Search NASA⌕ Search

SEARCH · Search NASA

Results for “dispersion analysis”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 361 records · Page 20

Corrosion of 310 stainless steel in H2-H2O-H2S gas mixtures: Studies at constant temperature and fixed oxygen potential

Corrosion of SAE 310 stainless steel in H2-H2O-H2S gas mixtures was studied at a constant temperature of 1150 K. Reactive gas mixtures were chosen to yield a constant oxygen potential of approximately 6 x 10 to the minus 13th power/cu Nm and sulfur potentials ranging from 0.19 x 10 to the minus 2nd power/cu Nm to 33 x 10 to the minus 2nd power/cu Nm. The kinetics of corrosion were determined using a thermobalance, and the scales were analyzed using metallography, scanning electron microscopy, and energy dispersive X-ray analysis. Two corrosion regimes, which were dependent on sulfur potential, were identified. At high sulfur potentials (p sub S sub 2 less than or equal to 2.7 x 10 to the minus 2nd power/cu Nm) the corrosion rates were high, the kinetics obeyed a linear rate equation, and the scales consisted mainly of sulfide phases similar to those observed from pure sulfication. At low sulfur potentials (P sub S sub 2 less than or equal to 0.19 x 10 to the minus 2nd power/cu Nm) the corrosion rates were low, the kinetics obeyed a parabolic rate equation, and scales consisted mainly of oxide phases.

Rao, D. B.↗

MC carbide structures in M(lc2)ar-M247

The morphologies and distribution of the MC carbides in Mar-M247 ingot stock and castings were investigated using metallographic, X-ray diffraction and energy-dispersive X-ray analysis techniques. The MC carbides were found to form script structures during solidification. The script structures were composed of three distinct parts. The central cores and elongated arms of the MC carbide script structures had compositions (Ti, Cr, Hf, Ta, W)C and lattice parameters of 4.39 A. The elongated script arms terminated in enlarged, angular "heads". The heads had compositions (Ti, Hf, Ta, W)C and lattice parameters of approximately 4.50 A. The heads had a higher Hf content than the cores and arms. The size of the script structures, as well as the relative amount of head-type to core and arm-type MC carbide, was found to be determined by solidification conditions. No carryover of the MC carbides from the ingot stock to the remelted and cast material was observed.

Wawro, S. W.↗

Fine particles in the Soufriere eruption plume

The size distributions of fine particles measured at tropospheric altitudes in the periphery of the eruption plume formed during the April 17, 1979 eruption of Soufriere Volcano and in the low-level effluents on May 15, 1979 were found to be bimodal, having peak concentrations at geometric mean diameters of 1.1 and 0.23 micrometers. Scanning electron microscopy and energy-dispersive X-ray analysis of the samples revealed an abundance of aluminum and silicon and traces of sodium, magnesium, chlorine, potassium, calcium, and iron in the large-particle mode. The submicrometer-sized particles were covered with liquid containing sulfur, assumed to be in the form of liquid sulfuric acid.

Woods, D. C.↗

RF sputtered silicon and hafnium nitrides: Properties and adhesion to 440C stainless steel

Silicon nitride and hafnium nitride coatings were deposited by reactive RF sputtering on oxidized and unoxidized 440C stainless steel substrates. Sputtering was done in mixtures of argon and nitrogen gases from pressed powder silicon nitride and from hafnium metal targets. Depositions were at two background pressures, 8 and 20 mtorr, and at two different fractions (f) of nitrogen in argon, 0.25 and 0.60, for hafnium nitride and at f = 0.25 for silicon nitride. The coatings and the interface between the coating and substrates were investigated by X-ray diffractometry, scanning electron microscopy, energy dispersive X-ray analysis and Auger electron spectroscopy. A Knoop microhardness of 1650 + or - 100 kg/sq mm was measured for hafnium nitride and 3900 + or - 500 kg/sq mm for silicon nitride. The friction coefficients between a 440C rider and the coatings were measured under lubricated conditions. Scratch test results demonstrate that the adhesion of hafnium nitride to both oxidized and unoxidized 440C is superior to that of silicon nitride. Oxidized 440C is found to have increased adhesion, to both nitrides, over that of unoxidized 440C.

