Iridium Interfacial Stack - IrIS

Iridium Interfacial Stack (IrIS) is the sputter deposition of high-purity tantalum silicide (TaSi2-400 nm)/platinum (Pt-200 nm)/iridium (Ir-200 nm)/platinum (Pt-200 nm) in an ultra-high vacuum system followed by a 600 C anneal in nitrogen for 30 minutes. IrIS simultaneously acts as both a bond metal and a diffusion barrier. This bondable metallization that also acts as a diffusion barrier can prevent oxygen from air and gold from the wire-bond from infiltrating silicon carbide (SiC) monolithically integrated circuits (ICs) operating above 500 C in air for over 1,000 hours. This TaSi2/Pt/Ir/Pt metallization is easily bonded for electrical connection to off-chip circuitry and does not require extra anneals or masking steps. There are two ways that IrIS can be used in SiC ICs for applications above 500 C: it can be put directly on a SiC ohmic contact metal, such as Ti, or be used as a bond metal residing on top of an interconnect metal. For simplicity, only the use as a bond metal is discussed. The layer thickness ratio of TaSi2 to the first Pt layer deposited thereon should be 2:1. This will allow Si from the TaSi2 to react with the Pt to form Pt2Si during the 600 C anneal carried out after all layers have been deposited. The Ir layer does not readily form a silicide at 600 C, and thereby prevents the Si from migrating into the top-most Pt layer during future anneals and high-temperature IC operation. The second (i.e., top-most) deposited Pt layer needs to be about 200 nm to enable easy wire bonding. The thickness of 200 nm for Ir was chosen for initial experiments; further optimization of the Ir layer thickness may be possible via further experimentation. Ir itself is not easily wire-bonded because of its hardness and much higher melting point than Pt. Below the iridium layer, the TaSi2 and Pt react and form desired Pt2Si during the post-deposition anneal while above the iridium layer remains pure Pt as desired to facilitate easy and strong wire-bonding to the SiC chip circuitry.

Spry, David↗

Nonadiabatic Effects on Defect Diffusion in Silicon-Doped Nanographenes

Single atom impurities in graphene, substitutional silicon defects in particular, have been observed to diffuse under electron beam irradiation. However, the relative importance of elastic and inelastic scattering in facilitating their mobility remains unclear. Here, we employ excited-state electronic structure calculations to explore potential inelastic effects, and find an electronically nonadiabatic excited-state silicon diffusion pathway involving “softened” Si–C bonding that presents an ~2 eV lower diffusion barrier than the ground-state pathway. Beam-induced transition rates to this state indicate that the excited-state pathway is accessible through irradiation of the defect site. However, even in the limit of fully elastic scattering, upward nonadiabatic transitions are also possible along the diffusion coordinate, increasing the diffusion barrier and further demonstrating the potential for electronic nonadiabaticity to influence beam-induced atomic transformations in materials. Additionally, we also propose some experimentally testable signatures of such excited-state pathways.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Multiorbital charge-density wave excitations and concomitant phonon anomalies in Bi 2 Sr 2 LaCuO 6+δ

Charge-density waves (CDWs) are ubiquitous in underdoped cuprate superconductors. As a modulation of the valence electron density, CDWs in hole-doped cuprates possess both Cu-3d and O-2p orbital character owing to the strong hybridization of these orbitals near the Fermi level. Here, we investigate underdoped Bi 2 Sr 1.4 La 0.6 CuO 6+δ using resonant inelastic X-ray scattering (RIXS) and find that a short-range CDW exists at both Cu and O sublattices in the copper-oxide (CuO 2 ) planes with a comparable periodicity and correlation length. Furthermore, we uncover bond-stretching and bond-buckling phonon anomalies concomitant to the CDWs. Comparing to slightly overdoped Bi 2 Sr 1.8 La 0.2 CuO 6+δ , where neither CDWs nor phonon anomalies appear, we highlight that a sharp intensity anomaly is induced in the proximity of the CDW wavevector (Q CDW ) for the bond-buckling phonon, in concert with the diffused intensity enhancement of the bond-stretching phonon at wavevectors much greater than Q CDW . Our results provide a comprehensive picture of the quasistatic CDWs, their dispersive excitations, and associated electron-phonon anomalies, which are key for understanding the competing electronic instabilities in cuprates.

