At least 505 records · Page 28

Fracture surface characteristics of off-axis composites

The fracture surface characteristics of off-axis high-modulus graphite-fiber/epoxy composite specimens were studied, using a scanning electron microscope (SEM). The specimens were subjected to tensile loading at various angles (0 deg - 90 deg) to the fiber direction. SEM photomicrographs of the fractured surfaces revealed three different load angle regions with distinct fracture characteristics. Based on these revelations, criteria were established which can be used to characterize fracture surfaces with respect to a predominant single stress fracture mode.

Sinclair, J. H.↗

The effect of microstructure and strength on the fracture toughness of an 18 Ni, 300 grade maraging steel

Fractography and metallographic sectioning were used to investigate the influence of microstructure and strength on the fracture toughness (KIc) and fracture mechanism of an 18 Ni, 300 grade maraging steel. Increased yield strength from 1442 to 2070 MN/m squared through precipitation hardening results in a KIc loss from 143 to 55 MN/m superscript 3/2. Ti (C,N) Ti2S, and TiC inclusions in sizes from 1 to 8, 1 to 15, and 0.1 to 2 microns respectively serve as sites for void nucleation and lead to fracture by the dimpled rupture process in all strength levels considered. TiC nucleated dimples occupy more than half the fracture in all conditions. Void nucleation rate and resultant number of dimples per unit area of fracture increase with increasing yield strength. Average dimple size decreases with increasing strength and/or overaging which follows from the decreasing amount of stable void growth measured by sectioning tensile specimens. Void growth is assisted by crack branching along a path of TiC inclusions. Coalescence occurs in the highest strength materials by a combination of TiC void nucleation and premature separation at strengthening precipitates.

Psioda, J. A.↗

Fracture surface characteristics of off-axis composites

The fracture surface characteristics of off-axis high-modulus graphite-fiber/epoxy composite specimens were studied using a scanning electron microscope (SEM). The specimens were subjected to tensile loading at various angles (0-90 deg) to the fiber direction. SEM photomicrographs of the fractured surfaces revealed three different load angle regions with distinct fracture characteristics. Based on these revelations, criteria were established which can be used to characterize fracture surfaces with respect to a predominant 'single-stress' fracture mode.

Sinclair, J. H.↗

Fracture toughness of silicon

The paper presents a study to determine the fracture toughness and to characterize fracture modes of silicon as a function of the orientation of single-crystal and polycrystalline material. It is shown that bar specimens cracked by Knoop microhardness indentation and tested to fracture under four-point bending at room temperature were used to determine the fracture toughness values. It is found that the lowest fracture toughness value of single crystal silicon was 0.82 MN/m to the 3/2 in the 111 plane type orientation, although the difference in values in the 111, 110, and 100 planes was small.

Chen, C. P.↗

Mode I fracture behavior of nonlinear materials

A finite element analysis is presented for the Mode I fracture behavior of cracked plates (stationary crack) made of different nonlinear materials (elastoplastic or elastic locking). The assumed stress-strain behavior of the nonlinear materials was piecewise linear. For each given 'stationary' crack size, the corresponding critical remote tensile stress was calculated based on the maximum crack-tip stress failure criterion. It was found that in the log-log plots of the critical remote stress versus critical crack length, the fracture data of the piecewise linear materials obey a 'stepwise-linear-inverse-square-root' fracture law. It is also shown how the fracture data of the piecewise linear materials can be fitted by proper piecewise graphical shifting of the classical 'inverse-square-root' fracture curve for the linearly elastic materials.

Ko, W. L.↗

On the feasibility of quantitative ultrasonic determination of fracture toughness: A literature review

The three main topics covered are: (1) fracture toughness and microstructure, (2) quantitative ultrasonic and microstructure; and (3) scattering and related mathematical methods. Literature in these areas is reviewed to give insight to the search of a theoretical foundation for quantitative ultrasonic measurement of fracture toughness. The literature review shows that fracture toughness is inherently related to the microstructure and in particular, it depends upon the spacing of inclusions or second particles and the aspect ratio of second phase particles. There are indications that ultrasonic velocity attenuation measurements can be used to determine fracture toughness. The leads to a review of the mathematical models available in solving boundary value problems related to microstructural factors that govern facture toughness and wave motion. A framework towards the theoretical study for the quantitative determination of fracture toughness is described and suggestions for future research are proposed.

