Parametric Optimization of Nanostructured Alumina Forming Austenitic Alloys

Alumina-forming austenitic (AFA) alloys provide excellent oxidation resistance through the formation of a stable alumina scale, but their relatively high Ni content might limit application in core structural components because of helium generation and swelling under irradiation. Increasing the density of nanoscale features in the microstructure is a promising route to improve sink strength and mitigate these effects. Conventional oxide dispersion–strengthened (ODS) steels achieve this through mechanical alloying (MA), but the approach is costly and difficult to scale. In this milestone, additive manufacturing was applied as an alternative pathway to fabricate nanostructured AFA (NAFA) alloys with dual precipitation of oxides and nitrides enabled by reactive atmosphere processing. In FY25, two compositions, NAFA-1 (AFA-05) and NAFA-2, were produced and compared. Both alloys achieved densities above 99% of theoretical values, but NAFA-2 exhibited microcracking associated with Nb-rich intermetallic formation, indicating the need for further chemistry optimization. Nitrogen and oxygen uptake was confirmed on selected builds, demonstrating the intended dual-precipitate dispersion. Mechanical testing showed that AM-processed NAFA alloys exceed conventionally produced ODS steels in high-temperature tensile strength and fracture toughness. Preliminary Cu ion irradiation results further suggest improved resistance compared to wrought austenitic alloys. While the current alloys are promising for their compatibility in high-temperature air or liquid Pb environments, modifications to composition will be required for long-term operation in high-temperature impure sodium systems. Future work will focus on refining alloy chemistry to suppress laser powder bed fusion–induced cracking and scaling production to reactor-relevant dimensions using directed energy deposition as a pathway toward net-shape cladding fabrication.

36 MATERIALS SCIENCE↗

Metallic Powder Core Tubular Wire (PCTW) Development for Additive Manufacturing

NASA Langley Research Center (LaRC) in Hampton, VA, and the Center for Welding, Joining, and Coating Research (CWJCR) in the Department of Metallurgical and Materials Engineering at the Colorado School of Mines (CSM) in Golden, CO, have collaborated for nearly fifteen years to develop metallic powder core tubular wire (PCTW) feedstock for additive manufacturing (AM) using electron beam deposition. The motivation for this development was to offset dealloying observed during deposition of titanium and aluminum alloy solid wire feedstock in the LaRC electron beam freeform fabrication (EBF3) system and to explore novel alloy compositions by tailoring the powder fill. EBF3 is a fusion-based AM process that is performed under vacuum and is consequently prone to vaporization loss of low vapor pressure alloying elements. Research spanning four graduate student research projects succeeded in developing the basic methodology to fabricate PCTW, the mass balance equations used to define the powder fill, microstructure control through particulate inoculation, and the feasibility of producing metal matrix composite materials. Metallic PCTW is comprised of a thin foil sheath wrapped around a powder blend. Fabrication of PCTW at CSM was accomplished using a tubular wire mill system to first bend a flat strip into a u-shaped cross section, deposit a powder fill, create a lap joint to seal the wire, and draw to final diameter. Powder management systems were developed to ensure uniform mixing of powder constituents and identify feed rates for optimum fill ratios. Processing parameters were successfully developed for titanium and aluminum alloy sheaths to account for material work hardening during drawing. Mass balance equations were developed to account for compositional contributions of the sheath and powder fill. PCTW composition can be adjusted through selection of the sheath or powder materials. PCTWs were successfully developed to offset Al loss in deposits of Ti-6-4 and Mg loss in Al 6061, resulting in deposits that were within the composition limits for each material. Ti-6-4 deposits were fabricated using PCTW comprised of commercially pure (CP) titanium sheath and a fill of pre-alloyed Ti-6-4 powder with additions of elemental Al and V powders. Additions of both elements were required to account for the CP Ti from the sheath, and Al was further enhanced to offset documented losses in EBF3 deposits. For Al 6061 deposits, composition was modulated through the choice of sheath material. The PCTW was made using an Al 5052 sheath to supplement Mg content and a fill composition of pre-alloyed 6061 powder with additions of Si and Cu.The slower solidification rate of the EBF3 process compared with laser powder bed fusion processes can lead to coarse-grained microstructures and mechanical property anisotropy. EBF3deposits of Ti-6-4 exhibited large epitaxially grown β grains, which result in degraded mechanical properties in the deposition direction. Microstructure refinement was achieved through a combination of electron beam modulation and the use of a PCTW designed for Ti-6-4 deposits and modified by the addition of powder made from Fe and B. Resulting deposits exhibited reductions in β grain size, α phase colony intercept length and lath width, and an increased volume fraction of β phase. The mechanism of microstructure refinement was related to precipitation of boride particles. Hardness testing confirmed that mechanical property anisotropy was reduced and an overall increase in hardness was achieved.Metal matrix composite (MMC) materials offer strength and stiffness benefits over unreinforced materials. Two methods were investigated using PCTW technology for producing Al 6061 basedMMC materials; the direct addition of SiC reinforcing particles and the in-situ generation of reinforcements through reaction synthesis of precursor powders. Al 6061 based MMCs reinforced with SiC exhibited particle clustering and formation of aluminum carbides during deposition. The application of a Ni coating to the SiC particles prior to incorporation into the powder fill eliminated aluminum carbide formation and aided particle distribution during deposition. Modulation of beam focus and power further reduced aluminum carbide formation and aided particle distribution. In reaction synthesis, precursor additions undergo an exothermic reaction during deposition to form new ceramic products, generally of finer scale than the initial precursor components. The product phases provide reinforcement in the MMC and act as nucleation sites during solidification, resulting in grain refinement, improved mechanical properties, and reduced susceptibility to solidification cracking. Higher tensile strength and stiffness were demonstrated in Al 6061 based MMCs with 2 vol% reinforcement. These combined research efforts demonstrate the potential of PCTW technology for customizing of alloy composition and achieving microstructure control. A manufacturing process for titanium- and aluminum-based PCTWs was developed based on iterative design, theoretical calculations, and empirical data. PCTW technology successfully mitigated Al loss from Ti-6-4 and Mg loss in Al 6061, resulted in grain refinement in Ti-6-4, and demonstrated fabrication of Al based MMCs

