Ca Metal Batteries and Sn Anode Alloying: Resolving Misconceptions in Ca–Sn Alloy Formation

Ca metal anode suffers from surface passivation and struggles to effectively plate and strip in conventional Ca electrolytes, making the development of alloy anode for calcium metal battery essential. This work systematically and carefully evaluates the electrochemical formation and feasibility of the Sn anode and its possibility of alloying with Ca using a combination of cyclic voltammetry, scanning electron microscopy with energy-dispersive X-ray spectroscopy (SEM/EDS), X-ray diffraction (XRD), and synchrotron transmission X-ray microscopy (TXM). Electrochemical measurements and SEM/EDS analyses indicate apparent Ca alloy formation. However, detailed XRD and TXM characterization reveal substantial lithium-ion involvement when lithium metal is employed as the reference electrode, even in electrolytes with high Ca salt concentrations. These findings highlight a significant risk of misinterpretation: Although limited Ca–Sn alloying may occur, the faster kinetics of Li + can dominate the alloying process, leading to a Li-driven reactions at the Sn anode. In contrast, cells constructed with Ca metal as both reference and counter electrodes exhibit distinct redox features only during the initial cycles, followed by rapid cell failure. The high oxidation currents induce severe Ca passivation, occurring nearly concurrently with Sn dealloying. Overall, this study provides critical insight into the practical limitations and common experimental artifacts associated with Ca metal battery systems and underscores the necessity for rigorous cell design and cautious interpretation when evaluating alloy chemistry in multivalent Ca-based batteries.

36 MATERIALS SCIENCE↗

Chemical factors controlling the behaviour of oxide cathodes in batteries

Oxide cathodes enable high-energy lithium-ion and sodium-ion batteries, with their performances fundamentally governed by three interrelated chemical factors: electronic configuration, chemical bonding, and chemical reactivity. Here, we illustrate how these factors dictate the redox energy, structural stability, ionic and electronic transport, and interfacial behavior in both layered oxide and polyanion oxide cathodes. We discuss how crystal-field effects and octahedral-site stabilization energies influence cation migration, and how inductive effects tune bond covalency and operating voltages. We also explain how chemical bonding governs thermal stability, gas evolution, and first-cycle capacity loss, and how alignment of transition-metal redox band with the oxygen 2p band determines electrolyte reactivity. Comparison between lithium and sodium layered oxides further reveals how differences in Li-O and Na-O bond ionicity affect chemical reactivity. Finally, we outline strategies including compositional tuning, surface doping, and electrolyte optimization, and emphasize how high-throughput, data-driven approaches in guiding the design of next-generation oxide cathodes.

25 ENERGY STORAGE↗

Pressure Heterogeneity and Material Utilization in Thin-Film Solid-State Cathodes

Intimate interfacial contact between the solid electrolyte and the cathode active material is critical for maximizing cathode utilization in solid-state batteries. However, volume changes during electrochemical cycling induce internal stresses that drive interfacial degradation, particularly under nonuniform stack pressure. In this study, we employ in situ energy-dispersive X-ray diffraction tomography to visualize and quantify reaction heterogeneities across a 3 mm-diameter solid-state cathode with a well-defined interface. Our results reveal that regions under a lower stack pressure exhibit reduced material utilization and reversibility, which negatively affect the high-pressure regions. Interfacial degradation further impedes lithium-ion transport and amplifies microscale reaction heterogeneity. These findings highlight the critical role of stack pressure distribution in governing interfacial stability and electrochemical performance, offering important design insights into practical solid-state battery systems.

36 MATERIALS SCIENCE↗

Lithium-Ion Battery Design for Grid-Scale Energy Storage App

A software that delivers parameters from energy storage system (ESS) to container, rack, module and single cell design, as well as data analysis on arbitrage energy and frequency regulation of ESS in different regions, has been developed. The Lithium-ion Battery Design for Grid-scale Energy Storage App V1.0 has the capability to output the system, module and cell design with the energy, power, capacity, group method, cost of single cell, and single cell test protocol which break down from input energy storage system data in different regions. The default chemistry of the battery is LiFePO4 and graphite. The energy density of the graphite/LiFePO 4 pouch cell ranges from 100 Wh/kg to 200 Wh/Kg in the software. Graphite/LiFePO 4 pouch cell (up to 1Ah in lab) manufacturing line is also built and can be used to evaluate the test protocol, moreover, for electrolyte evaluation in other ESMI seedling projects. The software enables rapid prototyping to accelerate energy storage research, development, and manufacturing.

