Structural, optical, and electronic stability of copper sulfide thin films grown by atomic layer deposition
Abstract not provided
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Abstract not provided
Explore the source record for details and available documents.
Explore the source record for details and available documents.
In this work, we studied an atomic layer deposition (ALD) process of ZrO 2 with the precursors of tetrakis(dimethylamido)zirconium(IV) and water. We investigated the growth characteristics and mechanism of the ALD ZrO 2 in the temperature range of 50–275 °C. Furthermore, the evolutions of film thickness and morphology were studied and discussed. It was found that the growth rate of ZrO2 decreased almost linearly with the increasing temperature from ~1.81 Å/cycle at 50 °C to ~0.8 Å/cycle at 225 °C. Interestingly, it was revealed that the growth of ZrO 2 films ceased after a certain number of ALD cycles at a temperature higher than 250 °C. Additionally, we also verified that the crystallinity of ZrO 2 evolved with deposition temperature from amorphous to crystalline phase. In addition, the wettability of ZrO 2 films was studied, showing a hydrophobic nature.
Atomically flat thin films of topological insulator Bi{sub 2}Se{sub 3} have been grown on double-layer graphene formed on 6H-SiC(0001) substrate by molecular beam epitaxy. By a combined study of reflection high energy electron diffraction and scanning tunneling microscopy, we identified the Se-rich condition and temperature criterion for layer-by-layer growth of epitaxial Bi{sub 2}Se{sub 3} films. The as-grown films without doping exhibit a low defect density of 1.0{+-}0.2x10{sup 11}/cm{sup 2}, and become a bulk insulator at a thickness of ten quintuple layers, as revealed by in situ angle resolved photoemission spectroscopy measurement.
A secondary electron emissive coating. The coating is formed by atomic layer deposition of CaF 2 on a substrate by ALD half cycle exposure of an alkaline metal amidinate and ALD half cycle exposure of a fluorinated compound, where the deposition occurs at a reaction temperature greater than a highest sublimation temperature of the first metal precursor and the second metal precursor and less than 50° C. above the highest sublimation temperature.
The authors report the effect of hydrogen plasma treatment on TiO{sub 2} thin films grown by atomic layer deposition as an effective approach for modifying the photoanode materials in order to enhance their photoelectrochemical performance. Hydrogen plasma treated TiO{sub 2} thin films showed an improved absorption in the visible spectrum probably due to surface reduction. XPS analysis confirmed the formation of Ti{sup 3+} states upon plasma treatment. Hydrogen plasma treatment of TiO{sub 2} films enhanced the measured photocurrent densities by a factor of 8 (1 mA/cm{sup 2} at 0.8 V versus normal hydrogen electrode) when compared to untreated TiO{sub 2} (0.12 mA/cm{sup 2}). The enhancement in photocurrent is attributed to the formation of localized electronic states in mid band-gap region, which facilitate efficient separation and transportation of photo excited charge carriers in the UV region of electromagnetic spectrum.
The atomic composition of films of a polyphenol antioxidant, namely, resveratrol (RVL), with a thickness of up to 50 nm thermally deposited on an oxidized silicon surface is studied by the method of X-ray photoelectron spectroscopy (XPS). It is found that the surface area of pores in the RVL film is about 15% of the total surface area. The results of studying the stability of the RVL films when their surface is treated with Ar{sup +} ions of 3 keV under the electric current of 1 μA passing through the sample for 30 s are given. The treatment gives rise to an increase in the area of pores to 30–40%, while the ratio of the concentration of C atoms to the concentration of O atoms in the RVL film both before and after the treatment of the surface with ions does not correspond to the chemical formula of RVL molecules. Using the method of atomic force microscopy (AFM) in contact mode with a scanning area size of about 10 × 10 μm, RVL coatings deposited on the oxidized silicon and polycrystalline Au surfaces are studied. It is found that the RVL films produce grainy and porous coatings on the substrate surfaces. The typical size of grains in the sample surface plane is 150–300 nm, and the characteristic elevation reaches 30 nm.
High-purity Ni films were deposited using hot-wire-assisted atomic layer deposition (HW-ALD) at deposition temperatures of 175, 250, and 350 °C. Negligible amount of nitrogen or carbon contamination was detected, even though the authors used NH{sub 2} radical as the reducing agent and nickelocene as the precursor. NH{sub 2} radicals were generated by the thermal decomposition of NH{sub 3} with the assist of HW and used to reduce the adsorbed metal growth precursors. To understand and improve the deposition process, the kinetics of HW-ALD were analyzed using a Langmuir-type model. Unlike remote-plasma-enhanced atomic layer deposition, HW-ALD does not lead to plasma-induced damage. This is a significant advantage, because the authors can supply sufficient NH{sub 2} radicals to deposit high-purity metallic films by adjusting the distance between the hot wire and the substrate. NH{sub 2} radicals have a short lifetime, and it was important to use a short distance between the radical generation site and substrate. Furthermore, the impurity content of the nickel films was independent of the deposition temperature, which is evidence of the temperature-independent nature of the NH{sub 2} radical flux and the reactivity of the NH{sub 2} radicals.
