At least 55 records · Page 3

In-Pile Fuel Rod Deformation Measurements Using Miniaturized LVDT Technology

Different types of materials are being considered for fuel, cladding, and structures in existing and advanced nuclear reactors. These materials can undergo significant dimensional changes during irradiation. Currently in the US, such changes are measured with the ‘cook and look’ method (i.e. repeatedly irradiating a specimen for a specified period of time, and then removing it from the reactor for evaluation) – which leads to costly and time consuming experiments. In addition, such techniques provide limited data, and handling may disturb the phenomena of interest. Therefore, in-pile detection of geometric changes is needed to understand real-time behavior during irradiation testing of fuels and materials in high flux US Material and Test Reactors (MTRs). The developmental results of an advanced Linear Variable Differential Transformer (LVDT)-based test rig capable of detecting real-time changes in diameter or length of fuel rods or other material samples during irradiation in US MTRs are presented. The LVDT is being developed at the Idaho National Laboratory (INL), and will provide experimenters with the capability to measure dimensional changes associated with fuel and clad swelling, pellet-clad interaction, and crud buildup. The LVDT design utilizes the MTR’s loop pressure to drive the test specimen at a constant rate. This leads to a simplified construction which only requires three pressure boundary penetrations. Further, the LVDT pressure boundary is a leak tight hydraulic ram capable of actuating under low differential pressure (e.g. 1 psid), and is able to survive the high irradiation tests at Pressurized Water Reactor (PWR) conditions.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

High-energy synchrotron study of in-pile-irradiated U–Mo fuels

Here synchrotron scattering analysis results on U–7wt.%Mo fuel specimens irradiated in the Advanced Test Reactor to three burnup levels (3.0, 5.2, and 6.3 × 1021 fission/cm3) are reported. Mature fission gas bubble superlattice was observed to form at intermediate burnup. The superlattice constant was determined to be 11.7 and 12.0 nm by wide-angle and small-angle scattering respectively. Grain sub-division takes place throughout the irradiation and causes the collapse of the superlattice at high burnup. The bubble superlattice expands the U–Mo lattice and acts as strong sink for radiation-induced defects. The evolution of dislocation loops was, therefore, suppressed until the bubble superlattice collapsed.

metallic nuclear fuel↗

Advanced Test Reactor Mini-Plate Hydraulic Testing

Currently, flow testing is being performed at Oregon State University (OSU) on the hydromechanical Fuel Test Facility (HMFTF) and the Endurance Flow Loop (EFL) to aid in the qualification of low enriched plate-type Uranium fuels for use in high performance research reactors in the US, under the Global Threat Reduction Initiative (GTRI). Under this project, varying geometries of small capsules proposed for irradiation testing in the Advanced Test Reactor (ATR) are being hydraulically testing prior to being placed in the ATR. The premise of this study was to conduct a number of flow tests on these capsules to characterize the pressure loss through each as a function of flow rate and compare the results against predicted theoretical values. Two categories of flow tests were performed in the Endurance Flow Loop to supplement flow testing of proposed LEU plate-type fuel for conversion of High Performance Research Reactors: Capsule Comparison Tests and Orifice Characterization Tests. The purpose of these tests were to determine the pressure drop across each experiment as a function of flow rate and to compare the results against a simple analytical model of the pressure loss through a pipe, to support the safety basis for the in-pile experiments. The capsule comparison tests compared the pressure loss through three types of capsules: RERTR, MP-1, and EMPIRE. In this category, nine flow tests were performed to determine the effect of having one, two, and three of each type of capsule placed in series in a test section. The analytical model accurately predicted, for each case, an increase in hydraulic resistance for each capsule that was added, though the values were conservative. The orifice characterization tests compared the pressure loss through various configurations of small orifice spacers in conjunction with blank spacers and the MP-1 capsules. The analytical model predicted that adding blank spacers would slightly increase the pressure drop due to added frictional effects, but indicated no change in the pressure drop based on the orientation of the capsules. The measured results indicated that the addition of the blank spacers had no measurable effect on the pressure drop, while changing the orientation of the capsules did. In all 15 flow tests, the theoretical model provides a conservative estimate of the pressure drop through each configuration for an equivalent flow rate, over that of the measured results.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Lunar Polar Environmental Testing: Regolith Simulant Conditioning