36 MATERIALS SCIENCE↗

Direct Visualization of Defect‐Controlled Diffusion in van der Waals Gaps

Abstract Diffusion processes govern fundamental phenomena such as phase transformations, doping, and intercalation in van der Waals (vdW) bonded materials. Here, the diffusion dynamics of W atoms by visualizing the motion of individual atoms at three different vdW interfaces: hexagonal boron nitride (BN)/vacuum, BN/BN, and BN/WSe 2 , by recording scanning transmission electron microscopy movies is quantified. Supported by density functional theory (DFT) calculations, it is inferred that in all cases diffusion is governed by intermittent trapping at electron beam‐generated defect sites. This leads to diffusion properties that depend strongly on the number of defects. These results suggest that diffusion and intercalation processes in vdW materials are highly tunable and sensitive to crystal quality. The demonstration of imaging, with high spatial and temporal resolution, of layers and individual atoms inside vdW heterostructures offers possibilities for direct visualization of diffusion and atomic interactions, as well as for experiments exploring atomic structures, their in situ modification, and electrical property measurements of active devices combined with atomic resolution imaging.

Chemistry↗

Investigation of Interfacial Layer for Friction Stir Scribe Welded Aluminum to Steel Joints

Friction stir scribe (FSS) welding as a recent derivative of friction stir welding has successfully fabricated a linear joint between automotive Al and steel sheets. However, there is a lack of understanding on its bonding mechanism. In this paper, the microstructures and phases at the bonding interface of FSS welded Al to ultra-high strength steel joints were studied using scanning electron microscopy and transmission electron microscopy. Based on the microstructural analysis, it is found that both mechanical and chemical bonding occurred simultaneously, and the energy-dispersive X-ray spectroscopy revealed that a thin intermetallic compound (IMC) layer was formed at the interface. Owing to the varied material flow and heat generation, the IMC layer thickness gradually decreased from the advancing side to the retreating side, and two IMCs (i.e. Fe2Al5 and Fe4Al13) were confirmed in different weld regions using diffraction pattern (or 1D fast Fourier transform pattern). Also, a Fe/Al solid solution was noticed in the IMC layer, and several Al fringes were found in the Fe-rich side in the scribe stir zone.

friction stir scribe welding, interfacial layer, i↗

In Situ Atomic Tracking on the Interfacial Etching and Reconfiguration of Cu-ReSe 2 Contact during Thermal Annealing

The Schottky barrier height can be greatly affected by the metal diffusion, reaction, and covalent bonding formation at the contact. Exploring novel methods and revealing the fundamental mechanisms for contact engineering are of vital importance for microelectronic devices. Here, in this study, the annealing induced interfacial reactions at Cu-ReSe 2 contact are dynamically revealed from the atomic scale. Accompanied by the diffusion of Se to Cu, ReSe 2 is gradually decomposed to a thin Re interlayer through a “chain-by-chain” manner. Theoretical calculations show that the Cu atoms can facilitate the chemical bond breaking of ReSe 2 , significantly lowering the Se diffusion energy barrier toward Cu. The formed Re/ReSe 2 heterostructure presents a metal-like band structure, which underscores the critical role of Cu in altering the interfacial chemistry and promoting carrier transport across the interface. Our results can provide vital insights into the contact properties of ReSe 2 and provide a possible method for fabricating high-performance ReSe 2 -based devices.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Alumina-Forming MAX Phases in Turbine Material Systems

Coatings for high temperature turbine components are based on low conductivity YSZ thermal barriers and protective NiAl, NiCoCrAlY bond coats. Good oxidation hot corrosion resistance, intermediate CTE, and strain tolerance of Ti2AlC and Cr2AlC MAX phases are thus of special interest. Their alumina scale growth follows a cubic law in accord with FeCrAlY alloys, with oxygen grain boundary diffusivity: Dgb 1.8 x 10-10 exp(-375 kJmole) m3s. Protective cubic kinetics are also found in high pressure burner rig (6 atm., 25 ms) and TGA tests of MAXthal 211Ti2AlC. The initial portion (0.1 hr) is dominated by fast TiO2 growth (with little evidence of scale volatility in high pressure water vapor, as found for SiO2 scales). Bulk Ti2AlC and Cr2AlC substrates show promise as potential bond coats for YSZ TBCs in 1000-1200 C furnace life (500 h) tests. Cr2AlC is proving to be very resistant to 700-900 C Na2SO4 hot corrosion and is of interest for disk alloys. Preliminary diffusion bonded Cr2AlC-superalloy hybrid couples have survived 1000 hr interrupted furnace tests at 800C with no indication of cracking or debonding. Diffusion zones of -NiAl+Cr7C3 were produced in these above 1000 C, but did not grow to any great extent after 1000 hr at 800 C. Processing as coatings presents challenges, however the basic properties of MAX phases provide novel opportunities for high temperature turbine components.

