Search NASA⌕ Search

SEARCH · Search NASA

Results for “electrode aging”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 73 records · Page 4

Computational Design of Batteries from Materials to Systems

Computer models are helping to accelerate the design and validation of next generation batteries and provide valuable insights not possible through experimental testing alone. Validated 3-D physics-based models exist for predicting electrochemical performance, thermal and mechanical response of cells and packs under normal and abuse scenarios. The talk describes present efforts to make the models better suited for engineering design, including improving their computation speed, developing faster processes for model parameter identification including under aging, and predicting the performance of a proposed electrode material recipe a priori using microstructure models.

25 ENERGY STORAGE↗

Shelf-life of ball-milled catalyst inks for the fabrication of fuel cell electrodes

A major factor driving fuel cell costs is the quantity of precious metal required. Therefore, it is important to understand a timeframe where inks can be reused. Here, in this work, we explore differences between a freshly prepared catalyst ink and one that has been stored for over a year – comparing ink properties, cathode catalyst layer microstructure, and their respective fuel cell performance. Ink studies revealed smaller agglomerate sizes and a decrease in shear viscosity for the aged ink. Longer storage time also results in fewer cracks and a more uniform ionomer distribution, as evidenced by microscopy characterization of rod-coated electrodes. Lastly, polarization curves show improved performance at higher current densities for the electrode prepared from the aged ink. We rationalize such effect in terms of enhanced ionomer adsorption onto the catalyst over time.

08 HYDROGEN↗

Electrolyte additive to improve performance of MCMB LiNi{sub 1/3}Co{sub 1/3}Mn{sub 1/3}O{sub 2} Li-ion cell.

The electrolyte additive, 3,9-divinyl-2,4,8,10-tetraoxaspiro[5,5] undecane (TOS), was investigated as a means to improve the life of mesocarbon microbead (MCMB)/Li1.1[Ni1/3Co1/3Mn1/3]0.9O2 (NCM) cells for high-power applications. With the addition of an appropriate amount of TOS (no more than 1 wt%) to MCMB/NCM cells, the capacity retention was significantly improved at 55 C compared with cells containing pristine electrolyte. Aging tests at 55 C indicated that the capacity retention of the negative electrode had benefited as a result of the formation of a stable passivation film at the surface of the carbon electrode due to TOS reduction. Electrochemical impedance spectroscopy showed that a TOS addition of more than 0.5 wt% increased the cell interfacial impedance. Differential scanning calorimetry showed that the thermal stability of lithiated MCMB was also improved with the TOS addition.

36 MATERIALS SCIENCE↗

Lithium-Ion Batteries with Lithium Manganese Iron Phosphate Cathodes and Lithium Titanate Anodes: Linking Electrode Dynamics to Cell Performance

This study examines the electrochemical performance, impedance behavior, and aging mechanisms of lithium-ion cells pairing lithium manganese iron phosphate (LiMn 0.6 Fe 0.4 PO 4 , LMFP64) cathodes with lithium titanate (Li 4 Ti 5 O 12 , LTO) anodes. LMFP64 half-cells display distinct Fe and Mn redox plateaus at ∼3.5 and ∼4.1 V, respectively, and deliver excellent rate capability. Three-electrode measurements show that LMFP64 dominates cell impedance, which changes sharply across the Fe–Mn redox transition and decreases with increasing temperature (30 °C–50 °C). Voltage hysteresis arises mainly from the cathode, with higher C-rates shortening redox plateaus and broadening the transition region. Elevated temperature lowers impedance, especially near the Mn-redox and transition regions, but accelerates capacity fade. Post-cycling analyses of electrodes confirm structural stability of LMFP64 and indicate loss of lithium inventory (LLI) as the source of capacity fade. This LLI causes potential slippage between the LMFP64 and LTO electrodes, which decreases the Fe-redox plateau width. Long-term cycling highlights the critical role of electrode overhang: cathode overhang mitigates capacity fade by buffering lithium loss, whereas anode overhang cells experience faster capacity decline due to uncompensated lithium depletion. These results clarify LMFP64/LTO battery impedance evolution, thermal effects, and degradation pathways and provide insights for their applications in electric vehicles.

