At least 73 records · Page 4

An Investigation of Chemo-Mechanical Phenomena and Li Metal Penetration in All-Solid-State Lithium Metal Batteries Using In Situ Optical Curvature Measurements

Solid-electrolytes (SEs) can provide a pathway to increase energy-density in lithium metal batteries. However, lithium metal penetration through garnet based LLZO solid electrolytes has been identified as a critical failure process. This phenomenon is related to chemo-mechanical processes which are difficult to probe. In particular, characterizing the dynamic mechanical deformations that occur in electrode-SE structures is very challenging. Here study reports in situ curvature measurements that are thus designed to probe chemo-mechanical phenomena that occur during lithium plating. The novel experimental cell configuration created for this work shows that pressure builds up in the Li metal during plating, up until the point where short circuits occur. The resulting data are analyzed with a detailed finite element model (FEM) to quantitatively evaluate stress evolution. The results show that Li metal plating within a surface flaw can produce stress build-up prior to short-circuiting. The combined results from both the experiments and the FEM suggest that it is critical to minimize surface defects and flaws during the manufacturing processes.

25 ENERGY STORAGE↗

The Role of Electrolyte Composition in Enabling Li Metal‐Iron Fluoride Full‐Cell Batteries

Abstract FeF 3 conversion cathodes, paired with Li metal, are promising for use in next‐generation secondary batteries and offer a remarkable theoretical energy density of 1947 Wh kg −1 compared to 690 Wh kg −1 for LiNi 0.5 Mn 1.5 O 4 ; however, many successful studies on FeF 3 cathodes are performed in cells with a large (>90‐fold) excess of Li that disguises the effects of tested variables on the anode and decreases the practical energy density of the battery. Herein, it is demonstrated that for full‐cell compatibility, the electrolyte must produce both a protective solid‐electrolyte interphase and cathode‐electrolyte interphase and that an electrolyte composed of 1:1.3:3 (m/m) LiFSI, 1,2‐dimethoxyethane, and 1,1,2,2‐tetrafluoroethyl‐2,2,3,3‐tetrafluoropropyl ether fulfills both these requirements. This work demonstrates the importance of verifying electrode level solutions on the full‐cell level when developing new battery chemistries and represents the first full cell demonstration of a Li/FeF 3 cell, with both limited Li and high capacity FeF 3 utilization.

25 ENERGY STORAGE↗

Simply Fabricatable Reference Electrode for Studying Li Metal Interfaces Operando

Reference electrodes are essential for studying Li metal interfaces, yet their integration into coin cells remains challenging due to geometric constraints and assembly complexity. Here, we present a simple three-electrode coin cell design in which a thin Cu film is evaporated directly onto a trilayer PP/PE/PP separator, forming a conductive and flexible in situ current collector. The microporous Cu preserves separator porosity and pressure uniformity, avoiding artifacts introduced by wire- or mesh-type references. It is easily activated by Li plating and provides stable potentials for over 10 days in ether-based electrolytes without affecting Coulombic efficiency (>99%) or Li deposition morphology. Operando measurements using this design reveal electrode-specific impedance evolution and voltage responses otherwise obscured in two-electrode setups, uncovering a correlation between the SEI resistance and electrolyte ionic conductivity. This microporous Cu reference electrode offers a robust and accessible platform for characterizing reactive interfaces under realistic cycling conditions.

Sacci, Robert [ORNL] (ORCID:0000000200735221)↗

Glass-fiber-reinforced polymeric film as an efficient protecting layer for stable Li metal electrodes

With numerous reports on protecting films for stable lithium (Li) metal electrodes, the key attributes for how to construct these efficient layers have rarely been fully investigated. Here, we report a rationally designed hybrid protective layer (HPL) with each component aligning with one key attribute; i.e., cross-linked poly(dimethylsiloxane) (PDMS) enhances flexibility, polyethylene glycol (PEG) provides homogeneous ion-conducting channels, and glass fiber (GF) affords mechanical robustness. A significant improvement of the electrochemical performance of HPL-modified electrodes can be achieved in Li/HPL@Cu half cells, HPL@Li/HPL@Li symmetric cells, and HPL@Li/LiFePO 4 full cells. Even with an industrial standard LiFePO 4 cathode (96.8 wt % active material), the assembled cell still exhibits a capacity retention of 90% after 100 cycles at 1 C. More importantly, the functionality of each component has been studied comprehensively via electrochemical and physical experiments and simulations, which will provide useful guidance on how to construct efficient protective layers for next-generation energy storage devices.

