At least 451 records · Page 25

Corrosion behavior of carbon steel in the monoethanolamine-H{sub 2}O-CO{sub 2}-O{sub 2}-SO{sub 2} system

The effects of operating parameters on the corrosion of carbon steel in the monoethanolamine (MEA)-H{sub 2}O-CO{sub 2}-O{sub 2}-SO{sub 2} system were investigated using two different corrosion measurement techniques. The corrosion studies were conducted using a 273A potentiostat using MEA, O{sub 2}, and SO{sub 2} concentrations and CO{sub 2} loading in the ranges of 1-7 kmol/m{sup 3}, 0-100%, 0-204 ppm, and 0-0.5 mol CO{sub 2}/mol MEA, respectively, at corrosion temperatures in the range of 303-353 K. The experimental results showed, for the first time, that a higher concentration of SO{sub 2} in a simulated flue gas stream induces a higher corrosion rate essentially because of the increase in the hydrogen ion concentration generated by reactions of SO{sub 2} and H{sub 2}O as well as SO{sub 2}, O{sub 2}, and H{sub 2}O. Also, an increase in oxygen concentration in the simulated flue gas stream causes a higher corrosion rate due to the increasing solubility of oxygen and, in turn, a higher amount of dissolved oxygen in the liquid phase. The results further show that an increase in the concentrations of MEA, O{sub 2}, and SO{sub 2} as well as CO{sub 2} loading will cause the generation of higher amounts of hydrogen or hydronium ions, as well as carbonic acid and bicarbonate ions, and this is what leads to a higher corrosion rate.

01 COAL, LIGNITE, AND PEAT↗

TEM Observations of Corrosion Behaviors of Platinized Carbon Blacks under Thermal and Electrochemical Conditions

Carbon blacks such as Vulcan XC-72 are widely used to support platinum (Pt) or Pt alloy catalysts in proton exchange membrane fuel cells. Despite their widespread use, carbon blacks are susceptible to corrosion during fuel cell operations. In this work, the corrosion behaviors of platinized Vulcan XC-72 nanoparticles under thermal and electrochemical conditions were monitored by transmission electron microscopy (TEM). The thermal corrosion experiment was carried out in a gas-cell TEM, which allows for a direct observation of the thermal oxidation behavior of the nanoparticles. The electrochemical corrosion experiment was performed outside of the TEM by loading the nanoparticles on a TEM grid and then electrochemically corroding them step by step followed by taking TEM images from exactly the same nanoparticles after each step. This work revealed four types of structural changes: (i) total removal of structurally weak aggregates, (ii) breakdown of aggregates via neck-breaking, (iii) center-hollowed primary particles caused by an inside-out corrosion starting from the center to outer region, and (iv) gradual decrease in the size of primary particles caused by a uniform removal of material from the surface. These structural changes took place in sequence or simultaneously depending on the competition of carbon corrosion dynamical processes. The results obtained from this work provide insight on carbon corrosion and its effects on fuel cells' long-term performance and durability.

30 DIRECT ENERGY CONVERSION↗

Quantitative Nanoscale 3D Imaging of Intergranular Corrosion of 304 Stainless Steel Using Hard X-Ray Nanoprobe

Multi-modal imaging, which visualizes changes in the structure and chemistry of the same region of interest in materials by combining various techniques, is becoming attractive to material scientists. Here, we describe a multi-modal approach to investigate intergranular (IG) corrosion of sensitized stainless steels using synchrotron-based nanoscale X-ray imaging with sensitivity to microstructure and chemical composition. Three-dimensional tomography of 304 stainless steel samples deteriorated by IG corrosion, was carried out using X-ray fluorescence and differential phase contrast imaging. These findings were further supported with surface imaging and chemical analysis using scanning electron microscopy and energy dispersive X-ray spectroscopy. The combined quantitative structural and chemical analysis indicates that chromium segregates along grain boundaries, cracking is due to IG corrosion, and Cr-enrichment occurs on the cracked surfaces. Such quantitative 3D imaging of Cr 23 C 6 nucleation at grain boundaries and Cr enriched oxides at cracked surfaces is a powerful tool to correlate IG corrosion mechanisms at nanoscale with buried grain boundary structure and alloy composition. Such understanding of IG corrosion mechanisms is critical for both the development of predictive multiscale corrosion models, and the engineering of corrosion resistant materials.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Report on accelerated corrosion studies.

