (Zircaloy) cladding behavior during the LOCA transient. A Technology Commercialization Fund (TCF) project was awarded to an Electric Power Research Institute (EPRI)/Idaho National Laboratory team to create a LOCA analysis tool that couples BISON to the systems/thermal-hydraulics code RELAP5-3D [1] for analysis of LOCA scenarios. In addition, further refinements to existing BISON models were identified as necessary to more accurately represent more recent experimental evidence from the Studsvik Cladding Integrity Project (SCIP) and other experimental programs.

11 - NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

MURR LEU structural and thermal hydraulics analyses: Part I – Preliminary irradiation thermo-mechanical behavior

The University of Missouri Research Reactor (MURR) is expected to be converted from highly enriched uranium (HEU, ≥ 20 wt% U-235) U-Al x dispersion fuel to low-enriched uranium (LEU, < 20 wt% U-235) with U-10Mo monolithic fuel. This work introduces high-fidelity irradiation thermo–mechanical (T-M) analysis of the MURR LEU focusing on changes in coolant channel gap thickness. Three-dimensional (3D) finite element (FE) models were developed to simulate the irradiation T-M behavior of the MURR LEU element with all 23 curved fuel plates, the two side plates, and the combs. It was shown that channel gap thickness changes were influenced not only by plate thickness variations due to fuel swelling and creep but also by the radial displacement of consecutive MURR LEU plates. Modeling the fuel element assembly captured side plate displacements, which were shown to reduce radial fuel plate displacements towards the convex side. The maximum local radial displacement in the element was predicted at the end of life (EOL) as 23.7 mil (602.0 µm) on the lateral centerline of plate 23 towards the convex side. The maximum stripe-averaged reduction in channel gap thickness, particularly relevant for thermal hydraulics (TH) safety analysis, was calculated as 15.9 mil (403.9 µm) in single-side heated channel 24 (the outermost channel). These results account for the thermal resistance from the oxide build-up on cladding surfaces which was shown to be up to 0.82 mil (20.8 µm) thick. It was demonstrated that accounting for oxide layer thermal resistance led to a 10 °C higher peak fuel temperature and a 4.4 mil (111.8 µm) greater maximum local radial displacement. The impact of the calculated channel gap thickness changes on the MURR LEU TH safety analysis is evaluated in Part II.

Irradiation thermo-mechanical analysis↗

Compatibility of Zircaloy-4 in eutectic PbSn and PbBiSn liquid metals

Here, a novel nuclear fuel concept has been proposed, consisting of UO₂ particles suspended in a liquid metal alloy. To evaluate its feasibility, the compatibility of Zircaloy-4 cladding with candidate eutectic PbSn and PbBiSn alloys—as well as with pure Pb, Bi, and Sn—was investigated through 1000-hour exposures at 400 °C and 600 °C. Severe degradation of the Zircaloy-4 specimens was observed in eutectic PbSn at 600 °C, whereas oxidation and oxygen diffusion were evident after exposure at 400 °C. At 600 °C, the formation of Zr₃Fe precipitates at the oxide–alloy interface was identified in specimens exposed to Pb and PbBiSn. Thermodynamic analysis suggested that the observed intermetallic formation resulted from the destabilization of Laves phases due to oxygen ingress at elevated temperatures.

Bismuth↗

A Historical Review of Cermet Fuel Development and the Engine Performance Implications

This paper reviews test data for cermet fuel samples developed in the 1960's to better quantify Nuclear Thermal Propulsion (NTP) cermet engine performance, and to better understand contemporary fuel testing results. Over 200 cermet (W-UO2) samples were tested by thermally cycling to 2500 deg (2770 K) in hydrogen. The data indicates two issues at high temperatures: the vaporization rate of UO2 and the chemical stability of UO2. The data show that cladding and chemical stabilizers each result in large, order of magnitude improvements in high temperature performance, while other approaches yield smaller, incremental improvements. Data is very limited above 2770 K, and this complicates predictions of engine performance at high Isp. The paper considers how this material performance data translates into engine performance. In particular, the location of maximum temperature within the fuel element and the effect of heat deposition rate are examined.

Ceramic Nuclear Fuel↗

Full-core high-burnup BWR LOCA fuel performance analysis and FFRD susceptibility

The susceptibility of the boiling water reactor (BWR) Limerick Unit 1 to fuel fragmentation, relocation, and dispersal during a postulated large-break loss-of-coolant accident (LBLOCA) was calculated using a multiphysics framework. The simulations include full-core, rod-resolved neutronic, thermal hydraulic, and fuel performance models using the VERA, TRACE, and BISON codes. This work focused on the transient BISON simulations, which include both the normal operation and LBLOCA periods in the same simulations. Cladding integrity was assessed using two correlations that are included with BISON. make page break Several new BWR-specific features were recently added to BISON. This work represents the first time these features have been included in a core-scale set of simulations. This study hence evaluates the performance of these new models for an operating reactor with realistic operating conditions. Simulation results showed that cladding integrity was maintained (i.e., no rods burst). Finally, future work to improve BWR and PWR predictions using this framework is suggested.