MAX phase↗

Interfacial characterization of SLM parts in multi-material processing: Metallurgical diffusion between 316L stainless steel and C18400 copper alloy

Multi-material processing in selective laser melting using a novel approach, by the separation of two different materials within a single dispensing coating system was investigated. 316L stainless steel and UNS C18400 Cu alloy multi-material samples were produced using selective laser melting and their interfacial characteristics were analyzed using focused ion beam, scanning electron microscopy, energy dispersive spectroscopy and electron back scattered diffraction techniques. A substantial amount of Fe and Cu element diffusion was observed at the bond interface suggesting good metallurgical bonding. Quantitative evidence of good bonding at the interface was also obtained from the tensile tests where the fracture was initiated at the copper region. Nevertheless, the tensile strength of steel/Cu SLM parts was evaluated to be 310 ± 18 MPa and the variation in microhardness values was found to be gradual along the bonding interface from the steel region (256 ± 7 HV{sub 0.1}) to the copper region (72 ± 3 HV{sub 0.1}). - Highlights: • Multi-material processing was successfully implemented and demonstrated in SLM. • Bi-metallic laminates of steel/Cu were successfully produced with the SLM process. • A substantial amount of Fe and Cu diffusion was observed at the bond interface. • Good metallurgical bonding was obtained at the interface of the steel/Cu laminates. • Highly refined microstructure was obtained due to rapid solidification in SLM.

36 MATERIALS SCIENCE↗

Structure of vapor-phase deposited Al-Ge thin films and Al-Ge intermediate layer bonding of Al-based microchannel structures.

Al-based high-aspect-ratio microscale structures (HARMS) are basic building blocks for all-Al microdevices. Bonding of Al-based HARMS is essential for device assembly. In this paper, bonding of Al-based HARMS to flat Al plates using Al-Ge thin film intermediate layers is investigated. The structure of sputter codeposited Al-Ge thin films was studied by high-resolution transmission electron microscopy as a function of the average film composition. The structure of the interface region between Al-based HARMS bonded to flat Al plates is studied by combining focused ion beam sectioning and scanning electron microscopy. An extended bonding interface region, {approx}100 {micro}m in width, is observed and suggested to result from liquidus/solidus reactions as well as diffusion of Ge in solid Al at the bonding temperature of 500 C. The extended interface region is suggested to be beneficial to Al-Al bonding via Al-Ge intermediate layers.

36 MATERIALS SCIENCE↗

Temperature-induced changes in the single-crystal structure of K{sub 9}H{sub 7}(SO{sub 4}){sub 8} {center_dot} H{sub 2}O

Interest in superprotonic crystals of M{sub m}H{sub n}(XO{sub 4}){sub (m+n)/2} is associated with the solution to the fundamental problem of modern condensed matter physics: investigations of structural phase transitions and the stabilization of phases with high proton conductivity with the aim of designing new functional materials. The available data suggest that changes in the physical properties in these crystals can occur through different structural mechanisms. To reveal the structural conditionality for anomalies in the physical properties, the crystals of K{sub 9}H{sub 7}(SO{sub 4}){sub 8} {center_dot} H{sub 2}O were studied by X-ray diffraction in the temperature range of 25-463 K, and the crystal structure of the high-temperature phase was determined at 418 K (sp. gr. Pcan). The results of the study indicate that the occurrence of high conductivity in K{sub 9}H{sub 7}(SO{sub 4}){sub 8} {center_dot} H{sub 2}O crystals at high temperatures is associated with the diffusion of water of crystallization, the hydrogen-bond network rearrangement, and the motion of K ions. The hydrogen-bond rearrangement and the hindered back diffusion of water to the crystal stabilize the high-temperature phase and ensure its supercooling to low temperatures.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Bonding large area silicon wafers

Diffusion welding of large area silicon wafers without altering electrical properties of semiconductor devices in wafers

Source record↗

Theory of activated penetrant diffusion in viscous fluids and colloidal suspensions

We heuristically formulate a microscopic, force level, self-consistent nonlinear Langevin equation theory for activated barrier hopping and non-hydrodynamic diffusion of a hard sphere penetrant in very dense hard sphere fluid matrices. Penetrant dynamics is controlled by a rich competition between force relaxation due to penetrant self-motion and collective matrix structural (alpha) relaxation. In the absence of penetrant-matrix attraction, three activated dynamical regimes are predicted as a function of penetrant-matrix size ratio which are physically distinguished by penetrant jump distance and the nature of matrix motion required to facilitate its hopping. The penetrant diffusion constant decreases the fastest with size ratio for relatively small penetrants where the matrix effectively acts as a vibrating amorphous solid. Increasing penetrant-matrix attraction strength reduces penetrant diffusivity due to physical bonding. For size ratios approaching unity, a distinct dynamical regime emerges associated with strong slaving of penetrant hopping to matrix structural relaxation. A crossover regime at intermediate penetrant-matrix size ratio connects the two limiting behaviors for hard penetrants, but essentially disappears if there are strong attractions with the matrix. Activated penetrant diffusivity decreases strongly with matrix volume fraction in a manner that intensifies as the size ratio increases. We propose and implement a quasi-universal approach for activated diffusion of a rigid atomic/molecular penetrant in a supercooled liquid based on a mapping between the hard sphere system and thermal liquids. Calculations for specific systems agree reasonably well with experiments over a wide range of temperature, covering more than 10 orders of magnitude of variation of the penetrant diffusion constant.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Titanium honeycomb panel testing

