At least 55 records · Page 3

Prevailing Torque Locking Feature in Threaded Fasteners Using Anaerobic Adhesive

This paper presents results from tests to assess the use of anaerobic adhesive for providing a prevailing torque locking feature in threaded fasteners. Test procedures are developed and tests are performed on three fastener materials, four anaerobic adhesives, and both unseated assembly conditions. Five to ten samples are tested for each combination. Tests for initial use, reuse without additional adhesive, and reuse with additional adhesive are performed for all samples. A 48-hour cure time was used for all initial use and reuse tests. Test data are presented as removal torque versus removal angle with the specification required prevailing torque range added for performance assessment. Percent specification pass rates for the all combinations of fastener material, adhesive, and assembly condition are tabulated and reveal use of anaerobic adhesive as a prevailing torque locking feature is viable. Although not every possible fastener material and anaerobic adhesive combination provides prevailing torque values within specification, any combination can be assessed using the test procedures presented. Reuse without additional anaerobic adhesive generally provides some prevailing torque, and in some cases within specification. Reuse with additional adhesive often provides comparable removal torque data as in initial use.

Hernandez, Alan

The Analysis of Adhesive Residue Failure

Adhesives have always been, and will continue to be, a crucial component of assembling flight hardware. Unfortunately, adhesives have a long standing history of being a source of costly contaminations. There are currently no existing documents that can aid a technician in discerning the proper adhesive/substrate combinations, nor the optimal solvent to use when removing adhesive residue. This project seeks to evaluate the performance of adhesive tapes on various flight hardware substrates in order to create an easy-to-use guide for spacecraft ground processing. The analyses performed were the adhesive/solvent solubility, SEM examinations, and peel adhesion tests. The solubility tests showed that amyl acetate, acetone, and MEK were the most successful in dissolving the adhesives. The SEM data gives preliminary insight into the morphology of the residues. Lastly, the peel adhesion testing proved that there is no relationship between the length of time the adhesive was applied and its adhesive strength.

Smiley, Adrienne

An Investigation of the Grain Size and Adhesion Strength of High-Speed Impact Ice

Ice accumulation on aircraft from supercooled water droplets (impact icing) can increase drag and decrease lift, leading to a decrease in fuel efficiency and a potential for unsafe situations. Anti-icing materials and coatings are of high interest to prevent aircraft icing. Because no anti-icing material suitable for in-flight situations has been realized, icing models aim to predict the accumulation and shape of the ice to understand its effects. In both cases, understanding the physical mechanism behind ice adhesion and shedding is necessary. A recent literature review has shown that the apparent ice adhesion strength to any specific material varies over several orders of magnitude across studies and test methods. One of the reasons for this high variance is likely to be the varying microstructure of the ice used for different studies. Although the microstructure of impact ice has been studied in the past, those conditions were not relevant to that of in-flight aircraft icing. The microstructure of the ice formed will determine both its bulk and surface properties, yet it has been overlooked in the ice adhesion community. Here, we use optical microscopy to study the non-uniform ice crystal grain size in impact ice accreted in NASA Glenn Research Center’s Icing Research Tunnel at various icing conditions. Similar to other environmental conditions studied in the literature, we show an increase in grain size at larger distances from the growth interface; however, the data shows substantially larger grains than what was expected from the prior literature. Ice accrued at lower temperatures has a smaller grain size at all distances from the growth interface. No change in grain size was noticed when varying only the wind speed. A correlational analysis shows that smaller grain sizes at the growth interface corresponded to an increase in the apparent ice adhesion strength when the adhesive failure was interfacial, but not when the failure was cohesive. These results may explain the overall trend in the literature of increasing apparent adhesion strength with decreasing temperature. Incorporating microstructure trends for various environmental conditions in icing models may increase the certainty in predicting ice adhesion strength and shedding, and will provide a better basis for comparison between adhesive tests on ice produced in different facilities and at different storage times.

