Search NASA⌕ Search

SEARCH · Search NASA

Results for “Mechanical Impedance”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 523 records · Page 29

Electrochemical Healing of Dendrites in Garnet-Based Solid Electrolytes

Garnet oxides are a promising material family for solid-state batteries (SSBs). Dendrite formation in solid electrolytes critically limits the applicability of SSBs because of limiting Coulombic efficiency and power capability. In this study, the authors report operando electrochemical healing of dendrites in a garnet-based solid electrolyte (SE). Dendrites were deliberately formed at high operational current density (2 mA cm –2 ) beyond the critical current density (0.55 mA cm –2 ) of the used garnet SE. Electrochemical impedance spectroscopy and scanning electron microscopy were used to confirm dendrite growth in the SE. Dendrites were subsequently healed electrochemically via plating and stripping at 20 and 1 μA cm –2 current densities. Removal of dendrites was shown by an increase in bulk and interfacial resistance and a progressive increase in polarization during galvanostatic plating and stripping. High local current density at the dendrite tips was identified as the mechanism for preferentially removing dendrites electrochemically. The dendrite detection and healing methods discussed here are crucial for extending the life of SSBs.

25 ENERGY STORAGE↗

Cycling Performance and Structure Evolution of Co-Free Lithium- and Manganese-Rich Layered Oxides in Lithium-Ion Batteries

Lithium- and manganese-rich (LMR) layered oxides are high-capacity cathode materials that are being considered for electric vehicle (EV) lithium-ion batteries (LIBs). Here, we investigate the electrochemical cycling behavior of cells containing a cobalt-free LMR oxide, 0.3Li 2 MnO 3 ·0.7LiMn 0.5 Ni 0.5 O 2 , paired with either Li or graphite anodes. Two- and three-electrode cells are cycled under varying conditions to examine the effects of oxide activation, upper cutoff voltage, separator type, and electrolyte composition. Post-cycling characterization of harvested electrodes, with electrochemical, X-ray absorption spectroscopy, and solid-state 6 Li nuclear magnetic resonance spectroscopy techniques, are used to correlate cell performance changes with redox state evolution in the oxide and Li inventory shifts in the cell. Our results show that capacity fade and impedance rise primarily originate at the graphite anode and LMR cathode, respectively. Notably, while Ni undergoes reversible redox, Mn shows no evidence of bulk redox activity even in highly-aged electrodes: only relithiated LMR electrodes show some reduction of Mn. Graphite electrodes degrade due to particle isolation and SEI growth, exacerbated by Mn dissolution and deposition on graphite anodes. These findings highlight the coupled structural and electrochemical degradation mechanisms in LMR/graphite cells and underscore lithium inventory retention and electrode interfacial stability as critical factors for enhancing long-term performance.

Badami, Pavan P. [Argonne National Laboratory (ANL↗

Evaluating proxies for the drivers of natural gas productivity using machine-learning models

We report the extensive development of unconventional reservoirs using horizontal drilling and multistage hydraulic fracturing has generated large volumes of reservoir characterization and production data. The analysis of this abundant data using statistical methods and advanced machine-learning (ML) techniques can provide data-driven insights into well performance. Most predictive modeling studies have focused on the impact that different well completion and stimulation strategies have on well production but have not fully exploited the available in situ rock property data to determine its role in reservoir productivity. We have used machine-learning techniques to rank rock mechanical properties, microseismic attributes, and stimulation parameters in the order of their significance for predicting natural gas production from an unconventional reservoir. The data for this study came from a hydraulically fractured well in the Marcellus Shale in Monongalia County, West Virginia. The data classes included measurements aggregated by well completion stage that included (1) gas production, (2) well-log-derived measurements including bulk density, elastic moduli, shear impedance, compressional impedance, brittleness, and gamma measurements, (3) microseismic attributes, (4) long-period long-duration (LPLD) event counts, (5) fracture counts, and (6) stimulation parameters that included the fluid injection volume and average pumping pressure. To identify observable proxies for the drivers of gas production, we evaluated five commonly used ML approaches including multivariate adaptive regression spline, Gaussian mixture model, random forest, gradient boosting, and neural network. We selected five variables including LPLD event count, seismogenic b-value, hydraulic diffusivity, cumulative moment, and fluid volume as the features most likely to impact gas productivity at the stage level in the study area. The data-driven selection of these parameters for their importance in determining gas production can help reservoir engineers design more effective hydraulic-fracture treatments in the Marcellus Shale and other similar unconventional reservoirs. Plain language summary: We use machine-learning methods and data-driven selection of reservoir parameters to rank and better understand their importance in determining gas production, which can help reservoir engineers design more effective hydraulic-fracture treatments in the Marcellus Shale and other similar unconventional reservoirs.

