Spectro-electrochemistry of vanadium ions in LiCl-KCl-VCl2,3

Owing to their relatively high thermal conductivity and corrosion resistance, and low radiation heating and embrittlement properties, vanadium (V) alloys are being considered for fusion blanket structural materials. As such, the fundamental behavior of these materials, including the speciation of their corrosion products in molten lithium salts, must be elucidated to enable quantitative lifetime prediction. Yuan et al. [REF#1] demonstrated the reduction and oxidation of vanadium ions in molten LiCl-KCl eutectic salt using a tungsten wire, indicating the possibility of metallic vanadium reduction from V3+ negative potentials

36 - MATERIALS SCIENCE↗

Radiation‐Resistant Aluminum Alloy for Space Missions in the Extreme Environment of the Solar System

Future human exploration of the solar system demands advanced materials capable of withstanding extreme environments, particularly exposure to solar energetic particle radiation. Current material selection criteria for space applications prioritize a high strength-to-weight ratio, high corrosion resistance and manufacturability, favoring age-hardenable Al-based alloys. However, conventional precipitation-hardened Al alloys suffer from irradiation-assisted dissolution of strengthening phases at doses as low as 0.2 displacements-per-atom (dpa), undermining their performance. Furthermore, these alloys develop radiation-induced defects, such as dislocation loops and voids, even at low doses. This study presents a novel ultrafine-grained (UFG) Al-based alloy, designed using the crossover alloying concept and strengthened by T-phase precipitates, featuring a chemically-complex structure with 162 atoms in its unit cell composed of Mg 32 (Zn,Al) 49 . It is showed that T-phase precipitates have exceptional radiation tolerance up to 24 dpa. Owing to the nanoscale UFG structure, dislocation loops are suppressed, and voids are only observed beyond 75 dpa. Microtensile tests up to 20 dpa confirm the preservation of mechanical performance under irradiation. The results underline the potential of this alloy as a radiation-resistant, lightweight material for future space applications. Three key strategies enable this performance: (i) stabilization of a UFG microstructure, (ii) T-phase precipitation featuring a highly negative Gibbs free energy and chemically-complex giant unit cell, and (iii) precise process control to prevent grain growth during heat treatment and irradiation.

36 MATERIALS SCIENCE↗

Rapid synthesis of phase-engineered tungsten carbide electrocatalysts via flash joule heating for high-current-density hydrogen evolution

Fabricating durable and high-performance electrocatalysts operating at high current densities for industrial acidic hydrogen evolution remains a daunting challenge. Tailoring the phase composition of electrocatalysts is a promising strategy to harness synergistic effects and improve charge transfer, thereby optimizing their performance. Here, this work presents a fast, green method based on flash joule heating (FJH) to synthesize phase-engineered tungsten carbide electrocatalysts for the acidic hydrogen evolution reaction (HER) at high current densities. Tungsten carbide electrodes with varying FJH treatment durations (3, 10, 30, and 60 s) are fabricated to fine-tune the mixture of tungsten monocarbide (WC) and tungsten semicarbide (W 2 C) phases. Results show that samples with a 30-s treatment (TC-3) exhibit an optimal balance between these phases, leading to a low overpotential of 180.97 and 387 mV at current densities of 10 mA/cm 2 and 4 A/cm 2 , respectively. TC-3 exhibits significantly lower charge transfer resistance compared to the other electrocatalysts, which can be attributed to its optimal phase ratio. Notably, the TC-3 electrocatalyst remains stable for over 9 days at 4 A/cm 2 due to their controlled phases and excellent corrosion-resistant properties. This work highlights a new method to fabricate cost-effective, high-performance tungsten carbide electrocatalysts with well-controlled phase compositions.

Acidic hydrogen evolution reaction↗

CRADA 2022-03 Final Report: Advanced Bearing Materials for Harsh Service Conditions

Develop advanced bearing materials for hydrogen gas turbines and wind turbines. Two candidate materials have been selected based on Ames lab’s recent work on high entropy alloys and shape memory alloys. These materials are designed to exhibit a balance of hardness, strength, toughness, and corrosion resistance. The hydrogen diffusion coefficient in the NiTi based shape memory alloy is two order of magnitude lower than that of the conventional case hardened bearing steel. We plan to atomize these materials into powders, additive manufacture cylindrical bearings, then test these bearing for rolling-contact fatigue, corrosion properties, and hydrogen embrittlement. We are a vertically integrated team comprises of national labs, bearing manufacturers, raw material powders makers, and aircraft gas turbine manufacturer.