• Ice Fabric

An Experimental and Numerical Study of Plasma Treatment Effects on Adhesive Joints of Metals, CFRTPs, and Metal–CFRTP Combinations

This work investigates the effects of plasma surface treatment on both the local adherend–adhesive interfacial strength and the global lap shear strength (LSS) of adhesively-bonded joints composed of metals, CFRTPs, and metal-CFRTP combinations, using AA6061 and CFRPPA as representative examples. Experimental and computational results show that plasma treatment improved the ratio of CFRPPA–adhesive interfacial normal strength to adhesive tensile strength (sint,n/scri,t,adhesive) from 0.59–1.00 to 0.91–1.73, leading to an average 90% increase in LSS for CFRPPA-related joints. In contrast, the LSS and sint,n/scri,t,adhesive values of AA6061–AA6061 joints (>=2.27) remained nearly unchanged after plasma treatment. The enhanced joint bonding was further supported by post-failure surface morphologies from three-dimensional profilometry and simulations, showing a transition from dominant interfacial failure to mixed modes involving interfacial, cohesive, and slight fiber-peeling failures. The LSS evolution with respect to sint,n/scri,t,adhesive was numerically established until the saturation of the LSS of various joints, and the behavior of AA6061–CFRPPA T-joints with varying interfacial strengths was also modeled. This study highlights the importance of local interfacial bonding strength, rather than global LSS, for understanding and optimizing the mechanical performance of adhesively-bonded composite–metal and composite-composite structures via different surface modification strategies.

Qiao, Yao (ORCID:0000000265867604)

Corrosion Resistance of Lignin-Based Thermoplastic Adhesive-Bonded Aluminum Joints

Adhesive-bonded joints are essential for lightweight, multimaterial automotive structures. We developed a lignin-based thermoplastic adhesive with adhesion strength comparable to conventional epoxy adhesives (20–23 MPa), while offering exceptional durability, recyclability, and corrosion resistance. Unlike commercial epoxy adhesives requiring refrigerated storage, our adhesive retains its bonding potential after a year of ambient conditioning. Bonded joints can be repeatedly disassembled and rejoined with less than 2% strength loss. After 500 h of salt fog exposure, the adhesive-bonded aluminum joints exhibited a 24% strength reduction, compared to 61% reduction in strength of joints based on a commercial epoxy adhesive.

Yu, Zeyang [ORNL] (ORCID:0000000209002374)

High-performance reversible adhesive from PET waste for underwater, structural, and pressure-sensitive applications

Developing versatile, tough, and sustainable adhesives that function effectively in both wet and dry environments is a major challenge. Here, we report a bioinspired design for versatile, tough, and reversible adhesives upcycled from consumer poly(ethylene terephthalate) (PET) waste. Our approach uses solvent-free, room-temperature dynamic cross-linking of deconstructed PET macromonomers with a diacetoacetate cross-linker, generating a dynamic, vinylogous urethane–bonded, amphiphilic adhesive. Tunable cross-linker concentration and amphiphilicity yield versatile adhesives suitable for underwater, structural, and pressure-sensitive applications on diverse substrates. Our adhesive exhibits high lap-shear strength and work of debonding under both wet and dry conditions, outperforming common commercial adhesives. The dynamic bonds enable thermal repair, on-demand multicycle debonding/rebonding, facile removal, and chemical recycling. Our strategy of transforming plastic waste into versatile, tough, and reversible adhesives offers a sustainable solution for both plastic waste management and next-generation adhesive design while also providing a commercially viable pathway for valorizing plastic waste.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH

Development of design allowables data for adhesives for attaching reusables surface insulation, addendum 1A

The task consisted of conducting mechanical and thermal tests to establish design allowables data on a new room temperature vulcanizing (RTV) silicone adhesive, X3-6004. Low modulus, coupled with relatively low density and good low-temperature properties of this adhesive, places it in contention as a candidate for attaching reusable surface insulation on the space shuttle. Data obtained show that the modulus values of X3-6004 are significantly lower than those of RTV-560 and the other three adhesives characterized at test temperatures from 550 to -175 F. At -175, -200 and -270 F, the modulus of X3-6004 is approximately the same as GE RTV-560 and the other three silicone adhesives. The X3-6004 adhesive exhibits good processing properties. It has a 12 percent lower density than RTV-560. Although lower in overall strength properties as compared to the other adhesives in the program, X3-6004 has adequate adhesion to 2024T81 aluminum to compete as an adhesive for attaching reusable surface insulation. It does exhibit some tendency to revert and soften at temperatures above 350 F when in a confined area.

Owen, H. P.