Sandia National Laboratories (SNL) conducted accelerated atmospheric corrosion testing for the U.S. Consumer Product Safety Commission (CPSC) to help further the understanding of the development of corrosion products on conductor materials in household electrical components exposed to environmental conditions representative of homes constructed with problem drywall. The conditions of the accelerated testing were chosen to produce corrosion product growth that would be consistent with long-term exposure to environments containing humidity and parts per billion (ppb) levels of hydrogen sulfide (H{sub 2}S) that are thought to have been the source of corrosion in electrical components from affected homes. This report documents the test set-up, monitoring of electrical performance of powered electrical components during the exposure, and the materials characterization conducted on wires, screws, and contact plates from selected electrical components. No degradation in electrical performance (measured via voltage drop) was measured during the course of the 8-week exposure, which was approximately equivalent to 40 years of exposure in a light industrial environment. Analyses show that corrosion products consisting of various phases of copper sulfide, copper sulfate, and copper oxide are found on exposed surfaces of the conductor materials including wires, screws, and contact plates. The morphology and the thickness of the corrosion products showed a range of character. In some of the copper wires that were observed, corrosion product had flaked or spalled off the surface, exposing fresh metal to the reaction with the contaminant gasses; however, there was no significant change in the wire cross-sectional area.

36 MATERIALS SCIENCE↗

Enhancing corrosion resistance of lightweight metal alloys through laser shock peening

In this study, we investigated the effects of laser shock peening (LSP) on the corrosion resistance of lightweight metal alloys, specifically AA6061 and AZ31. LSP was performed underwater, using a nanosecond pulse laser and without using a protective coating or layer on the workpiece. The corrosion behaviors of these alloys were analyzed through electrochemical tests, including open circuit potential, electrochemical impedance spectroscopy, and potentiodynamic polarization measurements. The results demonstrated that LSP significantly improved the polarization resistance, and higher laser power intensities led to increased corrosion resistance and reduced corrosion rates. This enhancement in anti-corrosion performance is attributed to the formation of a protective oxide layer on the surface, acting as a barrier against corrosion. In conclusion, the findings underscore the potential of laser surface treatment as a viable technique for enhancing the corrosion resistance of lightweight metal alloys.

36 MATERIALS SCIENCE↗

Smart Multifunctional Coatings for Corrosion Detection and Control in the Aerospace Industry

Nearly all metals and their alloys are subject to corrosion that causes them to lose their structural integrity or other critical functionality. It is essential to detect corrosion when it occurs, and preferably at its early stage, so that action can be taken to avoid structural damage or loss of function. Protective coatings are the most commonly used method of corrosion control. However, progressively stricter environmental regulations have resulted in the ban of many commercially available corrosion protective coatings due to the harmful effects of their solvents or corrosion inhibitors. This work concerns the development of a multifunctional, smart coating for the autonomous control of corrosion. This coating is being developed to have the inherent ability to detect the chemical changes associated with the onset of corrosion and respond autonomously to indicate it and control it.

Corrosion↗

Corrosion Control in the Aerospace Industry

Nearly all metals and their alloys are subject to corrosion that causes them to lose their structural integrity or other critical functionality. It is essential to detect corrosion when it occurs, and preferably at its early stage, so that action can be taken to avoid structural damage or loss of function. Protective coatings are the most commonly used method of corrosion control. However, progressively stricter environmental regulations have resulted in the ban of many commercially available corrosion protective coatings due to the harmful effects of their solvents or corrosion inhibitors. This work concerns the development of a multifunctional, smart coating for the autonomous control of corrosion. This coating is being developed to have the inherent ability to detect the chemical changes associated with the onset of corrosion and respond autonomously to indicate it and control it..