Argibay, Nicolas [Ames Laboratory (AMES), Ames, IA↗

Al-Ce Alloy-Based Compact Heat Exchanger for Refrigerant Charge Reduction and Unprecedented Durability (CRADA NFE-21-08888 Final Report)

Oak Ridge National Laboratory and Eck Industries produced and characterized durable and corrosion resistant Al-Ce-Mg alloy-based heat exchanger. Eck Industries successfully casted Al-Ce-Mg heat exchanger. ORNL characterized reaction bonding between Al-2Ce-6Mg alloy and stainless-steel tube in a heat exchanger header. Metallurgical bonds were achieved between stainless steel tubes and Al-Ce-Mg alloy cast headers. ORNL performed corrosion testing on Al-Ce-Mg alloy/stainless steel tube reactive bond interface. In most cases no significant changes to the reactive bond morphology or compositional distribution were observed in the samples after exposure to acid for 267h acid.

36 MATERIALS SCIENCE↗

Al-Ce Alloy-Based Compact Heat Exchanger for Refrigerant Charge Reduction and Unprecedented Durability

• Oak Ridge National Laboratory and Eck Industries produced and characterized durable and corrosion resistant Al-Ce-Mg alloy-based heat exchanger. • Eck Industries successfully casted Al-Ce-Mg heat exchanger. • ORNL characterized reaction bonding between Al-2Ce-6Mg alloy and stainless-steel tube in a heat exchanger header. • Metallurgical bonds were achieved between stainless steel tubes and Al-Ce-Mg alloy cast headers. • ORNL performed corrosion testing on Al-Ce-Mg alloy/stainless steel tube reactive bond interface. • In most cases no significant changes to the reactive bond morphology or compositional distribution were observed in the samples after exposure to acid for 267h acid.

36 MATERIALS SCIENCE↗

Tailoring composition and deformation modes at the microstructural level for next generation low-cost high-strength austenitic stainless steels

The objective of this project is to enable deliberate development of cost-effective, hydrogen resistant alloys by establishing detailed relationships specific to the effects of alloy composition, short-range order (SRO), and microsegregation in the presence of hydrogen on the transition between homogeneous deformation and localized plasticity in shear bands. In collaboration with the International Institute for Carbon-Neutral Energy Research, I2CNER, at Kyushu University in Japan, we conceptualized, designed, and manufactured four austenitic alloys that maintain corrosion resistance and ensure lower cost relative to baseline commercial alloys. The mechanical properties and deformation modes of the novel alloys (KU alloys) were assessed in the presence of hydrogen (H). Correlations between composition and performance revealed that two of the KU alloys are suitable replacements for 316 steel, while another is a viable replacement for 304 steel at room temperature. We found that, in the presence of other austenite stabilizing elements namely Mn and N, replacing Ni with Cu does not lead to martensite formation as has been previously reported.1–3 Furthermore, we found that the addition of Cu leads to an earlier onset of multiple slip resulting in an relative earlier onset of a higher work hardening rate (WHR). Greater understanding of the relationships between alloy composition and SRO required the development of a novel advanced electron diffraction methodology to characterize SRO in complex FCC alloys. This innovative approach, which combines fluctuation and correlation analyses of diffuse-scattering signals, successfully differentiated between SRO and long-range ordering (LRO). Further investigations into annealed austenitic stainless steels could provide insights into manipulating SRO and its effects on material properties. Atomistic simulations provided understanding of SRO behavior that was difficult to capture experimentally. This project created the first spin cluster expansion model that is able to capture and describe SRO effects in Fe-Ni-Cr FCC alloys, accounting for the non-negligible effects of magnetism. An automated computational workflow was established to provide reliable predictions of SRO in Fe-Ni-Cr austenitic alloys, both with and without the presence of H atoms. Analysis of the propensity for SRO in Fe-Ni-Cr alloys revealed that H tends to cluster with specific, well-defined SRO domains. The computational framework is general purpose and can be extended to realistic stainless steels across diverse composition ranges. With confidence that SRO is possible in austenitic stainless steels, we developed a discrete dislocation finite element code to understand the interaction of dislocations with SRO in the presence of H. By incorporating H effects on the dislocation emission and SRO stress field we show that the critical stress for the dislocation pileup to breakthrough the SRO domain decreases in the presence of H, which directly contributes localized deformation at the macroscale. Through the simulation of a uniaxial tension test, we demonstrated that H-induced weakening of SRO stress field and H-enhanced dislocation emission can lead to the onset of shear localization at lower macroscopic strains. As a whole, this project identified three novel alloys that show improvements in performance and cost efficiency for H-facing applications by studying correlations between alloy chemistry and deformation behavior. We also made significant advancements to experimental and computational methodologies necessary to study the chemistry and distribution of SRO across a range of alloys, which in turn allowed us to demonstrate how deformation mechanisms change due to the contributions of SRO in austenitic alloys in the presence of H. The combined advancements in fundamental understanding with novel alloy development in this project has increased the viability of next generation H-technologies for the broader public through accessible low-cost alloys and accelerated development towards future H-infrastructure.

