Search NASA⌕ Search

SEARCH · Search NASA

Results for “FCCI”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 55 records · Page 3

Characterization of phases formed between U-Pu-Mo alloys and Fe-12Cr cladding

Exposure to high temperatures and irradiation can lead to interaction between fuel and cladding constituents, inter-diffusion, and formation of brittle or low-melting phases. Therefore, understanding of fuel-cladding interaction (FCCI) is critical for evaluation of fuel performance in a reactor environment. In this contribution, phases formed between U-21.7Pu-4.3Mo and U-24.8Pu-14.6Mo (in wt%) fuel alloys and Fe-12Cr cladding were characterized using scanning and transmission electron microscopy (SEM/TEM) techniques. Phases formed within FCCI layers in both alloys were identified by implementing selective area diffraction pattern analysis as Cr0.3Mo0.7, Fe2U, FeUCr, and Fe2Pu. Phases formed at the end of the FCCI layer in the U-21.7Pu-4.3Mo alloy included FeUCr, Fe2U, and Cr2FeO4 while in the U-24.8Pu-14.6Mo alloy; the phases were consistent with Cr0.49Fe0.51, Cr0.8Fe0.2, and FeUCr.

36 MATERIALS SCIENCE↗

Novel Fuel Form Fabrication

Novel fuel form fabrication efforts have focused on casting of smaller diameter fuels in order to show the feasibility of the FAST test and the incorporation of a FCCI barrier either integral to the fuel or within the cladding tube. Casting of small diameter fuel slugs proved to be feasible at least one pin at a time using vacuum assisted arc casting. Integration of an integral FCCI barrier is also feasible although additional refinement will be necessary. If a sodium bonded fuel is employed, a more simple FCCI barrier may be to incorporate a thin barrier of material in the cladding before the sodium and fuel are loaded. Experiments have shown that sodium bonding of the barrier material and fuel is feasible.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Advanced Electron Microscopy Characterization of the Fuel-Cladding Chemical Interaction Region in a High Burnup U-10Zr Fuel

To support the development of U-10Zr metallic fuel, advanced characterization techniques have been applied to the fuel-cladding chemical interaction (FCCI) region in a Na-bonded solid U-10Zr fuel cross-section that was irradiated to a burnup of ~13.1 at.% at the Fast Flux Test Facility. 17 phases were identified in the FCCI region through a combination of high-resolution scanning transmission electron microscopy (STEM), STEM based energy dispersive X-ray spectroscopy (STEM-EDS), and TEM based selective area electron diffraction (TEM-SAED) analysis. In this talk, we will also discuss the implications of results on metallic fuel FCCI by focusing on the formation of Zr rind, fission product migration, and HT-9 cladding integrality under the investigated thermal irradiation conditions. This work complements our previous study on the TEM characterization of the fuel region of this high burnup fuel sample and serves as scientific basis to support metallic fuel development and qualification.

11 - NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Investigation of constituent redistribution in U-Pu-Zr fuels and its dependence on varying Zr content

This contribution investigates fuel constituent segregation and fuel-cladding chemical interactions (FCCI) in three U-Pu-Zr fuel pins irradiated to ~11% burnup in Experimental Breeder Reactor-II as part of the X441 DP-1 experiment. In examined pins, Zr content ranged from 6 to 10 and 14 wt.%, while Pu concentration was constant at 19 wt.% Pu. The primary goal of the investigation was to determine the role Zr content plays in fuel performance and this manuscript provides assessment of both constituent redistribution and FCCI as a function of axial position. FCCI was observed in all pins, though no cladding failure was noted. Optical and scanning electron microscopy (SEM) results show that variation in Zr content alters the number and relative size of constituent redistribution zones in the fuel. For example, larger Zr-rich central regions and smaller U-rich intermediate regions were observed in 14 wt.% Zr fuels. More importantly, all examined fuels have four or more discrete constituent redistribution regions, where each region has dissimilar morphological features. The existence of four to six distinctive regions deviates from traditionally accepted three region redistribution model, highlights complexity of constituent redistribution in this metal fuel, and identifies the need to conduct additional studies using state-of-the-art instrumentation.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

BISON fuel performance modeling optimization for experiment X447 and X447A using axial swelling and cladding strain measurements

