Search NASA⌕ Search

SEARCH · Search NASA

Results for “STRESS CORROSION”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 397 records · Page 22

Effect of thermal aging on microstructure and crack growth response of Alloy 152 weld

Nickel-based Alloy 690 and the associated weld Alloys 52 and 152 are typically used for nozzle penetrations in replacement heads for pressurized water reactor (PWR) vessels, because of their excellent overall resistance to general corrosion and environmental degradation, primarily stress corrosion cracking (SCC). However, many of the existing PWRs are expected to operate for 40-80 years. Likewise, advanced water-cooled small modular reactors (SMRs) will use Ni-Cr alloys and are expected to receive initial operating licenses for 60 years. Hence, the thermal stability of Ni-Cr alloys is a potential concern for the long-term performance of both existing and advanced nuclear power plants, and possibly spent fuel storage containers. The objective of this research is to understand the microstructural changes occurring in high-Cr, Ni-based Alloy 152 weldments during long time exposure to the reactor operating temperatures, and the effect of these changes on the service performance. One area of particular concern is the potential for long range ordering (LRO), i.e. formation of the intermetallic Ni2Cr phase under prolonged exposure to reactor temperatures and/or irradiation, which can increase strength, decrease ductility, and cause dimensional changes or lead to in-service embrittlement of components made with these alloys. Hence, this research focused on the microstructural evolution and the SCC response of Alloy 152 under accelerated thermal aging. The materials studied involved three heats of Alloy 152 used to produce a dissimilar metal weld (DMW) joining an Alloy 690 plate to an Alloy 533 low alloy steel (LAS) plate, thermally aged at three different temperatures (370°C, 400°C and 450°C) for up to 75,000h (equivalent to 60 years of service). The microstructural characterization by means of synchrotron X-ray did not find evidence of LRO in any of the three heats aged to an equivalent of 60 years of service. Testing in a primary water environment of a heat of Alloy 152 aged at 370°C to a 60-year service equivalent revealed a fatigue and corrosion fatigue crack growth responses similar to those measured on the un-aged alloy. However, the SCC CGR response of the aged sample appears to show a deterioration in performance.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

The Effect of Thermal Aging on the Performance of High-Cr Ni-based Alloys in Primary Water Environment

Nickel-based Alloy 690, and the associated weld Alloys 52 and 152, are used for nozzle penetrations in replacement heads for pressurized water reactor (PWR) vessels. They are chosen for their excellent overall resistance to general corrosion and environmental degradation, primarily stress corrosion cracking (SCC). However, many of the existing PWRs are expected to operate beyond their first or second license renewal (e.g., 40 to 60 years or beyond 60 years). Hence, the thermal stability of Ni-Cr alloys is a potential concern for the long-term performance of both existing and advanced nuclear power plants. Moreover, Ni-Cr alloys are being considered for high-level radioactive waste disposal containers that will be required to contain the waste for at least 10,000 years.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Environmentally Assisted Cracking Research for Current and Advanced Nuclear Structural Materials

Understanding environmentally assisted cracking is an important aspect of nuclear materials research, as it provides information about failure mechanisms that lead to safety concerns or shutdowns. Idaho National Laboratory has ongoing research to understand how materials behave in the harsh nuclear environments for both the current fleet of light water reactors, as well as advanced reactors, where materials are exposed to more extreme environments. Corrosion and cracking of current materials, advanced materials, and materials formed through advanced manufacturing techniques are being examined, with particular interest in irradiation effects on corrosion and cracking, as well as the effects of environmental impurities. Testing, such as stress corrosion cracking, corrosion fatigue, and in-situ crack growth measurements, as well as a suite of characterization tools, including electron microscopy techniques and x-ray computed tomography, are being utilized to better understand the material response, limitations, and cracking mechanisms to ensure safe and reliable nuclear plants.

36 MATERIALS SCIENCE↗

Summary of available data for estimating chloride-induced SCC crack growth rates for 304/316 stainless steel.