58 GEOSCIENCES↗

Do vestibular otolith organs participate in human orthostatic blood pressure control?

We hypothesized that vestibular otolith organ stimulation contributes to human orthostatic responses. Twelve subjects underwent three 60 degrees upright tilts: (1) with the neck flexed from 0 degrees to 30 degrees relative to the body during 60 degrees tilt, such that the head moved from horizontal to 90 degrees above horizontal (0 to 1 Gz otolith stimulation); (2) with the head and body aligned, such that they tilted together to 60 degrees (0 to 0.87 Gz otolith stimulation); and (3) with the neck flexed 30 degrees relative to the body during supine conditions, and the neck then extended to -30 degrees during 60 degrees body tilting, such that the head remained at 30 degrees above horizontal throughout body tilting (constant 0.5 Gz otolith stimulation). All three tilt procedures increased thoracic impedance, sympathetic nerve activity (N = 8 of 12), arterial pressure, and heart rate relative to supine conditions (all P < 0.04). Within the first 20 s of tilt, arterial pressure increased most obviously in the 0 to 1 Gz otolith condition. Thoracic impedance tended to increase more in otolith-constant conditions, but no dependent variable differed significantly between tilt conditions, and no significant time x tilt interactions emerged. Otolith inputs may contribute to early transient adjustments to orthostasis. However, lack of significant main effects of tilt condition and time x tilt interactions suggests that potential otolith effects on the variables we studied are relatively subtle and ephemeral, or that other mechanisms compensate for a lack of change in otolith input with orthostasis.

Non-NASA Center↗

A Computational and Experimental Study of Resonators in Three Dimensions

In a previous work by the present authors, a computational and experimental investigation of the acoustic properties of two-dimensional slit resonators was carried out. The present paper reports the results of a study extending the previous work to three dimensions. This investigation has two basic objectives. The first is to validate the computed results from direct numerical simulations of the flow and acoustic fields of slit resonators in three dimensions by comparing with experimental measurements in a normal incidence impedance tube. The second objective is to study the flow physics of resonant liners responsible for sound wave dissipation. Extensive comparisons are provided between computed and measured acoustic liner properties with both discrete frequency and broadband sound sources. Good agreements are found over a wide range of frequencies and sound pressure levels. Direct numerical simulation confirms the previous finding in two dimensions that vortex shedding is the dominant dissipation mechanism at high sound pressure intensity. However, it is observed that the behavior of the shed vortices in three dimensions is quite different from those of two dimensions. In three dimensions, the shed vortices tend to evolve into ring (circular in plan form) vortices, even though the slit resonator opening from which the vortices are shed has an aspect ratio of 2.5. Under the excitation of discrete frequency sound, the shed vortices align themselves into two regularly spaced vortex trains moving away from the resonator opening in opposite directions. This is different from the chaotic shedding of vortices found in two-dimensional simulations. The effect of slit aspect ratio at a fixed porosity is briefly studied. For the range of liners considered in this investigation, it is found that the absorption coefficient of a liner increases when the open area of the single slit is subdivided into multiple, smaller slits.