25 ENERGY STORAGE↗

Challenges for and Pathways toward Li-Metal-Based All-Solid-State Batteries

Solid-state batteries utilizing Li metal anodes have the potential to enable improved performance (specific energy >500 Wh/kg, energy density >1500 Wh/L), safety, recyclability, and potentially lower cost (<$100/kWh) compared to advanced Li-ion systems.1,2 These improvements are critical for the widespread adoption of electric vehicles (EVs) and trucks and could create a short-haul electric aviation industry.1-3 Expectations for solid-state batteries are high, but there are significant materials and processing challenges to overcome.

25 ENERGY STORAGE↗

Review on Interface and Interphase Issues in Sulfide Solid-State Electrolytes for All-Solid-State Li-Metal Batteries

All-solid-state batteries have emerged as promising alternatives to conventional Li-ion batteries owing to their higher energy density and safety, which stem from their use of inorganic solid-state electrolytes instead of flammable organic liquid electrolytes. Among various candidates, sulfide solid-state electrolytes are particularly promising for the development of high-energy all-solid-state Li metal batteries because of their high ionic conductivity and deformability. However, a significant challenge remains as their inherent instability in contact with electrodes forms unstable interfaces and interphases, leading to degradation of the battery performance. In this review article, we provide an overview of the key issues for the interfaces and interphases of sulfide solid-state electrolyte systems as well as recent progress in understanding such interface and interphase formation and potential solutions to stabilize them. In addition, we provide perspectives on future research directions in this field.

25 ENERGY STORAGE↗

NASICON Li 1.2 Mg 0.1 Zr 1.9 (PO 4 ) 3 Solid Electrolyte for an All‐Solid‐State Li‐Metal Battery

Abstract A thin solid electrolyte with a high Li + conductivity is used to separate the metallic lithium anode and the cathode in an all‐solid‐state Li‐metal battery. However, most solid Li‐ion electrolytes have a small electrochemical stability window, large interfacial resistance, and cannot block lithium‐dendrite growth when lithium is plated on charging of the cell. Mg 2+ stabilizes a rhombohedral NASICON‐structured solid electrolyte of the formula Li 1.2 Mg 0.1 Zr 1.9 (PO 4 ) 3 (LMZP). This solid electrolyte has Li‐ion conductivity two orders of magnitude higher at 25 °C than that of the triclinic LiZr 2 (PO 4 ) 3 . 7 Li and 6 Li NMR confirm the Li‐ions in two different crystallographic sites of the NASICON framework with 85% of the Li‐ions having a relatively higher mobility than the other 15%. The anode–electrolyte interface is further investigated with symmetric Li/LMZP/Li cell testing, while the cathode–electrolyte interface is explored with an all‐solid‐state Li/LMZP/LiFePO 4 cell. The enhanced performance of these cells enabled by the Li 1.2 Mg 0.1 Zr 1.9 (PO 4 ) 3 solid electrolyte is stable upon repeated charge/discharge cycling.