As ISRU system development approaches flight fidelity, there is a need to test hardware in relevant environments. Extensive laboratory and field testing have involved relevant soil (lunar regolith simulants), but the current design iterations necessitate relevant pressure and temperature conditions. Including significant quantities of lunar regolith simulant in a thermal vacuum chamber poses unique challenges. These include facility operational challenges (dust tolerant hardware) and difficulty maintaining a pre-prepared soil state during pump down (consolidation state, moisture retention).For ISRU purposes, the regolith at the lunar poles will be of most interest due to the elevated water content. To test at polar conditions, the regolith simulant must be doped with water to an appropriate percentage and then chilled to cryogenic temperatures while exposed to vacuum conditions. A 1m tall, 28cm diameter bin of simulant was developed for testing these simulant preparation and drilling operations. The bin itself was wrapped with liquid nitrogen cooling loops (100K) so that the simulant bed reached an average temperature of 140K at vacuum. Post-test sampling was used to determine desiccation of the bed due to vacuum exposure. Depth dependent moisture data is presented from frozen and thawed soil samples.Following simulant only evacuation tests, drill hardware was incorporated into the vacuum chamber to test auguring techniques in the frozen soil at thermal vacuum conditions. The focus of this testing was to produce cuttings piles for a newly developed spectrometer to evaluate. This instrument, which is part of the RESOLVE program science hardware, detects water signatures from surface regolith. The drill performance, behavior of simulant during drilling, and characteristics of the cuttings piles will be offered.

lunar regolith↗

Lunar Polar Environmental Testing: Regolith Simulant Conditioning

As ISRU system development approaches flight fidelity, there is a need to test hardware in relevant environments. Extensive laboratory and field testing have involved relevant soil (lunar regolith simulants), but the current design iterations necessitate relevant pressure and temperature conditions. Including significant quantities of lunar regolith simulant in a thermal vacuum chamber poses unique challenges. These include facility operational challenges (dust tolerant hardware) and difficulty maintaining a pre-prepared soil state during pump down (consolidation state, moisture retention).For ISRU purposes, the regolith at the lunar poles will be of most interest due to the elevated water content. To test at polar conditions, the regolith simulant must be doped with water to an appropriate percentage and then chilled to cryogenic temperatures while exposed to vacuum conditions. A 1m tall, 28cm diameter bin of simulant was developed for testing these simulant preparation and drilling operations. The bin itself was wrapped with liquid nitrogen cooling loops (100K) so that the simulant bed reached an average temperature of 140K at vacuum. Post-test sampling was used to determine desiccation of the bed due to vacuum exposure. Depth dependent moisture data is presented from frozen and thawed soil samples.Following simulant only evacuation tests, drill hardware was incorporated into the vacuum chamber to test auguring techniques in the frozen soil at thermal vacuum conditions. The focus of this testing was to produce cuttings piles for a newly developed spectrometer to evaluate. This instrument, which is part of the RESOLVE program science hardware, detects water signatures from surface regolith. The drill performance, behavior of simulant during drilling, and characteristics of the cuttings piles will be offered.

in situ resource utilization↗

(S)TEM/EDS study of native precipitates and irradiation induced Nb-rich platelets in high-burnup M5®