Tam, C. K. W.↗

A 300 kA Pulsed Power Supply for LBNF

The Long Baseline Neutrino Facility (LBNF) will produce the worlds most intense neutrino beam. Three series connected magnetic horns will require 5kV, 300kA, 800$\mu$s pulses at a rate of 0.7Hz to focus the beam. Fermilab has designed and built pulsed high current supplies for horns in the past. Pulsed currents of 205 kA for Neutrinos at Main Injector (NuMI - NOvA), focusing a 120 GeV beam, and 170 kA for Booster Neutrino Beam (BNB - MiniBooNE) for focusing an 8 GeV beam have been operational for about 18 years. While the magnetic horns are expected to be replaced, the LBNF horn power supply is expected to last the lifetime of the project, 30 years. A resonant, half sine wave pulser was used for NuMI and BNB and has many practical advantages. The system has impedance limited fault currents by design, albeit large ones. That along with the resonant behavior means that thyristor switches are well suited. Many fault modes of the system have also been calculated. Several circuit changes were incorporated so that a single fault can be tolerated. The supply must be reversable to enable both neutrinos and anti-neutrinos to be produced. These reversal requirements required a significant amount of mechanical design and consideration to allow for quick reversal of all the semiconductors.

43 PARTICLE ACCELERATORS↗

Characterizing Dynamic Test Fixtures Through the Modal Projection Error

Across many industries and engineering disciplines, physical components and systems of components are designed and deployed into their environment of intended use. It is the desire of the design agency to be able to predict whether their component or system will survive its physical environment or if it will fail due to mechanical stresses. One method to determine if the component will survive the environment is to expose the component to a simulation of the environment in a laboratory. One difficulty in doing this is that the component may not have the same boundary condition in the laboratory as is in the field configuration. This paper presents a novel method of quantifying the error in the modal domain that occurs from the impedance difference between the laboratory test fixture and the next level of assembly in the field configuration. The error is calculated from the projection from one mode shape space to the other, and the error is in terms of each mode of the field configuration. This provides insight into the effectiveness of the test fixture with respect to the ability to recreate the mode shapes of the field configuration. A case study is presented to show that the error in the modal projection between two configurations is a lower limit for the error that can be achieved by a laboratory test.

42 ENGINEERING↗

In-situ monitoring for liquid metal jetting using a millimeter-wave impedance diagnostic

Abstract This article presents a millimeter-wave diagnostic for the in-situ monitoring of liquid metal jetting additive manufacturing systems. The diagnostic leverages a T-junction waveguide device to monitor impedance changes due to jetted metal droplets in real time. An analytical formulation for the time-domain T-junction operation is presented and supported with a quasi-static full-wave electromagnetic simulation model. The approach is evaluated experimentally with metallic spheres of known diameters ranging from 0.79 to 3.18 mm. It is then demonstrated in a custom drop-on-demand liquid metal jetting system where effective droplet diameters ranging from 0.8 to 1.6 mm are detected. Experimental results demonstrate that this approach can provide information about droplet size, timing, and motion by monitoring a single parameter, the reflection coefficient amplitude at the input port. These results show the promise of the impedance diagnostic as a reliable in-situ characterization method for metal droplets in an advanced manufacturing system.

42 ENGINEERING↗

All‐Solid‐State Batteries With Mechanically Stable Interfaces Consisting of a Zero‐Strain Cation‐Disordered Rocksalt Cathode

Interface stabilization is critical to the development of working all‐solid‐state batteries. Rigid cathode/solid electrolyte interfaces often disintegrate due to anisotropic volume change of cathode‐active materials, resulting in irreversible capacity loss. Herein, we demonstrate that Li 1.211 Mo 0.467 Cr 0.3 O 2 (LMCO), a pioneering cation‐disordered rocksalt oxide (DRX) cathode that has intrinsically small volume change upon lithium intercalation, can be integrated with a thiophosphate‐based solid electrolyte for all‐solid‐state batteries. Interface stability of the all‐solid LMCO cell was investigated by electrochemical impedance spectroscopy, X‐ray micro‐computed tomography, and electron microscopy. Since LMCO was initially synthesized as a layered phase exhibiting a large volume change, interface disintegration can be observable in the early cycles. As layered LMCO phase‐transformed into DRX LMCO in subsequent cycles, reintegration of the interfaces occurs within a pressurized cell as a result of its zero‐stain behavior. Consequently, the DRX LMCO cathode maintains interface integrity, and thus electrical wiring, over an extended number of cycles, leading to improved capacity retention with small internal cell resistance.