With the recent need to qualify new reactor designs such as the Versatile Test Reactor (VTR), fuel performance calculations need to be performed to determine safety criteria of the proposed designs. In order to validate the fuel performance results obtained by a fuel performance code, BISON, for new reactor designs, legacy fuel from EBR-II and FFTF MFF with Post -Irradiation Examination (PIE) data need to be used as validation cases to benchmark models. Here in this work, BISON has been paired with the Fuels Irradiation & Physics Database (FIPD) and IFR Materials Information System (IMIS) to supply PIE data for comparison with simulations of EBR-II experiments X447/X447A. X447/X447A were assessed by implementing models for Fuel Cladding Chemical Interaction (FCCI) within BISON and optimizing the friction coefficient between the fuel surface and the cladding, the anisotropic swelling factor, and the HT9 first thermal creep scalar (which scales the first term in the HT9 creep equation) to best match the PIE axial fuel swelling height and cladding profilometry for all pins in X447/X447A. The optimal values were found using a generic algorithm developed to select different values for the three parameters until end criteria was met and error couldn’t be reduced further. The BISON-simulated cladding profilometry was evaluated using Standard Error of the Estimate (SEE) to account for the profile shape of the cladding profilometry. Optimal values for the friction coefficient, anisotropic fuel swelling factor, and HT9 first thermal creep scalar were found to best fit the BISON simulation results to the PIE measurements found in IMIS and FIPD. Improvements to current models are suggested to account for the underprediction of fuel swelling at low burnups and the overprediction of fuel swelling at higher burnups observed for the axial fuel swelling height. Although two pins in EBR-II X447/X447A (DP70 and DP75) were known to fail due to FCCI, none of the pins simulated in BISON reached a cumulative damage fraction (CDF) above 0.008 with FCCI correlations coupled in the BISON simulations. The error estimate generated for all pins in X447/X447A using optimal values was 209 µm, which is deemed acceptable.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Glovebox Advanced Casting System Casting Optimization

Casting optimization in the GACS included three broad areas; casting of U-10Zr pins, incorporation of an integral FCCI barrier, and development of a permanent crucible coating. U-10Zr casting was improved over last year’s results by modifying the crucible design to minimize contact with the colder mold. Through these modifications casting of a three pin batch was successful. Incorporation of an integral FCCI barrier also was optimized through furnace chamber pressure changes during the casting cycle to reduce gas pressures in the mold cavities which led to three full length pins being cast which incorporated FCCI barriers of three different thicknesses. Permanent crucible coatings were tested against a base case; 1500°C for 10 minutes in a U-20Pu-10Zr molten alloy. None of the candidate coating materials showed evidence of failure upon initial visual examination. In all areas of work a large amount of characterization will be needed to fully determine the effects of the optimization activities. The characterization activities and future work will occur next year.

36 MATERIALS SCIENCE↗

Magnification Determination for AGHCF Metallographic Images

Metallographic images generated in the Alpha Gamma Hot Cell Facility (AGHCF) have been used for quantitative and qualitative characterization of irradiated metallic fuel pins. Individual high-magnification images (micrographs) contained in AGHCF file folders and experimental notebooks are in the form of polaroid photographs labeled with AGHCF identification number, magnification, and surface condition (as-polished or etched). Low magnification composite images (photomosaics) are also available for fuel cross sections, for radial strips from the fuel center to the cladding outer diameter, and for circumferential strips of the cladding and outer fuel region. The individual images do not have scale bars. Only a few of the composite images contain scale bars. The purpose of this work is to describe and apply methods for checking the magnification (50X to 500X) of individual images and for determining the magnification (~25X to ~100X) of composite images. The metallographic images used to verify and/or determine magnification were generated during the 1989 to 1993 timeframe for cross sections of U-10Zr/HT9 fuel rods irradiated in EBR-II and for cross sections of irradiated U-10Zr/HT9 fuel-rod samples following elevated-temperature tests conducted in the out-of-pile AGHCF Fuel Behavior Test Apparatus (FBTA). Procedures are documented in the AGHCF Operations Manual for preparation of metallographic samples, for calibration verification, and for constructing composites from individual images. Calibration verification of magnification was performed at least semiannually. One standard used for calibration verification was a glass slide with vertical lines indicating distances of 1 mm, 0.1 mm and 0.01mm. Guidance is provided in the current work for determining magnification from images of the standard. In addition to the periodic calibration verification, consistency checks are recommended to verify the magnification of images taken between the routine calibration verifications. For cladding samples with or without significant fuel-cladding chemical interaction (FCCI), images taken at different magnifications (e.g., 150X and 200X) of the unaffected cladding thickness can be compared. This process is independent of changes in cladding thickness due to swelling and creep. For images taken at only one magnification of cladding regions with no FCCI, the cladding thickness determined from the images may be compared to the nominal as-built cladding thickness (15.0 ± 0.5 mils for examples used in current work)). This procedure works best for cladding that has not experienced significant swelling and/or creep (e.g., ≤2% circumferential strain at the cladding outer surface). Composite images were constructed by pasting together higher magnification images and photographing the composite to generate a negative from which the hard-copy photograph was developed. The primary purpose of the composite images was to identify interesting areas of the fuel and cladding for imaging at higher magnification. However, procedures are recommended in the current work for determining composite magnifications to allow quantitative characterization of the fuel. Composites are not recommended for determining cladding thickness or FCCI depth because magnifications are too low (generally ≤110X) and image contrast is low. Fuel cross-section composites were created by pasting together 50X or 75X images. The nominal magnification for the photographed fuel cross-section composites is 25.4X. A more precise magnification can be determined by comparing the average cladding outer diameter measured from the composite to the average cladding outer diameter measured by profilometry. Radial-strip composites were constructed by pasting together high-magnification (150X or 250X) images. The nominal magnification of radial-strip composites photographs is about 100X. A more precise method for determining the magnification of radial strips is to compare the cladding thick