Exploratory study on the effects of novel diamine curing agents and isocyanate precursors on the properties on new epoxy and urethane adhesives

Aromatic diamines based on diphenyl sulfone and benzophenone were studied as epoxy adhesive curing agents. Previously found differences in adhesive strengths for meta vs para orientation were not found in these series. The use of aluminum and alumina as fillers in a m,m prime-methylene dianiline-cured epoxy adhesive was not found to be beneficial to adhesive strength. Alumina filled adhesives had much lower strength than unfilled adhesives. The unfilled m,m prime-methylene dianiline-based epoxy adhesive had excellent resistance to moisture relative to a p,p prime-methylene dianiline-based adhesive and maintained good strengths up to 250 F. A glass fiber composite based on a m,m prime-methylene dianiline-cured epoxy appeared to be equivalent to the p,p prime-methylene dianiline-cured epoxy as judged by short beam shear tests.

Glasgow, D. G.

Evaluation of high temperature structural adhesives for extended service

Eight different Ti-6Al-4V surface treatments were investigated for each of 10 candidate resins. Primers (two for each resin) were studied for appropriate cure and thickness and initial evaluation of bond joints began using various combinations of the adhesive resins and surface treatments. Surface failure areas of bonded titanium coupons were analyzed by electron microscopy and surface chemical analysis techniques. Results of surface characterization and failure analysis are described for lap shear bond joints occurring with adhesive systems consisting of: (1) LARC-13 adhesive, Pasa jell surface treatment; (2) LARC-13 adhesive, 10 volt CAA treatment; (3) PPQ adhesive, 10 volt CAA treatment; and (4) PPQ adhesive, 5 volt CAA treatment. The failure analysis concentrated on the 10,000 hr 505K (450 F) exposed specimens which exhibited adhesive failure. Environmental exposure data being generated on the PPQ-10 volt CAA and the LARC-TPI-10 volt CAA adhesive systems is included.

Hill, S. G.

Hot melt adhesive pad surface attachment assembly concept for on-orbit operations

The use of a hot melt adhesive concept to develop a Surface Attachment Assembly (SAA) for on-orbit attachment and detachment operations for the Manned Maneuvering Unit (MMU) was investigated. The concept involved impregnation of the hot melt adhesive into a fiberglass covered pad which contained electrical heating and thermoelectric cooling devices. The polyamide hot melt adhesive selected can be repeatedly heated to its melting point in a vacuum and provide good adhesion to various surfaces, i.e., reusable surface insulation tiles, metals, and composites, when cooled. After a series of adhesive screening tests, Jet-Melt 3746 was selected from a group of commercially available thermoplastic adhesive candidates which met or exceeded many of the criteria established for the SAA system. The SAA system was designed and fabricted with the goal of proving the concept with a working model rather than attempting to optimize all facets of the system. This system evolved by investigating alternate attachment concepts, designing and fabricating electronic systems to heat and cool the adhesive, and then fabricating electronic systems to heat and cool the adhesive, and then fabricating and testing two prototype full-size units.

Progar, D. J.

Humidity effects on adhesion of nickel-zinc ferrite in elastic contact with magnetic tape and itself

The effects of humidity on the adhesion of Ni-Zn ferrite and magnetic tape in elastic contact with a Ni-Zn ferrite hemispherical pin in moist nitrogen were studied. Adhesion was independent of normal load in dry, humid, and saturated nitrogen. Ferrites adhere to ferrites in a saturated atmosphere primarily from the surface tension effects of a thin film of water adsorbed on the ferrite surfaces. The surface tension of the water film calculated from the adhesion results was 48 times 0.00001 to 56 times 0.00001 N/cm; the accepted value for water is 72.7 x 0.00001 N/cm. The adhesion of ferrite-ferrite contacts increased gradually with increases in relative humidity to 80 percent, but rose rapidly above 80 percent. The adhesion at saturation was 30 times or more greater than that below 80 percent relative humidity. Although the adhesion of magnetic tape - ferrite contacts remained low below 40 percent relative humidity and the effect of humidity was small, the adhesion increased considerably with increasing relative humidity above 40 percent. The changes in adhesion of elastic contacts were reversible on humidifying and dehumidifying.

Miyoshi, K.