DRX↗

Miniature Piezoelectric Macro-Mass Balance

Mass balances usually use a strain gauge that requires an impedance measurement and is susceptible to noise and thermal drift. A piezoelectric balance can be used to measure mass directly by monitoring the voltage developed across the piezoelectric balance, which is linear with weight or it can be used in resonance to produce a frequency change proportional to the mass change (see figure). The piezoelectric actuator/balance is swept in frequency through its fundamental resonance. If a small mass is added to the balance, the resonance frequency shifts down in proportion to the mass. By monitoring the frequency shift, the mass can be determined. This design allows for two independent measurements of mass. Additionally, more than one sample can be verified because this invention allows for each sample to be transported away from the measuring device upon completion of the measurement, if required. A piezoelectric actuator, or many piezoelectric actuators, was placed between the collection plate of the sampling system and the support structure. As the sample mass is added to the plate, the piezoelectrics are stressed, causing them to produce a voltage that is proportional to the mass and acceleration. In addition, a change in mass delta m produces a change in the resonance frequency with delta f proportional to delta m. In a microgravity environment, the spacecraft could be accelerated to produce a force on the piezoelectric actuator that would produce a voltage proportional to the mass and acceleration. Alternatively, the acceleration could be used to force the mass on the plate, and the inertial effects of the mass on the plate would produce a shift in the resonance frequency with the change in frequency related to the mass change. Three prototypes of the mass balance mechanism were developed. These macro-mass balances each consist of a solid base and an APA 60 Cedrat flextensional piezoelectric actuator supporting a measuring plate. A similar structure with 3 APA 120 Cedrat flextensional piezoelectric actuators spaced equidistantly at 120 degrees supporting the plate and a softer macro balance with an APA 150 actuator/sensor were developed. These flextensional actuators were chosen because they increase the sensitivity of the actuator to stress, allow the piezoelectric to be pre-stressed, and the piezoelectric element is a stacked multilayer actuator, which has a considerably lower input impedance than a monolithic element that allows for common instruments (e.g., input impedance of 10 megohms) to measure the voltage without rapidly discharging the charge/voltage on the piezoelectric actuator.

Sherrit, Stewart↗

Structural and electrochemical evolution of alloy interfacial layers in anode-free solid-state batteries

“Anode-free” solid-state batteries feature high energy density since there is no anode active material. Although the beneficial effects of interfacial layers at the anode-solid electrolyte interface have been demonstrated, the mechanisms through which they influence lithium plating/stripping are unclear. Here, in this study, we reveal the evolution of 100-nm silver and gold interfacial layers during lithium plating/stripping using electrochemical methods, electron microscopy, X-ray microcomputed tomography, and modeling. The alloy layers improve Coulombic efficiency and resistance to short circuiting, even though the alloys form solute regions or particulates that detach from the current collector during plating. In situ electrochemical impedance spectroscopy shows that the alloys return to the interface and mitigate contact loss at the end of stripping, avoiding a critical vulnerability of anode-free cells. Contact retention is driven by even Li thickness that promotes spatially uniform stripping, as well as local alloy delithiation in response to current concentrations that homogenizes current and diminishes voiding.

25 ENERGY STORAGE↗

Correlating work hardening with co-activation of stacking fault strengthening and transformation in a high entropy alloy using in-situ neutron diffraction

Transformation induced plasticity (TRIP) leads to enhancements in ductility in low stacking fault energy (SFE) alloys, however to achieve an unconventional increase in strength simultaneously, there must be barriers to dislocation motion. While stacking faults (SFs) contribute to strengthening by impeding dislocation motion, the contribution of SF strengthening to work hardening during deformation is not well understood; as compared to dislocation slip, twinning induced plasticity (TWIP) and TRIP. Thus, we used in-situ neutron diffraction to correlate SF strengthening to work hardening behavior in a low SFE Fe 40 Mn 20 Cr 15 Co 20 Si 5 (at%) high entropy alloy, SFE ~ 6.31 mJ m –2 . Cooperative activation of multiple mechanisms was indicated by increases in SF strengthening and γ-f.c.c. → ε-h.c.p. transformation leading to a simultaneous increase in strength and ductility. The present study demonstrates the application of in-situ, neutron or X-ray, diffraction techniques to correlating SF strengthening to work hardening.