ZnO thin film transistors (TFTs) are fabricated on Si substrates using atomic layer deposition technique. The growth temperature of ZnO channel layers are selected as 80, 100, 120, 130, and 250 °C. Material characteristics of ZnO films are examined using x-ray photoelectron spectroscopy and x-ray diffraction methods. Stoichiometry analyses showed that the amount of both oxygen vacancies and interstitial zinc decrease with decreasing growth temperature. Electrical characteristics improve with decreasing growth temperature. Best results are obtained with ZnO channels deposited at 80 °C; I{sub on}/I{sub off} ratio is extracted as 7.8 × 10{sup 9} and subthreshold slope is extracted as 0.116 V/dec. Flexible ZnO TFT devices are also fabricated using films grown at 80 °C. I{sub D}–V{sub GS} characterization results showed that devices fabricated on different substrates (Si and polyethylene terephthalate) show similar electrical characteristics. Sub-bandgap photo sensing properties of ZnO based TFTs are investigated; it is shown that visible light absorption of ZnO based TFTs can be actively controlled by external gate bias.
Miniaturization of microelectronic devices necessitates atomic precision in manufacturing techniques, particularly in the deposition of thin films. Atomic layer deposition (ALD) is recognized for its precision in controlling film thickness and composition on intricate three-dimensional structures. This study focuses on the ALD nucleation and growth mechanisms of ruthenium (Ru), a metal that has significant future implications for microelectronics. Despite its advantages, the deposition of a high surface-free energy material like Ru on a low surface-free energy material such as an oxide often faces challenges of large nucleation delays and non-uniform growth. To address these challenges, we explored the effectiveness of organometallic surface pretreatments using trimethylaluminum (TMA) or diethylzinc (DEZ) to enhance Ru film nucleation and growth. Our study employed a less-studied Ru precursor, cyclopentadienylethyl(dicarbonyl)ruthenium [RuCpEt(CO)2], which demonstrated promising results in terms of reduced nucleation delay and increased film continuity. Ru ALD was performed on silicon substrates with native oxide, using RuCpEt(CO)2 and O2 as coreactants. Our findings reveal that surface pretreatment significantly improves nucleation density and film thickness within the initial 60 ALD cycles, achieving up to a 3.2-fold increase in Ru surface coverage compared to nonpretreated substrates. Supported by density functional theory calculations, we propose that the enhanced nucleation observed with RuCpEt(CO)2 compared to previously-studied Ru(Cp)2 is due to two key mechanisms: the facilitated removal of CO ligands during deposition, which enhances the reactivity of the precursor, and a hydrogen-abstraction reaction involving the ethyl ligand of RuCpEt(CO)2 and the metal-alkyl groups on the surface. This study not only advances our understanding of Ru ALD processes but also highlights the significant impact of precursor chemistry and surface treatments in optimizing ALD for advanced microelectronic applications.
Supported precious metal single-atom catalysts have shown interesting activity and selectivity in recent studies. However, agglomeration of these highly mobile mononuclear surface species can eliminate their unique catalytic properties. In this paper, we study a strategy for synthesizing thin film stabilized single-atom Pd 1 catalysts using atomic layer deposition (ALD). The thermal stability of the Pd 1 catalysts is significantly enhanced by creating a nanocavity thin film structure. In situ infrared spectroscopy and Pd K-edge X-ray absorption spectroscopy (XAS) revealed that the Pd 1 was anchored on the surface through chlorine sites. The thin film stabilized Pd 1 catalysts were thermally stable under both oxidation and reduction conditions. The catalytic performance in the methanol decomposition reaction is found to depend on the thickness of protecting layers. While Pd 1 catalysts showed promising activity at low temperature in a methanol decomposition reaction, 14 cycle TiO 2 protected Pd 1 was less active at high temperature. Pd L 3 edge XAS indicated that the low reactivity compared with Pd nanoparticles is due to the strong adsorption of carbon monoxide even at 250 °C. Lastly, these results clearly show that the ALD nanocavities provide a basis for future design of single-atom catalysts that are highly efficient and stable.