We have investigated microstructure and microchemistry of precipitates and dislocation loops in high-burnup M5® using (scanning) transmission electron microscopy ((S)TEM) equipped with energy dispersive X-ray spectroscopy (EDS). Two (S)TEM lamellae were made by cryo-FIB from the same cladding sample. The Nb-rich native precipitates were found in the metal, in the suboxide and in the oxide. Upon diffraction analysis, most of the Nb-rich native precipitates in the metal matrix remain as β-Nb phase, while no β-Nb native precipitates were found in the oxide. Nearby the oxide and metal (O/M) interface, the native precipitates in the oxide were already oxidized into t-NbO2 phase. At further distance away from the O/M interface, the Nb-rich native precipitates were gradually oxidized and became amorphous. Besides the native precipitates, Nb-rich irradiation induced precipitates (IIPs) were found in the metal matrix. Using g = <0002> vector for imaging, the length of the IIPs was aligned with dislocation loops. However, no Nb segregation to the dislocation loops themselves was observed. For the first time, we report that IIPs indeed exist in the oxide but only within about 1.5 µm away from O/M interface. However, the oxidation state of the IIPs in the oxide is still unclear. The presence of both native precipitates and IIPs in the oxide may indicate the Nb concentration in the oxide solid solution remain low nearby the O/M interface, which may explain the reduced corrosion kinetics of in-pile M5®. On the other hand, no IIPs were observed in the oxide at further distance and this may indicate that they have eventually dissolved back into the oxide. A few mechanisms related to IIPs stability in the oxide are presented.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Long term out-of-pile thermocouple tests in conditions representative for nuclear gas-cooled high temperature reactors

During irradiation tests at high temperature, failure of commercial Inconel 600 sheathed thermocouples is commonly encountered. To understand and remedy this problem, out-of-pile tests were performed with thermocouples in carburizing atmospheres which can be assumed to be at least locally representative for High Temperature Reactors. The objective was to screen those thermocouples which would consecutively be used under irradiation. Two such screening tests have been performed with a set of thermocouples embedded in graphite (mainly conventional Type N thermocouples and thermocouples with innovative sheaths) in a dedicated furnace with helium flushing. Performance indicators such as thermal drift, insulation and loop resistance were monitored and compared to those from conventional Type N thermocouples. Several parameters were investigated: niobium sleeves, bending, thickness, sheath composition, temperature as well as the chemical environment. After the tests, Scanning Electron Microscopy (SEM) examinations were performed to analyze possible local damage in wires and in the sheath. The present paper describes the two experiments, summarizes results and outlines further work, in particular to further analyze the findings and to select suitable thermocouples for qualification under irradiation. (authors)

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Candidate Structural Materials for In-Core VHTR Application