36 MATERIALS SCIENCE↗

Unraveling interphase-driven failure pathways in LiMn0.6Fe0.4PO4/graphite pouch cells

LiMnxFe1−xPO4 (LMFP) is a promising high-voltage, thermally stable, and earth-abundant cathode material, yet its practical application is limited by interphase instability and Mn dissolution. In this work, we systematically evaluate LiMn0.6Fe0.4PO4/graphite pouch cells using three electrolyte formulations including control carbonate electrolyte, control + 2 wt% vinylene carbonate (VC), and control + 2 wt% VC + 1 wt% 1,3,2-dioxathiolane 2,2-dioxide (DTD), to establish how electrolyte composition governs interphase chemistry and long-term degradation. Electrochemical testing shows that both additives are preferentially reduced prior to ethylene carbonate (EC) during cell formation, generating robust cathode-electrolyte interphase (CEI) and solid-electrolyte interphase (SEI) layers that suppress gas evolution and raise the first-cycle coulombic efficiency to 89.3%. Additionally, the dual-additive electrolyte delivers the most stable performance, retaining over 85% capacity after 600 cycles while minimizing impedance growth under long-term cycling at C/3 and 40 °C. Soft X-ray absorption spectroscopy confirms that VC + DTD effectively suppresses electrolyte oxidation at the cathode surface, and micro-X-ray fluorescence shows substantially reduced Mn dissolution and deposition on the graphite anode. Density functional theory simulations further provided insights into the structural and energetic influences of alkoxide species on the cathode surface, proposing a Mn2+ extraction mechanism. The combined experimental and computational findings establish a mechanistic link between electrolyte composition and interphase evolution, highlighting the effectiveness of electrolyte engineering for extending the operational lifetime of LMFP-based lithium-ion batteries.

Chak, Chanmonirath Michael↗

The Influence of Cr-Additives on the Polarization Resistance of Praseodymium-Doped Ceria Cathodes for Solid Oxide Fuel Cells

While Cr poisoning of the oxygen reduction reaction (ORR) at SOFC cathodes is widely agreed to involve deactivation of oxygen exchange sites, the degradation mechanism remains ambiguous. Here, we selected an alternative cathode material Pr 0.1 Ce 0.9 O 2− δ , free of Sr segregation, to systematically investigate the effect of Cr-induced degradation in ORR. We expand on our previous studies in which the acidity/basicity of binary additives was found to be a strong indicator of the rate of oxygen surface exchange, by electrochemically investigating the ORR activity of the PCO cathode by impedance spectroscopy. Serial infiltration with acidic Cr-based oxides was found to degrade ORR activity as reflected in a 20-fold increase in area specific resistance (ASR) without corresponding changes in activation energy, with the opposite trend obtained with Ca-based oxides. Detected changes in total capacitance, attributed to changes in surface capacitance, also suggest depressed/enhanced PCO surface redox behavior with Cr/Ca-based infiltrants. Taken together, these results point to a more universal source of ORR poisoning/activation, based on acidity/basicity, rather than physical blocking of active sites. With this improved understanding, one can expect progress to be made in the coming years in optimizing means for protecting catalytic surfaces from degradation and/or improving their performance.

25 ENERGY STORAGE↗

Manufacturing the Harmonic Kicker Cavity Prototype for the Electron-Ion Collider

High-bunch-frequency beam-separation schemes, such as the injection scheme proposed for the Rapid Cycling Synchrotron at the Electron-Ion Collider, demand rise and fall times an order of magnitude below what can realistically be accomplished with a stripline kicker. Nanosecond-time-scale kick waveforms can instead be obtained by Fourier synthesis in a harmonically resonant quarter-wave radio-frequency cavity which is optimized for high shunt impedance. Originally developed for the Jefferson Lab Electron-Ion Collider (JLEIC) Circulator Cooler Ring, a hypothetical 11-pass ring driven by an energy-recovery linac at Jefferson Lab, our high-power prototype of such a harmonic kicker cavity, which operates at five modes at the same time, will demonstrate the viability of this concept with a beam test at Jefferson Lab. As the geometry of the cavity, tight mechanical tolerances, and number of ports complicate the design and manufacturing process, special care must be given to the order of the manufacturing steps. We present our experiences with the manufacturability of the present design, lessons learned, and first RF test results from the prototype.

