Search NASA⌕ Search

SEARCH · Search NASA

Results for “PDMS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 73 records · Page 4

Adhesion and Contact Aging of Acrylic Pressure-Sensitive Adhesives to Swollen Elastomers

Fluid-infused (or swollen) elastomers are known for their antiadhesive properties. The presence of excess fluid at their surface is the main contributor to limiting contact formation and minimizing adhesion. Despite their potential, the mechanisms for adhesion and contact aging to fluid-infused elastomers are poorly understood beyond contact with a few materials (ice, biofilms, glass). This study reports on adhesion to a model fluid-infused elastomer, poly(dimethylsiloxane) (PDMS), swollen with silicone oil. The effects of oil saturation, contact time, and the opposing surface are investigated. Specifically, adhesion to two different adherents with comparable surface energies but drastically different mechanical properties is investigated: a glass surface and a soft viscoelastic acrylic pressure-sensitive adhesive film (PSA, modulus ~25 kPa). Adhesion between the PSA and swollen PDMS [with 23% (w/w) silicone oil] retains up to 60% of its value compared to contact with unswollen (dry) PDMS. In contrast, adhesion to glass nearly vanishes in contact with the same swollen elastomer. Adhesion to the PSA also displays stronger contact aging than adhesion to glass. Contact aging with the PSA is comparable for dry and unsaturated PDMS. Moreover, load relaxation when the PSA is in contact with the PDMS does not correlate with contact aging for contact with the dry or unsaturated elastomer, suggesting that contact aging is likely caused by chain interpenetration and polymer reorganization within the contact region. Closer to full saturation of the PDMS with oil, adhesion to the PSA decreases significantly and shows a delay in the onset of contact aging that is weakly correlated to the poroelastic relaxation of the elastomer. Additional confocal imaging suggests that the presence of a layer of fluid trapped at the interface between the two solids could explain the delayed (and limited) contact aging to the oil-saturated PDMS.

36 MATERIALS SCIENCE↗

Selective sequential infiltration synthesis of ZnO in the liquid crystalline phase of silicon-containing rod-coil block copolymers

The combination of block copolymer (BCP) thin film self-assembly and selective infiltration synthesis of inorganic materials into one BCP block provides access to various organic–inorganic hybrids. Here, we apply sequential infiltration synthesis, a vapor-phase hybridization technique, to selectively introduce ZnO into the organic microdomains of silicon-containing rod-coil diblock copolymers and a triblock terpolymer, polydimethylsiloxane (PDMS)-b-poly{2,5-bis[(4-methoxyphenyl)-oxycarbonyl]styrene} (PDMS-b-PMPCS) and PDMS-b-polystyrene-b-PMPCS (PDMS-b-PS-b-PMPCS), in which the PMPCS rod block is a liquid crystalline polymer. The in-plane cylindrical PDMS-b-PMPCS and core–shell cylindrical and hexagonally perforated lamellar PDMS-b-PS-b-PMPCS films were infiltrated with ZnO with high selectivity to the PMPCS. The etching contrast between PDMS, PS and the ZnO-infused PMPCS enables the fabrication of ZnO/SiO x binary composites by plasma etching and reveals the core–shell morphology of the triblock terpolymer.

36 MATERIALS SCIENCE↗

Water-stable direct air capture of CO 2 with microcapsules of task-specific ionic liquid and their electrothermal regeneration