The majority of existing dry storage systems used for spent nuclear fuel (SNF) consist of a welded 304 stainless steel container placed within a passively-ventilated concrete or steel overpack. More recently fielded systems are constructed with dual certified 304/304L and in some cases, 316 or 316L. In service, atmospheric salts, a portion of which will be chloride bearing, will be deposited on the surface of these containers. Initially, the stainless steel canister surface temperatures will be high (exceeding the boiling point of water in many cases) due to decay heat from the SNF. As the SNF cools over time, the container surface will also cool, and deposited salts will deliquesce to form potentially corrosive chloride-rich brines. Because austenitic stainless steels are prone to chloride-induced stress corrosion cracking (CISCC), the concern has been raised that SCC may significantly impact long-term canister performance. While the susceptibility of austenitic stainless steels to CISCC in the general sense is well known, the behavior of SCC cracks (i.e., initiation and propagation behavior) under the aforementioned atmospheric conditions is poorly understood.

36 MATERIALS SCIENCE↗

Review of NDE Methods for Detection and Monitoring of Atmospheric SCC in Welded Canisters for the Storage of Used Nuclear Fuel

Dry cask storage systems (DCSSs) for used nuclear fuel (UNF) were originally envisioned for storage periods of short duration (~ a few decades). However, uncertainty challenges the opening of a permanent repository for UNF implying that UNF will need to remain in dry storage for much longer durations than originally envisioned (possibly for centuries). Thus, aging degradation of DCSSs becomes an issue that may not have been sufficiently considered in the design phase and that can challenge the efficacy of very long-term storage of UNF. A particular aging degradation concern is atmospheric stress corrosion cracking (SCC) of DCSSs located in marine environments. In this report, several nondestructive (NDE) methods are evaluated with respect to their potential for effective monitoring of atmospheric SCC in welded canisters of DCSSs. Several of the methods are selected for evaluation based on their usage for in-service inspection applications in the nuclear power industry. The technologies considered include bulk ultrasonic techniques, acoustic emission, visual techniques, eddy current, and guided ultrasonic waves.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Waste Chemistry Envelope for the Determination of Pitting Corrosion Susceptibility - 19554

Liquid radioactive wastes at the Hanford and Savannah River sites are stored in large underground carbon steel tanks. The high-level wastes are processed in several of the tanks and then transferred by piping to other site facilities for further processing before they are stabilized in a vitrified or grout waste form. Based on waste removal and processing schedules, many of the tanks, will be required to be in service for times exceeding the initial intended life (i.e., greater than 60 years). Until the waste is removed from storage, transferred, and processed, the materials and structures of the tanks must maintain a confinement function by providing a barrier to the environment and by maintaining acceptable structural stability during design basis events, which include loadings from both normal service and abnormal (e.g., earthquake) conditions. Administrative programs are in place to mitigate potential corrosion mechanisms and thereby maintain the structural and leak integrity functions of these waste tanks throughout their intended service life. Waste chemistry and temperature control are the means by which corrosion degradation of the waste tanks is minimized. Chemistry controls are based on in-situ coupon tests, waste tank experience, and laboratory testing. These requirements comprise the technical standards for corrosion control. The standards are utilized then as guidelines for operational procedures. The present waste chemistry controls for the Hanford DSTs were established in the 1980's in response to tank failures caused by stress corrosion cracking (SCC) at the DOE Savannah River Site (SRS). Portions of the SRS chemistry limits, which were developed at the Savannah River National Laboratory (SRNL) were coupled with corrosion testing results from Pacific Northwest National Laboratories (PNNL) and adopted for corrosion control of the double-shell tank (DST) waste at the Hanford Site. Since that time, the temperatures of the waste in the DSTs have decreased to less than 50 deg. C in most cases as the radioactive material has decayed. As a consequence, new chemistry controls were formulated for SCC in 2010. This testing however, did not address that potential for pitting in the supernatant and at the liquid-air interface. Indeed, initial tests indicated that the inhibitor requirements for SCC would be insufficient for the prevention of pitting. In addition to lower waste temperatures, future retrieval and process changes may impact the DST waste chemistry. Initial projections suggest that the waste chemistry of the DSTs may shift to a broader range of pH and higher aggressive anion concentrations (e.g., chloride, sulfate, etc.) than the wastes that are presently stored. Additionally, processes within the vitrification facility may result in streams that are returned to the tank farm for evaporation. These streams may also contain high concentrations of aggressive species. SRNL investigated the propensity for pitting of the carbon steel waste tanks at current and projected DST waste chemistries. A statistically designed series of tests provided a pitting factor that relates the ratio of the inhibitor species to the aggressive species and the probability of observing pitting. An acceptable pitting factor was determined and was utilized for the development of a new chemistry envelope. The new chemistry envelope was compared to the envelope that was established for SCC and was determined to be bounding. Validation of the new chemistry envelope was performed via model simulations and comparison with historical experimental results and approaches to establishing chemistry envelopes. The new chemistry envelope will eventually be part of an overall assessment of the condition of the tanks and any changes made to the overall structural integrity program for the Hanford DSTs. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