Corrosion Control↗

Smart Coatings for Corrosion Protection

Nearly all metals and their alloys are subject to corrosion that causes them to lose their structural integrity or other critical functionality. It is essential to detect corrosion when it occurs, and preferably at its early stage, so that action can be taken to avoid structural damage or loss of function. Protective coatings are the most commonly used method of corrosion control. However, progressively stricter environmental regulations have resulted in the ban of many commercially available corrosion protective coatings due to the harmful effects of their solvents or corrosion inhibitors. This work concerns the development of a multifunctional, smart coating for the autonomous control of corrosion. This coating is being developed to have the inherent ability to detect the chemical changes associated with the onset of corrosion and respond autonomously to indicate it and control it.

Coatings↗

Corrosion test of LWR cladding tubes in high temperature seawater

In the case of cooling system failure in spent fuel pools (SFP) due to station black out and/or loss of coolant accidents, a pool water level must be kept high enough to avoid overheat of spent fuels. Seawater is one of the candidate coolant materials in such emergencies. In the present work, we have studied the corrosion behavior of zirconium alloys in seawater. Tube samples of Zircaloy-2 and -4 claddings were immersed in artificial seawater (3, 10 and 20 wt.%) at high temperature (80 - 85 Celsius degrees). Boric acid was added to the seawater at a corrosion test of Zircaloy-4. Two types of specimens were prepared according to the simulation of circumferential tensile stress. One was a plugged tube specimen, which was pressurized to around fuel rod pressure in a spent fuel pool by argon gas. Another specimen was of C-ring shape, where large circumferential tensile stress was partially induced at the surface. A notch was longitudinally grooved to increase the local tensile stress on some of the C-ring specimens. The specimen surface was observed by a scanning electron microscopy (SEM) after the corrosion test. After the 200 day long corrosion test for the plugged tube specimens without boric acid, Mg(OH){sub 2} deposits were observed on the surface of Zircaloy-2 and -4 specimens whereas Mg(OH){sub 2} was not observed with boric acid because of probably a lower pH. Neither pitting corrosion nor stress corrosion cracking (SCC) was observed on the surface of all plugged tube specimens. Only in the C-ring specimens in 20 wt.% seawater without boric acid and in 3 and 10 wt.% seawater with boric acid, small cracks were observed at the notch. The results of the present work show that Zircaloy-2 and -4 have a high tolerance towards corrosion and SCC in high temperature seawater.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

PERFORMACE OF MULTI-PROBE CORROSION MONITORING SYSTEMS AT THE HANFORD SITE

Between 2007 and 2009, several different multi-probe corrosion monitoring systems were designed and installed in high-level nuclear waste tanks at the U.S. Department of Energy's Hanford Site in WaShington State. The probe systems are being monitored to ensure waste tanks operate in regions that minimize localized corrosion (i.e., pitting) and stress corrosion cracking. The corrosion monitoring systems have been installed in wastes with different chemistry types. An ongoing effort during the same time period has generated non-radioactive simulants that are tested in the laboratory to establish baseline corrosion monitoring system performance and characterize data to allow interpretation of readings from the multiple corrosion monitoring systems. Data collection from these monitoring systems has reached the point where the results allow comparison with the laboratory testing. This paper presents analytical results from the corrosion monitoring system development program.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Hanford Double Shell Waste Tank Corrosion Studies - Final Report FY2015

During FY15, SRNL performed corrosion testing that supported Washington River Protection Solutions (WRPS) with their double shell tank (DST) integrity program. The testing investigated six concerns including, 1) the possibility of corrosion of the exterior of the secondary tank wall; 2) the effect of ammonia on vapor space corrosion (VSC) above waste simulants; 3) the determination of the minimum required nitrite and hydroxide concentrations that prevent pitting in concentrated nitrate solutions (i.e., waste buffering); 4) the susceptibility to liquid air interface (LAI) corrosion at proposed stress corrosion cracking (SCC) inhibitor concentrations; 5) the susceptibility of carbon steel to pitting in dilute solutions that contain significant quantities of chloride and sulfate; and 6) the effect of different heats of A537 carbon steel on the corrosion response. For task 1, 2, and 4, the effect of heat treating and/ or welding of the materials was also investigated.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

