An improved diffusion welding technique for TD-NiCr
An improved diffusion welding technique has been developed for TD-NiCr sheet. In the most preferred form, the improved technique consists of diffusion welding 320-grit sanded plus chemically polished surfaces of unrecrystallized TD-NiCr at 760 C under 140 MN/m2 pressure for 1hr followed by postheating at 1180 C for 2hr. Compared to previous work, this improved technique has the advantages of shorter welding time, lower welding temperature, lower welding pressure, and a simpler and more reproducible surface preparation procedure. Weldments were made that had parent-metal creep-rupture shear strength at 1100 C.