Graphite moderated gas cooled reactors led the way into the nuclear age with the Chicago Pile-1 reactor, which provided the first sustained critical reaction in December, 1942. The first commercial nuclear plant, Calder Hall in the UK, went critical in 1956 with an outlet gas temperature of {approx}345 C. As depicted in Fig. 1, in five decades since Calder Hall, outlet temperature increased rapidly, reaching a plateau of {approx}950 C. This apparent ceiling is in large part due to limitations in the structural materials utilized within the core (e.g. control systems) and primary loop (hot duct, heat-exchangers etc.) Simply, the operating temperatures of Generation III (HTGR's) are very near performance limits of the structural alloys used, both in terms of elevated temperature and as-irradiated properties. This limitation remains today and is the reason the outlet temperature of the Generation IV Very High Temperature Reactor (VHTR) continues to be revised downward from the original optimistic goal of {approx}1200 C, to it's current target outlet temperature of {approx}950 C, a temperature consistent with the previous generation of HTGR's. An example of the challenges facing Generation IV VHTR is found by considering the control rods. For the Fort St. Vrain Reactor the control system consisted of thirty tubes each containing B4C control material. Alloy 800, originally developed by Inco in the 1950's under the trade-name Incoloy 800 and 800H had found widespread application is steam generators, turbines and was selected for this control rod application. These materials are included for Class 1 Nuclear Component by ASME section III. In addition to Ft. St Vrain, alloy 800H has found control rod application in the German HTR and Japanese HTTR reactors and is the primary choice Pebble Bed Modular Reactor (a HTGR) reactivity control system. Figure 2 gives the ASME allowed stress for Alloy 800H. Due to the loss in creep rupture strength, the allowed design stress for decreases substantially above {approx}500 C. For the operating temperature (and current maximum code temperature) of the Fort St. Vrain reactor ({approx}760 C) the control rod designed from Alloy 800H would be allowed approximately 20 MPa primary stress. For the anticipated temperature of the VHTR that stress would likely be under 10 MPa in the non-irradiated condition. Selection of VHTR in-core structural material will depend on the ability for the material to withstand extreme temperatures and irradiation. The use of Alloy 800H for control rod applications is preferred, but will require designing with a relatively low strength material which becomes brittle upon modest irradiaton. Presently, more fidelity in both design and the available Alloy 800H database are required to judge the lifetime this alloy will have in service. The only currently envisioned alternative to Alloy 800H are the CFC and SiC/SiC composites, which are currently challenged by code qualification issues. As with Alloy 800H, the composite irradiation data-base is inadequate, though it appears that the CFC service lifetime will be limited due to its anisotropic dimensional change under irradiation to doses somewhat higher than Alloy 800H (1-5 x 10{sup 25} n/m{sup 2}), while SiC/SiC composites appear to retain their mechanical properties to doses in excess of the VHTR lifetime dose. As the path to qualification of both CFC and SiC/SiC are similar, it appears that SiC/SiC is more attractive for high-dose Gen IV application unless high thermal conduction is required.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

As-run thermal-hydraulics analysis of the EPRI-2 experiment

The EPRI-2 experiment was designed to irradiate various types of reactor pressure vessel steels at a temperature of 288°C (PLN-3934). The specimens were irradiated in a non-instrumented test train inside a pressurized water loop in the center lobe of the ATR during PALM cycle 153B. Temperature was indicated by post-irradiation examination of melt wires placed within the test train. The purpose of this analysis is to calculate specimen temperature using measured data on reactor power and as-run calculations of heating rates of the test train. The experiment contains several melt wires spanning the temperature range 239°C to 327°C. The accuracy of the model is assessed by comparing the measured and calculated in-pile tube inlet to outlet temperature difference, and comparing the calculated specimen temperature to the temperature range indicated by examination of the melt wires.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Impulsive reconnection: 3D onset and stagnation in turbulent paradigms

Reconnection processes are ubiquitous in solar coronal loops, the earth's magnetotail, galactic jets, and laboratory configurations such as spheromaks and Z pinches. It is believed that reconnection dynamics are often closely linked to turbulence. In these phenomena, the bursty onset of reconnection is partly determined by a balance of macroscopic MHD forces. In a turbulent paradigm, it is reasonable to suppose that there exist many individual reconnection sites, each X-line being finite in axial extent and thus intrinsically three-dimensional (3D) in structure. The balance between MHD forces and flux pile-up continuously shifts as mutually tangled flux ropes merge or bounce. The spatial scale and thus the rate of reconnection are therefore intimately related to the turbulence statistics both in space and in time. We study intermittent 3D reconnection along spatially localized X-lines between two or more flux ropes. The threshold of MHD instability which in this case is the kink threshold is varied by modifying the line-tying boundary conditions. For fast inflow speed of approaching ropes, there is merging and magnetic reconnection which is a well known and expected consequence of the 2D coalescence instability. On the other hand, for slower inflow speed the flux ropes bounce. The threshold appears to be the Sweet Parker speed v{sub A}/S{sup 1/2}, where v{sub A} is the Alfven speed and S is the Lundquist number. Computations by collaborators at University of Wisconsin, Madison, Katholieke Universiteit Leuven, and LANL complement the experiment.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

