New heterojunction LWIR detector options

Researchers investigate the heterojunction internal photoemission (HIP) approach that potentially offers long wavelength infrared (LWIR) photovoltaic detector performance (single pixel) that is competitive with the best of other approaches being considered. Most significantly, this approach offers a relatively simple device technology that promises producible and uniform FPA's. Researchers emphasize an exciting process based on intervalence band absorption. They investigate both III-V and Si-based heterojunctions grown by molecular beam epitaxy (MBE) in which the barrier can be tailored to the desired cutoff wavelength. In addition, MBE allows one to optimize the device structure with precise control of doping profiles and layer thicknesses, and perform band structure engineering by control of composition and heterojunction strain. Researchers also consider free carrier absorption in heterojunctions. Acceptable absorption coefficients can be achieved in very heavily n(exp +) doped semiconductor layers (approx. equals 10(exp 20)cm(exp -3). However, in this case the appreciable filling of conduction band states leads to a Schottky-like photoresponse with a gradual (quadratic) turn-on above threshold. A more satisfactory approach would be to use p(exp +) doping so that with the higher density of states in the heavy hole valence band there would be a narrow band of occupied states. This gives the desirable effect of a more rapid (linear) turn-on above threshold. Unfortunately, the higher hole effective mass also reduces (inversely) the free carrier absorption. For this and other reasons, the intervalence band absorption process looks much more promising.

Maserjian, Joseph↗

Dielectric function of InGaAs in the visible

Measurements are reported of the dielectric function of thermodynamically stable In(x)Ga(1-x)As in the composition range 0.3 equal to or less than X = to or less than 0.7. The optically thick samples of InGaAs were made by molecular beam epitaxy (MBE) in the range 0.4 = to or less than X = to or less than 0.7 and by metal-organic chemical vapor deposition (MOCVD) for X = 0.3. The MBE made samples, usually 1 micron thick, were grown on semi-insulating InP and included a strain release structure. The MOCVD sample was grown on GaAs and was 2 microns thick. The dielectric functions were measured by variable angle spectroscopic ellipsometry in the range 1.55 to 4.4 eV. The data was analyzed assuming an optically thick InGaAs material with an oxide layer on top. The thickness of this layer was estimated by comparing the results for the InP lattice matched material, i.e., X = 0.53, with results published in the literature. The top oxide layer mathematically for X = 0.3 and X = 0.53 was removed to get the dielectric function of the bare InGaAs. In addition, the dielectric function of GaAs in vacuum, after a protective arsenic layer was removed. The dielectric functions for X = 0, 0.3, and 0.53 together with the X = 1 result from the literature to evaluate an algorithm for calculating the dielectric function of InGaAs for an arbitrary value of X(0 = to or less than X = to or less than 1) were used. Results of the dielectric function calculated using the algorithm were compared with experimental data.

Alterovitz, S. A.↗

Dielectric function of InGaAs in the visible

Measurements are reported of the dielectric function of thermodynamically stable In(x)Ga(1-x)As in the composition range 0.3 equal to or less than X = to or less than 0.7. The optically thick samples of InGaAs were made by molecular beam epitaxy (MBE) in the range 0.4 = to or less than X = to or less than 0.7 and by metal-organic chemical vapor deposition (MOCVD) for X = 0.3. The MBE made samples, usually 1 micron thick, were grown on semi-insulating InP and included a strain release structure. The MOCVD sample was grown on GaAs and was 2 microns thick. The dielectric functions were measured by variable angle spectroscopic ellipsometry in the range 1.55 to 4.4 eV. The data was analyzed assuming an optically thick InGaAs material with an oxide layer on top. The thickness of this layer was estimated by comparing the results for the InP lattice matched material, i.e., X = 0.53, with results published in the literature. The top oxide layer mathematically for X = 0.3 and X = 0.53 was removed to get the dielectric function of the bare InGaAs. In addition, the dielectric function of GaAs in vacuum, after a protective arsenic layer was removed. The dielectric functions for X = 0, 0.3, and 0.53 together with the X = 1 result from the literature to evaluate an algorithm for calculating the dielectric function of InGaAs for an arbitrary value of X (0 = to or less than X = to or less than 1) were used. Results of the dielectric function calculated using the algorithm were compared with experimental data.