Area Specific Impedance↗

Chemical Interplay of Silicon and Graphite in a Composite Electrode in SEI Formation

In this study, we investigated the effect of the Si/graphite weight ratio in half-cells on the solid electrolyte interphase (SEI) layer's chemistry. The nominal concentrations of active materials were (wt % Si/wt % Gr) 15/73, 30/58, 60/28, and 80/0. The electrolyte in the cells consisted of either 1.2 M LiPF 6 in ethylene carbonate/ethyl methyl carbonate (3:7 by wt) or 1.2 M LiPF 6 in ethylene carbonate:ethyl methyl carbonate (3:7 by wt) + 10 wt % fluoroethylene carbonate. These coin cells were cycled five times at the C/10 rate. As expected, the addition of silicon to the electrode significantly increased the measured capacity. Examination of the aged composite material showed that the electrolyte influenced the concentration of chemical environments on the surface. Depth profiling revealed that these concentrations of surface environments changed with sputtering time. A statistics-of-mixtures model was used to deconvolute how silicon and graphite interacted during the formation of these species and how the interaction changed with depth.

25 ENERGY STORAGE↗

Electrode behavior RE-visited: Monitoring potential windows, capacity loss, and impedance changes in Li 1.03 (Ni 0.5 Co 0.2 Mn 0.3 ) 0.97 O 2 /silicon-graphite full cells

Here, the capacity and power performance of lithium-ion battery cells evolve over time. The mechanisms leading to these changes can often be identified through knowledge of electrode potentials, which contain information about electrochemical processes at the electrode-electrolyte interfaces. In this study we monitor electrode potentials within full cells containing a Li 1.03 (Ni 0.5 Co 0.2 Mn 0.3 ) 0.97 O 2 –based (NCM523) positive electrode, a silicon-graphite negative electrode, and an LiPF6-bearing electrolyte, with and without fluoroethylene carbonate (FEC) or vinylene carbonate (VC) additives. The electrode potentials are monitored with a Li-metal reference electrode (RE) positioned besides the electrode stack; changes in these potentials are used to examine electrode state-of-charge (SOC) shifts, material utilization, and loss of electrochemically active material. Electrode impedances are obtained with a Li x Sn RE located within the stack; the data display the effect of cell voltage and electrode SOC changes on the measured values after formation cycling and after aging. Our measurements confirm the beneficial effect of FEC and VC electrolyte additives in reducing full cell capacity loss and impedance rise after cycling in a 3.0–4.2 V range. Comparisons with data from a full cell containing a graphite-based negative highlight the consequences of including silicon in the electrode. Our observations on electrode potentials, capacity, and impedance changes on cycling are crucial to designing long-lasting, silicon-bearing, lithium-ion cells.

25 ENERGY STORAGE↗

Model electrode structures for studies of electrocatalyst degradation.

Proton exchange membrane fuel cells are being extensively studied as power sources because of their technological advantages such as high energy efficiency and environmental friendliness. The most effective catalyst in these systems consists of nanoparticles of Pt or Pt-based alloys on carbon supports. Understanding the role of the nanoparticle size and structure on the catalytic activity and degradation is needed to optimize the fuel cell performance and reduce the noble metal loading. One of the more significant causes of fuel cell performance degradation is the cathode catalyst deactivation. There are four mechanisms considered relevant to the loss of electrochemically active surface area of Pt in the fuel cell electrodes that contribute to cathode catalyst degradation including: catalyst particle sintering such as Ostwald ripening, migration and coalescence, carbon corrosion and catalyst dissolution. Most approaches to study this catalyst degradation utilize membrane electrode assemblies (MEAs), which results in a complex system where it is difficult to deconvolute the effects of the metal nanoparticles. Our research addresses catalyst degradation by taking a fundamental approach to study electrocatalyst using model supports. Nanostructured particle arrays are engineered directly onto planar glassy carbon electrodes. These model electrocatalyst structures are applied to electrochemical activity measurements using a rotating disk electrode and surface characterization by scanning electron microscopy. Sample transfer between these measurement techniques enables examination of the same catalyst area before and after electrochemical cycling. This is useful to probe relationships between electrochemical activity and catalyst structure such as particle size and spacing. These model systems are applied to accelerated aging studies of activity degradation. We will present our work demonstrating the mechanistic aspects of catalyst degradation using this simplified geometric system. The active surface area loss observed in repeated cyclic voltammetry is explained through characterization and imaging of the same RDE electrode structures throughout the aging process.