08 HYDROGEN↗

Semi-Dynamic Leach Testing of Densified Silicon-based Iodine Waste Forms

Iodine waste forms (IWF) require a conceptual corrosion release model (CCRM) to provide iodine (I) release rates for performance modeling nuclear waste disposal repositories. To develop a CCRM, an understanding of the corrosion mechanisms of the IWF are required along with data from consistent test methods to parameterize the model. The present study has advanced both areas by providing and assessing the corrosion resistance of IWF types based on their processing history in minor variations of semi-dynamic leach tests. The test included a series of semi-dynamic leach tests using monolithic IWFs in deionized water (leachant). Several experiments were conducted under alternate test conditions with changes to temperature, leachant replacement, leachant pH, leachant volume, masking, and surface finish to elucidate if varying these conditions impacted IWF corrosion behavior. Tests were conducted on two classes of IWFs: (1) I-bearing silver-mordenite (AgZ) materials processed by hot isostatic pressing (HIP) at different temperatures, pressures, sizes, and times; and (2) I-bearing silver-functionalized silica aerogels (SFA) processed by either HIP or spark plasma sintering (SPS). The corrosion susceptibility of AgZ samples was influenced by HIP temperature and pressure. The SPS SFAs retained I far better than HIP SFAs. Additional findings in this study include: (1) The iodine dissolution rate decreased with decreasing temperature, (2) a common ion effect may occur and slow dissolution of the host phase if the leachant is not regularly replaced, (3) pH controls the dissolution rate, and (4) the iodine dissolution rate slows with extended test time (up to 224 days). Based on this work, these parameters should thus be represented when developing a CCRM.

corrosion↗

Elucidating the corrosion mechanism of commercial Ni-based Superalloys in UCl3 containing-chloride Molten Salt Systems

Molten salt reactors (MSRs) have gained renewed interest, providing several advantages over their predecessors, including the capability to consume spent fuels, enhancing the environmental sustainability of the uranium fuel cycle. For example, molten chloride fast reactors (MCFRs) can reach criticality with molten chloride spent fuel containing high concentrations of impurities, such as actinide products like uranium chloride (UCl3). However, the redox potential of chloride molten salt fuels may change in the presence of these impurities, dictating their corrosivity and in turn the corrosion performance of structural components, such as those constructed from nickel (Ni)-based alloys. The purpose of this investigation is to assess the extent of corrosion of Ni-based alloy, Inconel 617, when exposed to UCl3-LiCl-KCl eutectic salt. Inconel 617 one of only six structural materials that are fully qualified by the American Society for Mechanical Engineers (ASME) Boiler and Pressure Vessel Code for high-temperature nuclear reactor components, making it a technologically mature material to consider for constructing MCFRs. Inconel 617 specimens were submerged in a static LiCl-KCl-UCl3 eutectic salt mixture heated at 700 C for 1000 h under an inert atmosphere. Upon completion, the extent of corrosion was analyzed through a multi-modal characterization approach spanning the engineering to nanoscale, employing computed tomography, focused-ion beam, and transmission electron microscopy techniques. Results from this investigation will enhance our understanding of property-to-performance relationships of candidate structural materials for MSRs with respect to corrosion resistance and interactions between the salt and alloy interface.