Zhou, Qiongyu↗

Unveiling the Role of Lithium Iodide in Stabilizing Solid Interfaces in All-Solid-State Li Metal Batteries

A critical challenge in all-solid-state lithium metal batteries (ASSLMBs) is achieving a stable interface between the lithium metal anode and the solid electrolyte. Leveraging its success in Li/I 2 batteries, lithium iodide has garnered significant attentions for its potential to enhance interfacial stability and overall cell performance in ASSLMBs. Here, we elucidate the role of lithium iodide in stabilizing the solid interface in all-solid-state Li metal batteries with a Li argyrodite electrolyte, particularly focusing on its influence on lithium deposition behavior and interfacial evolution. Through in situ optical imaging, we demonstrate more uniform lithium deposition on an iodide-contained argyrodite electrolyte compared to a chloride-based counterpart. Complementary density functional theory calculations attribute improved lithium plating behavior to the enhanced lithiophilicity and better ionic conductivity of lithium iodide at the solid interface, effectively reducing localized current density. In conclusion, these findings provide useful insights into the mechanisms through which lithium iodide enhances the interfacial stability in ASSLMBs.

Anions↗

Multidimensional visualization of the dynamic evolution of Li metal via in situ/operando methods

The growing demands for high-energy density electrical energy storage devices stimulate the coupling of conversion-type cathodes and lithium (Li) metal anodes. While promising, the use of these “Li-free” cathodes brings new challenges to the Li anode interface, as Li needs to be dissolved first during cell operation. In this study, we have achieved a direct visualization and comprehensive analysis of the dynamic evolution of the Li interface. The critical metrics of the interfacial resistance, Li growth, and solid electrolyte interface (SEI) distribution during the initial dissolution/deposition processes were systematically investigated by employing multidimensional analysis methods. They include three-electrode impedance tests, in situ atomic force microscopy, scanning electrochemical microscopy, and cryogenic scanning transmission electron microscopy. The high-resolution imaging and real-time observations show that a loose, diffuse, and unevenly distributed SEI is formed during the initial dissolution process. This leads to the dramatically fast growth of Li during the subsequent deposition, deviating from Fick’s law, which exacerbates the interfacial impedance. The compactness of the interfacial structure and enrichment of electrolyte species at the surface during the initial deposition play critical roles in the long-term stability of Li anodes, as revealed by operando confocal Raman spectroscopic mapping. In conclusion, our observations relate to ion transfer, morphological and structural evolution, and Li (de)solvation at Li interfaces, revealing the underlying pathways influenced by the initial dissolution process, which promotes a reconsideration of anode investigations and effective protection strategies.

25 ENERGY STORAGE↗

Ultra-high-voltage Ni-rich layered cathodes in practical Li metal batteries enabled by a sulfonamide-based electrolyte

By increasing the charging voltage, a cell specific energy of >400 Wh kg-1 is in principle achievable with LiNi0.8Mn0.1Co0.1O2 in lithium-metal batteries (LMBs). However, stable cycling of high-nickel cathodes at ultra-high voltages is extremely challenging. Here we report that a rationally designed sulfonamide-based electrolyte enables stable cycling of commercial LiNi0.8Co0.1Mn0.1O2 with a cut-off voltage up to 4.7 V in LMBs. In contrast to commercial carbonate electrolytes, the electrolyte not only suppresses side reactions, intergranular cracking, transition-metal dissolution, and impedance growth on the cathode side, but also enables highly reversible Li metal stripping and plating leading to compact morphology and low pulverization. Our LMB delivers a specific capacity >230 mAh g-1 and an average Coulombic efficiency >99.65% over 100 cycles. Even under harsh testing conditions, the 4.7 V LMB can retain >88% capacity for 90 cycles, demonstrating significant advances in practical LMBs.

36 MATERIALS SCIENCE↗

The Chemistry, Formation and Passivation of Solid-Electrolyte Interphase (SEI) from FSI- Breakdown at Li-metal Potential