Liu, Dianying↗

Understanding Discharge‐Driven Growth of Cathode Impedance in Ni‐Rich NMC Cathodes

Degradation of LiNi x Mn y Co 1-x-y O 2 (NMC)-based lithium-ion batteries depends strongly on cut-off voltage ranges. In addition to the high upper cut-off voltage, a high depth of discharge (i.e., lower cut-off voltage) significantly worsens cathode impedance growth and capacity fade during long-term cycling. However, there is currently no consensus on the mechanism behind the negative role of a deep discharge. Here, this phenomenon was investigated in graphite||NMC cells with single-crystal cathodes (LiNi 0.6 Co 0.2 Mn 0.2 O 2 (NMC622) or LiNi 0.76 Co 0.14 Mn 0.10 O 2 (NMC76)) using targeted aging protocols (constant high-voltage holds vs. charge–discharge cycling), while monitoring transition-metal (TM) dissolution, cathode-electrolyte interface (CEI) impedance, and NMC surface composition. We demonstrate a correlation between discharge-driven CEI impedance growth and increased TM dissolution. Furthermore, this degradation pathway is more pronounced in lower-Ni NMC622 than in higher-Ni (NMC76) under comparable delithiation states at charge, with both compositions undergoing the H2→H3 phase transition. X-ray photoelectron spectroscopy (XPS) reveals NMC composition-dependent evolution of surface lattice oxygen and restructured surface layer composition between charged and discharged states. These findings add mechanistic depth to the role of discharge as an active driver of interfacial degradation and provide new insights into its composition dependence.

25 ENERGY STORAGE↗

Low-Rate Cycling Regeneration Sustains NMC811–Graphite Battery Performance through Extreme Ultrafast Charging

Urban air mobility (UAM) systems, such as electric vertical takeoff and landing (eVTOL) aircraft, require batteries capable of extreme ultrafast charging to support high-frequency operations. Here, in this work, we evaluate the electrochemical stability of NMC811–graphite full cells using a complex mixed-modal protocol designed to simulate the aggressive turnaround demands of UAM missions. We demonstrate that incorporating a periodic low-rate (0.3C) “regeneration” cycle enables cells to maintain 96% capacity retention over 900 cycles, despite repeated exposure to ultrafast pulses. To validate the efficacy of this regeneration mechanism, we performed simplified control experiments comparing continuous 10C charging against a 10C–0.3C interleaved protocol. Advanced characterization reveals that while mechanical particle fracture is pervasive at these rates, the regeneration cycles decelerate the electrochemical degradation by resolving spatially heterogeneous Ni oxidation states and relaxing lithium-ion concentration gradients. These findings provide a vital mechanistic framework for battery operation, proving that restorative charging can effectively delay and mitigate failure in demanding UAM applications.

batteries↗

Hypochlorite Redox Chemistry Enables High-Voltage and High-Power Saltwater Batteries

Saltwater batteries (SWBs) are promising alternatives to lithium-ion batteries for large-scale stationary energy storage. However, the performance of conventional oxygen redox-based saltwater battery systems is often constrained by sluggish oxygen evolution and reduction reactions (OER/ORR) at the cathode, leading to low voltage efficiency and limited power density. Here, OER and ORR are replaced by hypochlorite-based redox reactions through the introduction of sodium hypochlorite into saltwater. Operando pH and dissolved oxygen measurements confirm that OER and ORR are minimized and that hypochlorite redox reactions dominate the cathode behavior. Owing to the higher operating potential and faster reaction kinetics, the hypochlorite-redox-based SWBs delivers a higher discharge voltage of 3.3 V and reduced charge-discharge voltage polarization to 0.66 V. Further improvement is achieved by adjusting the saltwater pH to near-neutral conditions, increasing the discharge voltage to 3.5 V and more than doubling the peak power. The hypochlorite redox environment also exhibits chemical stability with key cell components, including the solid electrolyte and cathode current collectors. Operation of series-connected cells and cells employing hard carbon anodes demonstrates scalability and compatibility with alternative anode materials. These results provide a strong foundation for next-generation SWBs targeting large-scale stationary energy storage applications.