Microcapsules of the task specific ionic liquid (TSIL) 1-ethyl-3-methylimidazolium 2-cyanopyrrolide [EMIM][2CNpyr] with composite polydimethylsiloxane (PDMS) shells were fabricated for use in CO 2 direct air capture (DAC) conditions. The TSIL was encapsulated using an oil-in-oil emulsion as a templating procedure through two different approaches. In the first approach, a PDMS-polyurea (PU) shell was constructed by interfacial polymerization, while in the second approach, a graphene oxide (GO)-PDMS shell was constructed by cross-linking GO sheets. The composition and structure of both capsule types were fully characterized, and their CO 2 DAC performance was evaluated by gravimetric and breakthrough analysis. Both capsules exhibited competitive capacities, with the PDMS-PU capsules and the GO-PDMS capsules reaching 0.75 mol kg −1 and 0.66 mol kg −1 , respectively. We further demonstrate that both capsule systems can be regenerated with complementary electrothermal methods. Microwave (MW) regeneration was used for the PDMS-PU capsules, effectively releasing absorbed CO 2 in less than an hour. Owing to the electrical conductivity of GO, GO-PDMS capsules were regenerated via radio frequency heating (RF). This work highlights the importance and opportunity of tuning solid–liquid composite performance for advanced applications, including direct air capture of carbon dioxide.

Al-Mahbobi, Luma [Texas A&M University, College St↗

Tuning Thermal and Mechanical Properties of Polydimethylsiloxane with Carbon Fibers

In order to meet the needs of constantly advancing technologies, fabricating materials with improved properties and predictable behavior has become vital. To that end, we have prepared polydimethylsiloxane (PDMS) polymer samples filled with carbon nanofibers (CFs) at 0, 0.5, 1.0, 2.0, and 4.0 CF loadings (w/w) to investigate and optimize the amount of filler needed for fabrication with improved mechanical properties. Samples were prepared using easy, cost-efficient mechanical mixing to combine the PDMS and CF filler and were then characterized by chemical (FTIR), mechanical (hardness and tension), and physical (swelling, thermogravimetric analysis (TGA), differential scanning calorimetry (DSC), and coefficient of thermal expansion) analyses to determine the material properties. We found that hardness and thermal stability increased predictably, while the ultimate strength and toughness both decreased. Repeated tension caused the CF-filled PDMS samples to lose significant toughness with increasing CF loadings. The hardness and thermal degradation temperature with 4 wt.% CF loading in PDMS increased more than 40% and 25 °C, respectively, compared with the pristine PDMS sample. Additionally, dilatometer measurements showed a 20% decrease in the coefficient of thermal expansion (CTE) with a small amount of CF filler in PDMS. In this study, we were able to show the mechanical and thermal properties of PDMS can be tuned with good confidence using CFs.

degradation temperature↗

Self-Replenishing Vascularized Fouling-Release Surfaces

Inspired by the long-term effectiveness of living antifouling materials, we have developed a method for the self-replenishment of synthetic biofouling-release surfaces. These surfaces are created by either molding or directly embedding 3D vascular systems into polydimethylsiloxane (PDMS) and filling them with a silicone oil to generate a nontoxic oil-infused material. When replenished with silicone oil from an outside source, these materials are capable of self-lubrication and continuous renewal of the interfacial fouling-release layer. Under accelerated lubricant loss conditions, fully infused vascularized samples retained significantly more lubricant than equivalent nonvascularized controls. Tests of lubricant-infused PDMS in static cultures of the infectious bacteria Staphylococcus aureus and Escherichia coli as well as the green microalgae Botryococcus braunii, Chlamydomonas reinhardtii, Dunaliella sauna, and Nannochloropsis oculata showed a significant reduction in biofilm adhesion compared to PDMS and glass controls containing no lubricant. Further experiments on vascularized versus nonvascularized samples that had been subjected to accelerated lubricant evaporation conditions for up to 48 h showed significantly less biofilm adherence on the vascularized surfaces. These results demonstrate the ability of an embedded lubricant-filled vascular network to improve the longevity of fouling-release surfaces.