BISON↗

Potentialities of TEC topping: A simplified view of parametric effects

An examination of the benefits of thermionic-energy-conversion (TEC)-topped power plants and methods of increasing conversion efficiency are discussed. Reductions in the cost of TEC modules yield direct decreases in the cost of electricity (COE) from TEC-topped central station power plants. Simplified COE, overall-efficiency charts presented illustrate this trend. Additional capital-cost diminution results from designing more compact furnaces with considerably increased heat transfer rates allowable and desirable for high temperature TEC and heat pipes. Such improvements can evolve of the protection from hot corrosion and slag as well as the thermal expansion compatibilities offered by silicon-carbide clads on TEC-heating surfaces. Greater efficiencies and far fewer modules are possible with high-temperature, high-power-density TEC: This decreases capital and fuel costs much more and substantially increases electric power outputs for fixed fuel inputs. In addition to more electricity, less pollution, and lower costs, TEC topping used directly in coal-combustion products contributes balance-of-payment gains.

Morris, J. F.↗

Loss of Flow Conditions in a Modern Pool-type SFR and In-Pile Experiment Design

The metallic fuel safety performance under unprotected design-basis transients is a key consideration for the deployment of advanced sodium fast reactors (SFRs). Reliable data are needed to validate advanced safety codes, reduce uncertainty in cladding failure thresholds, and strengthen confidence in licensing approaches. To address this need, this report develops blueprints for a conceptual sodium loss-of-flow (LOF) experiment in the Mk-IIIR loop at the Transient Reactor Test Facility (TREAT), providing the technical foundation for future integral testing.

11 - NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Dispersal of high-burnup fuel fragment surrogate particles during and after loss-of-coolant accident tests

The issue of fuel fragmentation, relocation, and dispersal is critical in the licensing and use of high-burnup (>62 GWd/MTU) nuclear fuel in light water reactors (LWRs). In this work, two test series are reported that examine the fragment dispersal during a burst event and an additional dispersal following the burst due to vibrations in the rod, such as those induced by accident recovery systems. To examine dispersal during the balloon and burst portion of a Loss-of-Coolant Accident event, HfO 2 fragments and yttria-stabilized zirconia pellets were filled into an as-fabricated cladding tube, which was then pressurized and subjected to loss-of-coolant accident testing in steam. Results from this test were found to be highly non-prototypic, and dispersal was both significantly more violent and significantly greater in magnitude than identified for actual fuel tests. These findings were attributed to the conservative (more dispersive) nature of the particles chosen for dispersal and to the details of the test conditions used that led to particularly wide bursts. Further, the second set of tests examined dispersal following the burst when vibrations were induced in the rod, primarily via recovery activities such as Emergency Core Cooling System actuation leading to rapid water addition. Post-burst dispersal testing was performed by inducing sinusoidal oscillations with 2–25 nm peak-to-peak amplitude and 2–5 Hz frequencies in pre-burst rods that had been refilled with HfO 2 fragments or high-burnup fragment surrogate mixture of HfO 2 fragments and yttria-stabilized zirconia sands. Testing revealed that rods with large burst openings (7 mm wide in this work) led to unmitigated dispersal from above the burst zone but that smaller bursts (5 mm wide), although still much larger than the mean fragment size of 3 mm, led to effectively no dispersal because of interparticle locking. Additionally, mixture and moisture were found to impact the amount of dispersal: mixtures increased dispersal, and moisture drastically reduced it. The implications of these findings on likely dispersal from actual fuel are discussed.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Experiment to Investigate the On-set of Transient Fission Gas Release Under Simulated LOCA Conditions