On residual stress analysis and microstructural evolution for stainless steel type 304 spent nuclear fuel canisters weld joint: Numerical and experimental studies

Chloride-induced stress corrosion cracking (CISCC) in the weldments of austenitic stainless steel canisters is one of the primary safety concerns during the dry storage of used nuclear fuel at Independent Spent Fuel Storage Installations in coastal areas. In order to evaluate the CISCC behavior in the canister, a 3D sequentially coupled thermo-mechanical finite element model was built to simulate the residual stresses induced by two intersecting longitudinal and circumferential multi-pass welds in austenitic stainless steel mockup canister. Weld-induced residual stresses from simulation were in good agreement with the experimental measurement results by deep-hole drilling and contour methods. Through-wall high tensile axial and hoop stresses were observed in both the fusion zone and heat affected zone (HAZ) in the longitudinal and circumferential weld, respectively. On the other hand, the microstructure within the weldments of 304 stainless steel mockup was characterized using optical microscopy, scanning electron microscopy, electron back-scattered diffraction and energy dispersive X-ray spectroscopy methods. A few amount of MnS inclusions in both the base metal and HAZ, and a lot of (Mn,Si) x O y inclusions in the fusion zone were found. Meanwhile, there is some α'-martensite in the base metal, while the martensite was reversed in the HAZ. In the fusion zone, there is a lot of δ-ferrite. The martensite reversion phenomenon was also verified by the combination of Feritscope test and thermal simulation, which could predict a martensite reversion temperature as 400C°. The welding residual stresses and microstructure analysis results could offer the instructive information for the prediction of CISCC behavior of the spent nuclear fuel canisters.

36 MATERIALS SCIENCE↗

The Effect of Weld Residual Stress on Life of Used Nuclear Fuel Dry Storage Canisters

With the elimination of Yucca Mountain as the long-term storage facility for spent nuclear fuel in the United States, a number of other storage options are being explored. Currently, used fuel is stored in dry-storage cask systems constructed of steel and concrete. It is likely that used fuel will continue to be stored at existing open-air storage sites for up to 100 years. This raises the possibility that the storage casks will be exposed to a salt-containing environment for the duration of their time in interim storage. Austenitic stainless steels, which are used to construct the canisters, are susceptible to stress corrosion cracking (SCC) in chloride-containing environments if a continuous aqueous film can be maintained on the surface and the material is under stress. Because steel sensitization in the canister welds is typically avoided by avoiding post-weld heat treatments, high residual stresses are present in the welds. While the environment history will play a key role in establishing the chemical conditions for cracking, weld residual stresses will have a strong influence on both crack initiation and propagation. It is often assumed for modeling purposes that weld residual stresses are tensile, high and constant through the weld. However, due to the strong dependence of crack growth rate on stress, this assumption may be overly conservative. In particular, the residual stresses become negative (compressive) at certain points in the weld. The ultimate goal of this research project is to develop a probabilistic model with quantified uncertainties for SCC failure in the dry storage casks. In this paper, the results of a study of the residual stresses, and their postulated effects on SCC behavior, in actual canister welds are presented. Progress on the development of the model is reported.