Go, Wooseok [ORNL]↗

Prelithiated SiO x /Graphite-NMC811 Cells: Capacity Loss, Impedance Rise and Hidden Degradation Pathways Revealed Using Three-Electrode Diagnostics

Electrodes containing SiO x /graphite (Gr) materials are attractive as anodes for high-energy lithium-ion batteries. However, their mechanical deformation, electrochemical response, and impedance evolution during long-term cycling are strongly coupled, complicating accurate diagnosis of performance fade mechanisms. In this work, the behavior of electrochemically prelithiated SiO x /Gr anodes paired with NMC811 cathodes is systematically investigated using techniques that include in-situ dilatometry, three-electrode electrochemistry, and multiscale post-cycling microscopy. The SiO x /Gr electrode exhibits a maximum expansion of 49% upon lithiation to 10 mV vs Li + /Li, with 84% of the expansion and 91% of the capacity being reversible. In full cells, relatively stable cycling with only 12% capacity fade over 500 cycles is observed. Three-electrode experiments reveal cell-level impedance growth, which is dominated by the NMC811 cathode: the SiO x /Gr anode exhibits minimal net impedance rise and an initial impedance decrease at low potentials. Despite this apparent electrochemical stability, cross-sectional SEM, PFIB tomography, and cryo-STEM reveal irreversible anode thickening caused by the accumulation of an inorganic-rich solid electrolyte interphase (SEI) permeating the anode bulk. Electrode potential-shift analysis further demonstrates that Li + ions released from lithium reservoirs in the prelithiated anode mask true lithium inventory loss during aging. These results demonstrate that low-expansion SiO x /Gr anodes can simultaneously exhibit favorable cycling and impedance metrics while undergoing substantial, hidden degradation, underscoring the importance of electrode-resolved diagnostics for evaluating prelithiated silicon-based anodes.

25 ENERGY STORAGE↗

Direct regeneration of degraded LiFePO4 cathodes via a separator-enabled prelithiation strategy

A persistent challenge in lithium-ion batteries is the loss of active lithium due to the solid electrolyte interphase (SEI) formation and associated side reactions. While prelithiation employing lithium replenishment separator (LRS) has been proven effective in compensating for lithium loss, previous studies have largely been accompanied by gas evolution or solid residue formation during the prelithiation process. To surmount this challenge, we present a LRS based on 4-fluoro-1,2-dihydroxybenzene lithium salt (LiDF), capable of mitigating lithium loss while producing decomposition products that integrate directly into the electrolyte as functional additives which can assist with the stability of the SEI, free from gas or solid formation, thus establishing a sustainable and environmentally benign strategy for lithium compensation. Incorporation of the LRS enables the pristine LiFePO4||graphite (Gr) full cell to achieve 10.8% higher capacity than the cell with a polypropylene separator (PPS) after 200 cycles at 0.5C. Remarkably, the degraded LiFePO4 (D-LFP)||Gr full cell with the LRS exhibits a 135.8% capacity improvement over the PPS-based cell after 500 cycles. These findings establish the LRS as a powerful approach for both boosting high-performance lithium-ion batteries and recovering the capacity of degraded batteries.

Tao, Fujun↗

Development of Next Generation Hierarchical Hybrid Cu-Si anode Batteries via Direct-Ink Writing Application: End of (6th) Month Report - November 2025