Influence of interface ply orientation on fatigue damage of adhesively bonded composite joints

An experimental study of cracked-lap-shear specimens was conducted to determine the influence of adherend stacking sequence on debond initiation and damage growth in a composite-to-composite bonded joint. Specimens consisted of quasi-isotropic graphite/epoxy adherends bonded together with either FM-300 or EC 3445 adhesives. The stacking sequence of the adherends was varied such that 0 deg, 45 deg, or 90 deg plies were present at the adherend-adhesive interfaces. Fatigue damage initiated in the adhesive layer in those specimens with 0 deg nd 45 deg interface plies. Damage initiated in the form of ply cracking in the strap adherend for the specimens with 90 deg interface plies. The fatigue-damage growth was in the form of delamination within the composite adherends for specimens with the 90 deg and 45 deg plies next to the adhesive, while debonding in the adhesive resulted for the specimens with 0 deg plies next to the adhesive. Those joints with the 0 deg and 45 deg plies next to either adhesive has essentially the same fatigue-damage-initiation stress levels. These stress levels were 13 and 71 percent higher, respectively, than those for specimens with 90 deg plies next to the EC 3445 and FM-300 adhesives.

Johnson, W. S.

Evaluation of high temperature structural adhesives for extended service

High temperature stable adhesive systems were evaluated for potential Supersonic Cruise Research (SCR) vehicle applications. The program was divided into two major phases: Phase I 'Adhesive Screening' evaluated eleven selected polyimide (PI) and polyphenylquinoxaline (PPQ) adhesive resins using eight different titanium (6Al-4V) adherend surface preparations; Phase II 'Adhesive Optimization and Characterization' extensively evaluated two adhesive systems, selected from Phase I studies, for chemical characterization and environmental durability. The adhesive systems which exhibited superior thermal and environmental bond properties were LARC-TPI polyimide and polyphenylquinoxaline both developed at NASA Langley. The latter adhesive system did develop bond failures at extended thermal aging due primarily to incompatibility between the surface preparation and the polymer. However, this study did demonstrate that suitable adhesive systems are available for extended supersonic cruise vehicle design applications.

Hendricks, C. L.

Factors Affecting the Processing of Epoxy Film Adhesives

The increasing awareness that adhesive performance is controlled not only by the condition of the adherend surface but also the condition or state of the adhesive and the process parameters used during fabrication is expected to result in improved reliability, as well as bond performance. The critical process variables which have been found to control adhesive bond formation and ultimate bond strength in 250F and 350F curing epoxy adhesives are described in terms of fabrication parameters and adhesive characteristics. These include the heat-up rate and cure temperature during processing and the adhesive moisture content and age condition (degree of advancement). The diagnostic methods used to delineate the effects of these process variables on adhesive performance are illustrated. These are dielectric, thermomechanical (TMA) and dynamic mechanical (DMA) analyses. Correlation of test results with measured mechanical tensile lap shear strengths of bonded joints is presented and the results briefly discussed in terms of the additives and hardeners used in the adhesive systems.

Pike, R. A.

Influence of interface ply orientation on fatigue damage of adhesively bonded composite joints

An experimental study of cracked-lap-shear specimens was conducted to determine the influence of adherend stacking sequence on debond initiation and damage growth in a composite-to-composite bonded joint. Specimens consisted of quasi-isotropic graphite/epoxy adherends bonded together with either FM-300 or EC 3445 adhesives. The stacking sequence of the adherends was varied such that 0 deg, 45 deg, or 90 deg plies were present at the adherend-adhesive interfaces. Fatigue damage initiated in the adhesive layer in those specimens with 0 deg and 45 deg interface plies. Damaage initiated in the form of ply cracking in the strap adherend for the specimens with 90 deg interface plies. The fatigue-damage growth was in the form of delamination within the composite adherends for specimens with the 90 deg and 45 deg plies next to the adhesive, while debonding in the adhesive resulted for the specimens with 0 deg plies next to the adhesive. Those joints with the 0 deg and 45 deg plies next to either adhesive has essentially the same fatigue-damage-initiation stress levels. These stress levels were 13 and 71 percent higher, respectively, than those for specimens with 90 deg plies next to the EC 3445 and FM-300 adhesives.

Johnson, W. S.