Alterovitz, S. A.↗

Development of a Quantum Dot, 0.6 eV InGaAs Thermophotovoltaic (TPV) Converter

Thermophotovoltaic (TPV) power conversion has to date demonstrated conversion efficiencies exceeding 20% when coupled to a heat source. Current III-V semiconductor TPV technology makes use of planar devices with bandgaps tailored to the heat source. The efficiency can be improved further by increasing the collection efficiency through the incorporation of InAs quantum dots. The use of these dots can provide sub-gap absorption and thus improve the cell short circuit current without the normal increase in dark current associated with lowering the bandgap. We have developed self-assembled InAs quantum dots using the Stranski-Krastanov growth mode on 0.74 eV In0.53GaAs lattice-matched to InP and also on lattice-mismatched 0.6 eV In0.69GaAs grown on InP through the use of a compositionally graded InPAsx buffer structure, by metalorganic vapor phase epitaxy (MOVPE). Atomic force microscopy (AFM) measurements showed that the most reproducible dot pattern was obtained with 5 monolayers of InAs grown at 450 C. The lattice mismatch between InAs and In0.69GaAs is only 2.1%, compared to 3.2% between InAs and In0.53GaAs. The smaller mismatch results in lower strain, making dot formation somewhat more complicated, resulting in quantum dashes, rather than well defined quantum dots in the lattice-mismatched case. We have fabricated 0.6 eV InGaAs planer TPV cells with and without the quantum dashes

Forbes, David↗

Correlations between critical current density, j(sub c), critical temperature, T(sub c),and structural quality of Y1B2Cu3O(7-x) thin superconducting films

Correlations between critical current density (j(sub c)) critical temperature (T(sub c)) and the density of edge dislocations and nonuniform strain have been observed in YBCO thin films deposited by pulsed laser ablation on (001) LaAlO3 single crystals. Distinct maxima in j(sub c) as a function of the linewidths of the (00 l) Bragg reflections and as a function of the mosaic spread have been found in the epitaxial films. These maxima in j(sub c) indicate that the magnetic flux lines, in films of structural quality approachingthat of single crystals, are insufficiently pinned which results in a decreased critical current density. T(sub c) increased monotonically with improving crystalline quality and approached a value characteristic of a pure single crystal. A strong correlation between j(sub c) and the density of edge dislocations ND was found. At the maximum of the critical current density the density of edge dislocations was estimated to be N(sub D) approximately 1-2 x 10(exp 9)/sq cm.

Chrzanowski, J.↗

Strain-Layer-Superlattice Light Modulator

Conceptual device combines resonant reflection and photovoltaic action to enable one light beam to impose spatial and temporal modulation on another light beam. Such spatial light modulator, with high speed and multiplicity of parallel signal channels, used in image processing or similar computation requiring high data-throughput rates. Microstructures of GaAs and InAs with multiple quantum wells and compositional superlattices grown by molecular-beam epitaxy. Enhanced electro-optical properties of arrangement of alternating layers enables writing light beam to modulate reading light beam.

