Search NASA⌕ Search

SEARCH · Search NASA

Results for “polymeric elastomers”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 73 records · Page 4

Well-Tunable, 3D-printable, and Fast Autonomous Self-Healing Elastomers

Self-healing elastomers provide extended longevity of functional materials, due to their unique adaptability and durability. However, a major scientific challenge remains in developing materials with a rapid healing process combined with decent mechanical properties, that can be prepared by a relatively simple synthesis approach. Herein, we report a versatile design approach on self-healing elastomers by incorporating two different hydrogen bonding containing monomers, i.e., 2-[[(butylamino)carbonyl]oxy]ethyl acrylate (BCOE) and 2-ureido-4[1H]pyrimidinone (UPy) functionalized ethyl methacrylate. Poly(BCOE-r-UPy)s are synthesized by reversible addition-fragmentation chain-transfer (RAFT) polymerization, and controlling the ratio of two monomers enables well-tunable mechanical properties with tensile strength ranging from 0.04 to 6.3 MPa and tensile strain up to 3,000 %. The characteristic dissociation energy is calculated from a temperature dependence of terminal relaxation followed by subtracting the segmental relaxation. The rapid autonomous self-healing is achieved when the molar composition of Poly(BCOE-r-UPy) is tailored to BCOE/UPy = 99/1. The self-healing process is monitored in situ by a helium-ion microscope, and its macroscopic study using tensile tests indicates that Poly(BCOE-r-UPy1) with 1 % molar ratio of UPy recovers 70 % of its original toughness at ambient temperature within 10 mins. 3D printing of Poly(BCOE-r-UPy) affords a self-healable 3D structure, demonstrating the adaptability of Poly(BCOE-r-UPy) for on-demand fabrication. The simplicity of synthesis, well-tunable mechanical properties, unique self-healability, and 3D printing capability of Poly(BCOE-r-UPy)s indicate their potential for a range of applications.

36 MATERIALS SCIENCE↗

Mono‐Materials Created by Engineering a Continuum of P3HB Stereomicrostructures in a One‐Step Catalytic Process

Multi-material products that combine multiple complementary polymers can create products with desired performance but present challenges to end-of-life (EoL) management. The emerging mono-material product design based on a single polymer type addresses the fundamental EoL issue, but challenges of delivering vastly tunable material properties by the single polymer still remain. Here, we introduce a simple strategy to produce biodegradable poly(3-hydroxybutyrate) (P3HB) materials with a wide range of material properties by engineering a stereomicrostructure continuum, achieved through polymerizing diastereomeric mixtures of racemic and meso-dimethyl diolides at various feed ratios with a single catalyst. This one-step, one-pot process produces biodegradable P3HB mono-materials ranging from rigid to flexible thermoplastics, to tough thermoplastic elastomers, to a pressure-sensitive adhesive (PSA), which have been then combined to fabricate prototype all-P3HB PSA tapes, demonstrating the feasibility of designing mono-material products through engineering polymer stereomicrostructures.

36 MATERIALS SCIENCE↗

Monitoring Degradation of Nuclear Cable Insulation Subjected To Sequential and Simultaneous Thermal and Radiation Aging

Predicting useful remaining life of cables in nuclear power plants is a topic of growing interest as plant continue to age. A typical electrical cable consists of polymeric materials, such as the cable jacket and insulation, which are susceptible to degradation due to exposure to both elevated temperatures and gamma irradiation over decades of service. In this work two insulation materials, crosslinked polyethylene (XLPE) and ethylene propylene diene (EPDM) elastomer, were characterized to quantify aging using total color difference and indenter modulus. Since the effects of thermal and gamma radiation are not additive but coupled, the effects of different aging scenarios including sequential and simultaneous aging were also evaluated. In the case of sequential aging, two aging scenarios were explored where the order in which thermal and gamma radiation received were altered. Total color difference of XLPE showed that sequentially aged insulation specimens, which received radiation first, degraded slightly more at maximum exposure than specimens which received thermal first. Similarly, in the case of EPDM, the extent of degradation evaluated using total color difference was found to be most severe in the case of sequentially aged insulation specimens which received radiation first. Indenter modulus was found to be insensitive to aging for XLPE but trended for EPDM. The largest variations were observed for the sequentially aged insulation specimens which received radiation first, similar to what was observed for total color difference.

