Shear rupture of a directionally solidified eutectic gamma/gamma prime - alpha (Mo) alloy

Directionally solidified Mo alloys are evaluated to determine the shear rupture strength and to possibly improve it by microstructural and heat treatment variations. Bars of the alloy containing nominally 5.7% Al and 33.5% Mo by weight with balance Ni were directionally solidified at rates between 10 and 100 mm per hour in furnaces with thermal gradients at the liquid-solid interface of 250 or 100 C per cm. A limited number of longitudinal shear rupture tests were conducted at 760 C and 207 MPa in the as - solidified and in several heat treated conditions. It is shown that shear rupture failures are partly transgranular and that resistance to failure is prompted by good fiber alignment and a matrix structure consisting mainly of gamma prime. Well aligned as - solidified specimens sustained the shear stress for an average of 81 hours. A simulated coating heat treatment appeared to increase the transformation of gamma to gamma prime and raised the average shear life of aligned specimens to 111 hours. However, heat treatments at 1245 C and especially at 1190 C appeared to be detrimental by causing partial solutioning of the gamma prime, and reducing lives to 47 and 10 hours, respectively.

Harf, F. H.↗

Evaluation of directionally solidified eutectic superalloys for turbine blade applications

Alloys from the following systems were selected for property evaluation: (1) gamma/gamma-Mo (Ni-base, rods of Mo); (2) gamma-beta (Ni-base, lamellae or rods of (Ni, Fe/Co Al); and (3) gamma-gamma (Ni-base rods of Ni3Al gamma). The three alloys were subjected to longitudinal and transverse tensile and rupture tests from 750 C to 1100 C, longitudinal shear strength was measured at several temperatures, resistance to thermal cycling to 1150 C was determined, cyclic oxidation resistance was evaluated at 750 C and 1100 C, and each system was directionally solidified in an alumina shell mold turbine shape to evaluate mold/metal reactivity. The gamma/gamma Mo system has good rupture resistance, transverse properties and processability, and is a high potential system for turbine blades. The gamma-beta system has good physical properties and oxidation resistance, and is a potential system for turbine vanes. The gamma-gamma system has good high temperature rupture resistance and requires further exploratory research.

Henry, M. E.↗

Structure and creep rupture properties of directionally solidified eutectic gamma/gamma-prime-alpha alloy

A simple ternary gamma/gamma-prime-alpha alloy of nominal composition (wt-%) Ni-32Mo-6Al has been directionally solidified at 17 mm/h and tested in creep rupture at 1073, 1173, and 1273 K. A uniform microstructure consisting of square-shaped Mo fibers in a gamma + gamma-prime matrix was found despite some variation in the molybdenum and aluminum concentrations along the growth direction. Although the steady-state creep rate is well described by the normal stress temperature equation, the stress exponent (12) and the activation energy (580 kJ/mol) are high. The rupture behavior is best characterized by the Larson-Miller parameter where the constant equals 20.

Whittenberger, J. D.↗

Elevated temperature properties of aligned ferrous eutectics

Iron base alloys containing aluminum and chromium together with smaller amounts of yttrium and silicon are of interest for high temperature applications. Strengthening an inherently weak but oxidation resistant solid solution matrix with aligned in situ chromium carbides represents an attractive approach to achieving both surface stability and creep resistance at elevated temperatures. Aligned microstructures were produced in alloys of approximately 30 wt % (Cr + Mn), about 3 wt % C and the balance Fe consisting of a gamma matrix and the hexagonal carbide (Cr, Mn, Fe)7C3. The tensile and stress rupture strength to 2000 F of aligned Fe-20 w/t % Cr-10 wt % Mn-3.2 wt % C measured parallel to the carbide reinforcement exceeded those of the strongest iron-nickel superalloys, e.g., CRM-6D developed by Chrysler for automotive turbine application. The cyclic oxidation and sulfidation response of these alloys at elevated temperatures can be markedly improved by aluminum additions.

Lemkey, F. D.↗

Effect of convection on the microstructure of the MnBi/Bi eutectic

For the quasi-regular fibrous microstructure of MnBi formed at freezing rates of 9 mm/h and above, good agreement between experimental and theoretical results for fiber spacing, freezing rate, radial position, and ampoule rotation rate is found. For the irregular blade-like microstructure formed at lower freezing rates, convection is found to coarsen the microstructure somwhat more than predicted. The volume fraction of MnBi was also shown to depend on ampoule rotation and radial position, even in the absence of ampoule rotation. The two-fold finer microstructure observed in space-processed material could not be explained by the elimination of buoyancy-driven natural convection.

Eisa, Gaber Faheem↗

Influence of convection of spiral structures in lead-tin eutectic

Convection was generated during directional solidification by the accelerated crucible rotation technique (spin up/spin down). This stirring increased the rotation rate of the microstructure and reduced the length solidifying cooperatively, but had no influence on the lamellar spacing.