Continuing efforts to better understand the phenomenon of transient fission gas release in irradiated commercial light water reactor fuel undergoing a simulated loss of coolant accident (LOCA) will be discussed in this work. During heating associated with LOCA conditions there is an additional release of fission gas beyond what is typically released during steady state operation. The exact timing of this release could impact the cladding balloon and rupture as the LOCA progresses in an actual accident. Recent experiments performed on the upgraded Severe Accident Test Station at Oak Ridge National Laboratory have expanded the current assessment of transient fission gas release. This system evaluates fission gas release by sweeping fission gas out of the LOCA test furnace and into cryogenically cooled cold traps where radioactive noble gas fission products are measured by gamma spectrometry. Additionally, the sweep gas can be monitored by a gas mass spectrometer to provide additional data on noble gas release and changes in the sweep gas atmosphere during heating. Several different conditions have been evaluated that explored the response of irradiated fuel to different thermal ramp conditions and different overpressure conditions. This further confirmed the impact of an overpressure in suppressing transient fission gas release. Further experiments are planned to evaluate the on-set temperature of transient fission gas release under a known overpressure. This test will progressively step through different temperature conditions while maintaining hydrostatic pressure on the fuel that is representative of high burnup fuel conditions. The available results from this type of testing will be discussed. Post-test microscopy will be compared to other transient fission gas release and standard LOCA tests to further understand the microstructural source of transient fission gas release.

Harp, Jason [ORNL] (ORCID:0000000253458440)↗

Technical Considerations on MURR Control Blade Design Change and Testing using a New Metal Matrix Composite

The University of Missouri Research Reactor (MURR) is one of six research reactors, including a critical facility, that are pursuing conversion as part of a collaboration with the U.S. Department of Energy National Nuclear Security Administration Material Management and Minimization Office of Reactor Conversion and Uranium Supply, under the U.S. High Performance Research Reactors (USHPRR) conversion project. Five of the six USHPRR are planned to convert from highly enriched uranium (HEU) fuel using a low-enriched uranium (LEU) high assay monolithic alloy of uranium-10 wt% molybdenum (U-10Mo). As part of the conversion safety analysis, it is necessary to demonstrate the safety performance of the proposed core fueled with LEU as compared to the current HEU cores. The MURR reactor is planning to switch to a new control blade design that uses a metal matrix composite of boron carbide (B 4 C) and aluminum as the absorber in place of Boral®. Since MURR is expected to adopt the new metal matrix composite control blade design prior to conversion, the impact of the new blade design on the neutronics characteristics of the MURR cores for conversion are analyzed in this work through updates to incorporate the changes to the blade design in conversion models as they directly impact the LEU conversion safety analysis. The quantitative comparison shows that the neutronics and thermal hydraulic behavior of one metal matrix composite blade replacing a Boral blade is comparable for the two example MURR LEU and HEU cores states considered. Geometrical changes in the metal matrix composite blade design, combined with a 4% increase in areal boron density, showed local heating effects up to 20% higher than the Boral design. As expected, the metal matrix composite showed slightly lower heat depositions and absorber region temperatures for the LEU cases compared to HEU. Although this analysis was comparative for a single blade, maximum control blade temperatures for both Boral, metal matrix composite, and HEU/LEU remained below 100 °C, though additional analysis at a core level could differ. A qualitative irradiation behavior assessment concludes that the mechanisms that may drive swelling and blistering in the current Boral design are eased by the adoption of the metal matrix composite design. The work concludes that the two blade designs are essentially equivalent with regards to neutronics, thermal hydraulics, and expected material behavior under irradiation. However, due to the geometrical changes to the blades including redesigned and thinner cladding, new testing and increased surveillance for distortion and swelling are recommended to confirm the performance of the metal matrix composite control blade design. Where testing is completed prior to conversion, the only anticipated impacts on conversion to LEU U-10Mo fuel would be the need for models and safety analysis incorporating the metal matrix composite control blades.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Fatigue Testing and Characterization of Pre-hydrided Zircaloy-4 Cladding Tubes