The Electrochemical Corrosion Behavior of Plasma Electrolytic Oxidation Coatings Fabricated on Aluminum in Silicate Electrolyte

Plasma electrolytic oxidation (PEO) coatings were fabricated on the aluminum in silicate electrolyte. Microstructures and elemental compositions of these PEO coatings were examined by scanning electron microscopy (SEM) equipped with an energy-dispersive x-ray spectroscopy (EDS). Corrosion resistances of the coated samples were evaluated using the measurements of open-circuit potential (OCP), repetitive polarization and electrochemical impedance spectroscopy (EIS) in 3.5 wt.% NaCl solution. The results indicated that the PEO coatings not only act as a physical shield limiting the penetration of corrosive solution, but also establish an anodic location with high concentration of H{sup +} ions and other product ions as pitting corrosion begins. With the development of pitting corrosion, the accumulation of corrosion products inside the pits and pores of the coatings decreases the corrosion process effectively.

36 MATERIALS SCIENCE↗

Integrated High‐Throughput and Machine Learning Methods to Accelerate Discovery of Molten Salt Corrosion‐Resistant Alloys

Insufficient availability of molten salt corrosion-resistant alloys severely limits the fruition of a variety of promising molten salt technologies that could otherwise have significant societal impacts. To accelerate alloy development for molten salt applications and develop fundamental understanding of corrosion in these environments, here an integrated approach is presented using a set of high-throughput (HTP) alloy synthesis, corrosion testing, and modeling coupled with automated characterization and machine learning. By using this approach, a broad range of Cr-Fe-Mn-Ni alloys are evaluated for their corrosion resistances in molten salt simultaneously demonstrating that corrosion-resistant alloy development can be accelerated by 2 to 3 orders of magnitude. Based on the obtained results, a sacrificial protection mechanism is unveiled in the corrosion of Cr-Fe-Mn-Ni alloys in molten salts which can be applied to protect the less unstable elements in the alloy from being depleted, and provided new insights on the design of high-temperature molten salt corrosion-resistant alloys.

36 MATERIALS SCIENCE↗

Analysis of Brazing Effect on Hot Corrosion Behavior of a Nickel-Based Aerospace Superalloy

The effects of brazing and use of composite powder mixture as interlayer material on hot corrosion resistance of brazed IN738 superalloy were studied. Brazing was observed to result in significant reduction in the hot corrosion resistance of the superalloy. However, application of composite powder mixture, which consists of additive superalloy powder, enhanced the hot corrosion resistance of brazed samples. It is also found that although the use of composite powder mixture increased hot corrosion resistance of brazed alloy, if the additive powder completely melts, which is possible during brazing, it can significantly reduce the hot corrosion resistance of the brazed joint. Elemental micro-segregation during solidification of the joint with completely melted powder mixture produces chromium-depleted zones and consequently reduces hot corrosion resistance, since a uniform distribution and adequate chromium concentration are necessary to combat hot corrosion. This has not been previously reported in the literature and it is crucial to the use of composite powder mixture for enhancing the properties of brazed superalloys.

36 MATERIALS SCIENCE↗

Preliminary Investigation of the Corrosion Behavior of Proprietary Micro-alloyed Steels in Aerated and Deaerated Brine Solutions

