Search NASA⌕ Search

SEARCH · Search NASA

Results for “interdiffusion”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 379 records · Page 21

Two types of diffusions at the cathode/electrolyte interface in IT-SOFCs

Analytical transmission electron microscopy, in particular with the combination of energy dispersive X-ray spectroscopy (EDX) and electron energy-loss spectroscopy (EELS), has been performed to investigate the microstructure and microchemistry of the interfacial region between the cathode (La{sub 0.6}Sr{sub 0.4}Co{sub 0.8}Fe{sub 0.2}O{sub 3}, LSCF) and the electrolyte (Gd-doped ceria, GDC). Two types of diffusions, mutual diffusion between cathode and electrolyte as well as the diffusion along grain boundaries, have been clarified. These diffusions suggest that the chemical stability of LSCF and GDC are not as good as previously reported. The results are more noteworthy if we take into consideration the fact that such interdiffusions occur even during the sintering process of cell preparation. - Graphical Abstract: Two types of diffusions, the mutual diffusion and the diffusion along grain boundaries, occurred at the cathode/electrolyte interface of intermediate temperature solid state fuel cells, during cell preparation. The mutual diffusion is denoted by black arrows and the diffusion along grain boundaries assigned by pink arrows. Highlights: > All the cations in cathode (LSCF) and electrolyte (GDC) can mutually diffuse into each other. > Diffusing elements will segregate at grain boundaries or triple junctions around the cathode/electrolyte interface. > Two types of diffusions, the mutual diffusion and diffusion along grain boundaries, have been clarified thereafter.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

The Role of Electron and Atom Probe Tomography in Characterization of Nuclear Fuels

Dramatic advances in materials characterization capabilities over the last few years enabled microstructural and chemical 3D characterization of specimens at the atomic-scale with unprecedented quantitative precision and high data collection rates. These improvements allow for the transition of electron tomography (ET) and atom probe tomography (APT) techniques to a much broader research field and their implementation in the characterization of nuclear fuels and highly radioactive materials. Nanoscale characterization has been widely developed for non-nuclear applications, yet in the nuclear arena, particularly for fuels, these modern characterization techniques have not been applied in concert to elucidate fundamental material behavior in metal fuel. In this work, we present cross-correlated APT and ET data and provide atomic-scale representations of microstructure and chemistry of nuclear fuels, which is essential in the validation of current and future atomistic and meso-scale modeling efforts. A firm understanding of microstructural evolution in reactor materials is imperative and will lead to deeper understanding of in-reactor degradation behavior, creating a new generation of radiation-resistant materials and fuels with the potential for significant increases in burn-up. In summary, two complementary techniques were used to characterize phases formed as a result of interdiffusion between U-Pu-Zr metal fuel and cladding and fission gas bubbles produced in U-Mo fuel upon irradiation. Understanding in-reactor degradation behavior of these materials is critical to advancing nuclear energy technology. (authors)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

TEM Characterization of U-Mo Irradiated with High-Energy Xe Ions

U-Mo alloys (with 7-10 wt.% Mo) with a low U-235 enrichment (< 20%) have been developed to be used in high-performance research and test reactors, replacing the current highly enriched uranium (HEU) fuels. A number of in-pile irradiation tests of U-Mo fuels show that drastic microstructural changes occurred during reactor irradiation, including the formation of U-Mo-Al interaction products and large gas-filled pores. These microstructural changes might lead to breakaway swelling and deterioration of plate mechanical integrity. Hence, it is critical to understand the underlying mechanisms of these microstructural changes in order to improve the irradiation behavior of UMo fuels. Heavy ion irradiation was employed in this study to investigate separate effects of the irradiation behavior of U-Mo fuels. 1.7 mm diameter disks punched out from UMo/ Al dispersion fuel mini-plates were irradiated with 84 MeV Xe ions at the ATLAS accelerator at Argonne National Laboratory (ANL). This particular ion source was selected for two reasons: (1) to simulate the irradiation response of the fuel to fission fragment bombardments, and (2) to study fission gas behavior, as fission gas bubble formation and growth is the primary cause of U-Mo fuel swelling. The ion-irradiated samples have been characterized with scanning electron microscopy (SEM). This study focuses on the characterization of the samples using transmission electron microscopy (TEM). With the high magnification details, microstructures in U-Mo along the ion penetration depth were revealed. The U-7Mo/Al dispersion fuel sample irradiated with 84 MeV Xe ions to a dose of 2.9 x 10{sup 17} ions/cm{sup 3} was characterized using TEM. The TEM results exhibit that the sample microstructure varies along the ion penetration depth. Near the sample surface (zone A) is a layer of nano-crystalline U-Mo-Al interdiffusion product. After passing through zone A, the Xe ions resided in zone B, where gas bubbles formed in U-Mo. TEM images of this region displayed that large gas bubbles formed on grain boundaries and high-density nano-bubbles lay inside grains. The random distribution of intragranular bubbles indicates that the irradiation conditions of this sample cannot lead to gas bubble superlattice formation. Outside of the Xe penetration depth (zone C), significant amount of α-uranium precipitates were identified. The fact that no α-uranium precipitates were found in zone B suggests that the dose rate in this irradiation is sufficient to facilitate a phase reversal by means of a displacement spike mechanism. (authors)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Effect of Interaction Layer and U-Mo Size on Pore Growth in U-Mo/Al Fuel

