Evaluation of high temperature structural adhesives for extended service

The preliminary evaluation of crosslinked polyphenyl quinoxaline (X-PPQ), LARC-TPI, ethyl terminated polysulfone (ETPS), and crosslinked polyimide (X-PI) as adhesives is presented. Lap shear strength stability under thermal, combined thermal/humidity, and stressed and unstressed Skydrol exposure was determined. The X-PPQ, LARC-TPI, and X-PI exhibited good adhesive performance at 505K (450 F) after 1000 hours at 505K. These three polymers also performed well after exposure to combined elevated temperature/high humidity, as well as, to Skydrol while under stress. The ETPS exhibited good ambient temperature adhesive properties, but performed poorly under all other exposure conditions, presumably due to inadequate chain extension and crosslinking.

Hill, S. G.↗

Shock wave properties of anorthosite and gabbro

Hugoniot data on San Gabriel anorthosite and San Marcos gabbro to 11 GPA are presented. Release paths in the stress-density plane and sound velocities are reported as determined from particl velocity data. Electrical interference effects precluded the determination of accurate release paths for the gabbro. Because of the loss of shear strength in the shocked state, the plastic behavior exhibited by anorthosite indicates that calculations of energy partitioning due to impact onto planetary surfaces based on elastic-plastic models may underestimate the amount of internal energy deposited in the impacted surface material.

Boslough, M. B.↗

Wind Erosion and Dune Formation on High Frozen Bluffs

Frost penetration increases upslope on barren, windswept bluffs in cold environments. Along the south shore of Lake Superior, near the brow of 100 m high bluffs it typically exceeds 5 m. Frost increases the shear strength of damp sand to a level comparable to that of concrete, making winter slopes highly stable despite undercutting by waves and ground-water sapping along the footslope. Sublimation of interparticle ice in the slope face increases with wind speed and lower vapor pressures. The cold and dry winter winds of Lake Superior ablate these slopes through loss of binding ice. Wind erosion rates, based on measurements of sand accumulation on the forest floor downwind of the brow, show most airborne sand falls out within several meters of the brow, forming a berm 1 to 3 m high after many years. The spatial pattern of sand deposition, however, varies considerably over distances of several hundred meters along the top bluffs in response to frost conditions and the build-up of gravel lag on the slope face, sand exposure from mass movements, and local aerodynamics of the crest slope. The formation of perched sand dunes in the Great Lakes region is clearly related to wind erosion of sand from high bluffs in winter. Broadly similar processes may operate on Mars.

Marsh, W. M.↗

Rubber-toughened polyfunctional epoxies - Brominated vs nonbrominated formulated for graphite composites

A new, commercially available, trifunctional epoxy resin (tris-(hydroxyphenyl)-methane triglycidyl ether) was modified with synthetic rubber to increase the impact resistance of epoxy/graphite composites. These composites were reinforced with commercially available satin-weave carbon cloth using two formulations of epoxies (brominated and nonbrominated) containing various amounts of carboxy-terminated butadience acrylonitrile (CTBN) rubber that had been prereacted with epoxy resin. The impact resistance was determined by measuring the interlaminar shear strength of the composites after impact. The mechanical properties, such as flexural strength and modulus at room temperature and at 93 C, were also determined. Measurements were taken of the flammability and glass transition temperature (Tg); and a thermal-gravimetric analysis was made.

Nir, Z.↗

Processing study of a high temperature adhesive

An adhesive-bonding process cycle study was performed for a polyimidesulphone. The high molecular weight, linear aromatic system possesses properties which make it attractive as a processable, low-cost material for elevated temperature applications. The results of a study to better understand the parameters that affect the adhesive properties of the polymer for titanium alloy adherends are presented. These include the tape preparation, the use of a primer and press and simulated autoclave processing conditions. The polymer was characterized using Fourier transform infrared spectroscopy, glass transition temperature determination, flow measurements, and weight loss measurements. The lap shear strength of the adhesive was used to evaluate the effects of the bonding process variations.

Progar, D. J.↗

Strain measurement within a single-lap joint using embedded strain gages

An experimental method used to measure the in-plane normal-axial strains produced within a single-lap joint is described in which a resistance-foil strain gage is embedded within the joint prior to curing of the adhesive. Nominal dimensions of the titanium Ti-6-4 adherends were 0.13 x 2.5 x 12.7 cm and an overlap of 2.5 cm was used. The joint was bonded with FM-300 structural adhesive. The average ultimate shear strength of the gaged specimens and control specimens was 16.1 MPa and 14.1 MPa. A significant advantage of the proposed method is that strains internal to the joint are measured, rather than strains at an external edge. The presence of the gage was found to be not detrimental to bond performance.