The solubility of hydrogen in Zircaloy-4 (Zry-4) at the cladding operating temperature is near 100 wt. ppm. Above this solubility limit, excess hydrogen precipitates as δ-hydride platelets in the cladding material. Because of the effect of the thermal gradient across the cladding thickness on the migration and precipitation of hydrogen, hydride rims are often observed at the cladding outer surface; under excessive corrosion conditions hydride blisters are possible. It is well known that the fatigue of metal alloys, especially high cycle fatigue, is sensitive to the status of surface including the microstructure, roughness, and residual stress. Thus, the question considered herein, is whether excessive hydrogen pickup modifies the microstructure such that it has a degradation effect on the fatigue performance of cladding during operation. This report describes the evaluation of fatigue performance of a pre-hydrided Zry-4 cladding. A commercial Zry-4 was polished and pre-hydrided to 800 ppm and 1300 ppm H contents. The fatigue testing was conducted under strain control at 5 Hz with fully-reversed bending by using a cyclic integrated reversible bending fatigue tester (CIRFT). Six specimens with 1300 ppm and one specimen with 800 ppm were tested. Significant variation in test results were observed. While two of the 1300 ppm specimens failed with less than 1 ×10 5 cycles (at 0.32% and 0.41%), the four other samples did not fail over the strain amplitude range of 0.25% to 0.38%. Interestingly, the fracture initiation site of the failed samples was on the outside diameter (OD) surface rather than on the inside diameter (ID) surface as is typical for the as-polished cladding. This suggested a degrading effect of the hydriding process. Subsequently, three of the unfailed specimens were then further tested at ~0.43% to observe where failure initiation occurred. Significant variation was also observed in these three specimens. One specimen failed at ~9000 cycles while the two others failed at 43000 and 1.06 ×10 5 cycles. The performance here correlated to the location of failure initiation; failure initiated on the OD in the sample that failed after 9000 cycles while it initiated on the ID in the sample that failed after 43000 and 1.06 ×10 5 cycles. Flat features at the OD initiation sites suggest a brittle hydride feature on the surface of those samples was the cause of the degradation in fatigue performance, though the overall hydrogen levels in all samples was similar. A summary of all the observations is provided below: • The un-failed specimens with 1300 ppm H were cycled to failure with a higher amplitude near 0.43%. In addition, the fatigue-treated specimen tended to have a longer fatigue at the same induced amplitude. • Fractography revealed a mixed failure mode for the pre-hydrided specimen. Particularly, the specimen with fracture initiation site (FIS) located on the outer diameter surface of tube tended to have a shorter fatigue life than that of FIS on the inner diameter surface. • Etched cross section was shown to have hydride platelets aligned with tube longitudinal axis as expected, and the density of hydrides is at the similar level as in literature data. Meanwhile, a LECO procedure was applied for hydrogen concentration measurement, which showed the measured hydrogen contents are close to the nominal value. • With the polished cladding tube as baseline, O’Donnell-Lager (O-L) analysis showed that a decrease of about 50% in reduction-of-area (RA) would be needed for the O-L fitting to the fatigue data of 1300 ppm cladding. The suggestion for the next steps is provided.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Assessing the Heat Transfer Modeling Capabilities of CFD Software for Involute-Shaped Plate Research Reactors

The ongoing efforts to convert High-Performance Research Reactors (HPRRs) using Highly Enriched Uranium (HEU) to Low-Enriched Uranium (LEU) fuel require reliable thermal–hydraulic assessments of modified core designs. The involute-shaped fuel plates used in several major HPRRs present unique modeling challenges due to their compact core geometries and high heat flux conditions. This study evaluates the capability of three commercial CFD tools, STAR-CCM+, COMSOL, and ANSYS CFX, to predict cladding-to-coolant heat transfer using Reynolds-Averaged Navier–Stokes (RANS) methods within the thermal–hydraulic regimes of involute-shaped plate reactors. Broad sensitivity analysis was conducted across a range of reactor-relevant parameters using two turbulence models (k−ϵ and k−ω SST) and different near-wall treatment strategies. The results were benchmarked against the Sieder–Tate correlation and experimental data from historic studies. The codes produced consistent results, showing good agreement with the empirical correlation of Sieder–Tate and the experimental measurements. The findings support the use of these commercial CFD codes as effective tools for assessing the thermal–hydraulic performance of involute-shaped plate HPRRs and guide future LEU core development.

CFD↗

Feasibility of an on-line fission-gas-leak detection system

Calculations were made to determine if a cladding failure could be detected in a 100-kW zirconium hydride reactor primary system by monitoring the highly radioactive NaK coolant for the presence of I-131. The system is to be completely sealed. A leak of 0.01 percent from a single fuel pin was postulated. The 0.364-MeV gamma of I-131 could be monitored on an almost continuous basis, while its presence could be varified by using a longer counting time for the 0.638-MeV gamma. A lithium-drifted germanium detector would eliminate radioactive corrosion product interference that could occur with a sodium iodide scintillation detector.

Lustig, P. H.↗

Design and testing a high fuel volume fraction, externally finned, thermionic emitter.

A prototypical, high fuel volume fraction, thermionic emitter body was designed and tested. The emitter body is all tungsten, with a 1.40-cm ID, a 3.23-cm OD, and eight full-length axial fins. The emitter thickness is 0.15 cm while the fins and outer clad are 0.075 cm thick. Different methods of fabrication were used in making the test samples. Stress analysis was performed with a three-dimensional elastic code. Thermal testing of the samples, duplicating calculated radial temperature gradients, heatup and cooldown rates, and emitter body temperatures in operation, was performed with no structural failures noted (six heatup and cooldown cycles per sample). Further emitter analysis and testing is planned.

Peelgren, M. L.↗