Maserjian, Joseph↗

The evolution and growth of Al2O3 scales on beta-NiAl

The formation and growth of Al2O3 scales on (beta)-NiAl were studied using electron microscopy and other analytical techniques to gain an understanding of the oxidation properties of (beta)-NiAl and of alumina-forming alloys, in general. The transient and mature stages of oxidation were studied as well as the transformation stage during which the oxide scale transforms from metastable Al2O3 phases to the thermodynamically stable alpha-Al2O3 phase. The transient oxidation stages were studied at 800 deg C and for short times at 1100C. At 800C, the scales consist predominantly of delta-Al2O3 which forms by cation vacancy ordering in the defective spinel lattice of gamma-Al2O3. At 1100C, a fast-growth morphology of theta-Al2O3 forms as a surface layer over delta-Al2O3. For both oxidation temperatures, the scales are often epitaxially oriented with respect to the metal. The transient scales grow by outward cation diffusion as evidenced by surface growth morphologies. The transformation to alpha-Al2O3 occurs within 1 hour at 1100C by a nucleation and radial growth process. The large volume decrease associated with the transformation results in a highly strained alpha-Al2O3 microstructure. A change in scale growth mechanism from outward cation to inward anion diffusion allows transient surface morphologies to be smoothed by surface diffusion. The mature stage of oxidation involves the growth of an alpha-Al2O3 scale having the lacey morphology formed as a result of the gamma yields alpha transformation. Growth of the scale occurs by counterdiffusion along grain boundaries resulting in ridges formed by impingement of alpha-Al2O3 nuclei during the transformation stage. Also scale growth occurs by inward oxygen diffusion through healed cracks; the cracks result from transformation stresses. The measured growth rates of scales having the lacey morphology are an order of magnitude less than fine-grained alpha-Al2O3 scales. Metal orientations were found to have a large effect on oxide morpholoies during all stages of oxidation.

Doychak, J. K.↗

An exactly solvable model for calculating critical misfit and thickness in epitaxial superlattices - Layers of equal elastic constants and thicknesses

A parabolic interaction potential has been used to develop a model for calculating the misfit dislocation (MD) energy in the case of a superlattice of alternating layers of materials with equal elastic constants and thicknesses. The model, which is believed to be a good one for small misfits and to have some merit for covalent bonded materials, is exactly solvable for the critical thickness above which it is energetically favorable to lose coherency by the introduction of MDs into the interfaces. It was found, for a given misfit f, that the critical thickness for epitaxial superlattices free from their substrate is somewhat more than four times that for a single epilayer on a thick substrate. Furthermore, the critical thickness varies almost inversely with misfit to the power 1.22 when Poisson's ratio is 1/3. It was also shown that the critical misfit f(c) obtained by equating maximal misfit strain and MD energies is a significant overestimate of f(c). The results for a superlattice are compared with those of a thin layer on a thick substrate.

Van Der Merwe, Jan H.↗

Molecular beam epitaxial growth and transmission electron microscopy studies of thin GaAs/InAs(100) multiple quantum well structures

GaAs/InAs(100) multiple interface structures involving 7.4 percent lattice mismatch have been fabricated via molecular beam epitaxy and examined via transmission electron microscopy. It is found that high-quality, dislocation-free interfaces involving such high lattice mismatch can indeed be experimentally realized for very thin layers provided proper care is given to achieve a balance between the growth kinetics and the thermodynamics leading to the equilibrium ground state of the strained layer. The compressive strain is homogeneously accommodated and a tetragonal distortion is induced in the InAs layer with a perpendicular lattice constant in close agreement with that expected on the basis of the continuum theory and elastic constants of bulk InAs.

Grunthaner, F. J.↗

Study of Dislocation-Ordered In(x)Ga(1-x)As/GaAs Quantum Dots

A report describes an experimental study of dislocation-induced spatial ordering of quantum dots (QDs) comprising nanometer-sized In(x)Ga(1-x)As islands surrounded by GaAs. Metastable heteroepitaxial structures were grown by molecular-beam epitaxy of In(x)Ga(1-x)As onto n+ GaAs and semi-insulating GaAs substrates. Then the structures were relaxed during a post-growth annealing/self-organizing process leading to the formation of surface undulations that acted as preferential sites for the nucleation of QDs. Structural effects of annealing times and temperatures on the strain-relaxed In(x)Ga(1-x)As/GaAs and the subsequent spatial ordering of the QDs were analyzed by atomic-force microscopy and transmission electron microscopy. Continuous-wave spectral and time-resolved photoluminescence (PL) measurements were performed to study the effects, upon optical properties, of increased QD positional ordering, increased QD uniformity, and proximity of QDs to arrays of dislocations. PL spectral peaks of ordered QD structures formed on strain-relaxed In(x)Ga(1-x)As/GaAs layers were found to be narrower than those of structures not so formed and ordered. Rise and decay times of time-resolved PL were found to be lower at lower temperatures -- apparently as a consequence of decreased carrier-transport times within the barriers surrounding the QDs.