The corrosion performance of fairly new generation of micro-alloyed steels was compared in different concentrations of aerated and deaerated brines. Electrochemical polarization, weight loss and surface analyses techniques were employed. The results showed a threshold of corrosion rate at 3.5 wt.% NaCl in both aerated and deaerated solutions. The average corrosion current density for steel B, for example, increased from 1.3 µA cm{sup −2} in 1 wt.% NaCl to 1.5 µA cm{sup −2} in 3.5 wt.% NaCl, but decreased to 1.4 µA cm{sup −2} in 10 wt.% deaerated NaCl solutions. The aerated solutions exhibited an average of over 80% increase in corrosion current density in the respective concentrations when compared with the deaerated solution. These results can be attributed to the effects of dissolved oxygen (DO) which has a maximum solubility in 3.5 wt.% NaCl. DO as a depolarizer and electron acceptor in cathodic reactions accelerates anodic metal dissolution. The difference in carbon content and microstructures occasioned by thermo-mechanical treatment contributed to the witnessed variation in corrosion performance of the steels. Specifically, the results of the various corrosion techniques corroborated each other and showed that the corrosion rate of the micro-alloyed steels can be ranked as CR{sub Steel A} < CR{sub X65} < CR{sub Steel B} < CR{sub Steel C}.

36 MATERIALS SCIENCE↗

A Micro-Mechanism-Based Continuum Corrosion Fatigue Damage Model for Steels

A micro-mechanism-based corrosion fatigue damage model is developed for studying the high-cycle corrosion fatigue of steel from multi-scale viewpoint. The developed physical corrosion fatigue damage model establishes micro-macro relationships between macroscopic continuum damage evolution and collective evolution behavior of microscopic pits and cracks, which can be used to describe the multi-scale corrosion fatigue process of steel. As a case study, the model is used to predict continuum damage evolution and number density of the corrosion pit and short crack of steel component in 5% NaCl water under constant stress amplitude at 20 kHz, and the numerical results are compared with experimental results. It shows that the model is effective and can be used to evaluate the continuum macroscopic corrosion fatigue damage and study microscopic corrosion fatigue mechanisms of steel.

36 MATERIALS SCIENCE↗

Effect of pH on Corrosion Performance of Cu-Se and Cu-Se-Te Alloys in 3.5% Sodium Chloride Solution

The influence of pH (2, 7, 12) on the corrosion behavior of Cu-Se-Te and Cu-Se alloys in a 3.5% sodium chloride solution was investigated using static immersion testing and electrochemical methods. The morphologies of the alloys after corrosion were observed by scanning electron microscopy. The distribution of elements was detected by energy-dispersive spectrometry, and the phases were identified by x-ray diffraction. The results indicate that the corrosion rate decreases significantly with an increase in pH. No compact protective film forms on the alloy surface when pH is 2; meanwhile, Cu{sub 2}(OH){sub 3}Cl and Cu{sub 2}O films form on the alloy surface when pH is 7 or 12. The corrosion rates of alloys in the NaCl solution with different pH levels vary because the cathode reaction and the protective films affect the corrosion rate synthetically. In addition, the Cu-0.5Se alloy generally exhibits satisfactory conductivity, strength, and corrosion resistance. The corrosion resistance of the Cu-0.5Se alloy is higher than that of the Cu-Se-Te alloys, particularly at low pH levels.

36 MATERIALS SCIENCE↗

Effect of MgCl{sub 2} on the Corrosion Behavior of Copper Under Periodic Wet/Dry Cycle Condition

The corrosion behaviors of copper under periodic wet/dry cycle conditions were investigated. The characteristics of the corrosion product formed on copper were analyzed by x-ray diffraction, scanning electron microscopy, energy-dispersive spectroscopy, and in situ electrochemical impedance spectroscopy. Weight loss results showed that the corrosion of copper under an MgCl{sub 2} deposition condition was more severe than that under NaCl. The main corrosion products formed on the tested sample under NaCl deposition condition consisted of Cu{sub 2}Cl(OH){sub 3} and Cu{sub 2}O, while those under the MgCl{sub 2} deposition condition consisted of Cu{sub 2}Cl(OH){sub 3} and Mg{sub 2}(OH){sub 3}Cl·4H{sub 2}O. In the case of the NaCl deposition condition, a two-layered structure formed during the corrosion process. However, the corrosion product layer formed on copper under the MgCl{sub 2} deposition condition had an extremely loose structure. The effect of MgCl{sub 2} on the corrosion mechanism of copper is discussed.

36 MATERIALS SCIENCE↗