Fu, L. S.↗

The fracture morphology of nickel-base superalloys tested in fatigue and creep-fatigue at 650 C

The fracture surfaces of compact tension specimens from seven nickel-base superalloys fatigue tested at 650 C were studied by scanning electron microscopy and optical metallography to determine the nature and morphology of the crack surface in the region of stable growth. Crack propagation testing was performed as part of an earlier study at 650 C in air using a 0.33 Hz fatigue cycle and a creep-fatigue cycle incorporating a 900 second dwell at maximum load. In fatigue, alloys with a grain size greater than 20 micrometers, HIP Astroloy, Waspaloy, and MERL 76, exhibited transgranular fracture. MERL 76 also displayed numerous fracture sites which were associated with boundaries of prior powder particles. The two high strength, fine grain alloys, IN 100 and NASA IIB-7, exhibited intergranular fracture. Rene 95 and HIP plus forged Astroloy displayed a mixed failure mode that was transgranular in the coarse grains and intergranular in the fine grains. Under creep-fatigue conditions, fracture was found to be predominantly intergranular in all seven alloys.

Gayda, J.↗

Fatigue and fracture research in metals

Fatigue and fracture research on monolithic and laminated metals is discussed. The research concentrated on three areas: stress analyses of two and three dimensional cracked bodies, fatigue crack growth, and fracture toughness. Analytical methods were developed to predict fatigue crack growth and fracture strengths of cracked specimens. Such specimens represent typical aircraft structural details (such as cracks from holes). These specimens were subjected to simple constant amplitude loading and to more complex flight load histories. Test data from both in house tests and from the literature are used to substantiate the analytical methods. These analyses extended the theory of fracture mechanics to deal with fatigue crack growth and fracture of complex crack configurations that are typical of aircraft materials and structural details.

J. C. Newman, Jr.↗

Lithospheric flexure at fracture zones

Studies attempting to demonstrate that lithospheric flexure occurs across the Pioneer and Mendocino fracture zones, and that the flexural topography is a topographic expression at these fracture zones, are presented. The flexure is modelled and compared with predicted depths with five bathymetric profiles which cross the two fracture zones at different ages. The model uses a thin elastic plate overlying an incompressible fluid half-space, and incorporates a temperature-dependent effective elastic thickness. Several conclusions were derived from this study. First, it is found that no significant slip on the fossil fault planes of the Mendocino and Pioneer fracture zones exists. In addition, the flexural amplitude is determined to increase with age. Finally, it is concluded that there is elastic coupling between the Mendocino and Pioneer fracture zones since the separation is less than a flexural wavelength.

Sandwell, D.↗

Strength and fracture toughness of reaction-bonded Si3N4

Fracture strength and fracture toughness measurements were made on reaction-bonded Si3N4 materials with a range of alpha/beta ratios. The results do not indicate any clear relation between the modulus of rupture and the alpha/beta ratio over the range 1.5-9. Values for the modulus of rupture range from 219 to 290 MN per sq m, with an overall average of 238 MN per sq m. The notched beam fracture toughness is found to be constant over the range of microstructures produced, indicating that of the various microstructural features (e.g., alpha/beta ratio and pore size and distribution) no single element has a controlling influence over fracture toughness and the fracture surface energy.

Danforth, S. C.↗

Hygrothermomechanical fracture stress criteria for fiber composites with sense-parity

Hygrothermomechanical fracture stress criteria are developed and evaluated for unidirectional composites (plies) with sense-parity. These criteria explicity quantify the individual contributions of applied, hygral and thermal stresses as well as couplings among these stresses. The criteria are for maximum stress, maximum strain, internal friction, work-to-fracture and combined-stress fracture. Predicted results obtained indicate that first ply failure will occur at stress levels lower than those predicted using criteria currently available in the literature. Also, the contribution of the various stress couplings (predictable only by fracture criteria with sense-parity) is significant to first ply failure and attendant fracture modes.

Chamis, C. C.↗

Spartan Release Engagement Mechanism (REM) stress and fracture analysis

The revised stress and fracture analysis of the Spartan REM hardware for current load conditions and mass properties is presented. The stress analysis was performed using a NASTRAN math model of the Spartan REM adapter, base, and payload. Appendix A contains the material properties, loads, and stress analysis of the hardware. The computer output and model description are in Appendix B. Factors of safety used in the stress analysis were 1.4 on tested items and 2.0 on all other items. Fracture analysis of the items considered fracture critical was accomplished using the MSFC Crack Growth Analysis code. Loads and stresses were obtaind from the stress analysis. The fracture analysis notes are located in Appendix A and the computer output in Appendix B. All items analyzed met design and fracture criteria.

Marlowe, D. S.↗

Fracture modes in notched angleplied composite laminates

The Composite Durability Structural Analysis (CODSTRAN) computer code is used to determine composite fracture. Fracture modes in solid and notched, unidirectional and angleplied graphite/epoxy composites were determined by using CODSTRAN. Experimental verification included both nondestructive (ultrasonic C-Scanning) and destructive (scanning electron microscopy) techniques. The fracture modes were found to be a function of ply orientations and whether the composite is notched or unnotched. Delaminations caused by stress concentrations around notch tips were also determined. Results indicate that the composite mechanics, structural analysis, laminate analysis, and fracture criteria modules embedded in CODSTRAN are valid for determining composite fracture modes.

