Search NASA⌕ Search

SEARCH · Search NASA

Results for “Silicon Carbide Composite Cladding”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 73 records · Page 4

Thermal diffusivity and thermal conductivity of SiC composite tubes: the effects of microstructure and irradiation

Cladding thermal conductivity is an important physical property in assessing the performance of silicon carbide (SiC)-cladded fuels for nuclear reactors. However, there is a significant lack of reliable data, particularly for irradiated materials, because the geometry complicates the measurement. This study investigates the thermal diffusivity of coupons with a curvature, machined from SiC fiber–reinforced SiC matrix composite tubes, with and without neutron irradiation under light water reactor–relevant temperature and dose conditions. The tested materials included full composite and duplex SiC composite tubes. The measurements were conducted using a modern flash diffusivity apparatus. The analyzed area on the specimen during diffusivity testing was reduced for improved measurement accuracy due to sample curvature. Post-irradiation measurements showed that the effects of neutron irradiation on thermal conductivity (e.g. thermal defect resistivity) are different between SiC composite plates versus tubes. The difference was explained by higher matrix density of the tube than the plate. This study provides reliable thermal properties of prototypic SiC composite tubes useful for fuel performance modeling of SiC-based cladding.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

SiC/SiC Cladding Materials Properties Handbook

When a new class of material is considered for a nuclear core structure, the in-pile performance is usually assessed based on multi-physics modeling in coordination with experiments. This report aims to provide data for the mechanical and physical properties and environmental resistance of silicon carbide (SiC) fiber–reinforced SiC matrix (SiC/SiC) composites for use in modeling for their application as accidenttolerant fuel cladding for light water reactors (LWRs). The properties are specific for tube geometry, although many properties can be predicted from planar specimen data. This report presents various properties, including mechanical properties, thermal properties, chemical stability under normal and offnormal operation conditions, hermeticity, and irradiation resistance. Table S.1 summarizes those properties mainly for nuclear-grade SiC/SiC composites fabricated via chemical vapor infiltration (CVI). While most of the important properties are available, this work found that data for the in-pile hydrothermal corrosion resistance of SiC materials and for thermal properties of tube materials are lacking for evaluation of SiC-based cladding for LWR applications.

36 MATERIALS SCIENCE↗

High spatial resolution thermal conductivity mapping of SiC/SiC composites

Herein, silicon carbide (SiC) ceramic matrix composites are being investigated as a new generation of fuel cladding materials due to its higher accident tolerance compared to Zircaloy. Characterization of the thermal conductivity of SiC constituents and their interfaces and interphases in SiC/SiC composites is needed as inputs to models of cladding performance. We used time-domain thermoreflectance (TDTR) to map the thermal conductivity with a spatial resolution of 2 µm. The SiC/SiC composite is comprised of Hi-Nicalon Type S fibers in a matrix made by chemical vapor infiltration (CVI matrix). The interphase material is a pyrolytic carbon/SiC multilayer. We report thermal conductivity maps of the SiC fiber and SiC matrix at temperatures of 25 °C, 90 °C, 164 °C, and 250 °C. The fiber has a uniform and isotropic thermal conductivity of 22 W m -1 K -1 at 25 °C; the thermal conductivity of fiber is approximately independent of temperature. The matrix thermal conductivity is not uniform and varies from 50 to 120 W m -1 K -1 at 25 °C; the thermal conductivity of the matrix scales approximately with the inverse of the square root of temperature, i.e., ∝ 1/T 1/2 . The thermal conductivity of the interphase at room temperature is 6 W m -1 K -1 . The calculated spatially averaged thermal conductivity of this SiC/SiC composite at 1000°C is 29 W m -1 K -1 .