Marcia S Domack↗

On the Mechanical Behavior of LP-DED C103 Thin-Wall Structures

Laser Powder Directed Energy Deposition (LP-DED) can produce thin-wall features on the order of 1 mm. These features are essential for large structures operating in extreme environments such as regeneratively cooled nozzles and heat exchangers, which often make use of refractory metals. In this work, the mechanical behavior of LP-DED C103 was investigated via quasi-static tensile testing and low cycle fatigue (LCF) testing. The effects of vacuum stress relief (SR) and hot isostatic pressing (HIP) heat treatments were investigated for specimens in the vertical and horizontal build orientations during tensile testing. The AB and SR properties were lower than literature values for wrought and laser powder bed fusion (L-PBF) bulk components but higher than electron beam powder bed fusion (EB-PBF). The application of a HIP cycle improved strength by 7% and ductility by 27% past the initial as-built condition. Fracture images reveal that interlayer stress concentration sites are responsible for fracture in specimens in the vertical orientation. Meanwhile, fracture in the horizontal specimens mainly propagates at a slanted angle typical of plane stress conditions. The LCF results show cycles to failure ranging from 100 cycles to 8000 cycles for max strain levels of 2% and 0.5%, respectively. Fractography on the fatigue specimens reveals an increasing propagation zone as max strain levels are increased. The impact of these findings and future work are discussed in detail.

36 MATERIALS SCIENCE↗

Multiscale Modeling of Nanoparticle Precipitation in Oxide Dispersion-Strengthened Steels Produced by Laser Powder Bed Fusion