Evaluation of a metering, mixing, and dispensing system for mixing polysulfide adhesive

Tests were performed to evaluate whether a metered mixing system can mix PR-1221 polysulfide adhesive as well as or better than batch-mixed adhesive; also, to evaluate the quality of meter-mixed PR-1860 and PS-875 polysulfide adhesives. These adhesives are candidate replacements for PR-1221 which will not be manufactured in the future. The following material properties were evaluated: peel strength, specific gravity and adhesive components of mixed adhesives, Shore A hardness, tensile adhesion strength, and flow rate. Finally, a visual test called the butterfly test was performed to observe for bubbles and unmixed adhesive. The results of these tests are reported and discussed.

Evans, Kurt B.

Venous levels of shear support neutrophil-platelet adhesion and neutrophil aggregation in blood via P-selectin and beta2-integrin

BACKGROUND: After activation, platelets adhere to neutrophils via P-selectin and beta2-integrin. The molecular mechanisms and adhesion events in whole blood exposed to venous levels of hydrodynamic shear in the absence of exogenous activation remain unknown. METHODS AND RESULTS: Whole blood was sheared at approximately 100 s(-1). The kinetics of neutrophil-platelet adhesion and neutrophil aggregation were measured in real time by flow cytometry. P-selectin was upregulated to the platelet surface in response to shear and was the primary factor mediating neutrophil-platelet adhesion. The extent of neutrophil aggregation increased linearly with platelet adhesion to neutrophils. Blocking either P-selectin, its glycoprotein ligand PSGL-1, or both simultaneously by preincubation with a monoclonal antibody resulted in equivalent inhibition of neutrophil-platelet adhesion (approximately 30%) and neutrophil aggregation (approximately 70%). The residual amount of neutrophil adhesion was blocked with anti-CD11b/CD18. Treatment of blood with prostacyclin analogue ZK36374, which raises cAMP levels in platelets, blocked P-selectin upregulation and neutrophil aggregation to baseline. Complete abrogation of platelet-neutrophil adhesion required both ZK36374 and anti-CD18. Electron microscopic observations of fixed blood specimens revealed that platelets augmented neutrophil aggregation both by forming bridges between neutrophils and through contact-mediated activation. CONCLUSIONS: The results are consistent with a model in which venous levels of shear support platelet adherence to neutrophils via P-selectin binding PSGL-1. This interaction alone is sufficient to mediate neutrophil aggregation. Abrogation of platelet adhesion and aggregation requires blocking Mac-1 in addition to PSGL-1 or P-selectin. The described mechanisms are likely of key importance in the pathogenesis and progression of thrombotic disorders that are exacerbated by leukocyte-platelet aggregation.

NASA Discipline Cell Biology

Evaluation of Underwater Adhesives and Friction Coatings for In Situ Attachment of Fiber Optic Sensor System for Subsea Applications

Integrity and performance monitoring of subsea pipelines and structures provides critical information for managing offshore oil and gas production operation and preventing environmentally damaging and costly catastrophic failure. Currently pipeline monitoring devices require ground assembly and installation prior to the underwater deployment of the pipeline. A monitoring device that could be installed in situ on the operating underwater structures could enhance the productivity and improve the safety of current offshore operation. Through a Space Act Agreement (SAA) between the National Aeronautics and Space Administration (NASA) Johnson Space Center (JSC) and Astro Technology, Inc. (ATI), JSC provides technical expertise and testing facilities to support the development of fiber optic sensor technologies by ATI. This paper details the first collaboration effort between NASA JSC and ATI in evaluating underwater applicable adhesives and friction coatings for attaching fiber optic sensor system to subsea pipeline. A market survey was conducted to examine different commercial ]off ]the ]shelf (COTS) underwater adhesive systems and to select adhesive candidates for testing and evaluation. Four COTS epoxy based underwater adhesives were selected and evaluated. The adhesives were applied and cured in simulated seawater conditions and then evaluated for application characteristics and adhesive strength. The adhesive that demonstrated the best underwater application characteristics and highest adhesive strength were identified for further evaluation in developing an attachment system that could be deployed in the harsh subsea environment. Various friction coatings were also tested in this study to measure their shear strengths for a mechanical clamping design concept for attaching fiber optic sensor system. A COTS carbide alloy coating was found to increase the shear strength of metal to metal clamping interface by up to 46 percent. This study provides valuable data for assessing the feasibility of developing the next generation fiber optic senor system that could be retrofitted onto existing subsea pipeline structures.

Tang, Henry H.