U-Mo/Al dispersion fuel, composed of U-Mo alloy fuel particles embedded in the aluminum (Al) matrix, has been developed to convert high-enriched uranium fuel to low-enriched uranium for high-performance research reactors. The fueled zone, referred to as 'fuel meat,' is clad with aluminum alloy. Fuel meat and cladding are metallurgically bonded during fabrication. Irradiated U-Mo/Al dispersion fuel has shown stable performance in low fission rate and burnup ranges. However, excessive fuel meat swelling or breakaway swelling, which is believed an incipient failure, was observed at higher fission rate and burnup conditions. This breakaway swelling is believed to be a result from the combination of accelerated fuel swelling and interconnection of large pores formed outside of the UMo particles. These large pores were frequently found, particularly, at the interface between the Al and the fuel-matrix interaction layer (IL) that formed by irradiation-enhanced interdiffusion of U-Mo and Al. Kim et al. developed a model for pore growth using a mechanical equilibrium between gas pressure in the pore, interfacial energies, and the external stress at the pore surface. In this model, IL provides a path way for fission gas to reach the pores and also generates tensile stress fields. Hence, suppressing IL growth by applying a diffusion barrier, like a coating of the U-Mo particles, appears to be an effective method to prevent pore formation. Another remedy to prevent pore formation is to use large U-Mo fuel particles. Using larger U-Mo particles was thought advantageous because it reduces fission gas release. In this study, the effect of IL growth and U-Mo particle size on pore formation is examined using the model. The advantage was quantified in terms of porosity.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Oxide-nitride heteroepitaxy for low-loss dielectrics in superconducting quantum circuits

Superconducting qubits show great promise for the realization of fault-tolerant quantum computing, but lossy, amorphous dielectrics limit current technology. Identifying highly crystalline and stoichiometric dielectrics with intrinsically low microwave loss is therefore a central materials challenge, yet experimentally validated platforms remain scarce. In this work, we integrate a crystalline dielectric into a heteroepitaxial TiN/$γ$-Al$_2$O$_3$/TiN trilayer grown via pulsed laser deposition. Correlative high-resolution imaging, diffraction, and spectroscopy measurements confirm the single-crystal quality and chemical integrity of all layers, with minimal defects and limited anion interdiffusion across the oxide-nitride interfaces. Using microwave lumped-element resonators with parallel-plate capacitors, we report the first direct measurement of the dielectric loss of epitaxial $γ$-Al$_2$O$_3$, for which we find a low intrinsic two-level system loss, $δ_{\text{TLS}}^0 = (2.8 \pm 0.1) \times 10^{-5}$. These results establish heteroepitaxial oxides on transition metal nitrides as an attractive materials platform for superconducting quantum circuits, particularly for integration into compact device architectures such as merged-element transmons and microwave kinetic inductance detectors.

Garcia-Wetten, David A. [Northwestern U.]↗

Liquid-liquid interfaces of semifluorinated alkane diblock copolymers with water, alkanes, and perfluorinated alkanes.

The liquid-liquid interface between semifluorinated alkane diblock copolymers of the form F3C(CF2)n-1-(CH2)m-1CH3 and water, protonated alkanes, and perfluorinated alkanes are studied by fully atomistic molecular dynamics simulations. A modified version of the OPLS-AA (Optimized Parameter for Liquid Simulation All-Atom) force field of Jorgensen et al. has been used to study the interfacial behavior of semifluorinated diblocks. Aqueous interfaces are found to be sharp, with correspondingly large values of the interfacial tension. Due to the reduced hydrophobicity of the protonated block compared to the fluorinated block, hydrogen enhancement is observed at the interface. Water dipoles in the interfacial region are found to be oriented nearly parallel to the liquid-liquid interface. A number of protonated alkanes and perfluorinated alkanes are found to be mutually miscible with the semifluorinated diblocks. For these liquids, interdiffusion follows the expected Fickian behavior, and concentration-dependent diffusivities are determined.