As-run thermal hydraulics analysis of the EPRI-1 Experiment

The EPRI-1 experiment was designed to irradiate various types of reactor pressure vessel steels at a temperature of 288°C (PLN-3934). The specimens were irradiated in an instrumented test train inside a pressurized water loop in the center lobe of the ATR during cycle 157C. Temperature was monitored using thermocouples placed at the top of the test train. Additional temperature indications were obtained by post-irradiation examination of melt wires placed within the test train and spanning the temperature range 239°C to 327°C. The purpose of this analysis is to calculate specimen temperature using measured data on reactor power and as-run calculations of heating rates of the test train. The accuracy of the model is assessed by comparing the measured and calculated in-pile tube inlet to outlet temperature difference, comparing the measured and calculated thermocouple temperatures, and comparing the calculated specimen temperature to the temperature range indicated by the melt wires.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

As-run thermal-hydraulic analysis of the EPRI-3 experiment

The EPRI-3 experiment was designed to irradiate various types of reactor internal component steels at a temperature of 288°C. The specimens were irradiated in an instrumented test train inside a pressurized water loop in the center lobe of the ATR during cycles 155B and 158B. Temperature was monitored using thermocouples placed at the top of the test train and melt wires placed within the test train. The purpose of this analysis is to calculate specimen temperature using measured data on reactor power and as-run calculations of heating rates of the test train. The experiment contains four thermocouples and several melt wires spanning the temperature range 239°C to 327°C. The accuracy of the model is assessed by comparing the measured and calculated in-pile tube inlet to outlet temperature difference, comparing the measured and calculated thermocouple temperatures, and comparing the calculated melt wire temperature to the temperature range indicated by examination of the melt wires.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Design and Laboratory Evaluation of Future Elongation and Diameter Measurements at the Advanced Test Reactor

New materials are being considered for fuel, cladding, and structures in next generation and existing nuclear reactors. Such materials can undergo significant dimensional and physical changes during high temperature irradiations. In order to accurately predict these changes, real-time data must be obtained under prototypic irradiation conditions for model development and validation. To provide such data, researchers at the Idaho National Laboratory (INL) High Temperature Test Laboratory (HTTL) are developing several instrumented test rigs to obtain data real-time from specimens irradiated in well-controlled pressurized water reactor (PWR) coolant conditions in the Advanced Test Reactor (ATR). This paper reports the status of INL efforts to develop and evaluate prototype test rigs that rely on Linear Variable Differential Transformers (LVDTs) in laboratory settings. Although similar LVDT-based test rigs have been deployed in lower flux Materials Testing Reactors (MTRs), this effort is unique because it relies on robust LVDTs that can withstand higher temperatures and higher fluxes than often found in other MTR irradiations. Specifically, the test rigs are designed for detecting changes in length and diameter of specimens irradiated in ATR PWR loops. Once implemented, these test rigs will provide ATR users with unique capabilities that are sorely needed to obtain measurements such as elongation caused by thermal expansion and/or creep loading and diameter changes associated with fuel and cladding swelling, pellet-clad interaction, and crud buildup.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Conceptual Design Report for the I2 Instrumentation Experiment in ATRC

The US Department of Energy In-Pile Instrumentation (I2) program is tasked with developing advanced sensors for in-pile service as well as supporting the engineering required to implement existing nuclear sensor technologies in US high-power test reactors. The ATRC instrumentation test has been conceived to address both of these missions, specifically with respect to neutron flux measurements. Space has been allocated in the test for Self-Powered Neutron Detectors (SPNDs), fission chambers, and Micro-Pocket Fission Detectors (MPFDs). The real-time flux readings obtained from these instruments will be compared with time integrated data obtained from passive neutron dosimetry (i.e., “flux” wires). This work will be complementary to data obtained from the TREAT MIMIC-N experiment. This experiment is expected to support instrumentation efforts related to the proposed Medium-I loop and to instrumenting loop experiments conducted in the ATR center flux trap. While the MIMIC-N experiment was conducted in a dry environment, the ATRC I-19 experiment will be conducted in an aqueous environment, similar to the center flux trap loop experiments but will take place at ambient temperature and pressure, and at a much lower neutron flux. One of the challenges of the ATRC I-19 experiment will be low amplitude signals produced by the sensors in the low neutron fluxes of ATRC. However, related work conducted several years ago in ATRC was able to reliably detect signals using a similar instrument set.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Comparison of Subdivided Versus Full-Length Fuel Pin Burnup in the ATF-2 Safety Analysis