Alkali metal containing materials have become increasingly attractive in a world hunting for sustainable energy materials and green functional devices. Lithium- and sodium battery technology, lead-free piezo- and ferroelectric devices, and record-breaking alkali doped tandem perovskite solar cells are among the applications where alkali metal-containing thin films get increasing attention. Atomic layer deposition (ALD) is one of the enabling thin film deposition techniques that offer chemical and geometrical versatility to realize the implementation of such thin films on an applicable scale. The drawback has until recently been a lack of available precursor chemistry that offers self-limiting growth that is fundamental to ALD. The alkali metal tert-butoxides have been shown to exhibit the necessary properties to facilitate saturating growth for Li-, Na-, K-, and Rb-containing compounds. However, the behavior of the tert-butoxides in ALD-growth has been considered difficult to unravel, with processes exhibiting limited control and low reproducibility. Very little has been reported on trends in reaction mechanisms as the mass of the alkali metal increases. Herein, we summarize the existing literature on the use of alkali metal tert-butoxides as precursors in ALD. We consider differences in the structure and behavior of the tert-butoxides as the alkali metal cation becomes heavier. In addition, we present precursor synthesis routes and key information on precursor structure, stability, and mechanistic behavior. Finally, we provide the first ever report of Cs-containing films by ALD to complement previous work on its lighter counterparts.
Atomic layer deposition (ALD) of TiS{sub 2} is investigated with titanium tetrachloride and hydrogen sulfide precursors. In-situ quartz crystal microbalance and ex-situ x-ray reflectivity measurements are carried out to study self-limiting deposition chemistry and material growth characteristics. The saturated growth rate is found to be ca. 0.5 Å/cycle within the ALD temperature window of 125–200 °C. As grown material is found poorly crystalline. ALD grown TiS{sub 2} is applied as a photon harvesting material for solid state sensitized solar cells with TiO{sub 2} as electron transport medium. Initial results with Spiro-OMeTAD as hole conducting layer show ca. 0.6% energy conversion efficiency under 1 sun illumination.
We have fabricated ZnO source-gated thin film transistors (SGTFTs) with a buried TiW source Schottky barrier and a top gate contact. The ZnO active channel and thin high-κ HfO{sub 2} dielectric utilized are both grown by atomic layer deposition at temperatures less than 130 °C, and their material and electronic properties are characterized. These SGTFTs demonstrate enhancement-mode operation with a threshold voltage of 0.91 V, electron mobility of 3.9 cm{sup 2} V{sup −1} s{sup −1}, and low subthreshold swing of 192 mV/decade. The devices also exhibit a unique combination of high breakdown voltages (>20 V) with low output conductances.
In 1992, UAH (University of Alabama in Huntsville) conducted a unique experiment on STS-46 in which YBa2Cu3O7 (commonly known as '1-2-3' superconductor) high-T(c) superconducting thin film samples prepared at three different laboratories were exposed to 5 eV atomic oxygen in low Earth orbit on the ambient and 320 C hot plate during the first flight of the CONCAP-2 (Complex Autonomous Payload) experiment carrier. The resistance of the thin films was measured in flight during the atomic oxygen exposure and heating cycle. Superconducting properties were measured in the laboratory before and after the flight by the individual experimenters. Films with good superconducting properties, and which were exposed to the oxygen flux, survived the flight including those heated to 320 C (600 K) with properties essentially unchanged, while other samples which were heated but not exposed to oxygen were degraded. The properties of other flight controls held at ambient temperature appear unchanged and indistinguishable from those of ground controls, whether exposed to oxygen or not.
Using scanning tunneling microscopy (STM), X-ray photoemission spectroscopy (XPS) and density functional theory (DFT) calculations we have studied the reduction of ultra-thin films of FeO(1 1 1) grown on Pt(1 1 1) after exposure to atomic hydrogen at room temperature. A number of new ordered, partlyreduced FeOx structures are identified and as a general trend we reveal that all the reduced FeOx structures incorporate 2-fold coordinated Fe atoms as opposed to the original 3-fold coordinated Fe atoms in the FeO film. We find that when all the Fe atoms are 2-fold O-coordinated the FeOx surface structure is resistant to further reduction at room temperature. We observe that water easily dissociates on the most heavily reduced FeOx, structure in contrast to the initially inert FeO film, and reveal that it is possible to partially re-oxidize the FeOx film by heating the surface slightly in the presence of water.
Electronic and optoelectronic devices, namely, thin film transistors (TFTs) and metal–semiconductor–metal (MSM) photodetectors, based on GaN films grown by hollow cathode plasma-assisted atomic layer deposition (PA-ALD) are demonstrated. Resistivity of GaN thin films and metal-GaN contact resistance are investigated as a function of annealing temperature. Effect of the plasma gas and postmetallization annealing on the performances of the TFTs as well as the effect of the annealing on the performance of MSM photodetectors are studied. Dark current to voltage and responsivity behavior of MSM devices are investigated as well. TFTs with the N{sub 2}/H{sub 2} PA-ALD based GaN channels are observed to have improved stability and transfer characteristics with respect to NH{sub 3} PA-ALD based transistors. Dark current of the MSM photodetectors is suppressed strongly after high-temperature annealing in N{sub 2}:H{sub 2} ambient.