Laser Powder Bed Fusion (LPBF) enables the efficient production of near-net-shape oxide dispersion-strengthened (ODS) alloys, which possess superior mechanical properties due to oxide nanoparticles (e.g., yttrium oxide, Y-O, and yttrium-titanium oxide, Y-Ti-O) embedded in the alloy matrix. To better understand the precipitation mechanisms of the oxide nanoparticles and predict their size distribution under LPBF conditions, we developed an innovative physics-based multiscale modeling strategy that incorporates multiple computational approaches. These include a finite volume method model (Flow3D) to analyze the temperature field and cooling rate of the melt pool during the LPBF process, a density functional theory model to calculate the binding energy of Y-O particles and the temperature-dependent diffusivities of Y and O in molten 316L stainless steel (SS), and a cluster dynamics model to evaluate the kinetic evolution and size distribution of Y-O nanoparticles in as-fabricated 316L SS ODS alloys. The model-predicted particle sizes exhibit good agreement with experimental measurements across various LPBF process parameters, i.e., laser power (110–220 W) and scanning speed (150–900 mm/s), demonstrating the reliability and predictive power of the modeling approach. The multiscale approach can be used to guide the future design of experimental process parameters to control oxide nanoparticle characteristics in LPBF-manufactured ODS alloys. Additionally, our approach introduces a novel strategy for understanding and modeling the thermodynamics and kinetics of precipitation in high-temperature systems, particularly molten alloys.

Wang, Zhengming (ORCID:0000000241627112)↗

Strain-rate hardening enhances fatigue resistance of AlSi10Mg alloy at 350°C

The high cycle fatigue behavior of laser powder bed fusion processed AlSi10Mg has been investigated at 350 °C (T/T m ∼ 0.7). The alloy exhibited a fatigue strength of 30 MPa defined by runout after 10 7 cycles at a conventional loading frequency of 20 Hz, corresponding to a notable fatigue strength to ultimate tensile strength ratio of 0.73. The surprising fatigue resistance was attributed to the strain-rate hardening effect at high fatigue loading frequency relative to tensile loading rates at 350 °C. The strain-rate hardening effect was validated by performing ultrasonic fatigue tests (20 kHz loading frequency) with three orders of magnitude higher strain-rates than those at conventional loading frequency. The higher strain-rates in ultrasonic fatigue increased the magnitude of strain-rate hardening resulting in longer AlSi10Mg fatigue lives compared to fatigue at conventional frequency, thus confirming the strain-rate hardening effect. The fatigue crack initiation mechanism was strain-rate dependent. Post-mortem microstructural examination revealed intergranular cavitation inside clusters of fine equiaxed grains. The cavities interlinked with each other to initiate near-surface fatigue cracks at conventional frequency. Cavitation occurred to a lesser extent at the ultrasonic frequency. As a result, fatigue cracks initiated at pre-existing processing defects near the surface in ultrasonic fatigue samples. Finally, this investigation underscores the role of fine grain clusters in promoting high-temperature fatigue crack initiation and indicates a possible trade-off between printability via grain refinement and high-temperature fatigue resistance of additively manufactured alloys.

Additive manufacturing↗

Effect of Heat Treatment on the Microstructure and Mechanical Properties of Monel K500 Alloy Fabricated Via L-PBF and LP-DED

This study examines and compares the effect of different heat treatments (HT) on the microstructure and mechanical properties of Monel K500 fabricated using laser powder bed fusion (L-PBF) and laser powder directed energy deposition (LP-DED) technologies. The as-fabricated Monel K500 specimens exhibited dendritic microstructure and elemental micro-segregation due to high cooling rates induced during the fabrication process. The applicability of HT proposed in the literature for wrought Monel K500 was investigated for L-PBF and LP-DED using four different HT procedures involving hot isostatic pressing (HIP), solution annealing (SA), and aging. The mechanical properties of test specimens were evaluated using uniaxial tensile testing at room temperature. The microstructural evolution of test specimens during HT was analyzed using a scanning electron microscope. For all HT conditions investigated, L-PBF Monel K500 specimens consistently displayed higher strength and lower ductility compared to the LP-DED counterparts. The HT procedure involving HIP at 1160°C for 3hr at 100 MPa, SA at 1100°C for 15 min, and three step aging at 610°C for 16 hr, 540°C for 6 hr, and 480°C for 8 hr resulted in highest strength for both L-PBF and LP-DED fabricated Monel K500.

