Search NASA⌕ Search

SEARCH · Search NASA

Results for “STRESS INTENSITY FACTORS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 397 records · Page 22

Sound Assisted Low Temperature Spalling: Upscaling and Throughput

In evaluating the state-of-the-art spalling techniques, the key factor that is missing is the control of crack propagation, which is responsible for low quality wafers due to high surface roughness and Total Thickness Variation, TTV. This project has shown that acoustic waves can alter the conditions at the crack tip during thermal spalling, modifying the propagation speed and the stress field around it (stress intensity factor, K). Both factors are directly related to the roughness of the spalled surface, so as we control speed and stress, we can fine-tune the surface roughness through the entire wafer as suggested by Arakawa.

42 ENGINEERING↗

A sandwich plate with a part-through and a debonding crack.

The stress analysis of a metal base plate stiffened by a fiber-reinforced composite layer is considered. It is assumed that the two materials are bonded through an adhesive of constant thickness which is treated as a two-dimensional shear spring in the analysis. The metal plate is assumed to contain a through crack of finite length. The composite plate has no flaws. However, due to the high stress concentration around the crack and on the interface, a debonding crack is assumed to exist, encircling the crack in the base plate. The problem is reduced to a pair of integral equations of the second kind with Fredholm-type kernels. By solving these equations the stress intensity factor in the base plate, the boundary of the debonding crack, and the interface shear stresses acting on the adhesive are calculated.

Erdogan, F.↗

Penny-shaped crack in a fiber-reinforced matrix

Using a slender inclusion model developed earlier, the elastostatic interaction problem between a penny-shaped crack and elastic fibers in an elastic matrix is formulated. For a single set and for multiple sets of fibers oriented perpendicularly to the plane of the crack and distributed symmetrically on concentric circles, the problem was reduced to a system of singular integral equations. Techniques for the regularization and for the numerical solution of the system are outlined. For various fiber geometries numerical examples are given, and distribution of the stress intensity factor along the crack border was obtained. Sample results showing the distribution of the fiber stress and a measure of the fiber-matrix interface shear are also included.

Narayanan, T. V.↗

Penny-shaped crack in a fiber-reinforced matrix

Using the slender inclusion model developed earlier the elastostatic interaction problem between a penny-shaped crack and elastic fibers in an elastic matrix is formulated. For a single set and for multiple sets of fibers oriented perpendicularly to the plane of the crack and distributed symmetrically on concentric circles the problem is reduced to a system of singular integral equations. Techniques for the regularization and for the numerical solution of the system are outlined. For various fiber geometries numerical examples are given and distribution of the stress intensity factor along the crack border is obtained. Sample results showing the distribution of the fiber stress and a measure of the fiber-matrix interface shear are also included.

Narayanan, T. V.↗

Finite-element analysis of a weld-penetration problem

The stress concentration factor for a weld penetration defect is calculated by the finite-element method. A stress intensity factor is computed by use of the finite-element solution and the J-integral. The results are compared with experimental results.

Rogge, T. R.↗

Is spent nuclear fuel immune from delayed hydride cracking during dry storage? An IAEA coordinated research project - 2016-0048

Delayed hydride cracking (DHC) has been responsible for cracking in zirconium alloy pressure tubes and fuel cladding and is a concern for spent fuel storage. For cracking to start, sufficient hydrogen must be present for hydride to form at a flaw tip and the local tensile stress must be sufficiently large to crack the hydride (a crack will not extend if the threshold in the stress intensity factor, K{sub IH}, is not exceeded. A high-temperature limit exists when the yield stress of the cladding alloy becomes too low to crack the hydride. In this paper we describe measurements of K{sub IH} and the crack growth rate, V, in unirradiated Zircaloy-4 fuel cladding containing approximately 130 ppm hydrogen in the cold-worked stress-relieved condition representing pressurized water reactors (PWRs) and pressurized heavy-water (PHWR) reactors. Four methods are used to evaluate K{sub IH}. The test specimen and fixture used in these methods was the pin-loading tension configuration. The test temperature ranged from 227 to 315 deg. C. The mean value of K{sub IH} below 280 deg. C had little temperature dependence; it was about 5.5 MPa√m in the PWR cladding and slightly higher at 7 MPa√m in the PHWR material. At higher test temperatures, K{sub IH} increased dramatically to more than 12 MPa√m, whereas the crack growth rate declined toward zero. This behavior suggests that unirradiated Zircaloy-4 fuel cladding is immune from DHC above about 320 deg. C; this temperature may be increased to 360 deg. C by irradiation. The implications for spent fuel storage are that during early storage when the temperatures are high, any flaw will not extend by DHC, whereas at low temperatures, after many years of storage, flaws would have to be very large, approaching through wall, before being extended by DHC. To date, spent nuclear fuel is not known to have failed by DHC during storage, confirming the inference. (authors)