LiFSI-based liquid electrolytes are promising for realizing high Coulombic efficiency (CE) and long cycle life of next-generation high-energy Li metal battery. Nevertheless, the fundamentals of both the chemistry and formation of solid-electrolyte interphase (SEI) in these electrolytes have remained elusive. Herein, we extensively combine electrochemistry and X-ray photoelectron spectroscopy (XPS) to illustrate the reaction pathways of electrolyte decomposition, especially FSI- breakdown, as well as the dissolution trend of various inorganic SEI components. The SEI-forming reactions at Cu/electrolyte interface manifest a potential (E) dependence, driven by direct electron-transfer (ET) and Li underpotential-deposition (Li UPD) at high and low E regions, respectively. By closely correlating the XPS data obtained with and without solvent washing, we demonstrate that not all the products derived from SEI reactions are incorporated into forming a passivating surface layer, with a notable portion dissolving into liquid electrolyte instead. Importantly, high-CE electrolyte dictated by the chemical identity of solvent, is found to exhibit minimized interfacial reactivity of SEI formation enabling more effective interphasial passivation, via preferential integration of passivating ingredients such as LiF. Overall, this work formulates a systematic understating of bridging the SEI chemistry, formation and passivation while identifying key characteristics of high-performance electrolyte for guiding future design.

Bao, Zhenan [SLAC National Accelerator Laboratory ↗

Electrochemical formation of bis(fluorosulfonyl)imide-derived solid-electrolyte interphase at Li-metal potential

Lithium bis(fluorosulfonyl)imide-based liquid electrolytes are promising for realizing high Coulombic efficiency and long cycle life for next-generation Li-metal batteries. However, the role of anions in the formation of solid-electrolyte interphase remains unclear. Herein, we combine electrochemical analyses and X-ray photoelectron spectroscopy measurements both with and without sample washing, together with computational simulations, to propose the reaction pathways of electrolyte decomposition and correlate the interphase component solubility with the efficacy of passivation. Additionally, we discovered that not all the products derived from interphase-forming reactions were incorporated into the resulting passivation layer, with a notable portion present in the liquid electrolyte. Further, we found that the high-performance electrolytes can afford a sufficiently passivating interphase with minimized electrolyte decomposition, by incorporating more anion-decomposition products. Overall, this work presents a systematic approach of coupling electrochemical and surface analyses to paint a comprehensive picture of solid-electrolyte interphase formation, while identifying key attributes of high-performance electrolytes for guiding future designs.

Yu, Weilai [Stanford University, CA (United States↗

A Modified Sand’s Time Incorporating Li-Ion Transport Across the SEI: Basis for Understanding Li Dendrite Formation and Li-Metal Battery Electrolyte Selection

Abstract Understanding the initiation of lithium dendrites remains elusive, largely due to the intricate role of the solid electrolyte interphase (SEI) which forms on the Li surface during electrodeposition. Many studies have utilized the classical Sand’s equation to estimate the onset time when lithium dendrites begin to form. The Sand’s equation provides the time when the cation (Li+) concentration at the electrode-electrolyte interface approaches zero under diffusion-limited conditions in galvanostatic Li electrodeposition. However, recent experimental studies have revealed that the observed lithium dendrite onset time deviates considerably from the Sand’s time. Here, we show that this deviation from classical theory is likely due to the transport of Li+ ions through the SEI - a transport limitation that is much more dominant in controlling dendrite formation. We develop a ‘modified’ Sand's equation, incorporating the SEI layer and the diffusional transport across it to predict Li dendrite onset times. To validate this approach, we conducted Li electrodeposition experiments at various current densities using two distinct organic electrolytes. Analysis of the results demonstrates that the modified Sand's equation provides a more accurate prediction of dendrite onset times, highlighting the importance of incorporating SEI into transport models of Li plating in next-generation rechargeable Li-metal batteries.

Ma, Yuanman (ORCID:0000000200444811)↗

Synchrotron Imaging of Pore Formation in Li Metal Solid-State Batteries Aided by Machine Learning

High-rate capable, reversible lithium metal anodes are necessary for next generation energy storage systems. In situ tomography of Li/LLZO/Li cells is carried out to track morphological transformations in Li metal electrodes. Machine learning enables tracking the lithium metal morphology during galvanostatic cycling. Nonuniform lithium electrode kinetics are observed at both electrodes during cycling. Hot spots in lithium metal are correlated with microstructural anisotropy in LLZO. Mesoscale modeling reveals that regions with lower effective properties (transport and mechanical) are nuclei for failure. Advanced visualization combined with electrochemistry represents an important pathway toward resolving non-equilibrium effects that limit rate capabilities of solid-state batteries.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Highly-Cyclable Room-Temperature Phosphorene Polymer Electrolyte Composites for Li Metal Batteries