36 MATERIALS SCIENCE↗

Out-of-reactor test of corrosion and hydrogen pickup in fuel cladding materials in contact with nickel metal - 2016-0038

Increased reactor coolant hydrogen concentration in pressurized water reactors (PWRs) is under consideration for potential benefits in reducing primary water stress corrosion cracking (PWSCC) crack growth rate as well as increasing PWSCC crack initiation time in nickel-based alloys. Potential concerns related to fuel performance include possible increases in hydrogen pickup (HPU) by zirconium based alloys and the enhancement of the pickup through the so-called nickel-window effect. Although the risk of this occurrence may be low, the consequences of increased HPU could be substantial. We examined the impact of dissolved hydrogen (DH) concentrations on Zircaloy-4 corrosion and HPU when the samples are in contact with nickel sources. The work was completed in conjunction with a large project that evaluated the impact of dissolved hydrogen on various fuel cladding and spacer weld specimens of M5{sup R}, ZIRLO{sup R}, Optimized ZIRLO{sup TM}, Low-Tin ZIRLO{sup TM}, Optimized Low-Tin Zircaloy-4, and Zircaloy-2 in either as-received or pre-oxidized conditions for exposures up to 730 days in high-pressure, out-of-reactor autoclave systems operating with a simulated PWR coolant at three different DH concentrations: 30, 100, and 500 cm{sup 3} (cc) H{sub 2}/kg H{sub 2}O. A significant increase in HPU was observed for some Zircaloy-4 specimens in contact with synthetic crud at elevated DH levels. The HPU increased with increasing DH and a metallic nickel fraction in the synthetic crud. The formation of metallic nickel in the synthetic crud samples at elevated DH levels was confirmed. (authors)

36 MATERIALS SCIENCE↗

Corrosion in low dielectric constant Si-O based thin films: Buffer concentration effects

Organosilicate glass (OSG) is often used as an interlayer dielectric (ILD) in high performance integrated circuits. OSG is a brittle material and prone to stress-corrosion cracking reminiscent of that observed in bulk glasses. Of particular concern are chemical-mechanical planarization techniques and wet cleans involving solvents commonly encountered in microelectronics fabrication where the organosilicate film is exposed to aqueous environments. Previous work has focused on the effect of pH, surfactant, and peroxide concentration on the subcritical crack growth of these films. However, little or no attention has focused on the effect of the conjugate acid/base concentration in a buffer. Accordingly, this work examines the “strength” of the buffer solution in both acidic and basic environments. The concentration of the buffer components is varied keeping the ratio of acid/base and therefore pH constant. In addition, the pH was varied by altering the acid/base ratio to ascertain any additional effect of pH. Corrosion tests were conducted with double-cantilever beam fracture mechanics specimens and fracture paths were verified with ATR-FTIR. Shifts in the threshold fracture energy, the lowest energy required for bond rupture in the given environment, G{sub TH}, were found to shift to lower values as the concentration of the base in the buffer increased. This effect was found to be much larger than the effect of the hydroxide ion concentration in unbuffered solutions. The results are rationalized in terms of the salient chemical bond breaking process occurring at the crack tip and modeled in terms of the chemical potential of the reactive species.