36 MATERIALS SCIENCE↗

Mitigate Stress Corrosion Cracking (SCC) in High-strength Al Castings (CRADA 508)

Development of high strength, corrosion resistant, aluminum alloys is important to a number of industries, including automotive, aerospace, power, etc. Understanding how processing methods such as casting, chemistry, additives and recycle content affect an alloy’s microstructure and performance in real world environments is crucial to their implementation. One major concern is how the repeated exposure to saline solutions can be detrimental to the structural integrity of aluminum alloy components. This study was undertaken as a collaboration between Eck Industries and PNNL to investigate the stress corrosion cracking (SCC) and corrosion behavior of aluminum alloys. This work examines the SCC response of three different materials set. First is cast A206 Al alloy produced by three different casting techniques (i.e., permanent mold, and sand casting with and without chill) and with or without nano forming additives as potential grain refiners. The second materials set comprises Al alloy tubes extruded by PNNL’s ShAPE process and produced using raw material with three different ratios of twitch and pre-consumer Al 6061 scrap. Finally, the third materials set comprises two Al-Si-Mg-Fe alloys with controlled Si% and Fe% to mimic recycle grade Al alloys. The corrosion behavior of these materials was characterized using SCC testing and scanning electrochemical cell microscopy (SECCM) technique; mechanical behavior was characterized using tensile testing, and microstructure was characterized using optical and electron microscopy techniques. Of the A206 Al alloys, the samples with nano forming additives performed poorly compared to those without. The best SCC performance (i.e. least degradation in mechanical properties) was demonstrated by A206 alloy sand cast with chill while the permanent mold sample showed the worst SCC performance. The SECCM was performed on A206 alloy sand cast with chill to understand the effect of microstructure and determine the location-dependent corrosion properties on grain boundaries (GB) and inside grains (IG) on the sample. The corrosion potential and current measured on GB and IG at various points on the sample established that the GB locations are more cathodic and corrosive than the IG locations. Further work needs to be conducted to investigate the mechanisms behind the observed dependence of SCC on casting technique and nano forming additives. Among the ShAPE extruded tubes, SECCM data suggests the decreasing order of tendency to corrode as follows: 100% twitch > 75% twitch > 50% twitch. Finally, both variants of the Al-Si-Mg-Fe alloys showed a large volume fraction of Fe- and Si-containing intermetallics and additional work is needed to discern differences in their respective corrosion responses. In summary, correlating local electrochemical behavior (e.g. via SECCM) with micro/nanostructure, in conjunction with bulk mechanical behavior, can help identify the right fabrication method and alloy chemistry to minimize SCC issues in Al alloys.

36 MATERIALS SCIENCE↗

Reducing Mass of Steel Auto Bodies using Thin Advanced High Strength Steel with Carbon-Fiber Reinforced Epoxy

