Search NASA⌕ Search

SEARCH · Search NASA

Results for “STEELS - CLEANING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 613 records · Page 34

On the thermal coarsening and transformation of nanoscale oxide inclusions in 316L stainless steel manufactured by laser powder bed fusion and its influence on impact toughness

The thermal evolution of nanoscale oxide inclusions in 316L stainless steel (SS) manufactured by laser powder bed fusion additive manufacturing (AM) was explored. The size, chemical composition, morphology, and distribution of the oxides were characterized as the function of heat treatment conditions. The study revealed the mechanistic driving force of the rapid oxide coarsening during recrystallization. Ostwald ripening governs oxide coarsening. The active grain boundary-oxide interaction at the early stage of recrystallization accelerated oxide coarsening via enhanced solute diffusion along grain boundaries. Pipe diffusion along dislocation cellular boundaries has a negligible contribution to oxide coarsening. At high temperatures (T> 1065 °C), although lattice diffusion primarily controlled the oxide growth, the contribution from the grain-boundary diffusion was necessary. The transformation from MnSiO 3 to CrMn 2 O 4 took place in the un-recrystallized grains but was not observed when recrystallization started. The interaction of grain boundary and oxides during recrystallization resulted in a high fraction of oxides accumulated at grain boundaries. While oxide coarsening does not significantly alter the toughness value, grain-boundary oxides promote microvoid formation and intergranular fracture under Charpy impact in the recrystallized AM 316L SS.

36 MATERIALS SCIENCE↗

Indentation investigation of 304L stainless steel friction stir weld simulated crack repair

Simulated cracks were repaired in 304L stainless steel using low temperature friction stir welding. Indentation studies were carried out to understand the effect of microstructural features on the mechanical property variation across the weld and to measure the size of the weld zones with a quantitative technique. Microhardness and nanoindentation hardness profiles were constructed on a transverse section across the weld. The data obtained were correlated by extrapolating the nanoindentation hardness to greater depths which showed that the nanoindentation hardness closely reflects the microhardness values throughout the weld. Finally, grain size in the stir zone (SZ) was found to vary with the tool temperature which, in turn, alters the nanoindentation modulus variability and higher tool temperature resulted in widening of the SZ.

36 MATERIALS SCIENCE↗

In-situ neutron diffraction investigation of two-stage martensitic transformation in a 13%Mn steel with serrated deformation

Two stage austenite →ε-martensite →α-martensite phase transformation, phase-specific lattice strain evolution and load sharing during tensile deformation of a 13%Mn hot-rolled austenitic steel are revealed by in-situ neutron diffraction. In conclusion, direct evidence is provided that serrated deformation behavior is attributed to discontinuous martensitic transformation.

Austenitic steel↗

Phase-field modeling of diffusion bonding in 316H stainless steel: Impact of processing conditions on grain morphology and bonding quality

A novel multi-phase, multi-component phase‐field model is presented to study the diffusion bonding of 316H stainless steel. Combined with targeted experimental investigations, this model simulates the bond-growth process and predicts the bonding quality. Unlike previous models, our approach captures the simultaneous evolution of voids and grain structures, while quantifying bonding quality using defined bonding ratio. A comprehensive analysis of bond process control is performed by changing temperature, pressure and surface roughness observing the resulting bond structure, which is consistent with experimental observations and analytical predictions. Temperature is determined to be the dominant factor, with the transition from a flat to a robust bond occurring between 1000 °C and 1050 °C. At the ideal bonding temperature of 1050 °C, a surface roughness exceeding 0.6 μm or an applied stress below 4 MPa results in poor bonding quality. Beyond this, higher pressures and smoother surfaces reduce void size, accelerate void shrinkage, and lead to improved bond integrity. This diffuse-interface model can be extended to other material systems if supplied with appropriate thermodynamic and kinetic data. In conclusion, this makes it an effective modeling platform for optimizing high-temperature diffusion bonding and developing reliable bonded components such as compact heat exchangers.