08 HYDROGEN↗

Development of membranes for hydrogen separation: Pd-coated V-10Pd

Numerous Group IVB and VB alloys were prepared and tested as potential membrane materials but most of these materials were brittle or exhibited cracking during hydrogen exposure. One of the more ductile alloys, V-10Pd (at. %), was fabricated into a thin (107-{micro}m thick) composite membrane coated with 100 nm of Pd on each side. The material was tested for hydrogen permeability, resistance to hydrogen embrittlement, and long term hydrogen flux stability. The hydrogen permeability, {phi}, of the V-10Pd membrane was 3.86 x 10{sup -8} mol H{sub 2} m{sup -1} s{sup -1} Pa{sup -0.5} (avg. of three different samples) at 400 C, which is slightly higher than the permeability of Pd-23Ag at that temperature. A 1400 h hydrogen flux test at 400 C demonstrated that the rate of metallic interdiffusion was slow between the V-10Pd foil and the 100-nm-thick Pd coating on the surface. However, at the end of testing the membrane cracked at 118 C because of hydrogen embrittlement.

08 HYDROGEN↗

Performance of Al-Rich Oxidation Resistant Coatings for Fe-Base Alloys

Aluminum-rich coatings made by chemical vapor deposition and pack cementation on ferritic (e.g. Fe-9Cr-1Mo) and austenitic (Type 304L) substrates are being evaluated at 650-800 C. For oxidation testing, a humid air environment was used to quantify coating performance, as uncoated substrates experience rapid oxidation at these temperatures. A main goal of this work is to demonstrate the potential benefits and problems with alumina-forming coatings. The higher exposure temperatures were selected to accelerate the degradation of the coating by interdiffusion with the substrate. A general conclusion of this testing was that coatings with less Al and a ferritic Fe(Al) structure could be more durable than higher Al content aluminide coatings which have a large thermal expansion mismatch with these substrates. A lifetime model has been developed using diffusion and oxidation observations to predict coating performance as a function of temperature and initial coating composition. To test and improve the model, additional experiments are now being conducted to determine the effect of substrate composition (e.g. Cr content using Fe-12Cr and Fe-9Cr-2W substrates) and exposure temperature on the critical Al content for coating failure. Because of the unexpectedly low level of Al measured at coating failure ({approx}3.5at.% at 700 C), exposures of specimens with thick ({approx}200 {micro}m) high Al content coatings were stopped after 10kh at 800 C and 20kh at 700 C because extremely long times to failure were predicted. Post-exposure Al concentration profiles for these specimens were measured using electron microprobe.

36 MATERIALS SCIENCE↗

Performance of Al-Rich Oxidation Resistant Coatings For Fe-Base Alloys

Aluminum-rich coatings made by chemical vapor deposition and pack cementation on ferritic (e.g. Fe-9Cr-1Mo) and austenitic (Type 304L) substrates are being evaluated at 650-800 C. For oxidation testing, a humid air environment was used to quantify coating performance, as uncoated substrates experience rapid oxidation at these temperatures. A main goal of this work is to demonstrate the potential benefits and problems with alumina-forming coatings. The higher exposure temperatures were selected to accelerate the degradation of the coating by interdiffusion with the substrate. A general conclusion of this testing was that coatings with less Al and a ferritic Fe(Al) structure could be more durable than higher Al content aluminide coatings which have a large thermal expansion mismatch with these substrates. A lifetime model has been developed using diffusion and oxidation observations to predict coating performance as a function of temperature and initial coating composition. To test and improve the model, additional experiments are now being conducted to determine the effect of substrate composition (e.g. Cr content using Fe-12Cr and Fe-9Cr-2W substrates) and exposure temperature on the critical Al content for coating failure. Because of the unexpectedly low level of Al measured at coating failure ({approx}3.5at.% at 700 C), exposures of specimens with thick ({approx}200 {mu}m) high Al content coatings were stopped after 10kh at 800 C and 20kh at 700 C because extremely long times to failure were predicted. Post-exposure Al concentration profiles for these specimens were measured using electron microprobe.