Tuttle, M. E.↗

The Effect of Matrix and Fiber Properties on Impact Resistance

The basic material properties which control impact damage are identified and testing techniques are assessed. It is demonstrated that static indentation tests can provide better information about failure processes than impact tests, and they are simpler to conduct. In thin and thick laminates, it was found that the matrix shear strength controls the onset of delamination damage and that the fiber strength controlled the penetration phase. In thin laminates, tough matrices do little to enhance impact resistance.

Elber, W.↗

Composite Property Dependence on the Fiber, Matrix, and the Interphase

The matrix properties of a difunctional epoxy, Epon 828, were varied. The Hercules type A fiber was also utilized in this investigation. The fiber and the interface between fiber and matrix were examined in terms of shear strength. Micrographs of the epoxy matrix are presented.

Drzal, L. T.↗

Particle velocity experiments in anorthosite and gabbro

Shock wave experiments were conducted in San Gabriel anorthosite and San Marcos gabbra 10 11 GPa using a 40 mm-borne propellant gun. Particle velocities were measured directly at several points in each target by means of electromagnetic gauges. Hugoniot states were calculated by determining shock-transit time from the gauge records. Sound speeds indicate a loss of shear strength upon sock compression for both rocks, with the strength loss persisting upon release to zero stress om the anorthosite. Stress-density release paths in the anorthosite indicate possible transformation of albite to jadeite + (quartz or coesite), with the amount of material transformed increasing as a function of shock stress. Electrical interferene effects in the gabbro precluded the determination of accurate release paths for the rock.

Boslough, M. B.↗

Development of a heterogeneous laminating resin system

The factors which effect the impact resistance of laminating resin systems and yet retain equivalent performance with the conventional 450 K curing epoxy matrix systems in other areas were studied. Formulation work was conducted on two systems, an all-epoxy and an epoxy/bismaleimide, to gain fundamental information on the effect formulation changes have upon neat resin and composite properties. The all-epoxy work involved formulations with various amounts and combinations of eight different epoxy resins, four different hardeners, fifteen different toughening agents, a filler, and a catalyst. The epoxy/bismaleimide effort improved formulations with various amounts and combinations of nine different resins, four different hardeners, eight different toughening agents, four different catalysts, and a filler. When a formulation appeared to offer the proper combination of properties required for a laminating resin Celion 3K-70P fabric was prepregged. Initial screening tests on composites primarily involved Gardner type impact and measurement of short beam shear strengths under dry and hot/wet conditions.

Biermann, T. F.↗

Preparation and properties of silane-endcapped polyimide adhesives

Silane-endcapped polyimide high temperature adhesive formulations were prepared by reacting anhydride-terminated poly(amic acid), obtained from benzophenonetetracarboxylic dianhydride and a diamine (3,3'-, 3,4'- or 4,4'-diaminodiphenylmethane and 3,3', 3,4'- or 4,4'-diaminobenzophenone) with varying amounts of gama-aminopropyltriethoxysilane in dimethylacetamide. Resin properties were evaluated by torsional braid analysis and thermogravimetric analysis. Lap shear strengths of some of the adhesive bonds were determined at room temperature and at 177 C before and after ageing at 200 C for 2500 h and after boiling in water for 72 h.

Maudgal, S.↗

Shock wave properties of anorthosite and gabbro

Huyoniot data on San Gabriel anorthosite and San Marcos gabbro to 11 GPA are presented. Release paths in the stress-density plane and sound velocities are reported as determined from partial velocity data. Electrical interference effects precluded the determination of accurate release paths for the gabbro. Because of the loss of shear strength in the shocked state, the plastic behavior exhibited by anorthosite indicates that calculations of energy partitioning due to impact onto planetary surfaces based on elastic-plastic models may underestimate the amount of internal energy deposited in the impacted surface material.

Boslough, M. B.↗

SEM/XPS analysis of fractured adhesively bonded graphite fibre-reinforced polyimide composites

The surfaces of the graphite fiber-reinforced polyimide composites presently pretreated prior to bonding with polyimide adhesive contained variable amounts of a fluoropolymer, as determined by X-ray photoelectron spectroscopy. Lap shear strengths were determined for unaged samples and for those aged over 500- and 1000-hour periods at 177 and 232 C. Unaged sample lap strengths, which were the highest obtained, exhibited no variation with surface pretreatment, but a significant decrease is noted with increasing aging temperature. These thermally aged samples, however, had increased surface fluorine concentration, while a minimal concentration was found in unaged samples. SEM demonstrated a progressive shift from cohesive to adhesive failure for elevated temperature-aged composites.