Diffusion bonding↗

Influence of microstructure and temperature on impact toughness of H13 steel produced by binder jet additive manufacturing

Binder Jet Additive Manufacturing (BJAM) is a promising manufacturing pathway to produce H13 steel dies and tooling with complex geometries for applications in high pressure aluminum die casting, hot stamping, and injection molding. While fully dense H13 coupons produced using BJAM have been subjected to detailed microstructure characterization, properties which are critical and relevant to the aforementioned applications, such as impact toughness, have not been reported. Here, this work evaluated the influence of microstructural characteristics and test temperature on the impact toughness of H13 produced by BJAM. Coupons were produced from three different powder size distributions (PSDs), with nominal powder size ranges of −22 μm, 10-32 μm, and 15-53 μm. Coupons were printed, sintered, hot isostatically pressed (HIPed), and heat treated by quenching and tempering. After HIPing, the measured porosities of the different PSDs were all less than 0.015 vol%. The −22 μm PSD BJAM material exhibited the best impact toughness of all three PSDs across the entire test temperature range from 25 to 400 °C, and also exhibited an ambient temperature impact toughness of 10.9 J at a hardness of 46 HRC, equivalent to minimum threshold requirements for premium grade H13. However, all three BJAM PSDs exhibited moderately lower impact toughness than premium grade wrought H13 from RT to 400 °C. We attribute this in part due to the very large prior-austenite grain (PAG) sizes near 400 μm and segregation from former liquid channels leading to greater amounts of carbide precipitation on PAG boundaries. Technical pathways for optimizing processing and chemistry of BJAM H13 to further improve impact toughness are discussed.

Binder jet additive manufacturing↗

Process and feedstock driven microstructure for laser powder bed fusion of 316L stainless steel

Here in the pursuit of improving additively manufactured (AM) component quality and reliability, fine-tuning critical process parameters such as laser power and scan speed is a great first step toward limiting defect formation and optimizing the microstructure. However, the synergistic effects between these process parameters, layer thickness, and feedstock attributes (e.g. powder size distribution) on part characteristics such as microstructure, density, hardness, and surface roughness are not as well-studied. In this work, we investigate 316L stainless steel density cubes built via laser powder bed fusion (L-PBF), emphasizing the significant microstructural changes that occur due to altering the volumetric energy density (VED) via laser power, scan speed, and layer thickness changes, coupled with different starting powder size distributions. This study demonstrates that there is not one ideal process set and powder size distribution for each machine. Instead, there are several combinations or feedstock/process parameter ‘recipes’ to achieve similar goals. This study also establishes that for equivalent VEDs, changing powder size can significantly alter part density, GND density, and hardness. Through proper parameter and feedstock control, part attributes such as density, grain size, texture, dislocation density, hardness, and surface roughness can be customized, thereby creating multiple high-performance regions in the AM process space.

316L stainless steel↗

Sigma phase evolution and nucleation mechanisms revealed by atom probe tomography in a 347H stainless steel

The size evolution and phase composition of sigma phases were investigated for a 347H stainless steel subject to isothermal aging at 750 °C for up to 10,000 h. Scanning electron microscopy reveals that sigma phases are present before 336 h aging and they continue to grow for all aging times studied. Atom probe tomography shows little variation in the sigma phase composition with aging time up to 10,000 h, and only the C content decreases with aging time. The comparison of C concentration suggests that the sigma phase does not nucleate within the C-depleted matrix or precipitate free grain boundaries, leaving dissolving metastable M 23 C 6 as the only possible nucleation site. Based on the experimental results and thermodynamic simulations, the desirable Nb concentration is discussed to reduce the kinetics of sigma phase growth, and possible design directions are suggested to improve 347H.

36 MATERIALS SCIENCE↗

Influence of energy density on the microstructure, growth orientation, and anisotropy of magnetic properties in additively manufactured Fe-3.8wt%Si transformer steels

Fe-3.8wt%Si transformer steels were processed using two different additive manufacturing (AM) techniques, laser powder bed fusion (LPBF) and directed energy deposition (DED). While the LPBF processed samples exhibited a strong <001> orientation of the BCC grains along the build axis, the DED processed samples exhibited a randomized texture along the build axis. DED processed samples showed substantially coarser columnar grains as compared to their LPBF counterparts. Here, the columnar grains exhibited a substantial number of low-angle sub-grain boundaries. All samples exhibited very good soft magnetic properties, with saturation magnetization (M s ) values ranging from 205 - 232 emu/gm, and coercivity (H c ) values ranging from 1.2 – 4.2 Oe. The Coercivity (H c ) values were significantly lower when the magnetic field was applied parallel to the build axis, as compared to being perpendicular, which can be rationalized based on the columnar nature of the grains, resulting in a higher number density of grain boundaries in case of the field applied perpendicular to the build axis.