Howell, C↗

Porous Polymer Structures with Tunable Mechanical Properties Using a Water Emulsion Ink

Recently, the manufacturing of porous polydimethylsiloxane (PDMS) with engineered porosity has gained considerable interest due to its tunable material properties and diverse applications. An innovative approach to control the porosity of PDMS is to use transient liquid phase water to improve its mechanical properties, which has been explored in this work. Adjusting the ratios of deionized water to the PDMS precursor during blending and subsequent curing processes allows for controlled porosity, yielding water emulsion foam with tailored properties. The PDMS-to-water weight ratios were engineered ranging from 100:0 to 10:90, with the 65:35 specimen exhibiting the best mechanical properties with a Young’s Modulus of 1.17 MPa, energy absorption of 0.33 MPa, and compressive strength of 3.50 MPa. This led to a porous sample exhibiting a 31.46% increase in the modulus of elasticity over a bulk PDMS sample. Dowsil SE 1700 was then added, improving the storage capabilities of the precursor. The optimal storage temperature was probed, with -60 °C resulting in great pore stability throughout a three-week duration. The possibility of using these water emulsion foams for paste extrusion additive manufacturing (AM) was also analyzed by implementing a rheological modifier, fumed silica. Fumed silica’s impact on viscosity was examined, revealing that 9 wt% of silica demonstrates optimal rheological behaviors for AM, bearing a viscosity of 10,290 Pa·s while demonstrating shear-thinning and thixotropic behavior. This study suggests that water can be used as pore-formers for PDMS in conjunction with AM to produce engineered materials and structures for aerospace, medical, and defense industries as sensors, microfluidic devices, and lightweight structures.

36 MATERIALS SCIENCE↗

Superstretchable, Self-Healing Polymeric Elastomers with Tunable Properties

Utilization of self-healing chemistry to develop synthetic polymer materials that can heal themselves with restored mechanical performance and functionality is of great interest. Self-healable polymer elastomers with tunable mechanical properties are especially attractive for a variety of applications. In this paper, a series of urea functionalized poly(dimethyl siloxane)-based elastomers (U-PDMS-Es) are reported with extremely high stretchability, self-healing mechanical properties, and recoverable gas-separation performance. Tailoring the molecular weights of poly(dimethyl siloxane) or weight ratio of elastic cross-linker offers tunable mechanical properties of the obtained U-PDMS-Es, such as ultimate elongation (from 984% to 5600%), Young's modulus, ultimate tensile strength, toughness, and elastic recovery. The U-PDMS-Es can serve as excellent acoustic and vibration damping materials over a broad range of temperature (over 100 °C). The strain-dependent elastic recovery behavior of U-PDMS-Es is also studied. After mechanical damage, the U-PDMS-Es can be healed in 120 min at ambient temperature or in 20 min at 40 °C with completely restored mechanical performance. Lastly, the U-PDMS-Es are also demonstrated to exhibit recoverable gas-separation functionality with retained permeability/selectivity after being damaged.

36 MATERIALS SCIENCE↗

Backbone Stitching in Bottlebrush Copolymer Mesodomains and the Impact of Side Chain Crystallization

We synthesized bottlebrush statistical copolymers (BSCPs) having poly­(ethylene oxide) (PEO) and poly­(dimethylsiloxane) (PDMS) side chains attached to a polynorbornene backbone. Small-angle X-ray scattering analysis showed that for densely grafted BSCPs, the scattering length density gradually transitions between the PEO and PDMS domains. For loosely grafted BSCPs, the polymer backbone formed a distinct mesodomain, with a lower electron and mass density than both the PEO and PDMS domains. The bottlebrush backbone essentially “stitches” the PEO and PDMS side chains, looping back and forth from the PEO to PDMS domains with the backbone segments oriented normal to the domain interfaces. Self-consistent field theory (SCFT) calculations validated the stitching of the backbone driven by the microphase separation of PEO and PDMS, along with a strong segmental order of the side chains in the melt. The reduced birefringence upon PEO crystallization suggests the disruption of the strong segmental order by the crystallization. Both the static intrinsic and the form birefringences of the BSCPs decreased upon PEO crystallization. Solid-state NMR confirmed the rigidity of PEO crystallites and the bottlebrush backbone. Self-assembly of BSCPs containing polyhedral oligomeric silsesquioxane (POSS) pendent groups was also evaluated by X-ray scattering, showing the formation of lamellar microdomains that inhibited POSS crystallization.