36 MATERIALS SCIENCE↗

PROBABILITY BASED CORROSION CONTROL FOR WASTE TANKS - PART II

As part of an ongoing study to evaluate the discontinuity in the corrosion controls at the SRS tank farm, a study was conducted this year to assess the minimum concentrations below 1 molar nitrate, see Figure 1. Current controls on the tank farm solution chemistry are in place to prevent the initiation and propagation of pitting and stress corrosion cracking in the primary steel waste tanks. The controls are based upon a series of experiments performed with simulated solutions on materials used for construction of the tanks, namely ASTM A537 carbon steel (A537). During FY09, an experimental program was undertaken to investigate the risk associated with reducing the minimum molar nitrite concentration required to confidently inhibit pitting in dilute solutions (i.e., less than 1 molar nitrate). The experimental results and conclusions herein provide a statistical basis to quantify the probability of pitting for the tank wall exposed to various solutions with dilute concentrations of nitrate and nitrite. Understanding the probability for pitting will allow the facility to make tank-specific risk-based decisions for chemistry control. Based on previous electrochemical testing, a statistical test matrix was developed to refine and solidify the application of the statistical mixture/amount model to corrosion of A537 steel. A mixture/amount model was identified based on statistical analysis of recent and historically collected electrochemical data. This model provides a more complex relationship between the nitrate and nitrite concentrations and the probability of pitting than is represented by the model underlying the current chemistry control program, and its use may provide a technical basis for the utilization of less nitrite to inhibit pitting at concentrations below 1 molar nitrate. FY09 results fit within the mixture/amount model, and further refine the nitrate regime in which the model is applicable. The combination of visual observations and cyclic potentiodynamic polarization scans indicates a potential for significant inhibitor reductions at nitrate concentrations near 1.0 M without a significant increase in corrosion risk. The complete data sets from FY08 and FY09 testing have determined the statistical basis to confidently inhibit against pitting using nitrite inhibition with the current pH controls. Future testing will complete the spectrum of nitrate concentrations around 1 molar. These results will be combined to provide a complete spectrum for corrosion controls with a risk based component.

36 MATERIALS SCIENCE↗

MECHANISTIC UNDERSTANDING OF CAUSTIC CRACKING OF CARBON STEELS

Liquid waste generated by the PUREX process for separation of nuclear materials is concentrated and stored in Type IV single-shell carbon steel tanks at the Savannah River Site (SRS). The Type IV tanks for this waste do not have cooling coils and have not undergone heat treatment to stress-relieve the tanks. After the waste is concentrated by evaporation, it becomes very alkaline and can cause stress corrosion cracking (SCC) and pitting corrosion of the tank materials. SRS has experienced leakage from non-stress-relieved waste tanks constructed of A285 carbon steel and pitting of A212 carbon steel tanks in the vapor space. An investigation of tank materials has been undertaken at SRS to develop a basic understanding of caustic SCC of A285 and A212 grade carbon steels exposed to aqueous solutions, primarily containing sodium hydroxide (NaOH), sodium nitrate (NaNO{sub 3}), and sodium nitrite (NaNO{sub 2}) at temperatures relevant to the operating conditions of both the F and H area plants. This report presents the results of this corrosion testing program. Electrochemical tests were designed using unstressed coupons in a simulated tank environment. The purpose of this testing was to determine the corrosion susceptibility of the tank materials as a function of chemical concentration, pH, and temperature. A285 and A516 (simulates A212 carbon steel) coupons were used to investigate differences in the corrosion of these carbon steels. Electrochemical testing included measurement of the corrosion potential and polarization resistance as well as cyclic potentiodynamic polarization (CPP) testing of coupons. From the CPP experiments, corrosion characteristics were determined including: corrosion potential (E{sub corr}), pitting or breakdown potential (E{sub pit}), and repassivation potential (E{sub prot}). CPP results showed no indications of localized corrosion, such as pitting, and all samples showed the formation of a stable passive layer as evidenced by the positive hysteresis during the scan. Analysis of the CPP data was performed to compare the corrosion susceptibility of the samples under different environmental conditions. Test results indicated that the most important factors affecting corrosion of the steel are the solution temperature, hydroxide concentration, and the material used in constructing the tanks. Variables that did not significantly affect the corrosion susceptibility of the steel were the nitrate or nitrite concentration and the atmosphere in the tank. The passivation current of the coupons increased exponentially with temperature. Longer-term studies of the passivation current are suggested based on results from the literature for iron in highly caustic environments. Polarization resistance studies showed a significant increase in corrosion rate at 125 C and 12 M hydroxide concentration when compared with tests at lower temperatures and lower hydroxide concentrations. Within the temperature and pH range of these tests, iron oxide, Fe{sub 3}O{sub 4}, becomes unstable and could account for the increased corrosion susceptibility. The applicability of these conditions should be confirmed and detailed surface studies should be conducted to determine the corrosion resistance of A285 and A516 carbon steels under these conditions. Surface science studies should also be conducted to determine the role of the carbon steel composition in preventing corrosion under these conditions.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Effect of Retrogression Heat Treatment Time on Microstructure and Mechanical Properties of AA7010