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Understanding of a Novel Irradiation-induced Nanostructuring Process in SiC layer of TRISO fuel particles via Transmission Electron Microscopy

Metallic fission products are found to transport through the SiC layer of the tristructural isotropic (TRISO) nuclear fuel particle and various studies have been undertaken to understand the transport behavior [1, 2]. While the grain boundaries in SiC acts as a primary pathway to dissipate fission products in the form of multi-phased complex compounds, intragranular fission product precipitation has always been observed. Research on neutron irradiation damage tolerance of silicon carbide (SiC) and its composites, used in TRISO fuel, light water reactors (LWR) fuel cladding etc., has traditionally ignored the irradiation-induced “polymorphism” of SiC. In the post-irradiation advanced microscopy effort at Idaho National Laboratory, it has been recently discovered that the intragranular precipitation of fission products in SiC layer of TRISO coated fuels takes place via a dual step nucleation mechanism that involves cubic (?) ?hexagonal (?) SiC polymorphic transition, and subsequent metamorphosis of ?-SiC into fission product precipitates, as shown in Figure 1 [3]. This precipitation behavior cannot be explained by any reported nucleation mechanism. The extent of this precipitation has been observed to be influenced by the nature of the neutron irradiation induced damage structures. These damage structures (e.g., defect morphology and density) are also indicative of the irradiation temperature and neutron fluence levels experimented by the individual TRISO particles. The distinction of neutron irradiation damage structures as a function of the fuel kernel type, burn up level and fabrication histories of TRISO coated particles from the Advanced Gas reactor (AGR-1 and AGR-2) experiments has been examined and compared. This discovery not only adds new fundamental understanding of physical behavior of polymorphic ceramics under irradiation, but also provides the following beneficial traits for high temperature applications. 1) Since the extent of precipitation of the desired phase is directly dependent on the amount of precursor phase, the volume fraction of desired phase can be easily controlled by irradiation parameters. This eliminates the conventional limitation of volume fraction of a desired phase in the system as outlined by the phase diagram of the specific system. 2) Most of the precipitate-strengthened materials for high temperature applications suffer from degradation of size and shape of precipitate upon prolonged thermal exposures. But, precipitates are confined to the shape and size of the morphological template of surrogate phase (e.g. a Pd silicide precipitate is confined by the ?-SiC as shown in Figure 1(c)) in the present nucleation pathway. Hence, there is no possibility of desired phase to undergo any morphological degradation at high temperature that eventually will extend the lifetime of these materials at high temperature.

42 ENGINEERING↗

Post Irradiation Examination of SiC Tube Subjected to Simultaneous Irradiation and Radial High Heat Flux

Silicon carbide (SiC) based composite is considered among leading candidate materials for accident tolerant fuel (ATF) cladding in light water reactors (LWRs) because of its outstanding irradiation and oxidation resistance, as well as low neutron absorption. Under normal operation conditions, the synergism between neutron irradiation and a high radial heat flux though the cladding thickness is expected to produce significant stress. This stress is attributed to a significant through-thickness temperature gradient and the resulting differential swelling strain due the highly temperature-dependent point-defect swelling of SiC. Although modeling of the in-pile stress state of SiC cladding has been conducted using finite element analysis, the analysis is challenging because of the complex stress state that depends upon swelling, irradiation creep, and thermal conductivity, all of which are both temperature and dose-dependent. These integral models have not yet been verified by experiments. In order to experimentally validate the multi-physics thermo-mechanical models of ATF SiC cladding during operation, SiC tube specimens have been irradiated under a high radial heat flux. This paper reports preliminary results from the post-irradiation examination (PIE) in on-going project supported by the U.S. Department of Energy's Nuclear Science User Facility program. The objectives of the PIE are (1) determination of the irradiation temperature distribution within the tube specimens, and (2) evaluation of the state and magnitude of the stress within the tube specimens arising from the temperature gradient. This paper mainly presents findings for objective (1)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Pulsed Infrared Thermography Nondestructive Imaging of SiC-SiC f Composite Cladding Architectures; Understanding the Performance of SiC-SiC f Composite Cladding Architectures with Cr Coating in Normal Operating and Accident Conditions in LWRs and Advanced Reactors