36 MATERIALS SCIENCE↗

Modeling in High Temperature Corrosion: A Review and Outlook

Realizing higher operating temperatures to increase efficiency of future applications for energy conversion and storage while minimizing cost is a challenge for development of high-temperature materials. Simultaneous optimization of mechanical properties and corrosion resistance continues to be a difficult task but is essential due to the need to significantly accelerate the transition between technology readiness levels in the future. Furthermore, oxidation-induced degradation will be a critical life-limiting mechanism at increased operating temperatures. Suitable high-temperature materials cannot be solely identified by time-consuming experiments and reliable computational methods incorporating the relevant physics of processes must be considered to complement the experimental efforts. In the present work, a review of the methods employed to model oxidation-induced material degradation described in literature will be discussed. Furthermore, their capability to predict lifetime and aid in material selection will be evaluated.

36 MATERIALS SCIENCE↗

Diffusional Interaction between U-10 wt.% Zr and Fe at 903K, 923K and 953K (630°C, 650°C, and 680°C)

U-Zr metallic fuels cladded in Fe-alloys are being considered for application in an advanced Sodium-Cooled Fast Reactor (SFR) that can recycle the U-Zr fuels and minimize the long-lived actinide waste. To understand the complex fuel-cladding chemical interaction between the U-Zr metallic fuel with Fe-alloys, a systematic multicomponent diffusion study was carried out using solid-to-solid diffusion couples. The U-10 wt.% Zr vs. pure Fe diffusion couples were assembled and annealed at temperatures, 903, 923 and 953K for 96 hours. Development of microstructure, phase constituents, and compositions developed during the thermal anneals were examined by scanning electron microscopy, transmission electron microscopy and X-ray energy dispersive spectroscopy. Complex microstructure consisting of several layers that include phases such as U 6 Fe, UFe 2 , ZrFe 2 , α-U, β-U, Zr-precipitates, Χ, ε and λ were observed. Multi-phase layers were grouped based on phase constituents and microstructure, and the layer thicknesses were measured to calculate the growth constant and activation energy. The local average compositions through the interaction layer were systematically determined, and employed to construct semi-quantitative diffusion paths on isothermal U-Zr-Fe ternary phase diagrams at respective temperatures. The diffusion paths were examined to qualitatively estimate the diffusional behavior of individual components and their interactions. Furthermore, selected area diffraction analyses were carried out to determine, for the first time, the exact crystal structure and composition of Χ, ε and λ-phases. The Χ, ε and λ-phases were identified as Pnma(62) Fe(Zr,U), I4/mcm(140) Fe(Zr,U) 2 , and I4/mcm(140) U 3 (Zr,Fe), respectively.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Simulating the effect of aluminizing on a CoNiCrAlY-coated Ni-base superalloy

MCrAlY (M = Ni, Co) coatings are commonly used on gas-turbine components as oxidation resistant overlay coatings and bondcoats for thermal barrier systems. Here, we focus on the effect of the aluminizing process on the CoNiCrAlY coating microstructure. In the as-received condition the outer part of the coating consisted mostly of β-(Ni,Co)Al with interspersed precipitates of Cr-rich carbide and Cr-rich boride precipitates. Formation of σ-CoCr was observed at the interface between the β-layer and the inner initial CoNiCrAlY microstructure. Scanning electron microscopy (SEM) combined with energy and wavelength-dispersive X-ray spectroscopy (EDX/WDX) was employed to characterize the aluminized CoNiCrAlY coating. Phases were then identified by electron backscatter diffraction (EBSD). Detailed microstructural studies of the coating were corroborated with the help of coupled thermodynamic-kinetic calculations to model the aluminizing process. The calculations were performed with the in-house developed code employing the commercially available thermodynamic and kinetic databases (ThermoCalc). The mechanisms of the observed microstructural changes were elucidated with the help of the modelling donclusions.

36 MATERIALS SCIENCE↗

Evaluating the efficacy of aluminide coatings to improve oxidation resistance of high performance engine valve alloys

Increasing peak cylinder pressures and operating temperatures of turbo-charged internal combustion engines (ICEs) engines present new challenges for existing materials employed in engine exhaust valves. Oxidation induced degradation of current Ni based alloys for these components will be a life-limiting mechanism while strict cost margins in the automotive transportation industry further limit the choice of suitable candidate materials. Metallic diffusion aluminide coatings can provide a cost-effective way to improve the oxidation resistance of underlying materials. In this study, the high temperature oxidation behavior of diffusion nickel aluminide coatings on two Ni based alloys (commercially available alloy 31V and a developmental alloy) during cyclic oxidation behavior in air+10% H 2 O at 900 °C was investigated. A complete depletion of the beneficial Al-rich β-(NiFe)Al phase was observed in the coating on alloy 31V while a significant fraction of this phase was retained in the coating on the second alloy. A coupled thermodynamic-kinetic model showed that the disappearance of the Al-rich phase in the coating on 31V was mainly due to the combined effect of steeper chemical potential gradients of Al and Ti between the coating and the substrate and their faster diffusivities compared to the coated developmental alloy. Finally, a higher content of Fe was shown to support the retention of β-(NiFe)Al phase in the coating on the developmental alloy while the presence of Ti in the alloy was shown to be detrimental for long-term coating performance.