Hu, Mingqiu↗

Standalone Block Copolymer Nanoballoons: Decoupling Self-Assembly from Implementation in Nanomanufacturing

Here we report a facile method to produce isolatable hollow-core elastomeric vesicles, “nanoballoons”, prepared via block copolymer self-assembly in a polymer blend. Poly(isoprene-block-dimethylsiloxane) (PI-PDMS) diblock copolymers are blended with PDMS homopolymers (h-PDMS) as a “solvent” phase to template the self-assembly of PDMS-tethered vesicles with PI walls. The walls are subsequently crosslinked to yield mechanically stabilized elastomeric vesicles. The h-PDMS inner-core and matrix are separated from the vesicles by dialysis to yield the matrix-free nanoballoons. These objects, 0.3 – 1 μm in diameter, can be further reincorporated into a crosslinkable PDMS. Throughout the self-assembly, recovery, and reincorporation processes we apply several techniques including solvent dispersion/dynamic light scattering (DLS) measurements, transmission electron microscopy (TEM)/energy-dispersive X-ray spectroscopy (EDS), and small-angle X-ray scattering (SAXS) to provide a consilient body of evidence that the nanoballoon morphology is retained. Furthermore, this work presents advanced nanomanufacturing schema that illustrate the decoupling of the thermodynamic and dynamic factors that govern macromolecular self-assembly from the environment in which the self-assembled objects are deployed.

36 MATERIALS SCIENCE↗

Computational exploration of polymer nanocomposite mechanical property modification via cross-linking topology

Molecular dynamics simulations have been performed in order to study the effects of nanoscale filler cross-linking topologies and loading levels on the mechanical properties of a model elastomeric nanocomposite. The model system considered here is constructed from octa-functional polyhedral oligomeric silsesquioxane (POSS) dispersed in a poly(dimethylsiloxane) (PDMS) matrix. Shear moduli, G, have been computed for pure and for filled and unfilled PDMS as a function of cross-linking density, POSS fill loading level, and polymer network topology. The results reported here show that G increases as the cross-linking (covalent bonds formed between the POSS and the PDMS network) density increases. Further, G is found to have a strong dependence on cross-linking topology. The increase in shear modulus, G, for POSS filled PDMS is significantly higher than that for unfilled PDMS cross-linked with standard molecular species, suggesting an enhanced reinforcement mechanism for POSS. In contrast, in blended systems (POSS/PDMS mixture with no cross-linking) G was not observed to significantly increase with POSS loading. Finally, we find intriguing differences in the structural arrangement of bond strains between the cross-linked and the blended systems. In the unfilled PDMS the distribution of highly strained bonds appears to be random, while in the POSS filled system, the strained bonds form a net-like distribution that spans the network. Such a distribution may form a structural network 'holding' the composite together and resulting in increases in G compared to an unfilled, cross-linked system. These results are of importance for engineering of new POSS-based multifunctional materials with tailor-made mechanical properties.

36 MATERIALS SCIENCE↗

A laser ultrasound transducer using carbon nanofibers–polydimethylsiloxane composite thin film

The photoacoustic effect has been broadly applied to generate high frequency and broadband acoustic waves using lasers. However, the efficient conversion from laser energy to acoustic power is required to generate acoustic waves with high intensity acoustic pressure (>10 MPa). In this study, we demonstrated laser generated high intensity acoustic waves using carbon nanofibers–polydimethylsiloxane (CNFs-PDMS) thin films. The average diameter of the CNFs is 132.7 ± 11.2 nm. The thickness of the CNFs film and the CNFs-PDMS composite film is 24.4 ± 1.43 μm and 57.9 ± 2.80 μm, respectively. The maximum acoustic pressure is 12.15 ± 1.35 MPa using a 4.2 mJ, 532 nm Nd:YAG pulsed laser. The maximum acoustic pressure using the CNFs-PDMS composite was found to be 7.6-fold (17.62 dB) higher than using carbon black PDMS films. Furthermore, the calculated optoacoustic energy conversion efficiency K of the prepared CNFs-PDMS composite thin films is 15.6 × 10{sup −3 }Pa/(W/m{sup 2}), which is significantly higher than carbon black-PDMS thin films and other reported carbon nanomaterials, carbon nanostructures, and metal thin films. The demonstrated laser generated high intensity ultrasound source can be useful in ultrasound imaging and therapy.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Process Development for Removal of Siloxanes from ISS Atmosphere