Leon, Rose↗

High quality InP-on-Si for solar cell applications

InP on Si solar cells combine the low-cost and high-strength of Si with the high efficiency and radiation tolerance of InP. The main obstacle in the growth of single crystal InP-on-Si is the high residual strain and high dislocation density of the heteroepitaxial InP films. The dislocations result from the large differences in lattice constant and thermal expansion mismatch of InP and Si. Adjusting the size and geometry of the growth area is one possible method of addressing this problem. In this work, we conducted a material quality study of liquid phase epitaxy overgrowth layers on selective area InP grown by a proprietary vapor phase epitaxy technique on Si. The relationship between growth area and dislocation density was quantified using etch pit density measurements. Material quality of the InP on Si improved both with reduced growth area and increased aspect ratio (length/width) of the selective area. Areas with etch pit density as low as 1.6 x 10(exp 4) sq cm were obtained. Assuming dislocation density is an order of magnitude greater than etch pit density, solar cells made with this material could achieve the maximum theoretical efficiency of 23% at AMO. Etch pit density dependence on the orientation of the selective areas on the substrate was also studied.

Shellenbarger, Zane A.↗

InGaAs/InGaAsP/InP strained-layer quantum well lasers at about 2 microns

The first successful operation of InGaAs strained layer quantum well (Sl-QW) injection lasers at about 2 microns is reported. The threshold current density and the external differential quantum efficiency of 5 microns wide and 800 microns long ridge waveguide lasers were 2.5 kA/sq cm and 6 percent, respectively. The devices had a reverse leakage current of less than 20 micro-A at -1 V indicating epitaxial layers with low defect density.

Forouhar, S.↗

New class of Si-based superlattices - Alternating layers of crystalline Si and porous amorphous Si(1-x)Ge(x) alloys

Superlattices consisting of alternating layers of crystalline Si and porous amorphous Si(1-x)Ge(x) have been fabricated. This is accomplished by first growing a Si/Si(0.7)Ge(0.3) superlattice by molecular beam epitaxy, followed by Ar-ion milling to form mesa structures, and finally by immersion in HF:HNO3:H2O. This solution creates a porous structure similar to that created by anodic etching, and a high selectivity is observed for the conversion of the alloy layers relative to the Si layers. The degree of selectivity is found to depend on alloy-layer thickness and strain. Superlattices have been fabricated from 1-micron wide mesas with Si(0.7)Ge(0.3) layers fully converted to 5-nm thick porous amorphous material.

Fathauer, R. W.↗

In-situ ellipsometric studies of optical and surface properties of GaAs(100) at elevated temperatures

A rotating-polarizer ellipsometer was attached to an ultrahigh vacuum (UHV) chamber. A GaAs(100) sample was introduced into the UHV chamber and heated at anumber of fixed elevated temperatures, without arsenic overpressure. In-situ spectroscopic ellipsometric (SE) measurements were taken, through a pair of low-strain quartz windows, to monitor the surface changes and measure the pseudodielectric functions at elevated temperatures. Real-time data from GaAs surface covered with native oxide showed clearly the evolution of oxide desorption at approximately 580 C. In addition, surface degradation was found before and after the oxide desorption. An oxide free and smooth GaAs surface was obtained by depositing an arsenic protective coating onto a molecular beam epitaxy grown GaAs surface. The arsenic coating was evaporated immediately prior to SE measurements. A comparison showed that our room temperature data from this GaAs surface, measured in the UHV, are in good agreement with those in the literature obtained by wet-chemical etching. The surface also remained clean and smooth at higher temperatures, so that reliable temperature-dependent dielectric functions were obtained.