Sustainable renewable energy continues to be in dire need to effectively combat global warming. Emerging technology for electric vehicles/ devices remains in high demand that is not only lower in cost, more efficient, but safer in comparison to commercial materials on the market. Although first-generation lithium-ion batteries have exhibited extensive commercial application, conventional graphite no longer meets this increasing demand as an efficient anode material. Due to the fact that graphite has a subpar theoretical specific capacity (372 mAh g -1 ), thus significant limitations in rate capability (for potential faster charging at higher C-rates currently commercially available.). Alternatively, silicon has gained significant attention as a superior candidate to potentially surpass graphite. Due to silicon’s exceedingly high theoretical capacity (4,200 mAh g -1 ) in comparison to standard graphite, its abundance thus in turn it’s low-cost, in addition to exhibiting a significantly low working potential (< 0.4 V vs Li/Li + ). However, one of the main (and most detrimental) challenges is silicon’s tendency to expand in volume (> 300%) upon discharge as it begins the lithiation process. As a direct result, it causes not only for the particles to both crack and pulverize under mechanical stress as the volume continues to expand and contract during cycling. Upon assembling the cell, it needs to undergo ‘charging’ for initially discharging/ ‘activating’ the cell, otherwise commonly known as the ‘formation’ step. As a result a solid electrolyte interface (SEI) layer begins to form at the anode surface because some of the electrolyte begins to react during the formation process. However, this (SEI) layer is deemed as a ‘protective’ interlayer because in theory it prevents further reaction as the cell continues to cycle. However, due to the volume change it causes significant degradation at the interface. As cracking starts to occur at the anode surface, it results in a ‘new’ altered surface with each cycle that causes further reaction with the electrolyte as a byproduct quickly consuming active Li/ and more electrolyte. Thus, fracturing this ‘protective layer,’ causing significantly higher impedance as a result, and in turn a decline in capacity due to active Li-loss. In addition to the active material exfoliating off from the current collector, further contributing to the steady decline in capacity and overall performance. Current state of the art Si-anode batteries on the market range between a maximum content of 5-10 Si wt%. It has been previously reported Tesla has utilized SiO x -C anodes containing 5 wt% Si within their ‘Model 3/ Model X’ electric vehicles. However, more recent ‘Model 3’ vehicles have started to incorporate 10 Si wt%, in which they were able to increase their energy density upwards by approximately 30%. Recent effort has been focused on continuing to increase the wt% of Si being utilized, eventually to 100 wt% of Si, to maximize the energy density even further.

36 MATERIALS SCIENCE↗

Cobalt-free and high-rate stable 5V lithium nickel manganese oxide spinel cathodes enabled via surface oxygen vacancies

Spinel LiNi 0.5 Mn 1.5 O 4 offers both the high-rate, low-cost and safety advantages of LiFePO 4 and the high energy density of LiNiₓMnᵧCo₁₋ₓ₋ᵧO₂ and LiNiₓCoᵧAlzO₂ cathodes. However, the large operating voltage of these materials induces electrolyte oxidation, which degrades the interface and drives Mn dissolution. These reactions are further exacerbated at high rates due to temperature rise. In this study, we discover that ammoniacal treatment followed by annealing introduces a high density of oxygen vacancies in the “near-surface region” of LiNi 0.5 Mn 1.5 O 4 particles. These vacancies release electrons changing the oxidation state of Mn and suppressing its tendency to oxidize the electrolyte. Further, these vacancies enhance the electrode’s electronic conductivity (by ∼3-fold) and Li + diffusivity (by ∼2-fold) greatly improving charge transport, especially when operated at high rates. This results in an across-the-board improvement in self-discharge, specific capacity, energy density, rate capability, coulombic efficiency and cycling stability. When cycled at ∼200 mA g −1 , the capacity fade averaged over 3000 cycles for the surface vacancy-enriched material is ∼0.0167% per cycle compared to an order of magnitude higher fade rate for the baseline material. In conclusion, these findings reveal the potential of targeted surface oxygen vacancy doping to develop cobalt-free and high energy density cathodes that tolerate fast charging and deliver improved cycle life.