SiC-SiC f composites, consisting of silicon carbide fibers embedded in a silicon carbide matrix, are advanced materials with high thermal conductivity, temperature stability, and resistance to radiation damage. Traditional methods for quality control of fabricated SiC-SiC f composites involve nondestructive evaluation (NDE) with X-ray computed tomography (XCT). However, XCT imaging of typical SiC-SiC f structures for cladding applications can involve several hours. In this project, we investigate an alternative approach to NDE of SiC-SiC f composites that involves rapid (on the order of seconds) imaging with Pulsed infrared thermography (PIT). PIT images of a planar SiC-SiC f specimen show the structure of the surface monolith layer and internal SiC f structures. The capability of PIT imaging in visualizing SiC f structures is qualitatively confirmed by observing similarity in the PIT and X-ray transmission images of the same specimen. Computer vision analysis of defects in the PIT image of the monolith was performed with thresholding followed by topological structural analysis that computed geometric descriptors, including major/minor axes of fitted ellipses, area, perimeter, Feret diameter, circularity, roundness, and solidity.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

EBSD Characterization of Tubular Cladding Plasticity after Bend Testing: A Feasibility Study

The Light Water Reactor Sustainability (LWRS) Program developed a bend test method for tubular samples during FY12. The purpose of this report is to provide details of the Electron Backscattered Diffraction (EBSD) measurements performed on the various sample sets to provide a comparative baseline of the impact that the silicon carbide ceramic matrix composites (SiC-CMC) sleeves had on the deformation and plasticity properties of the Zircaloy-4 (Zr-4) cladding tube.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Delivery of completed irradiation vehicles and the quality assurance document to the High Flux Isotope Reactor for irradiation

This report details the initial fabrication and delivery of two Fuel Cycle Research and Development (FCRD) irradiation capsules (ATFSC01 and ATFSC02), with associated quality assurance documentation, to the High Flux Isotope Reactor (HFIR). The capsules and documentation were delivered by September 30, 2015, thus meeting the deadline for milestone M3FT-15OR0202268. These irradiation experiments are testing silicon carbide composite tubes in order to obtain experimental validation of thermo-mechanical models of stress states in SiC cladding irradiated under a prototypic high heat flux. This document contains a copy of the completed capsule fabrication request sheets, which detail all constituent components, pertinent drawings, etc., along with a detailed summary of the capsule assembly process performed by the Thermal Hydraulics and Irradiation Engineering Group (THIEG) in the Reactor and Nuclear Systems Division (RNSD). A complete fabrication package record is maintained by the THIEG and is available upon request.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Integral Heat Transfer Test Method for Determining Thermal Resistance of Silicon Carbide Cladding and Liquid Tin System at Elevated Temperatures - Master's Thesis Presentation University of Idaho

Presentation for master's work at University of Idaho discussing Integral Heat Transfer Test Method for Determining Thermal Resistance of Silicon Carbide Cladding and Liquid Tin System at Elevated Temperatures. Presentation covers slight literature review results/previous work, discussions on system design and approach for thermal property measurement of SiC composite and Tin system, modeling efforts, and results.

36 - MATERIALS SCIENCE↗

Pressure Loading with In-Situ Permeability Measurement of SiC Ceramic Matrix Composite Tube