The Accident Tolerant Fuels (ATF) campaign, under the Fuel Cycle Research and Development (FCRD) Advanced Fuels program, was developed after the Fukushima Daiichi Nuclear Power Plant disaster in 2011. Under ATF, fuel and cladding concepts are to be developed and tested that may more readily withstand an accident similar to the one that occurred at Fukushima Daiichi. ATF is a combination of industry, universities, and national laboratories in an effort to develop advanced accident tolerant cladding and fuel concepts. The end goal of the ATF program is to insert a lead test rod (LTR) or lead test assembly (LTA) into an operating commercial power light water reactor by 2022. In order to meet this 2022 insertion goal, ATF is split into three separate phases: ATF-1, ATF-2, and ATF-3. The first phase of the ATF program, ATF-1, is the concept feasibility study and early irradiation testing. Feasibility, fabrication, and out-of-pile testing are happening at universities and laboratories all over the United States. Irradiation testing of these concepts is happening at the Advanced Test Reactor (ATR) at the Idaho National Laboratory (INL). Early irradiation testing involves testing clad and/or fuel in drop-in capsules in the ATR. Currently, these capsules are in the relatively low-flux positions in the ATR, but some newer concepts and concepts that require higher burnup will be moved to the higher-flux positions later on during irradiation. Currently, Oak Ridge National Laboratory (ORNL), Westinghouse Electric Company, Areva, and General Electric (GE) have inserted capsules for ATF-1, although more concepts are planned. The second phase of ATF, ATF-2, is the focus of this paper. ATF-2 is the loop testing of fuel pins with new cladding and fuel concepts to simulate pressurized water reactor (PWR) and boiling water reactor (BWR) environments. ATF-2 will concurrently be happening at the ATR and at the Halden Reactor in Norway. The ATF-2 irradiation at the ATR will only simulate a PWR environment. ATF-2 will be inserted into the ATR pressurized water loop, Loop 2A, in the Center Flux Trap (CFT), where chemistry, temperature, and pressure can all be controlled separately from the primary coolant system and other loops in ATR. Loop 2A will be borated, pressurized to 2200 psi nominal, and have an average water temperature of 300 deg. C. A borated loop with fueled rodlets is extremely rare for Nuclear Energy experiments in the ATR, so ATF-2 will demonstrate new and unique capabilities for INL. ATF-3 is the testing of fresh and irradiated ATF concepts at the Transient Reactor Test (TREAT) Facility. The TREAT Reactor is planned for restart, re-establishing U.S. transient testing capabilities after nearly 20 years of non-operations. TREAT will test ATF concepts under transient conditions, such as a reactivity insertion accident. In addition to fresh fuel pins, TREAT will use from ATF2 and do transient testing on those irradiated pins. The information TREAT will provide to the vendors to support fuel licensing will be valuable, showing that these concepts do enhance the accident tolerance of the fuel in commercial reactors. (author)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Fuel-Coolant Interaction Results for High Energy In-Pile LWR Fuels Experiments