Additive manufacturing↗

L-PBF High-Throughput Data Pipeline Approach for Multi-modal Integration

Abstract Metal-based additive manufacturing requires active monitoring solutions for assessing part quality. Multiple sensors and data streams, however, generate large heterogeneous data sets that are impractical for manual assessment and characterization. In this work, an automated pipeline is developed that enables feature extraction from high-speed camera video and multi-modal data analysis. The framework removes the need for manual assessment through the utilization of deep learning techniques and training models in a weakly supervised paradigm. We demonstrate this pipeline’s capability over 700,000 high-speed camera frames. The pipeline successfully extracts melt pool and spatter geometries and links them to corresponding pyrometry, radiography, and processparameter information. 715 individual prints are examined to reveal melt pool areas that exceeds 0.07 mm 2 and pyrometry signal over a threshold (375 pyrometry units) were more likely to have defects. These automated processes enable massive throughput of characterization techniques.

36 MATERIALS SCIENCE↗

Nondestructive Modular Leak Detection in 3D Printed 316L Stainless Steel Pipes via Laser Powder Bed Fusion

This research investigates the leak detection features of 316L Stainless Steel pipe structures manufactured via Laser Powder Bed Fusion (LPBF). This work involves the design of a modular sensor system integrating nondestructive evaluation (NDE) methods, including thermal imaging and ultrasonic frequency detection to detect and characterize leaks in components. This aims to improve leak detection sensitivity within medium-pressure gas systems, during continuous operation without halting flow or introducing safety risks. The system could be adaptable for use on unmanned aerial vehicles (UAVs), enabling remote leak detection in active environments. A custom pneumatic system incorporating temperature and pressure sensors was assembled to detect leaks in LPBF-printed 316L SS tee pipes. Experimental results and simulations confirm the system’s effectiveness in leak detection and material evaluation. This research program also integrated a Python-based image recognition platform based on a metallography and optical microscopy to assess the porosity and complement the leak detection data on the printed structures. This allows a detailed analysis of pore distribution and internal leak paths, which could compromise structural integrity, critical for quality control during manufacturing. Findings suggest that the investigated approach holds potential for enhancing leak detection technologies and adapt them for advanced manufactured parts.

36 MATERIALS SCIENCE↗

Part-scale microstructure prediction for laser powder bed fusion Ti-6Al-4V using a hybrid mechanistic and machine learning model

Laser powder bed fusion (LPBF) Ti-6Al-4V is widely studied for use in structural applications in aerospace and medical industries, but mechanical anisotropy and microstructural inhomogeneity prohibits its wider adoption. Although successful microstructure prediction models have been developed, a remaining challenge is their limited integration across length/time scales and validation by experimental studies. Here, this work proposes a physics-augmented machine learning surrogate model to unite predictions of LPBF temperature, β phase morphology and texture, and α/α’ formation into a single framework that is calibrated and validated with experiments. First, a phase field (PF) model of the martensitic β→α’ transformation is developed and calibrated using data from in-situ synchrotron cyclic heating/cooling studies quantifying the variation of α phase fraction with time. In parallel, an established finite difference-Monte Carlo (FDMC) model predicts the part-scale temperature profile and β grain formation during solidification. A dataset is developed using LPBF cyclic temperature descriptors from the FDMC model as inputs and corresponding α/α’ phase fraction and width from the PF model as outputs. Five machine learning (ML) regression models are tested and optimized, having mean absolute error in testing ≤ 4 %, and the k-nearest neighbors (KNN) model is selected as the best performing. The KNN model is called at the nodal level during post-processing of the FDMC model to replace and downscale the response of the PF model. The combined agility and accuracy of the hybrid FDMC-ML model enables part-scale microstructure predictions that can be further used for property predictions to accelerate AM process optimization.

36 MATERIALS SCIENCE↗

The effect of heat treatment on the defect evolution in LPBF 316H stainless steel