Silicon carbide fiber in a silicon carbide matrix composite (SiC-SiC) has been actively researched as a potential structural material to be used in advanced high temperature gas reactors (HTGR) and as an accident tolerant cladding material for light water reactors (LWR). This ceramic composite material demonstrates desirable properties for use in nuclear reactor core that include retention of strength from ambient to LWR and HTGR operating and accident temperatures and stability under neutron radiation. However, the ceramic composite material must be designed to meet all the necessary, application driven requirements before it could be implemented in a reactor design. As one of the requirements for a fuel cladding material, the composite has to maintain high level of impermeability as to retain fission gases throughout the fuel cycle. General Atomics (GA) had previously reported results on permeability levels obtained by CVI produced SiC-SiC composites. It has been determined that for LWR size cladding tube that is 51 mm long the permeability allocation equivalent to currently used claddings is 7.3 E-10 atm*cc/sec. With high level of attention to possible sources of leaks in a test setup, it has been demonstrated that a CVI SiC-SiC composites produced by GA can achieve a leak rate of 1 E-12 atm*cc/sec, and therefore it meets the permeability allocation for a fuel cladding. Further study showed that a particular SiC-SiC composite tube can remain impermeable after being pressure loaded well above LWR normal operating conditions. In the study done by Deck et al., hoop stress was applied to a composite tube using pressure load on the inside surface in a load-unload stepwise sequence with increasing maximum applied stress at each step and measuring permeability between steps. The tested composite comprised of 70% thickness of SiC-SiC composite which provides fracture toughness and bears a majority of the applied stress and a 30% thickness of monolithic SiC layer on the outside surface to provide an impermeable barrier. The composite remained impermeable up to internal pressure of 56 MPa which is more than 2.5 times greater than a typical pressure at the end of life in a fuel rod.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Microstructural evolution of a silicon carbide-carbon coated nanostructured ferritic alloy composite during in-situ Kr ion irradiation at 300°C 450°C

This work focuses on irradiation behaviors of a novel silicon carbide and carbon coated nanostructured ferritic alloy (SiC-C@NFA) composite for potential applications as a cladding and structural material for next generation nuclear reactors. The SiC-C@NFA samples were irradiated with 1 MeV Kr ions up to 10 dpa at 300 and 450 °C. Microstructures and defect evolution were studied in-situ at the IVEM-Tandem facility at Argonne National Laboratory. The effects of ion irradiation on various phases such as α-ferrite matrix, (Fe,Cr) 7 C 3 , and (Ti,W)C precipitates were evaluated. The α-ferrite matrix showed a continuous increase in dislocation density along with spatial ordering of dislocation loops (or loop strings) at >5 dpa. The size of the dislocation loops at 450 °C was larger than that at 300 °C. The nucleation and growth of new (Ti,W)C precipitates in α-ferrite grains were enhanced with the ion dose at 450 °C. This study provides new insight into the irradiation resistance of the SiC-C@NFA system.

(FeCr)(7)C-3↗

Failure Characterization of SiC/SiC Woven Tubular Composites

In the nuclear power industry, fuel-pellet swelling and pellet-cladding interactions induce complex stress states in the cladding material. SiCf/SiC composite tubes (SiC fibers embedded in SiC matrix) have been proposed as a candidate material for the cladding material. SiCf/SiC has high resistance to radiation-damage, low neutron crosssection and good damage tolerance in extreme radiation environments. The drawback of using SiC is the brittle nature of the material. However, using SiC in a woven ceramic matrix composite introduces a pseudoductility effect without catastrophic failure. In the current work woven, tubular cladding with continuous silicon carbide fibers and a high-purity stoichiometric silicon-carbide matrix was compared with monolithic silicon carbide samples.

Nance, James↗

Investigating Grain Structure and Microcracking in SiCf-SiCm Composites Using 4D-STEM

Silicon carbide (SiC) fiber-reinforced SiC matrix composites (SiCf-SiCm) are promising materials for accident-tolerant fuel (ATF) cladding in light water reactors. This paper, using four-dimensional scanning transmission electron microscopy (4D-STEM), studied the microstructure of SiCf-SiCm at nanoscale and provided grain statistics at the CVI/fiber region. Here, the results reveal that CVI region mainly contain irregular sub-micron grains (115 nm to 1800 nm) with a preferred orientation, while the fiber region has nano equiaxed grains (21 nm to 78 nm) with random orientations. Centered dark field imaging over the fiber regions verified the grain size measurement by 4D-STEM. Through 4D-STEM virtual dark field imaging and orientation mapping, intragranular propagation was identified as the fracture mechanism for a microcrack observed within the CVI region. The amorphous pyrolytic carbon layer was also shown to effectively arrest the microcrack.