Diversitak, a company based in Detroit, MI, has developed a proprietary, low specific gravity, carbon fiber-reinforced epoxy (CFRE) under U.S. patent number 9,963,58832. Preliminary testing on this new material conducted in collaboration with ArcelorMittal Steel Company proved out the CFRE concept. A thin layer of this CFRE was applied to a stamped sheet of steel with residual stamping oils from a mill, in a time corresponding to automotive processing (e.g., ~15 seconds), and processed following automotive e-coat procedures (phosphating + 175–200°C heating), to complete the curing. No problems with adherence or performance were noted. While the CFRE does add weight to a thin gauge steel panel, it weighs much less than what is displaced by using thicker conventional mild steel gauges. The application of the coating showed a significant increased dent resistance, oil canning resistance, and part stiffness.This current two-year project was designed to mature this new technology to near manufacturing readiness to reduce the weight of a vehicle and lower the cost of weight reduction. The process involves the use of thinner gauge steels than are currently used. The collaborative development team included two industrial manufacturers: Diversitak and ArcelorMittal Steel Company; LightMAT; and two National Laboratories: Oak Ridge National Laboratory (ORNL) and Idaho National Laboratory (INL). The team developed a new manufacturing process to reduce the weight of a vehicle and lower the cost of weight reduction, as well as a better understanding of how to apply the coating so that it will perform to a high standard in-service. The team also performed an in-depth study to determine the long-term durability of the materials manufactured using this technology and well-known automotive industry standard tests.The overall process involved stiffening the thinner gauge steel by applying the CFRE on only one side. To accomplish this goal, the optimal reinforcement fiber length and fiber concentration was first determined. This was followed by measuring the coefficient of thermal expansion (CTE) in all three directions, so it could be fed into manufacturing models and methods for rapidly and inexpensively applying the coating. This was followed by panel level evaluations of the coating and steel combination, and then by full part demonstration of the technology on door panels. The final step was corrosion testing of the parts.ArcelorMittal characterized the advanced high strength steel (AHSS) (e.g., metallurgy-heat treatment for required AHSS properties as a function of the sheet thickness, state of internal stress) and quantified CFRE adhesion to the steel as a function of sheet preparation (e.g., rolling and stamping).ORNL optimized the fiber length, fiber concentration, and coating thickness for best vehicle function and performance at the least cost. Along with the suppliers, ORNL developed a durable CFRE application process (e.g., gun material, design, robotic dispensing process) and identified the adhesion stability of the CFRE during process holding. An approach to ensure that application/curing timing conforms to conventional assembly line speed and plant cycle times was determined. ORNL also determined the CTE of the material in all three directions and performed material scanning electron microscopy (SEM) analyses.INL characterized the corrosion properties of the steel panels coated with CFRE. The panels were investigated for corrosion resistance and stability as replacement materials used in automotive body panels to reduce mass. The coupons tested at INL were supplied by Diversitak after an optimized CFRE formulation was achieved in the already coated form for corrosion testing.

99 GENERAL AND MISCELLANEOUS↗

Composite coatings from polycarbosilane derived SiC and Al/SiC cermet active fillers as protective barriers against steel corrosion

Stainless steel is used throughout the world as a structural material. However, it undergoes corrosion damage when exposed to extremely corrosive media, such as the marine environment. An alternative to solve this problem lies in the development of coatings that can withstand extreme conditions but also be easily deposited with inherently corrosion-resistant materials such as silicon carbide (SiC). The present study shows a simple method to produce Al/SiC cermet powders by attrition milling. The resulting cermet powders with a metallic matrix and hemispherical morphology, were employed as fillers in polycarbosilane (PCS) solutions that were sprayed on A304 stainless steel substrates. Al/SiC composite coatings were produced after heating the sprayed suspensions at 700 °C for 1 h in Ar atmosphere. The resulting composite coatings exhibited low surface energies (< 35 mN/m), water contact angles of 53°, and adhesion strength of up to 30 MPa. Finally, corrosion tests were performed in a cyclic corrosion test chamber, showing that these coatings effectively reduced the corrosion rate of stainless steel by 87%, reaching corrosion rate values of 0.007 g/cm 2 year.

36 MATERIALS SCIENCE↗

Corrosion Testing of Refractory inContact with Molten Glasses Designed for Waste Vitrification - VSL Touchpoint Matrix Glasses