This work investigates the effect of processing and heat treatment on defect evolution and irradiation response of laser powder bed fusion (LPBF) 316H stainless steel, with comparisons to LPBF 316L and wrought 316L/316H. Using in-situ and ex-situ ion irradiations across a wide parameter space—temperature (300–675 °C), dose (0.2–25 dpa), dose rate (10 -3 –10 -5 dpa/s), and helium co-implantation (20–2500 appm)—we correlated void swelling, dislocation loop evolution, and segregation behavior with pre-irradiation microstructures (as-built, stress-relieved, solution-annealed, and cold-worked). Results show that swelling is strongly controlled by dislocation density: intermediate densities maximize swelling, while solution annealing or cold working reduce susceptibility to levels comparable to wrought alloys. Low dose rates and helium both promote cavity nucleation and lower the incubation barrier, with helium suppressing the role of dislocation density and driving swelling behavior toward wrought-like response. Loop evolution in SA LPBF 316H resembles wrought 316L but shows localized denuded zones near low-angle grain boundaries. STEM-EDS mapping further revealed Ni segregation at voids and sparse Al-rich oxides, without evidence of Ni–Si precipitates. Collectively, these findings identify dislocation density, helium content, and dose rate as the factors governing swelling in LPBF 316H and provide mechanistic datasets for model validation, supporting LAIN and the qualification of AM austenitic steels for nuclear service.

316 stainless steel↗

Collaborative or competitive phase transformation processes in an additively manufactured-maraging steel M300

Although retained austenite is present in minor amounts in as-built additively manufactured-maraging steels, its evolution during ageing is key to controlling the final microstructure. This study investigates the relationship between austenite reversion and precipitation evolution during ageing, particularly whether these processes compete or cooperate. Using Scanning/Transmission Electron Microscopy, Atom Probe Tomography and Thermo-Calc® PRISMA simulations, the presence and evolution of retained austenite, Ni 3 Ti and Fe 7 Mo 6 intermetallic phases was characterised across different ageing conditions. Experimental results revealed the presence of non-enriched austenite in the as-built condition. Nevertheless, with increasing ageing temperature, Ni and Mo segregation became evident. High-Resolution Transmission Electron Microscopy revealed that Ni 3 Ti precipitation primarily occurred within the martensitic matrix, while Fe 7 Mo 6 nucleated preferentially at the austenite-martensite interface. PRISMA simulations indicated early and rapid precipitation in solute-enriched areas (i.e., intercellular regions), with Ni 3 Ti forming prior to Fe 7 Mo 6 . Both experimental and simulation results suggested Ni diffusion controls retained austenite growth, while Ti and Mo drive Ni 3 Ti and Fe 7 Mo 6 precipitation, respectively. The evidence reported in this work supports a both collaborative and independent phase transformation mechanism, where austenite reversion and precipitation co-evolve.

42 ENGINEERING↗

Microstructural evolution, defect mitigation, and precipitation behavior in AA6061 via laser powder bed fusion with high-temperature substrate heating

Defects, particularly solidification cracking, remain persistent challenges in the laser powder bed fusion (LPBF) processing of AA6061 aluminum alloy. This study systematically investigates defect mitigation, microstructural evolution, and mechanical properties associated with high-temperature substrate preheating at 500 °C. Comprehensive microstructural analyses, including characterization of defects, grain structures, and precipitation behavior, were performed on samples in both as-built and T6 heat-treated states. Elevated preheating substantially reduced solidification cracking across a wide processing window, while demonstrating decreased crack sensitivity to laser parameters. Columnar cracks along the build direction were observed despite substrate preheating. Lack-of-fusion and keyhole porosity were effectively eliminated, though gas-induced microporosity persisted at higher powers. In-depth characterization of two distinct laser power and speed conditions confirmed the formation of micron-sized, non-coherent Mg 2 Si precipitates under heated substrate conditions, alongside α-AlFeCrMnSi intermetallic phases indicative of in-situ thermal effects during fabrication. Subsequent T6 heat treatment revealed the formation of fine, coherent needle-shaped β″ strengthening precipitates. Despite substantial differences in processing parameters, comparable mechanical properties were measured in the as-built samples (∼52 MPa yield strength, ∼130 MPa tensile strength), primarily due to reduced strain hardening effects and consistent precipitation characteristics. Meanwhile, the T6 heat treatment led to significant improvement in properties, enhancing yield strength by over 400%, aligning closely with the performance of conventional wrought AA6061-T6. These findings underscore that high-temperature substrate preheating offers an effective means to suppress cracks, control precipitation, and enhance mechanical performance in LPBF-processed AA6061.

36 MATERIALS SCIENCE↗