36 MATERIALS SCIENCE↗

Post-build stress-relief optimization for laser powder bed fusion 316H stainless steel

Nuclear energy remains a critical component of a diversified and efficient energy portfolio, offering reliable, high-capacity, and low-carbon power. However, in the U.S., aging infrastructure and the slow qualification and deployment of advanced materials and manufacturing techniques hinder progress in next-generation reactor technologies. This study explores the application of laser powder bed fusion (LPBF) additive manufacturing for stainless steel 316H, with a focus on optimizing post-build heat treatments to enhance material properties for high-temperature nuclear applications. The research targets the optimization of stress-relief temperatures to alleviate postbuild residual stresses, ensuring improvements in the microstructural corelated properties. A series of microstructural and mechanical evaluations were performed on LPBF-printed SS-316H samples which were subjected to annealing at temperatures varying between 650 °C and 850 °C. X-ray diffraction, scanning electron microscopy, and transmission electron microscopy analyses revealed that increasing the heattreatment temperature accelerated dislocation recovery. Vickers microhardness measurements showed an initial reduction in values, followed by stabilization over extended durations at all the temperatures. While higher temperatures facilitated faster recovery, they also promoted carbide precipitation along grain and solidification cell boundaries, narrowing the safe processing window. In contrast, heat treatment at 650°C preserved the cellular substructure and enabled controlled carbide precipitation over time. In conclusion, these findings highlight the importance of time–temperature optimization and suggest that 650°C for up to 2 h provides the most favorable balance between recovery and carbide control for a stress-relief treatment.

316 stainless steel↗

Clarification of creep deformation mechanism in heat-affected zone of 9Cr steels with In Situ experiments

This work quantified nonuniform creep deformation across the heterogeneous heat-affected zone (HAZ) of Grade 91 steel with sophisticated experiments, including an electric-thermal finite element model–assisted Gleeble thermomechanical simulation and a high-temperature creep testing with in situ digital image correlation (DIC). High temperature creep properties of HAZ sub-zones were quantitatively measured by the DIC. Furthermore, by utilizing peak temperature, hardness, local creep strain, and underlying microstructures, creep deformation mechanisms in HAZ were further understood. DIC measurements reveal a creep-vulnerable zone (CVZ) exposed to a peak temperature of 932°C (close to A C3 ) in the intercritical HAZ experienced the fastest creep strength degradation instead of the soft zone with the lowest hardness prior to creep. The significantly reduced precipitation strengthening from misplacement of undissolved and coarsened M 23 C 6 carbides led to a faster recrystallization of tempered martensite in the CVZ. Weak untransformed tempered martensite (ferrite grains) stabilized by local Cr enrichment from dissolved M 23 C 6 also harmed the CVZ's creep resistance.

36 MATERIALS SCIENCE↗

Complexity of segregation behavior at localized deformation sites formed while in service in a 316 stainless steel baffle-former bolt

Here, post-irradiation evaluation was performed on a 316 stainless steel baffle former bolt harvested after 40 years of service in a pressurized water reactor. Microstructure analysis revealed the presence of defect-free dislocation channels and strain-induced twins, indicative of loading at a stress level close to yield stress at least once while in service. Primary radiation-induced Ni/Si precipitates were destroyed during channel and twin formation, and secondary, significantly coarser Ni/Si precipitates formed along newly formed Σ3 boundaries during the continued irradiation. Additionally, an elevated phosphorus level was observed inside the strain-induced twin. Complex chemistry inside the strain-induced feature may overlap with dislocation pileups and impact localized corrosion, material long-term performance, and safety.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