Grill, A.↗

The atmosphere of Titan - An analysis of the Voyager 1 radio occultation measurements

The equatorial atmosphere of Titan was probed by means of two coherently related radio signals transmitted from Voyager 1 at 13.0 and 3.6 cm wavelengths during the November 12, 1980 occultation of the spacecraft by the Saturn satellite. An analysis of the differential dispersive frequency measurements did not reveal any ionization layers in the upper atmosphere of Titan. The gas refractivity data, which extend from the surface to about 200 km altitude, were interpreted in two different ways. In the first, it is assumed that N2 makes up virtually all of the atmosphere, with small amounts of CH4 and other hydrocarbons present. In the second interpretation of the refractivity data, it is assumed that the 3.5 km altitude level corresponds to the bottom of a CH4 cloud layer and that N2 and CH4 were perfectly mixed below this level.

Lindal, G. F.↗

Metallurgical characterization of the fracture of several high strength aluminum alloys

The fracture behavior for structural aluminum alloys (2024, 6061, 7075, and 7178) was examined in selected heat treatments. The investigation included tensile, shear, and precracked notch-bend specimens fractured at ambient temperature under monotonic loading. Specimens were obtained from thin sheets and thick plates and were tested in longitudinal and transverse orientations at different strain rates. Microstructures of alloys were examined using the optical microscope and the scanning electron microscope with associated energy dispersive X ray chemical analysis. Several different types of second phase particles, some not reported by other investigators, were identified in the alloys. Fracture morphology was related to microstructural variables, test variables, and type of commercial product. Specimen orientation examined in the present investigation had little effect on fracture morphology. Test strain rate changes resulted in some change in shear fracture morphology, but not in fracture morphology of tensile specimens.

Bhandarkar, M. D.↗

Laboratory degradation of Kapton in a low energy oxygen ion beam

An atomic oxygen ion beam, accelerated from a tunable microwave resonant cavity, was used at Lewis Research Center to bombard samples of the widely used polyimide Kapton. The Kapton experienced degradation and mass loss at high rates, which may be comparable to those found in Space Shuttle operations if the activation energy supplied by the beam enabled surface reactions with the ambient oxygen. The simulation reproduced the directionality (ram-wake dependence) of the degradation, the change in optical properties of the degraded materials, and the structure seen in scanning electron micrographs of samples returned on the Shuttle Trails with a substituted argon ion beam produced no rapid degradation. Energy Dispersive X-ray Analysis (EDAX) showed significant surface composition changes in all bombarded samples. Mass loss rates and surface composition changes are discussed in terms of the possible oxidation chemistry of the interaction. Finally, the question of how the harmful degradation of materials in low Earth orbit can be minimized is addressed.

Ferguson, D. C.↗

RF sputtered silicon and hafnium nitrides as applied to 440C steel

Silicon nitride and hafnium nitride coatings were deposited on oxidized and unoxidized 440C stainless steel substrates. Sputtering was done in mixtures of argon and nitrogen gases from pressed powder silicon nitride and from hafnium metal targets. The coatings and the interface between the coating and substrate were investigated by X-ray diffractometry, scanning electron microscopy, energy dispersive X-ray analysis and Auger electron spectroscopy. Oxide was found at all interfaces with an interface width of at least 600 A for the oxidized substrates and at least 300 A for the unoxidized substrates. Scratch test results demonstrate that the adhesion of hafnium nitride to both oxidized and unoxidized 440C is superior to that of silicon nitride. Oxidized 440C is found to have increased adhesion, to both nitrides, over that of unoxidized 440C. Coatings of both nitrides deposited at 8 mtorr were found to have increased adhesion to both oxidized and unoxidized 440C over those deposited at 20 mtorr.

Grill, A.↗

LSS 4300 - A hot counterpart of Upsilon Sagittarii and KS Persei?