30 DIRECT ENERGY CONVERSION↗

Cycle life evaluation of 3Ah Li{sub x}Mn{sub 2}O{sub 4}-based lithium-ion secondary cells for low-earth-orbit satellites. II. Harvested electrode examination.

Lithium-ion batteries are a candidate for the energy storage system onboard low-earth-orbit satellites. Terrestrial experiments are able to capture the performance degradation of cells in orbit, therefore providing the opportunity for lifetime investigations. The lifetime performance of 3 Ah commercial Li{sub x}Mn{sub 2}O{sub 4}-based pouch cells was evaluated in a matrix of different cycling depths-of-discharge (DODs: 0, 20, 40%) and temperatures (25, 45 C). Aged cells were disassembled and the electrochemical performance of harvested electrodes investigated with two- and three-electrode pouch cells. The positive electrode had a larger decrease in capacity than the negative electrode. Both the positive and negative electrode contributed to the increase of cell impedance measured at high states-of-charge (SOCs). The data at low SOCs indicated that the increase of cell impedance was associated with the positive electrode, which showed a significant increase in the magnitude of the high-frequency semi-circle. This SOC-dependence was observed for cells cycled for either extended periods of time or at higher temperatures with a 40% DOD swing. Low-current cycling of positive electrodes revealed a change in the second potential plateau, possibly reflecting a structural change of the Li{sub x}Mn{sub 2}O{sub 4}. This could impact on the electrode kinetics and provide a possible explanation for the SOC-dependent change of the impedance.

25 ENERGY STORAGE↗

Interplay between Swelling Kinetics and Nanostructure in Perfluorosulfonic Acid Thin-Films: Role of Hygrothermal Aging

Impacts of processing, storage, and operation on thin-film perfluorosulfonic acid (PFSA) ionomer coatings used in electrodes of electrochemical devices remains unestablished. In this work, alteration of structure–function relationship in ionomers is achieved via exposure to elevated temperature and humidity (hygrothermal aging). Findings reflect a strong inverse correlation between aging-induced ionomer thin-film domain orientation and water-transport kinetics evaluated from swelling. Finally, impact of aging is shown to be more pronounced on platinum due to interactions with PFSA, as evidenced by greater increase in nanodomain orientation parallel to substrate accompanied by reduced water transport, in contrast to silicon support.

36 MATERIALS SCIENCE↗

Fast-Charging Aging Considerations: Incorporation and Alignment of Cell Design and Material Degradation Pathways

Fast charging of batteries for electric vehicles is seen as one of the most direct ways to enhance adoption. Currently, fast charging is limited by increased cell aging, which is primarily driven by Li plating and degradation of cathode materials. Here, using combined sets of experimental and computational analysis and a suite of different charge protocols, we begin to examine the interplay between failure mode, cell designs, and ultimately aging mechanisms. Slight variation in cell design and the subsequent impacts that charge protocols have on aging can create distinct cell-to-cell variation. As little as 2% difference in porosity change at the cell negative electrode during cycling due to early Li metal plating has been found to alter the aging pathway and either accelerate or inhibit the loss due to Li plating.

25 ENERGY STORAGE↗

Brain stem auditory evoked responses in human infants and adults

Brain stem evoked potentials were recorded by conventional scalp electrodes in infants (3 weeks to 3 years of age) and adults. The latency of one of the major response components (wave V) is shown to be a function both of click intensity and the age of the subject; this latency at a given signal strength shortens postnatally to reach the adult value (about 6 msec) by 12 to 18 months of age. The demonstrated reliability and limited variability of these brain stem electrophysiological responses provide the basis for an optimistic estimate of their usefulness as an objective method for assessing hearing in infants and adults.