In-situ synchrotron X-ray investigation of phase evolution in gas atomized powder enabling manufacturing of nanoscale oxide-dispersion strengthened ferritic steels

Here, we present an investigation of Fe-14Cr-3W-0.4Y-0.4Zr-0.18Ti (wt.%) as a reduced-activation oxide-dispersion strengthened (ODS) ferritic steel, an alternative to the “14YWT” structural alloys designed for nuclear energy applications. Gas atomization reaction synthesis (GARS) was used to produce these Zr-modified powders with a non-equilibrium (metastable) phase that enable a heat treatment (delayed) route for producing nanoscale oxide-dispersion strengthening. In situ synchrotron X-ray diffraction and transmission electron microscopy were used to analyze phase evolution as a function of temperature and time, revealing formation of highly dispersed oxide nanoprecipitate phases at temperatures above those needed for powder consolidation and shaping of components. This would allow fabrication of net-shape parts using conventional powder-processing methods prior to thermal activation of a reaction producing nanocrystalline Y-(Ti, Zr)-O particles, with a size of 20 ± 7 nm. These results can inform processing of tubes, cladding, sheets, and plates for use in advanced fission and fusion reactors.

In-situ synchrotron X-ray diffraction↗

Acoustic focusing of microplastics in microfabricated and steel tube devices: An experimental study on the effects from particle size and medium density

The contamination of aquatic systems with microplastics is becoming a severe threat to living organisms. Microplastics found in the environment consist of a wide range of particle sizes thus give rise to several challenges to current purification methods. Acoustic focusing has been utilized as a particle concentrating method in biological and non-biological applications. In this study, we investigate the feasibility of using acoustic focusing technology to isolate microplastics in aqueous samples and find that a two-stage mechanism is essential to concentrate microplastics of wide size ranges of the same material. We demonstrate for the first time experimentally that when the particle size is comparable to the resonance wavelength, they deviate from typical pressure nodal focusing and show pressure antinodal focusing. Further, we have expanded microplastics isolation beyond microfluidic systems and demonstrate their extraction capabilities relatively at higher flow rates using microplastics of polystyrene, polyethylene, and polymethyl methacrylate ranging from 6 µm to 300 µm diameter and in devices fabricated with cylindrical steel tubes. We could extract 70% of microplastics smaller than 180 µm and 82% of microplastics greater than 180 µm in diameter from an aqueous sample at a flow rate of 12 mL/min. In conclusion, we demonstrate that small microplastics focus on acoustic pressure nodes regardless of the medium density. However, focusing of large microplastics of the same material depends on the medium density.

42 ENGINEERING↗

Fracture toughness evaluation for thin-shell stainless steel weldment

Integrity of spent nuclear fuel (SNF) interim storage canisters are very important to the safety of the back-end nuclear fuel cycle. Stress corrosion cracking (SCC) potential of interim storage canister has been considered as a high priority. Because no post-weld heat treatment was required for forming these canisters, the high tensile residual stress existed within these canister welds. This can change the fracture resistance capacity significantly as well as increase SCC potential. Due to relative thin shell thickness of a canister weldment, the spiral notch torsion test (SNTT) method of small specimen approach was used to estimate the canister weldment fracture toughness. Most SNTT weldment samples fracture initiation sites are at heat-affected zone (HAZ) regions. The estimated fracture toughness $J_Q'$ for the baseline SS304 steel is at 283 kJ/m 2 . The estimated $J_Q'$ for the SS304/308 weld from HAZ and weld specimens are 126 kJ/m 2 and 148.9 kJ/m 2 , respectively.