Irvine, T. B.↗

Fracture toughness of fibrous composite materials

Laminates with various proportions of 0 deg, 45 deg, and 90 deg plies were fabricated from T300/5208 and T300/BP-907 graphite/epoxy prepreg tape material. The fracture toughness of each laminate orientation or lay-up was determined by testing center-cracked specimens, and it was also predicted with the general fracture-toughness parameter. The predictions were good except when crack-tip splitting was large, at which time the toughness and strengths tended to be underpredicted. By using predictions, a parametric study was also made of factors that influence fracture toughness. Fiber and matrix properties as well as lay-up were investigated. Without crack-tip splitting, fracture toughness increases in proportion to fiber strength and fiber volume fraction, increases linearly with E(22)/E(11), is largest when the modulus for non-0 deg fibers is greater than that of 0 deg fibers, and is smallest for 0(m)/90(p)(s) lay-ups. (The E(11) and E(22) are Young's moduli of the lamina parallel to and normal to the direction of the fibers, respectively). For a given proportion of 0 deg plies, the most notch-sensitive lay-ups are 0(m)/90(p)(s) and the least sensitive are 0(m)/45(n)(s) and alpha(s). Notch sensitivity increases with the proportion of 0 deg plies and decreases with alpha. Strong, tough matrix materials, which inhibit crack-tip splitting, generally lead to minimum fracture toughness.

Poe, C. C., Jr.↗

Influence of the resin on interlaminar mixed-mode fracture

Both literature review data and new data on toughness behavior of seven matrix and adhesive systems in four types of tests were studied in order to assess the influence of the resin on interlaminar fracture. Mixed mode (i.e., various combinations of opening mode 1, G sub 1, and shearing mode 2; G sub 2) fracture toughness data showed that the mixed mode relationship for failure appears to be linear in terms of G sub 1 and G sub 2. The study further indicates that fracture of brittle resins is controlled by the G sub 1 component, and that fracture of many tough resins is controlled by total strain-energy release rate, G sub T. Regarding the relation of polymer structure and the mixed mode fracture: high mode 1 toughness requires resin dilatation; dilatation is low in unmodified epoxies at room temperature/dry conditions; dilatation is higher in plasticized epoxies, heated epoxies, and in modified epoxies; modification improves mode 2 toughness only slightly compared with mode 1 improvements. Analytical aspects of the cracked lap shear test specimen were explored.

Johnson, W. S.↗

Interlaminar fracture of random short-fiber SMC composite

In the experimental phase of the present study of the interlaminar fracture behavior of a randomly oriented short fiber sheet molding compound (SMC) composite, the double cantilever beam fracture test is used to evaluate the mode I interlaminar fracture toughness of different composite thicknesses. In the analytical phase of this work, a geometrically nonlinear analysis is introduced in order to account for large deflections and nonlinear load deflection curves in the evaluation of interlaminar fracture toughness. For the SMC-R50 material studied, interlaminar toughness is an order of magnitude higher than that of unreinforced neat resin, due to unusual damage mechanisms ahead of the crack tip, together with significant fiber bridging across crack surfaces. Composite thickness effects on interlaminar fracture are noted to be appreciable, and a detailed discussion is given on the influence of SMC microstructure.

Wang, S. S.↗

Fracture of thick graphite/epoxy laminates with part-through surface flaws

Fracture behavior of tensile specimens containing through-the-thickness flaws and part-through semi-elliptic surface flaws was investigated. The material was T300/5208 graphite/epoxy, with a stacking sequence 0/+ or - 45/90 sub ns. Laminate thicknesses ranged from 8 to 120 plies. Fracture toughness for specimens with through-the-thickness flaws was a function of laminate thickness. Fracture toughness was also independent of crack size. Fracture toughness for the thick laminates was also independent of specimen geometry (center-cracked tension specimen, compact tension specimen, and three-point bend specimen). Using the asymptotic value of facture toughness and linear elastic isotropic fracture mechanics, the notched strength of tensile specimens with semi-elliptic surface flaws was predicted. The strength ratio is a function of the flaw depth (a/t) and flaw aspect (a/c) ratios. Comparisons between predicted and experimental strengths are good for large values of a/t. The notched strength of filament wound graphite/epoxy tensile specimens with part-through surface flaws was also predicted.

Morris, D. H.↗

Dynamic fracture mechanics

Dynamic fracture and crack propagation concepts for ductile materials are reviewed. The equations for calculating dynamic stress integrity and the dynamic energy release rate in order to study dynamic crack propagation are provided. The stress intensity factor versus crack velocity relation is investigated. The uses of optical experimental techniques and finite element methods for fracture analyses are described. The fracture criteria for a rapidly propagating crack under mixed mode conditions are discussed; crack extension and fracture criteria under combined tension and shear loading are based on maximum circumferential stress or energy criteria such as strain energy density. The development and use of a Dugdale model and finite element models to represent crack and fracture dynamics are examined.

Kobayashi, A. S.↗