Hecox, K.↗

Lithium Plating Characteristics in High Areal Capacity Li-Ion Battery Electrodes

Li-ion battery degradation and safety events are often attributed to undesirable metallic lithium plating. Since their release, Li-ion battery electrodes have been made progressively thicker to provide a higher energy density. However, the propensity for plating in these thicker pairings is not well understood. Herein, we combine an experimental plating-prone condition with robust mesoscale modeling to examine electrode pairings with capacities ranging from 2.5 to 6 mAh/cm 2 and negative to positive (N/P) electrode areal capacity ratio from 0.9 to 1.8 without the need for extensive aging tests. Using both experimentation and a mesoscale model, we identify a shift from conventional high state-of-charge (SOC) type plating to high overpotential (OP) type plating as electrode thickness increases. Further, these two plating modes have distinct morphologies, identified by optical microscopy and electrochemical signatures. We demonstrate that under operating conditions where these plating modes converge, a high propensity of plating exists, revealing the importance of predicting and avoiding this overlap for a given electrode pairing. Further, we identify that thicker electrodes, beyond a capacity of 3 mAh/cm 2 or thickness >75 μm, are prone to high OP, limiting negative electrode (NE) utilization and preventing cross-sectional oversizing the NE from mitigating plating. Here, it simply contributes to added mass and volume. The experimental thermal gradient and mesoscale model either combined or independently provide techniques capable of probing performance and safety implications of mild changes to electrode design features.

25 ENERGY STORAGE↗

In Situ X-ray Absorption Spectroscopy Study of the Capacity Fading Mechanism in Hybrid Sn 3 O 2 (OH) 2 /Graphite Battery Anode Nanomaterials

In situ x-ray absorption spectroscopy (XAS) of an electrode material under electrochemical control has enabled a detailed examination of the aging mechanism in a hybrid nanomaterial, Sn3O2(OH)2/graphite, that is considered for use as a high capacity lithium-ion battery anode. By the use of an original one-pot solvothermal synthesis technique, Sn3O2(OH)2 nanoparticles were directly deposited on the surface of nano-thin graphite and were charged/discharged in situ for several cycles while XAS spectra at the Sn K-edge were taken. Modeling of collected extended x-ray absorption fine structure (EXAFS) spectra provides detailed information on the Sn-O, Sn-Sn and Sn-Li coordination numbers and atomic distances for each charged and discharged electrode state. Based on the changes in atomic arrangement deduced from the EXAFS fitting results, including the first unambiguous observation of Sn-Li near neighbors, an aging mechanism is proposed in which metallic tin clusters are created surrounded by a highly disordered Li2O shell that is formed on first charge. The metallic tin cluster participates in lithiation and delithiation on the following charge/discharge cycles, however the clusters slowly lose electrical contact with the rest of the electrode and become excluded from further participation in electrochemical reactions, resulting in the reduced capacity of this anode material.

36 MATERIALS SCIENCE↗

Achieving high rate performance in hybrid pristine-recycled cathodes using model-informed electrode designs

Direct recycling lithium-ion battery cathodes, a process that retains the engineered oxide structures from end-of-life materials, presents a cost-effective and energy-efficient alternative to other battery recycling methods. However, while direct-recycled cathodes have demonstrated performance comparable to that of pristine materials at low cycling rates, their high-rate performance remains uncertain. Morphology changes in cathode particles, a main mode of degradation, directly impact rate performance by limiting surface kinetics and solid-phase diffusion. If direct recycling processes do not sufficiently restore pristine-like morphologies, the recycled materials may retain structural defects that hinder high-rate performance. The present work uses a physics-based pseudo-2D model to simulate hybrid electrodes with pristine and artificially “aged/recycled” NMC materials to investigate potential impacts of incorporating performance-limited aged cathode materials into cells. The study highlights how differences in transport and kinetic properties can influence rate capabilities in mixed electrodes — particularly in high-loading cells in high-demand applications. However, model results also reveal a possible mitigation strategy via dual-layer electrode architectures with lower-performing materials positioned near the current collector. Simulations of 4.0 mAh cm −2 cells cycled at 4C using a dual-layer architecture provided approximately 5%–30% more capacity in constant-current protocols compared to homogeneously blended electrode architectures with the same loadings and mixed-material compositions. These findings highlight the importance of strategic electrode design in minimizing potential performance losses and facilitating the integration of recycled materials into high-performance batteries, advancing sustainable and cost-effective battery manufacturing.