The paper describes the procedures of thermal mechanical tests carried out at the NASA Dryden Flight Research Facility on two tianium honeycomb wing panels bonded using liquid interface diffusion (LID) technique, and presents the results of these tests. The 58.4 cm square panels consisted of two 0.152-cm-thick Ti 6-2-4-2 face sheets LID-bonded to a 1.9-cm-thick honeycomb core, with bearing plates fastened to the perimeter of the upper and the lower panel surfaces. The panels were instrumented with sensors for measuring surface temperature, strain, and deflections to 315 C and 482 C. Thermal stress levels representative of those encountered during aerodynamic heating were produced by heating the upper panel surface and restraining all four edges. After more than 100 thermal cycles from room temperature to 315 C and 50 cycles from room temperature to 482 C, no significant structural degradation was detected in the panels.

Richards, W. L.↗

Interaction of vacuum ultraviolet excimer laser radiation with fused silica: II. Neutral atom and molecule emission

We report mass-resolved time-of-flight measurements of neutral Si, O, and SiO from ultraviolet-grade fused silica during pulsed 157-nm irradiation at fluences well below the threshold for optical breakdown. Although the emission intensities are strongly affected by thermal treatments that affect the density of strained bonds in the lattice, they are not consistently affected by mechanical treatments that alter the density of point defects, such as polishing and abrasion. We propose that the absorption of single 157 nm photons cleave strained bonds to produce defects that subsequently diffuse to the surface. There they react with dangling bonds to release neutral atoms and molecules. Hartree-Fock calculations on clusters containing these defects support the contention that defect interactions can yield emission. More direct emission by the photoelectronic excitation of antibonding chemical states is also supported.

36 MATERIALS SCIENCE↗

Inhibitive formation of nanocavities by introduction of Si atoms in Ge nanocrystals produced by ion implantation

Germanium nanocrystals (Ge-nc) were successfully synthesized by co-implantation of Si and Ge ions into a SiO{sub 2} film thermally grown on (100) Si substrate and fused silica (pure SiO{sub 2}), respectively, followed by subsequent annealing at 1150 °C for 1 h. Transmission electron microscopy (TEM) examinations show that nanocavities only exist in the fused silica sample but not in the SiO{sub 2} film on a Si substrate. From the analysis of the high-resolution TEM images and electron energy-loss spectroscopy spectra, it is revealed that the absence of nanocavities in the SiO{sub 2} film/Si substrate is attributed to the presence of Si atoms inside the formed Ge-nc. Because the energy of Si-Ge bonds (301 kJ·mol{sup −1}) are greater than that of Ge-Ge bonds (264 kJ·mol{sup −1}), the introduction of the Si-Ge bonds inside the Ge-nc can inhibit the diffusion of Ge from the Ge-nc during the annealing process. However, for the fused silica sample, no crystalline Si-Ge bonds are detected within the Ge-nc, where strong Ge outdiffusion effects produce a great number of nanocavities. Our results can shed light on the formation mechanism of nanocavities and provide a good way to avoid nanocavities during the process of ion implantation.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Kinetic Monte Carlo Simulations of Oxygen Diffusion in Environmental Barrier Coating Materials

Ceramic Matrix Composite (CMC) materials are of interest for use in next-generation turbine engine components, offering a number of significant advantages, including reduced weight and high operating temperatures. However, in the hot environment in which such components operate, the presence of water vapor can lead to corrosion and recession, limiting the useful life of the components. Such degradation can be reduced through the use of Environmental Barrier Coatings (EBCs) that limit the amount of oxygen and water vapor reaching the component. Candidate EBC materials include Yttrium and Ytterbium silicates. In this work we present results of kinetic Monte Carlo (kMC) simulations of oxygen diffusion, via the vacancy mechanism, in Yttrium and Ytterbium disilicates, along with a brief discussion of interstitial diffusion. An EBC system typically includes a bond coat located between the EBC and the component surface. Bond coat materials are generally chosen for properties other than low oxygen diffusivity, but low oxygen diffusivity is nevertheless a desirable characteristic, as the bond coat could provide some additional component protection, particularly in the case where cracks in the coating system provide a direct path from the environment to the bond coat interface. We have therefore performed similar kMC simulations of oxygen diffusion in this material.

Good, Brian S.↗