Dimethylsilanediol (DMSD) has been identified as a problematic organic contaminant aboard the ISS. This contaminant was initially identified in humidity condensate and in the Water Processor Assembly (WPA) product water in 2010 when routine water quality monitoring an increasing total organic carbon (TOC) trend in the WPA product water. Although DMSD is not a crew health hazard at the levels observed in the product water, it can degrade the WPA catalytic reactor's effectiveness and cause early replacement of Multifiltration Beds. DMSD may also degrade the performance of the Oxygen Generation System (OGS) which uses the WPA product water for electrolysis. An investigation into the source of DMSD has determined that polydimethylsiloxane (PDMS) compounds are likely hydrolyzing in the Condensing Heat Exchangers (CHX) to form DMSD. PDMS compounds are prevalent aboard ISS from a variety of sources, including crew hygiene products, adhesives, caulks, lubricants, and various nonmetallic materials. PDMS compounds are also known to contribute to CHX hydrophilic coating degradation by rendering it hydrophobic and therefore adversely affecting its ability to effectively transmit water to the condensate bus. Eventually this loss in performance results in water droplets in the air flow exiting the CHX, which may lead to microbial growth in the air ducts and may impact the performance of downstream systems. Several options have been evaluated to address these concerns. Modifications to the Water Processor Multifiltration Beds and Catalytic Reactor for removal of DMSD were not considered viable, and did not address the issue with PDMS compound degradation of the CHX coating. Design concepts are now in development for removing PDMS compounds from the air stream before they can reach the CHX coating, thus preventing coating degradation and hydrolysis of the PDMS compounds to DMSD. This paper summarizes the current status of the effort to treat these contaminants on ISS.

Carter, Layne↗

Surface Monitoring of CFRP Structures for Adhesive Bonding

Adhesive bonding of composite materials requires reliable monitoring and detection of surface contaminants to assure robust and durable bonded structures. Surface treatment and effective monitoring prior to bonding is essential in order to obtain a surface free from contaminants that may degrade structural performance. Two techniques which monitor the effectiveness of the laser surface treatment of carbon fiber reinforced polymer (CFRP) materials are being investigated: laser induced breakdown spectroscopy (LIBS) and optically stimulated electron emission (OSEE). The applicability of LIBS to detect silicone contaminants on CFRP composites is studied using ~35 ns Nd:YAG laser pulses at 355 nm with a pulse energy of 45 mJ. The LIBS regime in which pulse energies are < 100 mJ is referred to as mLIBS. CFRP surfaces were contaminated with polydimethylsiloxane (PDMS), a major component of silicone based mold release agents. The presence of PDMS is found by inspecting the Si I emission line at 288.2 nm. Untreated CFRP samples and CFRP contaminated with PDMS were tested. The PDMS areal density ranged from 0.36 Â+/- 0.04 to 0.51 Â+/- 0.16 mg/cm2. The results demonstrate the successful detection of PDMS on CFRP using mLIBS. In addition, OSEE was used to measure CFRP surface cleanliness pre- and post-treatment by laser ablation on specimens contaminated with PDMS coatings from 8 nm to 1311 nm in thickness. The results showed a significant increase in the OSEE photocurrent after laser surface treatment.