Fuel-coolant interaction (FCI) has long been a subject of interest in severe-accident reactor safety applications. Significant chemical interaction also frequently results at the high temperature associated with these events in a water environment. Historical rapid, high energy transient irradiation test results are reviewed for experiments performed in transient experimental reactors in Idaho. Though such events are not credible for any deployed nuclear reactor technology, the pressure waves produced by FCI on surrounding containment structures are of importance to advanced light water reactor designs and for transient experiment design considerations. A brief introduction to steam explosion and related studies is provided in the context of these experiments. Extensive reactivity initiated accident testing programs were carried out in the Transient REActor Test (TREAT) facility, the Special Power Excursion Reactor Test (SPERT) facility, and the Power Burst Facility (PBF) from the 1960’s through the late 1970’s. A variety of fuel forms including waterlogged rods were tested in capsules containing water coolant at standard temperature pressure. A few tests were performed at high pressure and temperature in the water loop of PBF. In many of these experiments, energy deposition was high enough to greatly exceed melting temperatures of the fuel, resulting in some fraction of the fuel being dispersed into the coolant. A purpose of many of these tests was to determine the nuclear-to-mechanical energy conversion ratio as well as the extent of metal-water reaction. Relevant data collected from these tests included transient energy deposition, pressure response of the coolant, water column velocity, total hydrogen generation, and resulting particle size distributions and particle characterization. In this paper, the mechanical configuration of each experiment facility is reviewed and discussed relative to the measured responses. The empirical results for source pressure and extent of metal-water reaction are presented in the context of the experimental conditions. The results of these experiments provide a unique understanding for behavior of fuel under severe accident conditions in a reactor environment.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Testing and Characterization to Develop a Mechanistic Explanation for Unsaturated Drift of Fiber Optic Sensors during High-Dose Irradiation

The primary limitation for any optical fiber-based sensor for nuclear reactor applications is radiation-induced attenuation (RIA) of the transmitted and/or reflected signals. Based on several recent studies, RIA is tolerable for some fused silica optical fibers with the proper choice of sensing wavelength and fiber dopants. For extreme temperature applications (> 1000°C), sapphire optical fibers have been proposed; however, recent optical transmission measurements performed on bulk sapphire samples showed prohibitively large RIA. For some sensors, radiation-induced dimensional changes in the fiber materials can also cause significant drift. Moreover, the drift that was observed in numerous experiments performed in the High Flux Isotope Reactor (HFIR), the Advanced Test Reactor, the Massachusetts Institute of Technology Reactor, and other international facilities far exceeded what would be expected based on compaction of fused silica glass. Clearly, additional work is needed to better understand the origins of both RIA and radiation-induced drift in both silica and sapphire optical fiber-based sensors before these sensors can be reliably deployed for nuclear applications. This work evaluated the underlying mechanisms that may be responsible for RIA and drift in silica and sapphire materials. First, detailed characterization was performed on bulk fused silica glass samples that were previously irradiated to different neutron fluences at different temperatures to better understand the structural changes that drive radiation-induced drift in the absence of coating effects that are discussed later. Results show that the non-monotonic compaction that occurs with increasing neutron fluence continues up to fast neutron fluences approaching 10 22 n/cm 2 , which has important implications for physics-based models that may be used to compensate for the sensor drift. Initial Raman spectroscopy and synchrotron x-ray diffraction provide insights into the nature of the structural changes. Next, detailed characterizations were performed on silica fibers with various coatings that were subjected to several different thermal treatments. The hypothesis is that the coatings convert to carbon-rich materials that compact under irradiation, putting a large compressive strain on the fiber. Out-of-pile testing confirms that both polyimide and acrylate fiber coatings convert to glassy carbon (GC) materials when heated under inert conditions, and the degree of order (i.e., graphitization) increases with increasing temperature. The results provide increasingly strong evidence that the combination of polymeric coatings and inert (or vacuum) conditions render fiber optic sensors susceptible to significant radiation-induced drift that would not otherwise exist in uncoated fibers. Finally, transmission electron microscopy was performed on bulk sapphire samples that were irradiated to two neutron fluences at different temperatures to gain insights into the potential mechanisms driving the prohibitive RIA at higher neutron fluences and temperatures. Contrary to previous hypotheses, results show that scattering from radiation-induced voids cannot explain the observed RIA. Similarly, models for scattering losses from dislocation loops also do not agree with the experimental results. Instead, fitting to the experimental data shows that increased absorption from aluminum vacancy centers is the most likely explanation for the the prohibitively large RIA that was observed at high irradiation temperature and dose. In addition, the voids that formed in these single-crystal samples were found to align along the basal plane (a-axis) as opposed to that seen in previous observations of c-axis alignment in polycrystalline samples, which could have important implications for anisotropic swelling and other phenomena that could affect sensor performance at high neutron fluence.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Testing and Characterization to Develop a Mechanistic Explanation for Unsaturated Drift of Fiber Optic Sensors during High-Dose Irradiation