Yao, Huade↗

Transport Equations for CAD Modeling of Al(x)Ga(1-x)N/GaN HEMTs

BEMTs formed from Al(x)Ga(1-x)N/GaN heterostructures are being investigated for high RF power and efficiency around the world by many groups, both academic and industrial. In these devices, the 2DEG formation is dominated by both spontaneous and piezoelectric polarization fields, with each component having nearly the same order of magnitude. The piezoelectric portion is induced by the mechanical strain in the structure, and to analyze these devices, one must incorporate the stress/strain relationships, along with the standard semiconductor transport equations. These equations for Wurtzite GaN are not easily found in the open literature, hence this paper summarizes them, along with the constitutive equations for piezoelectric materials. The equations are cast into the format for the Wurtzite crystal class, which is the most common way GaN is grown epitaxially.

Freeman, Jon C.↗

Recent Results from Epitaxial Growth on Step Free 4H-SiC Mesas

This paper updates recent progress made in growth, characterization, and understanding of high quality homoepitaxial and heteroepitaxial films grown on step-free 4H-SiC mesas. First, we report initial achievement of step-free 4H-SiC surfaces with carbon-face surface polarity. Next, we will describe further observations of how step-free 4H-SiC thin lateral cantilever evolution is significantly impacted by crystal faceting behavior that imposes non-uniform film thickness on cantilever undersides. Finally, recent investigations of in-plane lattice constant mismatch strain relief mechanisms observed for heteroepitaxial growth of 3C-SiC as well as 2H-AlN/GaN heterofilms on step-free 4H-SiC mesas will be reviewed. In both cases, the complete elimination of atomic heterointerface steps on the mesa structure enables uniquely well-ordered misfit dislocation arrays to form near the heterointerfaces with remarkable lack of dislocations threading vertically into the heteroepilayers. In the case of 3C-SiC heterofilms, it has been proposed that dislocation half-loops nucleate at mesa edges and glide laterally along the step-free 3C/4H interfaces. In contrast, 3C-SiC and 2H-AlN/GaN heterofilms grown on 4H-SiC mesas with steps exhibit highly disordered interface misfit dislocation structure coupled with 100X greater density of dislocations threading through the thickness of the heteroepilayers. These results indicate that the presence of steps at the heteroepitaxial interface (i.e., on the initial heteroepitaxial nucleation surface) plays a highly important role in the defect structure, quality, and relaxation mechanisms of single-crystal heteroepitaxial films.

Neudeck, Philip G.↗

Surface morphology of molecular-beam epitaxially grown Si(1-x)Ge(x) layers on (100) and (110) Si

The surface morphology and dislocation structure of Si(1-x)Ge(x) layers grown on (100) and (110) Si substrates have been investigated using atomic force microscopy, and scanning and transmission electron microscopy. The layers, which have up to a 1.2 percent lattice mismatch with the substrates, were grown by molecular-beam epitaxy at 550 C at thicknesses above those required for the introduction of dislocations. Si(1-x)Ge(x) layers grown on (100) show a crosshatch morphology which is correlated to the underlying misfit dislocation network. Annealing greatly enhances the surface roughness producing a partial islanding growing on the preexisting crosshatch morphology. On the (110) substrates no annealing is necessary to produce a roughened surface. The roughened surface morphology is analyzed as a strain-reducing growth mode which enables partial relaxation of the near-surface atomic planes.

Pike, W. T.↗

Room-temperature operation of MOCVD-grown GaInAs/InP strained-layer multiquantum well lasers in 1.8 micron range

The first successful room-temperature pulsed operation is reported of InGaAs strained layer multiquantum well injection lasers grown by MOVPE on InP substrates in the 1.8 micron range. The threshold current density and the external differential quantum efficiency of the 10 micron wide ridge waveguide lasers were 2.5 kA/sq cm (cavity length = 1 mm) and 5 percent (cavity length = 400 microns), respectively. Broad-area lasers, 100 microns wide and 1 mm long, had a reverse leakage current of less than 10 microamps at -1 V indicating high quality of the epitaxial layers.

Forouhar, S.↗