Ledesma, Rodolfo↗

Tailored Silicone Network Architecture for Ultimate Mechanical Reinforcement

Hydrosilylation cured silicone elastomers are subject to reaction inefficiency, leading to incomplete and non-uniform crosslink networks, restricting the potential of mechanical reinforcement. This work investigates pre-synthesized, functional PDMS architectures as additives to improve ultimate mechanical performance relative to conventional single-step curing. Three custom, functional structures were prepared: a partially crosslinked PDMS scaffold (Structure A), a bottle-brush PDMS (Structure B), and a star-shaped PDMS derived from an MQ resin (Structure C). Rheological characterization was used to identify the ultimate design space and proper stoichiometric ratio for Structure A, and confirm successful formation of all structures for suitable incorporation into a base silicone formulation at 30wt%. Mechanical tests indicated that all three structures increased in ultimate tensile strength relative to their single-step counterparts, with Structure A providing additional improvements to toughness (432 vs. 258 kJ/m3) and ultimate elongation (158 vs. 115%). Furthermore, Structure B remained very soft in the unfilled state, while Structure C provided hardness (23 vs. 18 Shore A) and stiffness (780 vs. 420 kPa Young’s modulus) increases. In silica filled systems, Structure A retained increased strength but reduced elongation, while Structure B indicated strong reinforcement in terms of strength, toughness, and stiffness. Thermal analysis on the cure profiles of these materials suggested that pre-formation of network architectures enable a more complete reaction than a single-step process (15.9 vs. 15.1 J/g). Ultimately, these results indicate that tailoring PDMS architecture before the final cure can improve ultimate mechanical properties via improved network development in silicone elastomers. Furthermore, this work offers a promising strategy for designing higher-performance, more tunable silicone formulations.

36 MATERIALS SCIENCE↗

Investigation of porous polydimethylsiloxane structures with tunable properties induced by the phase separation technique

This article reports the fabrication and characterization of porous polydimethylsiloxane (PDMS) structures developed by the solvent evaporationinduced phase separation technique. Here, ternary systems containing water/ tetrahydrofuran (THF)/PDMS with various concentrations are produced to form a stable solution. The porous PDMS structures are formed by removing the solvent (THF) and nonsolvent (water) phases during the stepping heat treatment procedure. The analytical ternary phase diagram is constructed based on the thermodynamic equilibrium state in the polymer solution to explain the stable/unstable formulations and the possible composition change path. The results show that the isolated pores with the adjustable pore size ranging from 330 to 1900 μm are obtained by tuning the water to the THF ratio. The mechanical properties of the porous PDMS structures are determined by conducting the tensile tests on the prepared dog bone-shaped specimens. A wide range of elastic modulus ranging between 0.49 and 1.05 MPa was achieved without affecting the density of the porous sample by adjusting the solvent and non-solvent content in the solution. It is shown that the flexibility of the porous structures can be improved by reducing the ratio of water to THF and decreasing the PDMS content. The porosity measurements reveal that the PDMS concentration is the major phase controlling the porosity of the structure, while the effect of water/THF is negligible.

42 ENGINEERING↗

Temperature controlled transformations of giant unilamellar vesicles of amphiphilic triblock copolymers synthesized via microfluidic mixing