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

EXTENDING SODIUM FAST REACTOR DRIVER FUEL USE TO HIGHER TEMPERATURES

Calculations of potential sodium-cooled fast reactor fuel temperatures were performed to estimate the effects of increasing the outlet temperature of a given fast reactor design by increasing pin power, decreasing assembly flow, or increasing inlet temperature. Based upon experience in the U.S., both metal and mixed oxide (MOX) fuel types are discussed in terms of potential performance effects created by the increased operating temperatures. Assembly outlet temperatures of 600, 650 and 700 °C were used as goal temperatures. Fuel/cladding chemical interaction (FCCI) and fuel melting, as well as challenges to the mechanical integrity of the cladding material, were identified as the limiting phenomena. For example, starting with a recent 1000 MWth fast reactor design, raising the outlet temperature to 650 °C through pin power increase increased the MOX centerline temperature to more than 3300 °C and the metal fuel peak cladding temperature to more than 700 °C. These exceeded limitations to fuel performance; fuel melting was limiting for MOX and FCCI for metal fuel. Both could be alleviated by design ‘fixes’, such as using a barrier inside the cladding to minimize FCCI in the metal fuel, or using annular fuel in the case of MOX. Both would also require an advanced cladding material with improved stress rupture properties. While some of these are costly, the benefits of having a high-temperature reactor which can support hydrogen production, or other missions requiring high process heat may make the extra costs justified.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Full-length U-xPu-10Zr (x=0, 8, 19 wt%) Fast Reactor Fuel Test in FFTF

The Integral Fast Reactor-1 (IFR-1) experiment performed in the Fast Flux Test Facility (FFTF) was the only U-Pu-10Zr (Pu-0, 8 and 19 wt%) metallic fast reactor test with commercial-length (91.4 cm active fuel column length) conducted to date. With few remaining test reactors there is little opportunity for performing another test with a long active fuel column. The assembly was irradiated to the goal burnup of 10 at.%. The beginning of life (BOL) peak cladding temperature of the hottest pin was 608?C, cooling to 522?C at end of life (EOL). Selected fuel pins were examined non destructively using neutron radiography, precision axial gamma scanning, and both laser and spiral contact cladding profilometry. Destructive exams included plenum gas pressure, volume, and gas composition determinations on a number of pins followed by optical metallography, electron probe microanalysis (EPMA), and alpha and beta gamma autoradiography on a single U-19Pu-10Zr pin. The post-irradiation examinations (PIEs) showed very few differences compared to the short-pin (34.3 cm fuel column) testing performed on fuels of similar composition in Experimental Breeder Reactor-II (EBR-II). The fuel column grew axially slightly less than observed in the short pins, but with the same pattern of decreasing growth with increasing Pu content. There was a difference in the fuel-cladding chemical interaction (FCCI) in that the maximum cladding penetration by interdiffusion with fuel/fission products did not occur at the top of the fuel column where the cladding temperature is highest, as observed in EBR-II tests. Instead, the more exaggerated fission-rate profile of the FFTF pins resulted in a peak FCCI at ~0.7 X/L axial location along the fuel column. This resulted from a lower production of rare earth fission products higher in the fuel column as well as a much smaller delta-T between fuel center and cladding, and therefore less FCCI, despite the higher cladding temperature. This behavior could actually help extend the life of a fuel pin in a “long pin” reactor design to a higher peak fuel burnup.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Nd, SbNd and Sb 3 Nd 4 and their interactions with the cladding alloy HT9