It is known that the predictive life of the refractory ceramic liner of nuclear waste glass melters is conservative, as demonstrated by performance of these materials such as in the Defense Waste Processing Facility (DWPF). The motivation for this task is to maximize the useful life of the melters that will be operated at the Waste Treatment and Immobilization Plant (WTP), which will in turn minimize procurement and disposal costs and melter outage times, as well as to identify maximum loadings in the waste glass of those species that corrode melter components. This task was initiated jointly with Pacific Northwest National Laboratory (PNNL) with the objective to develop a methodology and model to enable more accurate prediction of refractory service life under prototypic conditions from laboratory-scale material corrosion tests. Refractory corrosion is generally reported as physical material loss, measured in units of distance (e.g., inch) or as physical material loss rate, measured in units of distance per time (e.g., inch/day). In post-operational melters, the refractory corrosion is measured directly, sometimes reported as corrosion depth. Crucible tests are used in the laboratory to accelerate the refractory corrosion to facilitate a meaningful measurement in a commensurate amount of time. Crucible tests are particularly useful in understanding refractory corrosion across a large glass composition space, where operational testing would be prohibitive. Some of the critical parameters that are known to influence refractory corrosion by molten glass in a crucible test are temperature, system redox, molten salt phases, glass chemistry, and test duration. The majority of data collected for Monofrax® K-3 (hereafter referred to as K-3) corrosion is from crucible tests, but a small amount comes directly from scaled and production melters. Crucible test data has been collected under varying conditions, whereas data collected from operational melters is relatively fewer and represents conditions specific to the melter campaign. The result is that the published data can be grouped and analyzed in multiple ways, not all of which are readily comparable. The Standard Test Method for Isothermal Corrosion Resistance of Refractories to Molten Glass (ASTM C621) outlines the general guidelines used across industry. That method describes a sealed, static test in which the surface area of the refractory coupon and the volume of glass are fixed. A significant portion of the crucible data pertaining to nuclear waste glasses has been collected in a modified configuration; the most notable differences being the surface area of the refractory coupon to volume of the glass and use of a method for bubbling the melt. To our knowledge, the influence of those parameters on the refractory corrosion has not been quantified. In this work, it was determined that static tests and bubbled tests would be performed. Savannah River National Laboratory (SRNL) was tasked with setting up and performing static testing while PNNL was tasked with setting up and performing bubbled testing. Initial activities were performed to establish laboratory methods that reproduce data comparable to existing data sets of K-3 refractory corrosion by low activity waste (LAW) and high-level waste (HLW) glass compositions. Later activities were focused on refining the test parameters to establish a standard test practice to be used between Laboratories and collecting additional data to be used in the enhanced waste glass model development. This document serves primarily to convey the refractory loss measurement results from corrosion testing of K-3 refractory with waste glass compositions developed for use in the WTP melters. The data will be used in the enhanced property/composition models being developed for waste glass vitrification and melter operations.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

On Stability and Electrochemical Performance of 316 Stainless Steel in Wastewater: Implications for Resource Recovery

Electrochemical nutrient recovery systems rely on stable electrode materials capable of operating in chemically complex wastewater environments. We investigated corrosion resistance and interfacial electrochemical behavior of 316 stainless steel (SS316) in a synthetic wastewater matrix representative of centrate streams, a key knowledge gap in electrochemical phosphorus recovery. A comprehensive suite of electrochemical techniques (chronoamperometry, cyclic voltammetry, potentiodynamic polarization, and electrochemical impedance spectroscopy (EIS)) and surface characterization methods (scanning electron microscopy, X-ray diffraction) were employed. Results revealed that wastewater containing typical ionic constituents (such as PO 4 3- , NH 4 + , and divalent cations) exhibited enhanced cathodic activity and the formation of a more stable, protective surface film on SS316 that mitigated chloride-induced corrosion. In contrast, SS316 in the NaCl solution showed significant susceptibility to passive layer breakdown and localized corrosion. Time-resolved EIS further confirmed improved interfacial stability and restricted charge transfer in WW over time, in stark contrast to the progressive passive layer degradation in NaCl. Surface analyses corroborated these findings, showing limited surface attack in WW compared to distinct localized corrosion features in NaCl. These findings indicate that competing ionic species in WW effectively mitigate chloride aggressiveness, enhance SS316 stability, and demonstrate improved electrode longevity and reliability for sustainable wastewater-based electrochemical phosphorus recovery applications.