Cobalt-free cathodes↗

Manganese‐Based Spinel Cathodes: A Promising Frontier for Solid‐State Lithium‐Ion Batteries

Recently, all-solid-state lithium-ion batteries (ASSLIBs), which exhibit improved safety and enhanced energy density compared to conventional commercialized lithium-ion batteries (LIBs), thereby have garnered extensive research interest. Among the promising cathode candidates, Mn-based spinel cathodes LiMn 2 O 4 (LMO) and LiNi 0.5 Mn 1.5 O 4 (LNMO), with the unique characteristics of low cost, structural stability, and 3D Li-ion diffusion channels, have demonstrated excellent performance in LIBs and presented great potential in ASSLIBs applications. However, several challenges, including structural degradations, poor interfacial contact, large interfacial resistance, and Mn-dissolution/diffusion during the electrochemical cycling, hinder their practical applications and commercialization in the ASSLIBs. Particularly, the high-voltage LNMO cathodes suffer from the challenge of electrochemical incompatibility with most of the solid-state electrolytes (SSEs). Herein, the spinel structure, the electrochemical behavior, and the structural degradation of the LMO/LNMO are explored. The characteristics and recent progress of the mitigating strategies to the challenges of various SSEs, including polymer-, oxide-, composite-, sulfide-, halide-, and LiPON-based SSEs, are introduced when paired with LMO/LNMO. Finally, the directions for future research to advance Mn-based spinel cathodes and fulfill the requirements of the next-generation ASSLIBs are also discussed.

Dou, Yu [Concordia University, Montreal, QC (Canad↗

Electrolyte Design for Fast‐Charging Lithium‐Based Batteries

Fast charging is essential for the widespread adoption of lithium (Li)-ion batteries, but it is fundamentally limited by sluggish interfacial kinetics, Li plating, and electrolyte instability at high current densities. Over the past decade, electrolyte engineering has emerged as a key strategy to address these challenges. This review summarizes the development of fast-charging electrolytes over the past ten years and outlines a design framework. Electrolyte formulations are first deconstructed into their main components—solvents, salts, and functional additives—and representative strategies for tuning solvation structure and interphase chemistry are discussed to suppress Li plating and improve interfacial kinetics. The discussion then extends to advanced electrolyte systems, particularly localized high-concentration electrolytes (LHCEs), and their compatibility with different anode chemistries. Advanced characterization techniques are also summarized and categorized based on destructiveness, spatial and temporal resolution, quantitative analysis, and the chemical species or processes probed across multiple length scales. Recent progress in AI-enabled electrolyte discovery and battery management system (BMS) strategies for optimized fast-charging protocols is further highlighted. Finally, perspectives are presented on translating electrolyte innovations from academic research to practical applications, with emphasis on cell format, realistic operating conditions, and manufacturability.

25 ENERGY STORAGE↗

Novel Zwitterionic Polyurethane-in-Salt Electrolytes with High Ion Conductivity, Elasticity, and Adhesion for High-Performance Solid-State Lithium Metal Batteries

This study presents a novel polymer-in-salt (PIS) zwitterionic polyurethane-based solid polymer electrolyte (zPU-SPE) that offers high ionic conductivity, strong interaction with electrodes, and excellent mechanical and electrochemical stabilities, making it promising for high-performance all solid-state lithium batteries (ASSLBs). The zPU-SPE exhibits remarkable lithium-ion (Li+) conductivity (3.7 × 10⁻⁴ S cm−1 at 25 °C), enabled by exceptionally high salt loading of up to 90 wt.% (12.6 molar ratio of Li salt to polymer unit) without phase separation. It addresses the limitations of conventional SPEs by combining high ionic conductivity with a Li+ transference number of 0.44, achieved through the incorporation of zwitterionic groups that enhance ion dissociation and transport. The high surface energy (338.4 J m−2) and elasticity ensure excellent adhesion to Li anodes, reducing interfacial resistance and ensuring uniform Li+ flux. When tested in Li||zPU||LiFePO₄ and Li||zPU||S/C cells, the zPU-SPE demonstrated remarkable cycling stability, retaining 76% capacity after 2000 cycles with the LiFePO4 cathode, and achieving 84% capacity retention after 300 cycles with the S/C cathode. Molecular simulations and a range of experimental characterizations confirm the superior structural organization of the zPU matrix, contributing to its outstanding electrochemical performance. The findings strongly suggest that zPU-SPE is a promising candidate for next-generation ASSLBs.