We report on a simple approach for synthesis of temperature-responsive giant unilamellar vesicles (GUVs) from poly(N-vinylcaprolactam) 15 -block-poly(dimethylsiloxane) 65 -block-poly(N-vinylcaprolactam) 15 (PVCL 15 -PDMS65-PVCL 15 ) triblock copolymer and non-temperature responsive small and giant vesicles from novel poly(N-vinylpyrrolidone)-block-poly(dimethylsiloxane)-block-poly(N-vinylpyrrolidone) (PVPON 15 -PDMS 65 -PVPON 15 and PVPON 6- PDMS 30- PVPON 6 ) triblock copolymers using microfluidic mixing at 25 °C. We show that temperature-responsive PVCL 15 -PDMS 65- PVCL 15 GUVs with the average diameter of 1.4 ± 0.2 µm while being stable at room temperature for at least 14 days, transformed irreversibly into small vesicles of 168 ± 40 nm after incubation of their aqueous solution at 42 °C for 24 h. We hypothesized that this transformation is induced by local compressive stresses of the vesicle membrane due to the collapse of PVCL blocks above the copolymer lower critical solution temperature (LCST) leading to the decrease of the vesicle membrane thickness. Consequently, we found that the temperature-induced size transformation of the PVCL-based GUVs at 42°C can be suppressed by substituting PVCL with its hydrophilic homologue PVPON, or by suppressing the PVCL's LCST behavior through hydrogen-bonding with tannic acid molecules. In the former case, novel PVPON n -PDMS m -PVPON n triblock copolymers (n = 15, m = 65 and n = 6, m = 30) assemble into vesicles stable from 25 °C to 55 °C as confirmed by optical and electron microscopy, dynamic light scattering (DLS) and small-angle neutron scattering (SANS). In the latter, hydrogen bonding interactions of PVCL with the polyphenol tannic acid (TA) at room temperature resulted in stable PVCL-based GUVs at 42°C as confirmed by optical, electron, and atomic force microscopies. We also found that physical crosslinking of the PVCL corona through hydrogen bonding with TA in PVCL 15- PDMS 65- PVCL 15 GUVs will delay their low pH-induced degradation at 37°C by 48 h compared to non-modified GUVs. Our findings open opportunities for the development of temperature-regulated stable micro-vehicles that would change their structural characteristics in the physiologically relevant temperature range from 25 to 42°C and can be utilized for cell mimicking studies. The developed GUVs also have potential in theranostic drug delivery as substitutes for polymer microcapsules and lipid microbubbles as well as for stimuli-triggered sensing, protection, and rapid response in an aqueous environment.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Poly(dimethylsiloxane- b -methyl methacrylate): A Promising Candidate for Sub-10 nm Patterning

We report herein the modular synthesis and nanolithographic potential of poly(dimethylsiloxane-block-methyl methacrylate) (PDMS-b-PMMA) with self-assembled domains approaching sub-10 nm periods. A straightforward and modular coupling strategy, optimized for low molecular weight diblocks and using copper-catalyzed azide–alkyne “click” cycloaddition, was employed to obtain a library of PDMS-b-PMMA and poly(dimethylsiloxane-block-styrene) (PDMS-b-PS) diblock copolymers. Flory–Huggins interaction parameters, determined from small-angle X-ray scattering experiments, were high for PDMS-b-PMMA (χ ~ 0.2 at 150 °C), suggesting this diblock copolymer system has promise for sub-10 nm lithographic applications when compared to the corresponding PDMS-b-PS diblock copolymers (χ ~ 0.1 at 150 °C). Furthermore, performance evaluation in thin film self-assembly experiments allowed domain periods as small as 12.1 nm to be obtained, which is among the smallest highly ordered nanoscale patterns reported hitherto for thermally annealed materials.

36 MATERIALS SCIENCE↗

Polystyrene-block-Polydimethylsiloxane as a Potential Silica Substitute for Polysiloxane Reinforcement

We report here on microphase-separated poly(styrene-block-dimethylsiloxane) (PS-b-PDMS) as a reinforcing filler in PDMS thermosets that overcomes the long-standing problem of aging in the processing of silica-reinforced silicone. Surprisingly, PS-b-PDMS reinforced composites display comparable mechanical performance to silica-modified analogs, even though the modulus of PS is much smaller than that of silica and there is no evidence of percolation with respect to the rigid PS domains. We have found that a few unique characteristics contribute to the reinforcing performance of PS-b-PDMS. The strong self-assembly behavior promotes batch-to-batch repeatability by having well-dispersed fillers. The structure and size of the fillers depend on the loading and characteristics of both filler and matrix, along with the shear effect. The reinforcing effect of PS-b-PDMS is mostly brought by the entanglements between the corona layer of the filler and the matrix, rather than the hydrodynamic reinforcement of the PS phase.

36 MATERIALS SCIENCE↗