Lanthanide fission products, such as neodymium, formed during the irradiation of metallic fuels are known to cause deleterious effects from chemical interactions occurring at the fuel-cladding interface; a phenomenon known as fuel-cladding chemical interaction (FCCI). The use of fuel-based additives that bind with the lanthanide elements within the fuel meat, alleviating their interactions at the fuel-cladding interface, is one potential method proposed to mitigate the FCCI phenomenon and extend the burnup potential of such metallic fuel systems. In this study, antimony (Sb) is evaluated as one such additive, and neodymium (Nd) is used to represent the lanthanides. A Sb-Nd alloy is fabricated, which consists of two intermetallic phases, SbNd and Sb 3 Nd 4 . Isothermal diffusion couple experiments are carried out at 675 °C for 24 h between Nd and the Fe-12Cr based HT9 cladding alloy. The results are compared against similar diffusion couple experiments carried out between the Sb-Nd alloy and also HT9. Inter-diffusion between Nd/HT9 diffusion couple is characterized and the phases Fe 17 Nd 5 and Fe 17 Nd 2 were found to form whereas no interactions were observed in the Sb-Nd/HT9 diffusion couple. The lack of compound forming tendencies between Fe, the primary alloying constituent of HT9, and SbNd is elucidated through density functional theory (DFT) calculations on enthalpy of mixing, aligning well with the experimental observations. Lastly, the strong binding of Nd with Sb appears to be favorable, alleviating Nd interactions with HT9 constituent elements.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

SEM characterization of two advanced fuel alloys: U-10Zr-4.3Sn and U-10Zr-4.3Sn-4.7Ln

Tin is being investigated as a potential additive to metallic fuel to control fuel-cladding chemical interaction (FCCI). A primary cause of FCCI is the lanthanide fission products moving to the fuel periphery and interacting with the cladding. This interaction will lead to wastage of the cladding and eventually to a cladding breach. The current paper is a scanning electron microscopy (SEM) characterization of as-cast and annealed U-10Zr-4.3Sn and U-10Zr-4.3Sn-4.7Ln, where Ln = 53Nd-25Ce-16Pr-6La. Finally, the present study shows that tin preferentially binds the lanthanides, which will prevent lanthanide migration and interaction with the cladding.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Microstructural characterization of annealed U-12Zr-4Pd and U-12Zr-4Pd-5Ln: Investigating Pd as a metallic fuel additive

Here, palladium is being investigated as a potential additive to metallic fuel to control fuel-cladding chemical interaction (FCCI). A primary cause of FCCI is the lanthanide fission products moving to the fuel periphery and interacting with the cladding. This interaction will lead to wastage of the cladding and eventually to a cladding breach. The current study is a scanning electron microscopy (SEM) and transmission electron microscopy (TEM) characterization of annealed U-12Zr-4Pd and U-12Zr-4Pd-5Ln, where Ln=53Nd-25Ce-16Pr-6La. The present study shows that Pd preferentially binds the lanthanides, which will prevent lanthanide migration and interaction with the cladding. The SEM analysis indicates the 1:1 Pd-Ln compound is being formed, while the TEM analysis, due to higher resolution, found the 1:1 compound, as well as Pd-rich compounds Pd 2 Ln and Pd 3 Ln 2 .

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Microstructural characterization of as-cast U-20Pu-10Zr-3.86Pd and U-20Pu-10Zr-3.86Pd-4.3Ln

Palladium is being investigated as a potential additive to metallic fuel to bind fission product lanthanides, with the goal of reducing or preventing fuel-cladding chemical interactions (FCCI). A primary cause of FCCI is the lanthanide fission products moving to the fuel periphery and interacting with the cladding. This interaction will lead to wastage of the cladding and eventually to a cladding breach. The current study is a scanning electron microscopy (SEM) and transmission electron microscopy (TEM) investigation of as-cast U-20Pu-10Zr-3.86Pd and U-20Pu-10Zr-3.86Pd-4.3Ln in wt%, where Ln = 53Nd-25Ce-16Pr-6La. In U-20Pu-10Zr-3.86Pd, PdZr2 is forming, along with a possible ternary phase between Pu, Zr, and Pd. Pu is also present in the Pd-Ln precipitates formed in U-20Pu-10Zr-3.86Pd-4.3Ln. In the LnPd phase, Pu appears to be substitutional, forming (Ln,Pu)Pd. The other prominent phase, which appears to be Ln7Pd3, has a fine, lamellar structure. As a result, the lanthanides remain essentially constant across this fine structure, but Pu and Pd alternate as to which has the higher concentration.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Assessment of Te as a U-Zr fuel additive to mitigate fuel-cladding chemical interactions