Wang, Kun↗

Laser ablation of high-loading Li-ion battery electrodes improves accessible capacity and cycle life for Behind-the-Meter Storage

Adoption of Behind-the-Meter Storage (BTMS) requires design of batteries that enable high safety, long cycle life, and low cost at the system level. Pairing Li 4 Ti 5 O 12 (LTO) with LiMn 2 O 4 (LMO) achieves targets related to safety and cycle life, but these materials' low energy densities contribute to higher cost at the system scale. Increasing electrode loading is a simple approach to improve energy density, but comes with a trade-off in electrode utilization due to long, tortuous Li + diffusion pathways. Here, laser ablation is used to microstructure (pattern) high-loading electrodes to enhance electrode performance through improved Li + diffusion pathways. Four cell types, comprising combinations of standard or patterned anode and cathode, were prepared to evaluate the effects of laser ablation at each electrode. A rate test shows that patterning electrodes enhances active material utilization at ≳1C rates. Patterning the cathode yields the most benefit, as cells with a patterned cathode demonstrate a ~20% higher accessible capacity than those without at 1.4C. Additionally, 1C capacity retention of cells with patterned cathode (91% through 3000 cycles) is significantly improved over cells with only the anode patterned (64%) and non-patterned electrodes (50%). Characterization of post-mortem cells before and after refreshing their electrolyte suggests that 1C capacity retention is improved by mitigation of electrode "dry-out". We hypothesize that the microstructure acts as a reservoir of additional electrolyte, or a path for gas to escape, so that active material remains wetted throughout long-term cycling, and/or the microstructure may reduce localized, gas-forming overpotentials in the high-loading electrode.

25 ENERGY STORAGE↗

Turn-On Conductivity with Proton-Coupled Electron Transport in Metal–Organic Frameworks

Proton-coupled electron transfer (PCET) has been studied for decades in the context of molecular reactivity, but its impact on long-range electron transport is barely understood. When defined broadly as ion-coupled charge transport (ICCT), relevant systems include lithium-ion battery electrodes, electrochromic coatings, and myriad electrocatalysts. Despite ample evidence that ion-electron coupling enhances or diminishes the performance of these devices, little is known about the experimental signatures of ICCT and the microscopic factors that govern its mechanism. Here, we expect that ion-electron coupling becomes especially relevant in high surface area materials, such as the layered electrodes of intercalation batteries, due to the close proximity of itinerant electrons and electrolyte. Here, we report an electrochemical investigation into a family of metal-organic frameworks (MOFs) that serves as a well-defined platform for understanding the effect of ICCT on both elec- tronic and ionic conductivity. Through photochemical doping of e - –H + pairs and introduction of solvent guest molecules, the Ti-containing MOFs convert from electronic-only insulators conductors (σ e ≈ 10 -12 S cm -1 ) to mixed ion-electron semiconduc- tors (σ e ≈ 10 -7 S cm -1 , σ ion ≈ 10 -5 S cm -1 ). Direct current and alternating current techniques support the existence of proton- electron coupling and, critically, that improved ionic conductivity enhances electronic conductivity. Taken together, these results provide direct evidence that PCET enables long-range charge transport and generalized electrochemical tools and synthetic methods for studying ion-electron coupling in materials broadly.

Charge transport↗

Molecularly engineered Li compensation agent-integrated separator enabling regeneration of degraded LiFePO 4

Lithium replenishment separators (LRSs) integrating pre-lithiation agents can regenerate degraded lithium cathodes via facile reassembly with a fresh anode and the LRS. A persistent challenge is the formation of gas or solid residues during pre-lithiation. To address this, for the first time, we develop an LRS based on a molecularly engineered dilithium salt of tetrafluorohydroquinone, which compensates for lithium loss while generating decomposition products that dissolve in the electrolyte as a favorable additive, without forming gas or solid residues, thus offering a green route for lithium compensation. A pristine LiFePO 4 ‖graphite full cell with the LRS exhibits 9.3% higher overall capacity than a polypropylene separator (PPS) cell after 50 cycles at 0.5C, and the degraded LiFePO 4 ‖graphite full cell incorporating this LRS achieves a 44.9% higher capacity than the PPS-based cell after 200 cycles at 0.5C. Our LRS demonstrates strong potential for high-performance lithium-ion batteries and spent battery regeneration.

Tao, Fujun [Worcester Polytechnic Institute, MA (U↗