36 MATERIALS SCIENCE↗

Development and testing of coarse-grained models for ultrasonic simulations of cast austenitic stainless steel

Ultrasonic inspection of cast austenitic stainless steel (CASS) in the nuclear industry is particularly challenging because of sound field scatter and attenuation caused by the coarse-grained microstructure. Modeling and simulation are important tools in ultrasonic testing, as they can be used to help address key aspects of inspections, such as developing new probe designs, predicting inspection reliability, and testing phased-array focal laws. However, developing a useful and reliable CASS model is challenging due to the many grain interfaces and crystalline orientations that must be captured. We demonstrate a method of creating a realistic CASS model that is usable in CIVA, a commercially available modeling and simulation software platform. Using polished and chemically etched sections, we generate models of a coarse-grained equiaxed specimen and a columnar specimen. We also test an alternative method of generating a coarse-grained model using Voronoi regions. We qualitatively compare sound field scatter and quantitatively compare sound field attenuation and beam partitioning in simulated sound fields to those of laboratory-measured sound fields. Results show that the Voronoi models perform as well as or better than the models based on actual grain morphology. Here we also show that model-to-model randomness in Voronoi grain structure can impact the magnitude of a simulated echo response by a factor of two or more. Although CASS models are potentially a good depiction of reality for a given scenario, they should not be considered representative since CASS morphology can change significantly from specimen to specimen or within the same specimen.

36 MATERIALS SCIENCE↗

Carbon nanotube (CNT) reinforced 316L stainless steel composites made by laser powder bed fusion: Microstructure and wear response

Carbon nanotube (CNT) reinforced 316L stainless steel (SS) composites were fabricated by laser powder bed fusion (LPBF) additive manufacturing (AM). This study focuses on microstructure evolution, hardness, and wear behavior. The wear behavior for AM 316L SS and 1 wt% CNT/316L SS was studied by a dry sliding test under normal loads of 10, 15, and 25 N. The addition of CNT to 316L SS led to the change of solidification mode from cellular/columnar to dendritic growth, producing grain refinement. Nanoscale dendrites were observed. Although TEM characterization confirmed the existence of CNT in cell interior, most CNT were damaged, resulting in carbon material segregation along cellular/dendritic boundaries. The wear rate was found dramatically decreased due to the improved hardness. Compared to the adhesive and abrasive wear in AM 316L SS, the wear mechanism of CNT/316L composite was adhesion and oxidative wear. Furthermore, enhanced cellular/dendritic boundary strengthening by carbon segregation was the main strengthening mechanism of CNT/316L composite.

36 MATERIALS SCIENCE↗

Macroscale Superlubricity Induced by MXene/MoS 2 Nanocomposites on Rough Steel Surfaces under High Contact Stresses

Toward the goal of achieving superlubricity, or near-zero friction, in industrially relevant material systems, solution-processed multilayer Ti 3 C 2 T x -MoS 2 blends are spray-coated onto rough 52100-grade steel surfaces as a solid lubricant. The tribological performance was assessed in a ball-on-disk configuration in a unidirectional sliding mode. The test results indicate that Ti 3 C 2 T x -MoS 2 nanocomposites led to superlubricious states, which has hitherto been unreported for both individual pristine materials, MoS 2 and Ti 3 C 2 T x , under macroscale sliding conditions, indicating a synergistic mechanism enabling the superlative performance. Furthermore, the processing, structure, and property correlation were studied to understand the underlying phenomena. Raman spectroscopy, scanning electron microscopy, and transmission electron microscopy revealed the formation of an in situ robust tribolayer that was responsible for the performance at high contact pressures (>1.1 GPa) and sliding speeds (0.1 m/s). This report presents the lowest friction obtained by either MoS 2 or MXene or any combination of the two so far.

36 MATERIALS SCIENCE↗

Radionuclide tracing based in situ corrosion and mass transport monitoring of 316L stainless steel in a molten salt closed loop

In the study, we report an in situ corrosion and mass transport monitoring method developed using a radionuclide tracing technique for the corrosion study of 316L stainless steel (316L SS) in a NaCl–MgCl 2 eutectic molten salt natural circulation loop. This method involves cyclotron irradiation of a small tube section with 16 MeV protons, later welds at the hot leg of the molten salt flow loop, generating radionuclides 51 Cr, 52 Mn, and 56 Co at the salt–alloy interface. By measuring the activity variations of these radionuclides at different sections along the loop, both the in situ monitoring of the corrosion attack depth of 316L SS and corrosion product transport and its precipitation in flowing NaCl–MgCl 2 molten salt are achieved. While 316L SS is the focus of this study, the technique reported herein can be extended to other structural materials being used in a wide range of industrial applications.

36 MATERIALS SCIENCE↗