25 ENERGY STORAGE↗

Mechanistic Understanding of Interphase-driven Aging in Silicon Anodes

Conventional solid electrolyte interphases (SEIs) strongly adhere to micro-silicon (µ-Si) and crack under volume changes, causing poor cycling performance. Nano-silicon improves cycling performance but remains costly with limited calendar life. Here potentiostatic ageing tests demonstrate that both calendar and cycle ageing are governed by SEI cracking and dissolution with different relative contributions. When the system is not dominated by SEI dissolution, the relative calendar life of Si anodes could correlates positively with their cycle life. LiF-rich SEI that enables long cycle life in µ-Si is therefore expected to enhance calendar life as well. Using this framework, we screened electrolytes, SEIs and electrodes and validated them with full-cell storage. LiF-rich SEI minimizes cracking and dissolution, enabling μ-Si to achieve excellent calendar life, whereas nano-silicon suffers from SEI dissolution and needs reduced electrolyte–electrode contact for better calendar life. This work clarifies calendar-ageing behaviour and accelerates electrolytes and SEI development for long-life Si anodes.

Johnson, Christopher S.↗

Nanoscale Three-Dimensional Imaging of Degradation in Composite Si-Containing Anodes

The use of silicon (Si) in next-generation lithium-ion battery (LIB) anodes has the potential to dramatically improve electrochemical performance over current LIB graphite (Gr) anodes, due to silicon’s higher specific capacity.1 However, widespread implementation of Si-containing anodes is inhibited by issues such as significant Si volume expansion during lithiation and an unstable solid-electrolyte interphase (SEI), resulting in unreliable performance and poor cycle life. Currently, composite anodes with both Si and graphite active materials are used to increase capacity and mitigate some of the limitations associated with Si. In composite electrodes with a heterogeneous distribution of components with varying electrical properties (including Si, Gr, conductive carbon additive, and binder), it is important to understand the local distribution of each component to correlate with electrochemical processes, particularly localized degradation and heterogeneous aging, and to optimize performance. To investigate Si-containing composite anodes in the nanoscale, we use scanning spreading resistance microscopy (SSRM), a form of scanning probe microscopy (SPM) that probes local electronic resistivity. By examining the intrinsic electronic resistivity contrast between the anode components, separate phases can be distinguished and understood within the composite structure.2 This work studies the effect of electrochemical cycling in two different electrolytes on component distribution and aging by comparing the electrical and structural evolution of composite Si-graphite electrodes and SEI before and after charge-discharge cycling. 1. W. J. Zhang. A review of the electrochemical performance of alloy anodes for lithium-ion batteries J. Power Sources 196 13–24 (2011). 2. C. Stetson, Z. Huey, A. Downard, Z. Li, B. To, A. Zakutayev, C.-S. Jiang, M. Al-Jassim, D. Finegan, S.-D. Han and S. DeCaluwe: Three-Dimensional Mapping of Resistivity and Microstructure of Composite Electrodes for Lithium-Ion Batteries. ACS Nano Letters Accepted (2020).

ADVANCED PROPULSION SYSTEMS↗

Strain and Conductivity in Lithium Ion Battery Binders

Lithium batteries provide high energy density storage with applications ranging from consumer electronics to electric vehicles. However, they have a limited lifespan and experience capacity loss with aging. Multiple mechanisms contribute to battery aging. The battery binder plays two important roles in the electrodes, and the damage it sustains during cycling may play a role in the degradation of the overall battery performance. Mechanical stress during battery operations occurs as a result of the swelling and shrinking of the electrodes because of the movement of lithium with cycling. The yield stress of the swollen polyvinylidene fluoride carbon black (PVDFCB) binder was measured at approximately 4MPa for PVDF with carbon black CB weight fractions between 10-30% swollen in propylene carbonate. This is far less stress than is typically experienced in an electrode during cycling. The effects of this permanent damage to the binder were explored by measuring the conductivity loss with strains in excess of the binder yield.

25 ENERGY STORAGE↗