4D-STEM↗

SiC-CMC-Zircaloy-4 Nuclear Fuel Cladding Performance during 4-Point Tubular Bend Testing

The U.S. Department of Energy Office of Nuclear Energy (DOE NE) established the Light Water Reactor Sustainability (LWRS) program to develop technologies and other solutions to improve the reliability, sustain the safety, and extend the life of current reactors. The Advanced LWR Nuclear Fuel Development Pathway in the LWRS program encompasses strategic research focused on improving reactor core economics and safety margins through the development of an advanced fuel cladding system. Recent investigations of potential options for “accident tolerant” nuclear fuel systems point to the potential benefits of silicon carbide (SiC) cladding. One of the proposed SiC-based fuel cladding designs being investigated incorporates a SiC ceramic matrix composite (CMC) as a structural material supplementing an internal Zircaloy-4 (Zr-4) liner tube, referred to as the hybrid clad design. Characterization of the advanced cladding designs will include a number of out-of-pile (nonnuclear) tests, followed by in-pile irradiation testing of the most promising designs. One of the out-of-pile characterization tests provides measurement of the mechanical properties of the cladding tube using four point bend testing. Although the material properties of the different subsystems (materials) will be determined separately, in this paper we present results of 4-point bending tests performed on fully assembled hybrid cladding tube mock-ups, an assembled Zr-4 cladding tube mock-up as a standard and initial testing results on bare SiC-CMC sleeves to assist in defining design parameters. The hybrid mock-up samples incorporated SiC-CMC sleeves fabricated with 7 polymer impregnation and pyrolysis (PIP) cycles. To provide comparative information; both 1- and 2-ply braided SiC-CMC sleeves were used in this development study. Preliminary stress simulations were performed using the BISON nuclear fuel performance code to show the stress distribution differences for varying lengths between loading points and clad configurations. The 2-ply sleeve samples show a higher bend momentum compared to those of the 1-ply sleeve samples. This is applicable to both the hybrid mock-up and bare SiC-CMC sleeve samples. Comparatively both the 1- and 2-ply hybrid mock-up samples showed a higher bend stiffness and strength compared with the standard Zr-4 mock-up sample. The characterization of the hybrid mock-up samples showed signs of distress and preliminary signs of fraying at the protective Zr-4 sleeve areas for the 1-ply SiC-CMC sleeve. In addition, the microstructure of the SiC matrix near the cracks at the region of highest compressive bending strain shows significant cracking and flaking. The 2-ply SiC-CMC sleeve samples showed a more bonded, cohesive SiC matrix structure. This cracking and fraying causes concern for increased fretting during the actual use of the design. Tomography was proven as a successful tool to identify open porosity during pre-test characterization. Although there is currently insufficient data to make conclusive statements regarding the overall merit of the hybrid cladding design, preliminary characterization of this novel design has been demonstrated.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Thermo-mechanical analysis of SiC and FeCrAl cladding behavior under a loss-of- coolant accident

Alternative cladding materials have been proposed to replace the currently used zirconium (Zr)-based alloys, in order to improve the accident tolerance of light water reactor (LWR) fuel. Of these materials, there is a particular focus on iron-chromium-aluminum (FeCrAl) alloys and silicon carbide composite materials that exhibit much slower oxidation kinetics in high-temperature st eam than Zr-alloys. This behavior should decrease the energy release due to oxidation and allow the cladding to remain integral longer in the presence of high temperature steam, making accident mitigation more likely.