Devilbiss, T. A.↗

Lubricants and Additives Affect Spur-Gear Fatigue

Surface-fatigue tests conducted with AISI 9310 steel spur gears show surface-fatigue life of AISI 9310 steel spur gears increased as much as 400 percent by addition of small amount of phosphorus-type extreme-pressure (EP) additive in lubricant. Antiwear or EP additives either absorbed onto surface or react with surface to form protective coating or surface film. Boundary film provides barrier that prevents contact of metal surfaces and provides low shear strength, which reduces friction coefficient below base metal.

Scibbe, H.↗

Ultrasonic evaluation of mechanical properties of thick, multilayered, filament wound composites

A preliminary investigation is conducted to define capabilities and limitations of ultrasonic and acousto-ultrasonic measurements related to mechanical properties of filament wound graphite/epoxy composite structures. The structures studied are segments of filament wound cylinders formed of multiple layers of hoop and helical windings. The segments consist of 24 to 35 layers and range from 3.02 to 3.34 cm in wall thickness. The resultant structures are anisotropic, heterogeneous, porous, and highly attenuating to ultrasonic frequencies greater than 1 MHz. The segments represent structures to be used for space shuttle booster cases. Ultrasonic velocity and acousto-ultrasonic stress wave factor measurement approaches are discussed. Correlations among velocity, density, and porosity, and between the acousto-ultrasonic stress wave factor and interlaminar shear strength are presented.

Kautz, H. E.↗

Investigation of Low-temperature Solders for Cryogenic Wind Tunnel Models

The advent of high Reynolds number cryogenic wind tunnels has forced alteration of manufacturing and assembly techniques and eliminated usage of many materials associated with conventional wind tunnel models. One of the techniques affected is soldering. Solder alloys commonly used for wind tunnel models are susceptible to low-temperature embrittlement and phase transformation. The low-temperature performance of several solder alloys is being examined during research and development activities being conducted in support of design and fabrication of cryogenic wind tunnel models. Among the properties examined during these tests are shear strength, surface quality, joint stability, and durability when subjected to dynamic loading. Results of these tests and experiences with recent models are summarized.

Firth, G. C.↗

Thermo-oxidative stability of graphite fiber/PMR-15 polyimide composites at 350 deg C

A series of graphite fiber/PMR-15 polyimide composites were subjected to isothermal aging at 350 C in flowing air (100 cc/min and 1000 cc/min) over a 520 hr time period. The graphite fibers were analyzed by ISS/SIMS techniques before composite fabrication. Fibers exposed at the surface of the composite due to the isothermal aging process were also analyzed by the ISS/SIMS method. Component and composite weight less studies were also conducted for similarly exposed materials. Optical micrograph investigations of composites to follow the progress of the thermo-oxidative process were also conducted. Flexural and interlaminar shear strengths of the imaged and aged composites were measured. The relationship of component and composite properties as they relate to the thermo-oxidative behavior of the materials was discussed.

Scola, D. A.↗

The 371 deg C mechanical properties of graphite/polyimide composites

A series of condensation polyimides based on pyromellitic dianhydride is synthesized and evaluated for potential application at 371 C. Several three-and four-ring benzenoid diamine systems containing oxygen bridging groups are investigated. Thermomechanical analysis of neat resin specimens indicate that the polyimide prepared from the dimethyl ester of pyrometallitic acid (PMDE) and 2,2-bis4-(4'-aminophenoxy) phenyl]-1,1,1,3,3,3- hexafluoropropane (BDAF) is the only resin system which has a glass transition temperature (Tg) above 371 C. The Tg of the PMDE/BDAF polyimide is found to be 390 C after a postcure air at 371 C for 24 hr. Unidirectional composites are fabricated from the PMDE/BDAF system and unsized Celion 6000 graphite fibers. Final cure temperatures in the range of 371 to 427 C with an applied pressure of 10.34 to 13.78 MPa are investigated. The void content of the composites ranges from 4.6 to 8.6 percent. Composites cured at 399 C under a pressure of 10.34 MPa and postcured in air at 371 C for 24 hr exhibit the highest 371 C interlaminar shear strength (ILSS, 40.7 MPa) and flexural strength (758 MPa). The thermo-oxidative stability of the composites is determined by subjecting specimens to isothermal exposure at 371 C in air at atmospheric pressure, as well as a pressure of 0.52 MPa. Specimens exposed at atmospheric pressure exhibit a weight loss of 12 percent after 200 hr of exposure and 88 percent retention of its original 371 C ILSS. In contrast, the specimens exposed at 0.52 MPa pressure exhibit a comparable weight loss after only 72 hr, and a 71 percent retention of its original 371 C ILSS.

Delvigs, P.↗