36 MATERIALS SCIENCE↗

Solid-State Ionic Rectification in Perovskite Nanowire Heterostructures

Halide perovskites have attracted increasing research attention with regard to their potential for optoelectronic applications. Because of its low activation energy, ion migration is implicated in the long-term stability and many unusual transport behaviors of halide perovskite devices. However, direct observation and precise control of the ionic transport in halide perovskite crystals remain challenging. Here, we have designed an axial CsPbBr 3 -CsPbCl 3 nanowire heterostructure, in which electric-field-induced halide ion migration was clearly visualized and quantified. We demonstrated that halide ion migration is dependent on the applied electric field and exhibits ionic rectification in this solid-state system, which is due to the nonuniform distribution of the ionic vacancies in the nanowire that results from a competition between electrical screening and their creation/destruction at the electrodes' interfaces. Furthermore, the asymmetric heterostructure characteristics add an additional knob to control the ion movement in the design of advanced ionic circuits with halide perovskites as building blocks.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Exchange of Ions across the TiN/TaO x Interface during Electroformation of TaO x -Based Resistive Switching Devices

The valence change model describes the resistive switching in metal oxide-based devices as due to electroreduction of the oxide and subsequent electromigration of oxygen vacancies. Here, we present cross-sectional X-ray energy-dispersive spectroscopy elemental maps of Ta, O, N, and Ti in electroformed TiN/TaO 2.0 /TiN structures. O, N, and Ti were exchanged between the anode and the functional oxide in devices formed at high power (~1 mW), but the exchange was below the detection limit at low power (<0.5 mW). All structures exhibit a similar Ta-enriched and O-depleted filament formed by the elemental segregation in the functional oxide by the temperature gradient. The elemental interchange is interpreted as due to Fick’s diffusion caused by high temperatures in the gap of the filament and is not an essential part of electroformation.

36 MATERIALS SCIENCE↗

Understanding the Solid-State Electrode–Electrolyte Interface of a Model System Using First-Principles Statistical Mechanics and Thin-Film X-ray Characterization

Intermixing of atomic species at the electrode-electrolyte boundaries can impact the properties of the interfaces in solid-state batteries. Herein, this work uses first-principles statistical mechanics along with experimental characterization to understand intermixing at the electrode-electrolyte interface. For the model presented in this work, lithium manganese oxide (LiMn 2 O 4 , LMO) and lithium lanthanum titanate (Li 3x La 2/3-x TiO 3 , LLTO) are employed as the cathode and electrolyte, respectively. The results of the computational work show that Ti-Mn intermixing at the interface is significant at synthesis temperatures. The experimental results in this work find that, at some critical temperatures between 600 and 700 degrees C for material preparation, the interface of LLTO-LMO becomes blurred. Calculations predict that the interface is unstable with regard to Ti-Mn intermixing starting at 0 K, suggesting that the critical temperature found in the experiment is related to kinetics. The work overall suggests that, in designing a solid-state battery, the fundamental reactions such as intermixing need to be considered.

25 ENERGY STORAGE↗

Cr/B{sub 4}C multilayer mirrors: Study of interfaces and X-ray reflectance

We present an experimental study of the effect of layer interfaces on the x-ray reflectance in Cr/B{sub 4}C multilayer interference coatings with layer thicknesses ranging from 0.7 nm to 5.4 nm. The multilayers were deposited by magnetron sputtering and by ion beam sputtering. Grazing incidence x-ray reflectometry, soft x-ray reflectometry, and transmission electron microscopy reveal asymmetric multilayer structures with a larger B{sub 4}C-on-Cr interface, which we modeled with a 1–1.5 nm thick interfacial layer. Reflectance measurements in the vicinity of the Cr L{sub 2,3} absorption edge demonstrate fine structure that is not predicted by simulations using the currently tabulated refractive index (optical constants) values for Cr.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