A number of recent observations indicate that the star LSS 4300 (HDE 320156) is a high-temperature analog of the hydrogen-deficient binaries Upsilon Sgr and KS Per. A preliminary model-atmosphere analysis based on high dispersion spectra obtained at Kitt Peak and Cerro Tololo yields Teff = 14,400 K, log (g) = 1.4, n(H)/n(He) = 0.003, and n(N)/n(C) = 20 for the visible component. The optical emission-line spectrum of LSS 4300 is nearly identical to that of Upsilon Sgr, including strong, broad H-alpha, Fe II, and forbidden Ca II emission; and JHKL photometry obtained at Cerr Tololo reveals an infrared excess nearly identical to that of Upsilon Sgr. It is suggested that LSS 4300, like Upsilon Sgr and KS Per, is a close binary system consisting of a helium supergiant of about 1 solar mass, which is undergoing its second mass loss, and a less luminous secondary, which is accreting matter from the primary.

Schoenberner, D.↗

Laboratory degradation of Kapton in a low energy oxygen ion beam

An atomic oxygen ion beam, accelerated from a tunable microwave resonant cavity, was used at Lewis Research Center to bombard samples of the widely used polyimide Kapton. The Kapton experienced degradation and mass loss at high rates, which may be comparable to those found in Space Shuttle operations if the activation energy supplied by the beam enabled surface reactions with the ambient oxygen. The simulation reproduced the directionality (ram-wake dependence) of the degradiation, the change in optical properties of the degraded materials, and the structure seen in scanning electron micrographs of samples returned on the Shuttle Trails with a substituted argon ion beam produced no rapid degradation. Energy Dispersive X-ray Analysis (EDAX) showed significant surface composition changes in all bombarded samples. Mass loss rates and surface composition changes are discussed in terms of the possible oxidation chemistry of the interaction. Finally, the question of how the harmful degradation of materials in low earth orbit can be minimized is addressed.

Ferguson, D. C.↗

Lunar sample 14425 - Characterization and resemblance to high-magnesium microtektites

Measurements by energy-dispersive X-ray analysis of the surface of lunar sample 14425, a large glass bead, yield a noritic composition enriched in aluminum and magnesium and, as compared with other norites, depleted in iron and especially calcium. The sample is close in composition to the most basic microtektites. Spherical inclusions of nickel-iron, flattened where they protrude, are found to be enriched in sulfur and phosphorus, at least at the surface. The inclusions form approximately 1 percent of the volume.

Berliner, L.↗

RF-sputtered silicon and hafnium nitrides - Properties and adhesion to 440C stainless steel

Silicon nitride and hafnium nitride coatings were deposited by reactive RF sputtering on oxidized and unoxidized 440C stainless steel substrates. Sputtering was done in mixtures of argon and nitrogen gases from pressed powder silicon nitride and from hafnium metal targets. Depositions were at two background pressures, 8 and 20 mtorr, and at two different fractions (f) of nitrogen in argon, 0.25 and 0.60, for hafnium nitride and at f = 0.25 for silicon nitride. The coatings and the interface between the coating and substrates were investigated by X-ray diffractometry, scanning electron microscopy, energy dispersive X-ray analysis and Auger electron spectroscopy. A Knoop microhardness of 1650 + or 100 kg/sq mm was measured for hafnium nitride and 3900 + or 500 kg/sq mm for silicon nitride. The friction coefficients between a 440C rider and the coatings were measured under lubricated conditions. Scratch test results demonstrate that the adhesion of hafnium nitride to both oxidized and unoxidized 440C is superior to that of silicon nitride. Oxidized 440C is found to have increased adhesion, to both nitrides, over that of unoxidized 440C.

Grill, A.↗

Mapping the Structure of Heterogeneous Materials

Image-processing microdensitometer/Fourier analyzer yields statistics of subcomponent distribution. Nondestructive method for studying structure heterogeneous materials uses energy-dispersive X-ray analysis in scanning electron microscope. Scanning microdensitometer/Fourier analyzer (SMFA) is applied to SEM images to obtain statistics about sample structure. Method originally developed for studying effect on combustion of fine structure of composite solid propellants.