The effect of retrogression time during retrogression and re-aging (RRA) treatment of AA7010 is evaluated by performing tensile tests and characterizing the microchemistry of the grain boundary precipitates (GBPs) using transmission electron microscope coupled with the energy-dispersive spectroscopy. Retrogression time is evaluated so that the ultimate tensile strength of the RRA-treated sample is equal to that of the T6-treated sample and the grain boundary microstructure similar to that of the over-aged (T7451) condition. The investigation reveals that the sample retrogressed at 200 °C for 20 min has UTS of 586 MPa which is equivalent to that of the T6 sample and 11.5% higher than that of the T7451 condition. The fracture toughness of the RRA-treated sample was 41 MPa√m. Microstructure of the RRA-treated sample is similar to T7451, along the grain boundaries and in the grain interior similar to that of the T6-treated sample. Energy-dispersive spectroscopy confirmed the increment of Cu content on the GBP’s with increase in the retrogression time, which is expected to improve the stress corrosion cracking resistance of the alloy.

36 MATERIALS SCIENCE↗

ADAPTATION OF CRACK GROWTH DETECTION TECHNIQUES TO US MATERIAL TEST REACTORS

A key component in evaluating the ability of Light Water Reactors to operate beyond 60 years is characterizing the degradation of materials exposed to radiation and various water chemistries. Of particular concern is the response of reactor materials to Irradiation Assisted Stress Corrosion Cracking (IASCC). Some test reactors outside the United States, such as the Halden Boiling Water Reactor (HBWR), have developed techniques to measure crack growth propagation during irradiation. The basic approach is to use a custom-designed compact loading mechanism to stress the specimen during irradiation, while the crack in the specimen is monitored in-situ using the Direct Current Potential Drop (DCPD) method. In 2012 the US Department of Energy commissioned the Idaho National Laboratory and the MIT Nuclear Reactor Laboratory (MIT NRL) to take the basic concepts developed at the HBWR and adapt them to a test rig capable of conducting in-pile IASCC tests in US Material Test Reactors. The first two and half years of the project consisted of designing and testing the loader mechanism, testing individual components of the in-pile rig and electronic support equipment, and autoclave testing of the rig design prior to insertion in the MIT Reactor. The load was applied to the specimen by means of a scissor like mechanism, actuated by a miniature metal bellows driven by pneumatic pressure and sized to fit within the small in-core irradiation volume. In addition to the loader design, technical challenges included developing robust connections to the specimen for the applied current and voltage measurements, appropriate ceramic insulating materials that can endure the LWR environment, dealing with the high electromagnetic noise environment of a reactor core at full power, and accommodating material property changes in the specimen, due primarily to fast neutron damage, which change the specimen resistance without additional crack growth. The project culminated with an in-pile demonstration at the MIT Reactor. The test rig and associated support equipment were used to apply loads to a representative Compact Tensile specimen during one MITR operating cycle, while measuring crack growth using the DCPD method. Although the test period was short (approximately 70 days), and the accumulated neutron dose relatively small, successful operation of the test rig was demonstrated. The specimen was cycled more than 8000 times (more than would be typical for a long term IASCC test), which was sufficient to propagate a crack of over 2 mm.