36 MATERIALS SCIENCE↗

Dugdale plastic zone size and CTOD equations for the compact specimen

With the aim of applying the Dugdale model to the compact specimen, the equations for stress intensity factor and crack surface displacement are obtained for a pair of pin loads and a uniform stress acting on a segment of the crack surface. The plastic zone size is calculated from the 'finiteness' condition of Dugdale, and the results agree well with collocation results from Terada (1983). The load that causes incipient yielding at the compression point of the compact specimen is calculated from a finite element strip yield analysis for an elastic-perfectly plastic material. The crack tip opening displacement for the compact specimen is calculated by adding the displacement at the tip of the physical crack length due to the pin load and due to the uniform stress. The results are within 1.5 percent of current collocation results.

Newman, J. C., Jr.↗

Modelling the graphite fracture mechanisms

In order to define a design criterion for graphite components, it is important to identify the physical phenomena responsible for the graphite fracture, to include them in a more effective modelling. In a first step, a large panel of experiments have been realised in order to build up an important database; results of tensile tests, 3 and 4 point bending tests on smooth and notched specimens have been analysed and have demonstrated an important geometry related effects on the behavior up to fracture. Then, first simulations with an elastic or an elastoplastic bilinear constitutive law have not made it possible to simulate the experimental fracture stress variations with the specimen geometry, the fracture mechanisms of the graphite being at the microstructural scale. That is the reason why a specific F.E. model of the graphite structure has been developed in which every graphite grain has been meshed independently, the crack initiation along the basal plane of the particles as well as the crack propagation and coalescence have been modelled too. This specific model has been used to test two different approaches for fracture initiation: a critical stress criterion and two criteria of fracture mechanic type. They are all based on crystallographic considerations as a global critical stress criterion gave unsatisfactory results. The criteria of fracture mechanic type being extremely unstable and unable to represent the graphite global behaviour up to the final collapse, the critical stress criterion has been preferred to predict the results of the large range of available experiments, on both smooth and notched specimens. In so doing, the experimental observations have been correctly simulated: the geometry related effects on the experimental fracture stress dispersion, the specimen volume effects on the macroscopic fracture stress and the crack propagation at a constant stress intensity factor. In addition, the parameters of the criterion have been related to experimental observations: the local crack initiation stress of 8 MPa corresponds to the non-linearity apparition on the global behavior observed experimentally and the the maximal critical stress defined for the particle of 30 MPa is equivalent to the fracture stress of notched specimens. This innovative combination of crack modelling and a local crystallographic critical stress criterion made it possible to understand that cleavage initiation and propagation in the graphite microstructure was driven by a mean critical stress criterion. (authors)

36 MATERIALS SCIENCE↗

Simulating the Fracture of Notched Mortar Beams through Extended Finite-Element Method and Peridynamics

This paper simulates fracture in notched mortar beams under three-point bending using extended finite element method (XFEM) and peridynamics. A three-phase microstructure (i.e., cement paste, aggregates, and paste-aggregate interface) is used for constitutive modeling of the mortar to obtain the elastic properties for simulation. In the XFEM approach, the simulated homogenized elastic modulus is used along with the total fracture energy of the cement mortar in a damage model to predict the fracture response of the mortar including crack propagation and its fracture parameters (Mode I stress intensity factor, K IC and critical crack tip opening displacement, CTOD C ). The damage model incorporates a maximum principal stress-based damage initiation criteria and a traction-separation law for damage evolution. In the peridynamics approach, a bond-based model involving a prototype microelastic brittle (PMB) material model is used. The elastic properties and fracture energy release rates are used as inputs in the PMB model, along with the choice of peridynamic horizon size. Comparison with experimental fracture properties ( K IC , CTOD C ) as well as crack propagation paths from digital image correlation show that both the approaches yield satisfactory results, particularly for K IC and crack extension. Furthermore, both these methods can be adopted for fracture simulation of cement-based materials.

42 ENGINEERING↗

Fracture angle and strain-energy-density-factor of a crack at hole at an arbitrary angle

For both the maximum stress criterion and strain-energy-density-factor (S) theory, fracture angle (the initial angle of crack growth) is predicted by using opening and sliding mode stress intensity factors. These theoretical predictions are consistent with experimental fracture angles. For the S theory, the crack spreads in the direction of the negative fracture angle in a plane for which S is a minimum. This quantity was obtained analytically. The experimental data of the critical S on plexiglass fracture specimens remains essentially constant.