Overstreet, S. A.↗

Computationally Guided Design of Multiple Impurities Tolerant Electrode (Final Report)

The current project was based on a combined experimental and computational approach, which can help recommend better cathode materials under multiple impurities conditions. The PI will mainly take in charge of experimental and computational thermodynamics of the selected cathode materials for the SOFC applications under multiple impurities. While the co-PI will run the electrochemical tests of the cathodes recommended and eventually the long-term degradation tests. At the end of the project, a multiple tolerant cathode material based on the combined experimental and computational approach will be recommended and the reliability of the commonly used accelerated testing will be evaluated. It will address multiple impurities poisoning effect of SO2, CO2, Cr and H2O on the LSM, LSCF and LNO cathodes by identifying the formation of the detrimental secondary phases by XRD, SEM and TEM techniques. And further recommended cathode material will be subjected to electrochemical testing and the most promising ones will be applied to long-term tests. The hybrid approach the PI proposed will not only be applied to the design of multiple impurities tolerant cathodes but will also be considered in the future oxygen electrode applications in SOECs or reversible SOCs. This hybrid computational and experimental approach includes four sections: 1) Investigation of single impurity poisoning on LSM, LSCF and LNO cathodes in the presence of SO2, CO2, Cr. In this section, LSM, LSCF cathodes from FuelCellMaterials and LNO cathodes from Sol-Gel synthesis will be heat-treated in the above single impurity. And the formation of the secondary phases as well as the corresponding simulations will be cross compared, which shows good agreement between each other. Meanwhile, the accelerated testing approach will be evaluated in these systems compared with the previous published work to understand the reliability of the approach. 2) Investigation of multiple impurities poisoning on LSM, LSCF and LNO cathodes in the presence of Cr+H2O, SO2+Cr and SO2+Cr+H2O conditions. We have also applied these 3 candidate cathodes under these multiple impurities’ conditions and the long-term degradation mechanism of the multiple impurities will be understood with the help of the combined experimental and computational approach. Meanwhile, the synergistic effect of those impurities will be compared with the individual ones in the same cathode system to further reveal the actual operating conditions. 3) Electrochemical testing and polarization of the recommended cathode. We have demonstrated very low polarization resistance in LSCF (core)-LSM (shell) electrodes using MSD process and analyzed impedance spectra using DRT analysis and confirming that the low polarization resistance in LSM infiltrated MSD cells is due to reduction in polarization resistance associated with O2-adsorption process. 4). Long-term degradation testing. We have developed a versatile MSD-based process to deposit various continuous coatings onto porous scaffolds and established baseline for longer term Cr-impurity testing in future projects.

36 MATERIALS SCIENCE↗

Manufacturing the Harmonic Kicker Cavity Prototype for the Electron-Ion Collider

High-bunch-frequency beam-separation schemes, such as the injection scheme proposed for the Rapid Cycling Synchrotron at the Electron-Ion Collider, demand rise and fall times an order of magnitude below what can realistically be accomplished with a stripline kicker. Nanosecond-time-scale kick waveforms can instead be obtained by Fourier synthesis in a harmonically resonant quarter-wave radio-frequency cavity which is optimized for high shunt impedance. Originally developed for the Jefferson Lab Electron-Ion Collider (JLEIC) Circulator Cooler Ring, a hypothetical 11-pass ring driven by an energy-recovery linac at Jefferson Lab, our high-power prototype of such a harmonic kicker cavity, which operates at five modes at the same time, will demonstrate the viability of this concept with a beam test at Jefferson Lab. As the geometry of the cavity, tight mechanical tolerances, and number of ports complicate the design and manufacturing process, special care must be given to the order of the manufacturing steps. We present our experiences with the manufacturability of the present design, lessons learned, and first RF test results from the prototype.

Overstreet, S. A.↗