Tellurium was investigated as a potential additive to metallic fuel (e.g. U-10Zr) to mitigate fuel-cladding chemical interaction (FCCI). A primary cause of FCCI is the lanthanide fission products migrating to the fuel periphery and interacting with cladding, Te therefore was used to bind the lanthanides into stable compounds in the U-10Zr. The present work investigates the microstructures of as-cast and annealed U-10Zr-4Te and U-10Zr-4Te-4Ce alloys (weight percent) with scanning electron microscope and transmission electron microscopy. In conclusion, tellurium was found to bind Ce and form CeTe compound, which will mitigate lanthanides migration to the cladding.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Microstructural characterization of annealed U-20Pu-10Zr-3.86Pd and U-20Pu-10Zr-3.86Pd-4.3Ln

Palladium is being investigated as a potential additive to metallic fuel to bind fission product lanthanides, with the goal of reducing or preventing fuel-cladding chemical interactions (FCCI). A primary cause of FCCI is the lanthanide fission products moving to the fuel periphery and interacting with the cladding. This interaction will lead to wastage of the cladding and eventually to a cladding breach. The current study is the microstructural characterization of annealed U-20Pu-10Zr-3.86Pd and U-20Pu-10Zr-3.86Pd-4.3Ln in wt. %, where Ln = 53Nd-25Ce-16Pr-6La, using scanning electron microscopy (SEM), transmission electron microscopy (TEM), and X-ray diffraction (XRD). In both alloys, the matrix is comprised of ζ-U 0.4 Pu 0.6 and δ-(U,Pu)Zr 2 . Based on the matrix compositions, modifications to the room temperature extrapolated U-Pu-Zr ternary phase diagram are suggested. In U-20Pu-10Zr-3.86Pd, there is very little δ phase, due to formation of PdZr 2 . In U-20Pu-10Zr-3.86Pd-4.3Ln, a lanthanide-rich phase is present, although it does not have the crystal structure for 53Nd-25Ce-16Pr-6La. Furthermore this phase cannot be identified based on known compounds. (Ln,Pu)Pd is the primary lanthanide phase, with Pu substituting into the crystal structure in place of Nd.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Interactions and immobilization of lanthanides with dopants in uranium-based metallic fuels

In uranium-based fuels, production and migration of lanthanide fission products and subsequent chemical interactions with cladding constituents lead to fuel–cladding chemical interaction (FCCI), limiting fuel performance. In general, dopant addition to the fuel matrix to arrest lanthanides within the fuel by forming intermetallics is found to be effective in mitigating FCCI. Recently, we proposed ab-initio based alloy-design principles, which can be useful in identifying dopant(s) that can bind a lanthanide (Nd) inside the fuel matrix. Here, we demonstrate the robustness of such principles by performing a systematic study to choose dopants to form compounds with a range of experimentally-observed lanthanide fission products. Results reveal that for a given dopant, lanthanide Ce and La exhibit similar behavior in their compound-forming tendencies compared to Nd and Pr, which is linked to lanthanide intrinsic characteristics such as the electronic configurations. Our predicted lanthanide-dopant intermetallic formation is verified experimentally in selective cases. Finally, we showed alloy design principles that accurately identify previously known dopants like Pd, and also predict new dopants As and Se, that can be effective in binding all lanthanides within the uranium matrix. Altogether, this research helps to develop generic alloy-design principles for complex multi-component systems based on lanthanide and dopant intrinsic characteristics.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Postirradiation characterization of palladium as an additive for fuel cladding chemical interaction mitigation in metallic fuel

This work describes the microstructural and elemental characterization of irradiated metallic fuels containing palladium as an additive. The use of additives has been proposed to control Fuel-Cladding Chemical Interaction (FCCI) and thus to promote higher fuel utilization (i.e., higher burnup). In this work, Pd has been investigated as a potential additive to metallic fuel to bind lanthanides, impeding their migration and attack on the cladding. The influence of Pd on the microstructure, chemistry and performance of metallic fuel has been characterized via scanning electron microscopy for two metallic fuel designs—namely, annular and solid fuel. Pd was observed to play an important role in the chemistry of the fuel. Indeed, the addition of Pd leads to the formation of new phases. Pd was detected to combine not only with the lanthanides, as intended, but also with Zr, a main element of the fuel matrix. While Pd proved to be effective in preventing lanthanide migration and their attack on the cladding, the Pd-Zr compound may potentially lead to other unexpected fuel-performance issues, such as the formation of low-melting point phases and increased unalloyed U available for FCCI interaction with Fe in the cladding. Even the increase of Zr to 13wt%. did not completely mitigate this adverse phenomenon generated by the Pd-Zr interaction. Furthermore, the efficacy of using this additive needs further investigation.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