Crack Growth↗

EFFECTS OF LASER SHOCK PEENING ON SCC BEHAVIOR OF ALLOY 600

In this study, the effects of laser shock peening (LSP) on stress corrosion cracking (SCC) behavior of Alloy 600 in tetrathionate solution were investigated. The degree of sensitization was quantified using double loop electrochemical potentiokinetic reactivation (DLEPR) tests. The sensitized Alloy 600 was demonstrated to be susceptible to intergranular SCC in tetrathionate solution. Following LSP, residual stresses and the amount of plastic strain introduced in Alloy 600 were characterized. The effects of LSP on SCC susceptibility of Alloy 600 in tetrathionate solution were evaluated by slow strain rate tests and constant load tests. Results indicate a significant increase in resistance to crack initiation and decreased susceptibility to SCC after LSP.

36 MATERIALS SCIENCE↗

Reduced yield stress for zirconium exposed to iodine: Reactive force field simulation

Iodine-induced stress-corrosion cracking (ISCC), a known failure mode for nuclear fuel cladding, occurs when iodine generated during the irradiation of a nuclear fuel pellet escapes the pellet through diffusion or thermal cracking and chemically interacts with the inner surface of the clad material, inducing a subsequent effect on the cladding’s resistance to mechanical stress. To complement experimental investigations of ISCC, a reactive force field (ReaxFF) compatible with the Zr-I chemical and materials systems has been developed and applied to simulate the impact of iodine exposure on the mechanical strength of the material. The study shows that the material’s resistance to stress (as captured by the yield stress of a high-energy grain boundary) is related to the surface coverage of iodine, with the implication that ISCC is the result of adsorption-enhanced decohesion.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Integrated Simulation of Weld Residual Stress Evolution and Crack Propagation Using XFEM

Nuclear power plant components operate in environments that promote multiple degradation mecha- nisms, several of which involve crack initiation and growth. An ongoing effort in the U.S. Department of Energy’s Nuclear Energy Advanced Modeling and Simulation (NEAMS) program is developing a general capability within the Multiphysics Object Oriented Simulation Environment (MOOSE) framework for simulating three-dimensional crack growth under a range of driving conditions, including fatigue, stress corrosion cracking (SCC), brittle fracture, and stress-relaxation cracking. This report demonstrates an end-to-end workflow that uses this capability to model weld-residual-stress-driven SCC in the J-groove weld of a pressurized-water reactor control rod drive mechanism penetration in the vessel head. The workflow consists of a thermomechanical welding simulation with temperature-dependent plasticity, followed by cooldown to ambient conditions, and a restart of the simulation using the MOOSE extended finite element method (XFEM) module to propagate a three-dimensional crack through the residual stress field. New welding capabilities were developed to properly initialize newly activated elements in the weld region, and robustness improvements were made to the mesh-based algorithm for defining cutting planes in the 3D XFEM algorithm, allowing it to handle complex crack fronts and stress fields. Together these advances allowed the simulated SCC crack to grow from an initial elliptical flaw in the weld, across the weld, through the tube wall, and almost to the triple point (where the weld, tube, and reactor pressure vessel head intersect) over roughly 36 years of simulated service. These results demonstrate a workflow that can be extended to fully three-dimensional welding simulations and more complex crack interaction problems.

42 - ENGINEERING↗

Evaluation of Manual Ultrasonic Examinations Applied to Detect Flaws in Primary System Dissimilar Metal Welds at North Anna Power Station

During a recent inservice inspection (ISI) of a dissimilar metal weld (DMW) in an inlet (hot leg) steam generator nozzle at North Anna Power Station Unit 1, several axially oriented flaws went undetected by the licensee's manual ultrasonic testing (UT) technique. The flaws were subsequently detected as a result of outside diameter (OD) surface machining in preparation for a full structural weld overlay. The machining operation uncovered the existence of two through-wall flaws, based on the observance of primary water leaking from the DMW. Further ultrasonic tests were then performed, and a total of five axially oriented flaws, classified as primary water stress corrosion cracking (PWSCC), were detected in varied locations around the weld circumference.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