36 MATERIALS SCIENCE↗

Neutronic Consideration of TREAT Facility Fuel SiC Recladding

The Transient Reactor Test (TREAT) Facility is an air-cooled reactor composed of graphite-urania fuel encapsulated in zirconium alloy canisters and surrounded by ~2 ft (~61 cm) of nuclear grade graphite. The primary role of TREAT is to provide in-pile nuclear-heated safety research via transient testing [1]. Benchmark efforts have demonstrated sensitivity of TREAT neutronics models to graphite cross section data and key neutron poisons found in the fuel assemblies [2]. During fabrication of TREAT fuel assemblies, a small concentration of boron was inadvertently introduced with variable concentration into the aggregate of fuel blocks prepared for TREAT use. The concentration of boron, and its respective uncertainty, represent the most sensitive component in a neutronics study; unfortunately, nothing can be done to reduce or otherwise mitigate its impact. Hydrogen in the fuel blocks reduces the mean free path of the core and its true quantity and uncertainty is approximated. The hydrogen remains from pitch binder used in the fuel fabrication process and was not completely released due to incomplete fuel graphitization. Destructive fuel testing is necessary to quantify the actual hydrogen content and to improve benchmark model quality. A third neutron poison of some significance is the hafnium impurity in the Zircaloy-3 (Zry-3) assembly cladding. The quantity of hafnium is expected to be within nominal manufacturing limits for nuclear grade zircaloy. Recladding the fuel assemblies with material that is less neutron absorbing is expected to benefit reactor neutron economy. Moreover, TREAT’s total transient energy is restricted based on the rate of Zry-3 oxidation in TREAT’s air coolant environment. Hence, cladding with more benign air reaction kinetics could dramatically uprate the facility’s experimental capability. Silicon carbide (SiC) has been proposed as a candidate material for recladding TREAT assemblies, as SiC/SiC demonstrate favorable properties within nuclear environments [3]. The current operational limits of TREAT are restricted by the oxidation of Zry-3. Change of the cladding to SiC could feasibly double the current temperature limitation. Recladding opportunities allow for previously damaged fuel assemblies to be returned to service, as Zry-3 is not commercially available. The initial effort required to consider proceeding with any recladding effort is to neutronically characterize key reactor parameters while replacing Zry-3 with SiC. A characterization summary, with respective results, is provided herein.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

A Standardized Analysis Process Using Digital Image Correlation to Calculate In Situ Cladding Strain from Modified Burst Tests for Fuel Performance Code Validation

Historical data collection on nuclear fuel cladding materials has focused on generating a statistically significant amount of data to assess the material and its failure behavior. Furthermore, data generated to support material model and failure criteria development were previously posttest evaluations, so a large number of tests was required to gain new understanding. A way to expedite this process is to develop techniques capable of generating large, high-fidelity data sets from a single test with lower uncertainty or quantified uncertainty. One such example of this approach is Oak Ridge National Laboratory’s use of modified burst tests (MBTs) to analyze the mechanical behavior and failure conditions of cladding during a simulated reactivity-initiated accident (RIA). Each test incorporates digital image correlation (DIC) analysis techniques that are used to assess the accumulated strain in situ, as well as eventual cladding failure. This work has been fruitful in defining strain-to-failure conditions for materials like silicon carbide (SiC) fiber–reinforced/SiC matrix composite tubes (SiC/SiC), iron-chromium-aluminum (FeCrAl) alloy tubes, and chromium-coated Zircaloy-4 tubes. However, there are numerous DIC software available, including open-source and proprietary software. The different DIC software use various algorithms to process images and calculate displacement values. Using these different software and algorithms can lead to varying results, and perhaps larger-than-expected uncertainties. In the present study, previously published MBT data encompassing a variety of test conditions were reanalyzed with two different DIC software to assess the variance in the calculated strain results. The data consisted of SiC/SiC, FeCrAl, and chromium-coated Zircaloy-4 tubes. Plots of the calculated strains during the transient revealed good agreement between the two DIC software. The average root-mean-square errors between the two software was 0.20% strain, which is slightly larger than a previously reported error value for these tests. In conclusion, this variance in results is low enough that this analysis method can be used for code validation.

Reactivity-initiated accident↗