36 MATERIALS SCIENCE↗

Integrated process-structure–property–performance optimization of cold-sprayed zinc coatings on AZ91 magnesium alloy

High-pressure die cast (HPDC) AZ91 magnesium alloy is widely used in automotive components such as transmission housings and brackets for its excellent strength-to-weight ratio. Zinc-based cold spray coatings can be applied selectively to vulnerable areas to enhance corrosion resistance, minimize galvanic coupling with dissimilar metals, and eliminate the need for full-surface oxide coatings, making the process more efficient and targeted. A comprehensive evaluation of 16 combinations of nitrogen carrier gas temperatures and pressures led to the identification of an optimal range of process parameters, yielding Zn coatings with porosity <0.5 % by area, wear rates reduced by a factor of two compared to uncoated AZ91, and adhesion strengths up to 35 MPa. The enhanced mechanical performance of the coating is attributed to the low porosity and the formation of a metallurgical bond at the coating-substrate interface. Corrosion studies using macroscale potentiodynamic polarization (PDP) and electrochemical impedance spectroscopy (EIS) revealed a significant decrease in corrosion rate and a shift to more noble corrosion potentials (ZCP) for coated substrates. Furthermore, the Zn cold-sprayed samples exhibited significantly lower corrosion-induced evolved hydrogen content compared to the base AZ91 substrate and AZ91 coated with industrial coatings, demonstrating that the Zn layer effectively protects the substrate from the corrosive environment. Overall, cold spray Zn coatings significantly improve the mechanical and corrosion performance of AZ91 Mg alloys, addressing key material challenges and enabling their broader use in automotive applications.

Corrosion performance↗

Evaluation of NETL’s Self-Healing Metallic Coating for Internal Corrosion Protection of Natural Gas Pipelines: Field Test

Steel pipelines are a safe, reliable, and affordable way to transport natural gas. However, the presence of impurities (e.g., water, carbon dioxide, and hydrogen sulfide) in the natural gas can cause internal corrosion, which can lead to pipeline leaks and failure. This paper reports on field tests of an innovative self-healing, corrosion-resistant, metallic coating developed at the National Energy Technology Laboratory (NETL) for protecting the interior surfaces of pipelines.

carbon dioxide (CO2)↗

Status Report on the Development of Cladding Inner-wall and Outer-wall Coatings

Advanced cladding is critical for nuclear reactors with enhanced performance in radiation tolerance, neutron transparency and reactor safety. Using advanced cladding will ensure the adequate thermal conductivity and mechanical stability of the cladding base material, corrosion resistance and high-temperature coolant compatibility of the cladding surface, and chemical stability in the cladding inner wall against fuel cladding chemical interaction (FCCI). An innovative cladding with a three-layer structure (i.e., a modified outer surface, a robust clad base material, and a modified inner wall) promises to meet all these requirements. In this status report, the initial efforts on the development of cladding inner-wall and outer-wall coatings are summarized. The activities covered in this report are (1) High-resolution TEM studies of TiN/HT-9 interface atomic structure and chemistry after ion irradiation, (2) High-resolution TEM studies of TiN/14YWT ODS interface atomic structure after thermal cycling, (3) Inner-wall TiN coating for an experimental 14YWT ODS cladding, and (4) Corrosion test of TiN coated Ziracloy-4 bar samples.

36 - MATERIALS SCIENCE↗

Comparative Study of Zinc Cold-Spray Coating and Pre-treatments for Magnesium Alloys

Magnesium (Mg) alloys are appealing for automotive lightweighting owing to their high specific strength. However, their susceptibility to corrosion in harsh environments remains a major challenge. Conventional industrial pre-treatment coatings, including zinc phosphate, chromate conversion, and non-chromate conversion, often exhibit discontinuities and microcracks, leading to localized corrosion near fasteners and parting lines. Here, this study investigates cold-sprayed zinc (Zn) coatings as a novel pre-treatment alternative for high-pressure die cast (HPDC) AZ91 Mg alloys, demonstrating significant improvements in wear and corrosion performance. Cold spray produces uniform and robust coatings, reducing wear rate by over 50% and reducing corrosion rate by over 99.3%, as measured by evolved hydrogen release, compared to traditional pre-treatments. Multimodal corrosion testing reveals that Zn cold-spray coatings form a protective layer during exposure, minimizing general and filiform corrosion, and exhibiting corrosion potential (E corr ) that is nobler by ~ 400 mV than the surfaces of both pre-treated and uncoated AZ91. Scalability of cold spray for selective application around multimaterial joints further strengthens their industrial viability. This work establishes Zn cold-spray coatings as highly effective pre-treatment solutions for the advancement of corrosion resistant Mg alloy components in automotive applications.