Hsu, Y. C.↗

Stress-free end problem in layered materials

In this paper the plane elastostatic problem for a medium which consists of periodically arranged two sets of bonded dissimilar layers or strips is considered. First it is assumed that one set of strips contains a crack which crosses the bimaterial interfaces. Then, by letting the collinear cracks join, the stress-free end problem is formulated. The singular behavior of the solutions at the point on intersection of the stress-free boundary and the interfaces is examined and appropriate stress intensity factors are defined. The results of some numerical examples are then presented which include the cases of both plane stress and plane strain.

Erdogan, F.↗

MSFC crack growth analysis computer program, version 2 (users manual)

An updated version of the George C. Marshall Space Flight Center Crack Growth Analysis Program is described. The updated computer program has significantly expanded capabilities over the original one. This increased capability includes an extensive expansion of the library of stress intensity factors, plotting capability, increased design iteration capability, and the capability of performing proof test logic analysis. The technical approaches used within the computer program are presented, and the input and output formats and options are described. Details of the stress intensity equations, example data, and example problems are presented.

Creager, M.↗

Fracture of composite panels

The fracture problem in panels consisting of periodically arranged load carrying and buffer strips of different materials is considered. The main emphasis is placed on the problem of a crack terminating at and crossing the interfaces and on the stress free end problem. The problem is formulated in terms of a system of singular integral equations, and numerical solutions are obtained for certain material combinations. With the study of possible crack propagation and delamination in mind, certain stress intensity factors are defined and calculated. A main result is that when the crack touches or intersects a bimaterial interface, the stress state has no longer the standard square root singularity, and, to study further propagation of the crack, the conventional fracture models need to be modified, or new models need to be developed.

Erdogan, F.↗

Elastic-Plastic Fracture Mechanics Analysis of Critical Flaw Size in ARES I-X Flange-to-Skin Welds

NASA's Ares 1 Upper Stage Simulator (USS) is being fabricated from welded A516 steel. In order to insure the structural integrity of these welds it is of interest to calculate the critical initial flaw size (CIFS) to establish rational inspection requirements. The CIFS is in turn dependent on the critical final flaw size (CFS), as well as fatigue flaw growth resulting from transportation, handling and service-induced loading. These calculations were made using linear elastic fracture mechanics (LEFM), which are thought to be conservative because they are based on a lower bound, so called elastic, fracture toughness determined from tests that displayed significant plasticity. Nevertheless, there was still concern that the yield magnitude stresses generated in the flange-to-skin weld by the combination of axial stresses due to axial forces, fit-up stresses, and weld residual stresses, could give rise to significant flaw-tip plasticity, which might render the LEFM results to be non-conservative. The objective of the present study was to employ Elastic Plastic Fracture Mechanics (EPFM) to determine CFS values, and then compare these values to CFS values evaluated using LEFM. CFS values were calculated for twelve cases involving surface and embedded flaws, EPFM analyses with and without plastic shakedown of the stresses, LEFM analyses, and various welding residual stress distributions. For the cases examined, the computed CFS values based on elastic analyses were the smallest in all instances where the failures were predicted to be controlled by the fracture toughness. However, in certain cases, the CFS values predicted by the elastic-plastic analyses were smaller than those predicted by the elastic analyses; in these cases the failure criteria were determined by a breakdown in stress intensity factor validity limits for deep flaws (a greater than 0.90t), rather than by the fracture toughness. Plastic relaxation of stresses accompanying shakedown always increases the calculated CFS values compared to the CFS values determined without shakedown. Thus, it is conservative to ignore shakedown effects.

Chell, G. Graham↗

Nonmonotonic effect of chemical heterogeneity on interfacial crack growth at high-angle grain boundaries in Fe-Ni-Cr alloys

Here, an intermittent pattern is observed in the modeling of interfacial cyclic-loading crack growth at high-angle grain boundaries in ternary Fe-Ni-Cr alloys. Different from conventional wisdom of stress-intensity factor, the abrupt crack advances are found driven by extreme value statistics—namely, the aggregation of atoms with most compressive residual stresses. In addition, inherently non-affine atomic stress fluctuations are discovered, and the fluctuations peak at intermediate level of chemical heterogeneity, causing the fastest crack growth. Implications of such nonmonotonic mechanism in regard to the origin of intermediate-temperature embrittlement phenomena are also discussed.

36 MATERIALS SCIENCE↗

Use of three-dimensional photoelasticity in fracture mechanics

The philosophy of fracture mechanics is reviewed and utilized to formulate a simplified approach to the determination of the stress-intensity factor photoelastically for three-dimensional problems. The method involves a Taylor Series correction for the maximum in-plane shear stress (TSCM) and does not involve stress separation. The results are illustrated by applying the TSCM to surface flaws in bending fields. Other three-dimensional problems solved by the TSCM are cited.

Smith, C. W.↗