Popov, Dimitar↗

The influence of processing parameters on microstructural development of low-weight-percent primary, pro-eutectic, dendritic alloys during directional solidification

Alloy compositions centering about Sn- 5 to 15 wt pct Al and Pb- 4 to 20 wt pct Cu have been directionally solidified as a function of growth rate and orientation with respect to earth's gravity vector. The effect of these processing variables on macrosegregation is presented, and the consequence of a structural transition from primary columnar to equiaxed dendritic growth is examined. Effects detrimental to microstructure and attributed to density variations are shown to be minimized by a novel processing technique. In view of the ground-based results, some considerations follow regarding what might be gained by solidifying these alloys in a microgravity environment.

Grugel, R. N.↗

Experimental partitioning studies near the Fe-FeS eutectic, with an emphasis on elements important to iron meteorite chronologies (Pb, Ag, Pd, and Tl)

Partitioning coefficients for metal/sulfide liquid, troilite/sulfide liquid, and schreibersite/sulfide liquid were determined for Ag, Au, Mo, Ni, Pd, and Tl (using EMPA and proton-induced X-ray microprobe and ion microprobe analyses) in order to understand the chronometer systems of iron meteorites. In general, the obtained schreibersite/metal and troilite/metal partition coefficients for 'compatible' elements were quite similar to those inferred from natural assemblages, reinforcing an earlier made conclusion that there is a class of elements for which experimental troilite/metal and schreibersite/metal partition coefficients approximate those inferred from natural samples. The consistency between experimental and natural assemblages, however, was not observed for Ag, Pb, and Tl, indicating that the abundances of these elements determined in 'metal' and 'troilite' separates from iron meteorites are influenced by trace minerals that concentrate incompatible elements.

Jones, J. H.↗

Thermal Cycling Fatigue in DIPs Mounted with Eutectic Tin-Lead Solder Joints in Stub and Gullwing Geometries

It has long been known that solder joints under mechanical stress are subject to failure. In early electronic systems, such failures were avoided primarily by avoiding the use of solder as a mechanical structural component. The rule was first to make sound wire connections that did not depend mechanically on solder, and only then to solder them. Careful design and miniaturization in modern electronic systems limits the mechanical stresses exerted on solder joints to values less than their yield points, and these joints have become integral parts of the mechanical structures. Unfortunately, while these joints are strong enough when new, they have proven vulnerable to fatigue failures as they age. Details of the fatigue process are poorly understood, making predictions of expected lifetimes difficult.

fatigue failure solder joints failure mechanisms s↗

Visual and x-ray inspection characteristics of eutectic and lead free assemblies

For high reliability applications, visual inspection has been the key technique for most conventional electronic package assemblies. Now, the use of x-ray technique has become an additional inspection requirement for quality control and detection of unique defects due to manufacturing of advanced electronic array packages such as ball grid array (BGAs) and chip scale packages (CSPs).

x-ray↗

Development of Large Bandgap Materials Using Reactive Growth in Al-SI Eutectic for Optical and RF Applications

Carbon was utilized as reactive element to modify the microstructure using forced mixing during crystallization of the Al-Si alloy by rotation and stirring. We nucleated the material on SiC substrates while the Al-Si melt was rotated with a speed of 30rpm in a graphite crucible. Several experiments were performed and parameters such as time of mixing, soaking temperature, rotation rate of the substrate and rate of cooling during the solidification was changed. We observed dendrite and cell morphologies during the solidification of rotating melt. The microstructure was characterized by optical microscopy and SEM-EDX and compositional spectroscopy. The effect of carbon impurities was studied on the solidifying microstructure. When we used the longer soak time of the melt in presence of carbon impurities we observed the destruction of dendritic morphology and the formation of cellular and colony structures. Similar approach has been used for Ga2O3, a novel large bandgap material also.

Singh, N. B.↗

All-Climate and Ultrafast Rechargeable Aluminum Batteries Enabled By Ternary Eutectic Electrolytes

For Rechargeable Aluminum Batteries (RABs), electrolytes emerge as the most crucial and decisive component due to the following aspects: (i) Sluggish reaction kinetics due to high gravimetric density of Al (2.70 g/cm 3 vs. 0.53 g/cm 3 for Li) and high surface charge density, (ii) a limited safe potential window owing to moderate standard redox potential values. The state-of-the-art electrolytes in the field exhibits a limited stability window (<2.6V vs. Al/Al +3 ), leading to undesired side reactions, such as Cl 2 gas generation, and self-discharge in RABs. Exploration of RABs low-temperature performance is restricted by electrolyte limitations.

Raju Vadthya↗