The primary limitation for any optical fiber-based sensor for nuclear reactor applications is radiation-induced attenuation (RIA) of the transmitted and/or reflected signals. Based on several recent studies, RIA is tolerable for some fused silica optical fibers with the proper choice of sensing wavelength and fiber dopants. For extreme temperature applications (> 1000°C), sapphire optical fibers have been proposed; however, recent optical transmission measurements performed on bulk sapphire samples showed prohibitively large RIA. For some sensors, radiation-induced dimensional changes in the fiber materials can also cause significant drift. Moreover, the drift that was observed in numerous experiments performed in the High Flux Isotope Reactor (HFIR), the Advanced Test Reactor, the Massachusetts Institute of Technology Reactor, and other international facilities far exceeded what would be expected based on compaction of fused silica glass. Clearly, additional work is needed to better understand the origins of both RIA and radiation-induced drift in both silica and sapphire optical fiber-based sensors before these sensors can be reliably deployed for nuclear applications. This work evaluated the underlying mechanisms that may be responsible for RIA and drift in silica and sapphire materials. First, detailed characterization was performed on bulk fused silica glass samples that were previously irradiated to different neutron fluences at different temperatures to better understand the structural changes that drive radiation-induced drift in the absence of coating effects that are discussed later. Results show that the non-monotonic compaction that occurs with increasing neutron fluence continues up to fast neutron fluences approaching 10 22 n/cm 2 , which has important implications for physics-based models that may be used to compensate for the sensor drift. Initial Raman spectroscopy and synchrotron x-ray diffraction provide insights into the nature of the structural changes. Next, detailed characterizations were performed on silica fibers with various coatings that were subjected to several different thermal treatments. The hypothesis is that the coatings convert to carbon-rich materials that compact under irradiation, putting a large compressive strain on the fiber. Out-of-pile testing confirms that both polyimide and acrylate fiber coatings convert to glassy carbon (GC) materials when heated under inert conditions, and the degree of order (i.e., graphitization) increases with increasing temperature. The results provide increasingly strong evidence that the combination of polymeric coatings and inert (or vacuum) conditions render fiber optic sensors susceptible to significant radiation-induced drift that would not otherwise exist in uncoated fibers. Finally, transmission electron microscopy was performed on bulk sapphire samples that were irradiated to two neutron fluences at different temperatures to gain insights into the potential mechanisms driving the prohibitive RIA at higher neutron fluences and temperatures. Contrary to previous hypotheses, results show that scattering from radiation-induced voids cannot explain the observed RIA. Similarly, models for scattering losses from dislocation loops also do not agree with the experimental results. Instead, fitting to the experimental data shows that increased absorption from aluminum vacancy centers is the most likely explanation for the the prohibitively large RIA that was observed at high irradiation temperature and dose. In addition, the voids that formed in these single-crystal samples were found to align along the basal plane (a-axis) as opposed to that seen in previous observations of c-axis alignment in polycrystalline samples, which could have important implications for anisotropic swelling and other phenomena that could affect sensor performance at high neutron fluence.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