Strand, L. D.↗

Oxidation and emittance of superalloys in heat shield applications

Recently developed superalloys that form alumina coatings have a high potential for heat shield applications for advanced aerospace vehicles at temperatures above 1095C. Both INCOLOY alloy MA 956 (of the Inco Alloys International, Inc.), an iron-base oxide-dispersion-strengthened alloy, and CABOT alloy No. 214 (of the Cabot Corporation), an alumina-forming nickel-chromium alloy, have good oxidation resistance and good elevated temperature strength. The oxidation resistance of both alloys has been attributed to the formation of a thin alumina layer (alpha-Al2O3) at the surface. Emittance and oxidation data were obtained for simulated Space Shuttle reentry conditions using a hypersonic arc-heated wind tunnel. The surface oxides and substrate alloys were characterized using X-ray diffraction and scanning and transmission electron microscopy with an energy-dispersive X-ray analysis unit. The mass loss and emittance characteristics of the two alloys are discussed.

Wiedemann, K. E.↗

Aluminum oxide barriers in MCrAlY superalloy systems

An investigation was made of sputtered aluminum oxide diffusion barriers to protect gas turbine engine blade and vane alloys from their coatings. MAR M200 + Hf coated with sputtered NiCoCrAlY and MAR M509 coated with sputtered FeCrAlY were obtained both with and without 1 and 2 micron sputtered Al2O3 barrier layers. Electron dispersive X-ray analysis was used to determine the concentration profiles of as-received and heat treated samples.

Kreider, Kenneth G.↗

In-situ integrated processing and characterization of thin films of high temperature superconductors, dielectrics and semiconductors by MOCVD

In this strategy of depositing the basic building blocks of superconductors, semiconductors, and dielectric having common elements, researchers deposited superconducting films of Y-Ba-Cu-O, semiconductor films of Cu2O, and dielectric films of BaF2 and Y2O3 by metal oxide chemical vapor deposition (MOCVD). By switching source materials entering the chamber, and by using direct writting capability, complex device structures like three-terminal hybrid semiconductors/superconductors transistors can be fabricated. The Y-Ba-Cu-O superconducting thin films on BaF2/YSZ substrates show a T(sub c) of 80 K and are textured with most of the grains having their c-axis or a-axis perpendicular to the substrate. Electrical characteristics as well as structural characteristics of superconductors and related materials obtained by x-ray defraction, electron microscopy, and energy dispersive x-ray analysis are discussed.

Singh, R.↗

Surface composition of solid-rocket exhausted aluminum oxide particles

Particulate samples of aluminum oxide were collected on Teflon filters from the exhaust plume of the Space Shuttle (STS-61A, October 30, 1985) over the altitude interval 4.6-7.6 km immediately after launch. These particles were analyzed using SEM, energy-dispersive X-ray analysis, electron spectroscopy for chemical analysis, X-ray fluorescent spectroscopy, and conventional wet-chemical techniques. The samples were 0.6-1.0 percent surface-chlorided (chlorided meaning predominantly aluminum chlorides and oxychlorides, possibly including other adsorbed forms of chloride) by weight. This level of chloriding is about one-third of the amount determined previously from laboratory-prepared alumina and surface site samples of solid-rocket-produced alumina (SRPA) after both had been exposed to moist HCl vapor at temperatures down to ambient. This level is equivalent to previous laboratory results with samples exposed to moist HCl at temperatures above the boiling point of water. It is suggested that the present lower chloriding levels, determined for samples from a 'dry' Shuttle exhaust cloud, underscore the importance of a liquid water/hydrochloric acid phase in governing the extent of surface chloriding of SRPA. The reduced chloriding is not trivial with respect to potential physical/chemical modification of the SRPA particle surfaces and their corresponding interaction with the atmosphere.

Cofer, Wesley R., III↗