Despite significant interest toward solid-state electrolytes owing to their superior safety in comparison to liquid-based electrolytes, sluggish ion diffusion and high interfacial resistance limit their application in durable and high-power density batteries. Here, a novel quasi-solid Li + ion conductive nanocomposite polymer electrolyte containing black phosphorous (BP) nanosheets is reported. The developed electrolyte is successfully cycled against Li metal (over 550 h cycling) at 1 mA cm -2 at room temperature. The cycling overpotential is dropped by 75% in comparison to BP-free polymer composite electrolyte indicating lower interfacial resistance at the electrode/electrolyte interfaces. Molecular dynamics simulations reveal that the coordination number of Li + ions around (trifluoromethanesulfonyl)imide (TFSI - ) pairs and ethylene-oxide chains decreases at the Li metal/electrolyte interface, which facilitates the Li + transport through the polymer host. Here, density functional theory calculations confirm that the adsorption of the LiTFSI molecules at the BP surface leads to the weakening of N and Li atomic bonding and enhances the dissociation of Li + ions. This work offers a new potential mechanism to tune the bulk and interfacial ionic conductivity of solid-state electrolytes that may lead to a new generation of lithium polymer batteries with high ionic conduction kinetics and stable long-life cycling.

2D materials↗

A New General Paradigm for Understanding and Preventing Li Metal Penetration through Solid Electrolytes

The use of lithium (Li) or sodium (Na) metal anodes together with highly ion-conductive solid electrolytes (SEs) could provide batteries with a step improvement in volumetric and gravimetric energy densities. Unfortunately, these SEs face significant technical challenges, in large part because Li and Na dendrites can penetrate through SEs, leading to short circuits. The ability of such a soft material (Li or Na metal) to penetrate through ceramic is surprising from the point of view of models widely used in the Li-battery field. We introduce a concept, new to the battery field, for preventing penetration of lithium dendrites through SEs by putting the SE surfaces into a state of residual compressive stress. For a sufficiently high compressive stress, cracks have difficulty forming, and cracks that do form are forced to close, inhibiting dendrite penetration. This approach is widely used to solve commercially important stress corrosion cracking problems in metals and static fatigue problems in ceramics and glasses (e.g., Gorilla Glass). However, the technique will not be useful for SEs if the Li-ion transport rate through a SE is substantially reduced when the SE is under compression. Our molecular dynamics calculations for Li-ion transport through a common SE demonstrate that the introduction of even very high residual compressive stresses (~10 GPa) has only a modest effect on Li-ion transport kinetics, suggesting that this approach is viable and capable of providing a new paradigm for developing high-performance and mechanically stable SEs.

25 ENERGY STORAGE↗

Evolution and Degradation Patterns of Electrochemical Cells Based on the Analysis of Interfacial Phenomena at Li Metal Anode/Electrolyte Interfaces

In this work, we report the results of a theoretical–computational analysis of the solid electrolyte interphase (SEI) growth and degradation dynamics occurring in lithium metal batteries during cycling. We use ab initio-kinetic Monte Carlo simulations to generate a synthetic data set, which is analyzed by machine learning methods. We aim to determine: (i) how modifications in interfacial interaction energies between solid electrolyte interphase (SEI) blocks and between Li ions and SEI facets impact the Coulombic efficiency (CE) of the battery and (ii) what factors, including reactions, microscopic transport, and other interfacial events, may lead to cell performance “failure” during prolonged charge and discharge cycles, signaled as a sharp decay in the CE over cycling. The demonstration of our approach is done on a cell including a Li metal surface interfacing with a previously introduced state-of-the-art electrolyte, and the idea can be applied to any electrochemical system. Outcomes include the identification of the leading chemical, physical, and structural variables causing cell failure and relating them to the electrolyte formulation, thus paving the way to future more refined analysis and electrolyte design.

batteries↗