Pallaka, Madhusudhan Reddy↗

Sequential versus Simultaneous Aging of EPDM Nuclear Cable Insulation Subjected to Elevated Temperature and Gamma Radiation

Electrical cables are integral to power, control, and instrumentation systems within nuclear power plants (NPPs). Exposure of cable systems within nuclear containment to elevated temperatures and gamma radiation during decades-long operation of NPPs can lead to degradation of cable polymeric insulation. Prediction of nuclear cable insulation degradation is complicated as thermal and radiation stress are not additive. In this work, we explore the relative effects of simultaneous and sequential thermal and gamma irradiation on the aging of ethylene-propylene-diene (EPDM) elastomer insulation to better understand realistic scenarios of cable insulation degradation. Cable insulation samples of EPDM were subjected to up to 320 kGy of gamma radiation at a dose rate of 300 Gy/hr in two heating scenarios: (1) simultaneously aged samples were heated at 150°C during irradiation and (2) sequentially aged samples were heated at 150°C for designated durations followed by corresponding periods of irradiation at ambient temperature. The mass, tensile elongation at break, and carbonyl index were assessed to quantify aging of the polymers. The simultaneous aging scenario was found to the more severe of the two for EPDM insulation degradation.

ethylene-propylene-diene elastomer, EPDM, nuclear ↗

Evaluation of bifacial module technologies with combined–accelerated stress testing

In view of the increasing interest and market share of bifacial cells and modules, suitable substrates such as glass and transparent backsheets along with ethylene vinyl acetate (EVA) and polyolefin elastomer (POE) encapsulants were examined in combined-accelerated stress testing (C-AST) to evaluate and compare degradation modes. Testing with both monofacial and bifacial cells, we found glass-glass modules with monofacial cells led to greater grid finger breakage than those with polymeric backsheets. Furthermore, this is attributed to previous X-ray topography and modeling work showing higher stress in cells and interconnections in glass-glass modules than glass-backsheet modules. Consistent with the objectives of C-AST, which stresses modules at levels corresponding to the limits seen in the natural environment, we observed the UV-fluorescence signatures of modules tested in C-AST (considering the degradation associated with developing chromophores, moisture penetration and photobleaching effects) to be like those in fielded modules, more so than other chamber stress testing implemented for comparison. We found light-induced degradation (LID) in module types with regenerated (inactive) cells with C-AST, suggesting the possibility of LID destabilization in some field conditions. We could also distinguish potential-induced degradation (PID) on the back of the bifacial passivated emitter and rear cells (PERC) in C-AST. Confirming with ex-situ tests, we found polarization-type PID most prevalent in glass-glass modules with EVA as would be anticipated considering the greater leakage current through such module encapsulation. Unlike PID tests performed in the dark, which can lead to false positive PID test results, field-representative illumination is experienced by the modules on the front and back side while –1200 V system voltage is applied in C-AST, supporting the conclusion that this module type with glass-glass construction would be susceptible to PID in the field.

14 SOLAR ENERGY↗

Evaluation of Bifacial Modules and PV Technologies with Combined-Accelerated Stress Testing

In view of the increasing interest and market share of bifacial cells and modules, suitable substrates such as glass and transparent backsheets along with ethylene vinyl acetate (EVA) and polyolefin elastomer (POE) encapsulants were examined in combined-accelerated stress testing (C-AST) to evaluate and compare degradation modes. Testing with both monofacial and bifacial cells, we found glass-glass modules with monofacial cells led to greater grid finger breakage than those with polymeric backsheets. This is attributed to previous x-ray topography work showing higher stress in cells in glass-glass modules than glass backsheet modules. Consistent with the objectives of C-AST, which stresses modules at levels corresponding to the limits seen in the natural environment, we observed the UV-fluorescence signatures of modules tested in C-AST (considering the degradation associated with developing chromophores, moisture penetration and photobleaching effects) to be like those in fielded modules, more so than other chamber stress testing implemented for comparison. Finally, among multiple cell degradation modes that we observed such as light-induced degradation (LID), we differentiated susceptibility to potential-induced degradation (PID) on the back of the bifacial Passivated Emitter Back Cells (PERC) in C-AST. Confirming with ex-situ tests, we found polarization-type PID most prevalent in glass/glass modules with EVA as would be anticipated considering the greater leakage current through such module encapsulation. Unlike PID tests performed in the dark, which can lead to false positive PID test results, field-representative illumination is experienced by the modules on the front and back side while -1200 V system voltage is applied in C-AST, supporting the conclusion that this module type would be susceptible to PID in the field.

bifacial modules↗

HYDROPHOBIC CHARACTERISTICS OF COMPOSITE INSULATORS IN SIMULATED INLAND ARID DESERT ENVIRONMENT

Presently along with traditional insulators i.e. glass and porcelain, etc., the polymeric insulators are also used world widely. These polymeric insulators are very sensitive to various environmental parameters e.g. UV radiations, heat, etc. The UV radiation level in the central region of Saudi Arabia is high as compared to the recommended IEC-61109 standard for the accelerated aging of the composite insulators. In this study, thermoplastic elastomer (TPE) and Ethylene Propylene Diene Monomer (EPDM) insulators were subjected to accelerated aging stress as per IEC standard as well as modified IEC standard simulating the inland arid desert's atmospheric conditions. The hydrophobic characteristics were studied by measuring the contact angle along the insulator surface before and after the accelerated aging of the samples. It was found that TPE loses its hydrophobic properties more as compared to EPDM insulator. This loss was proportional to the intensity of UV irradiation. The rate of recovery is also low for both the tested materials as compared to Silicone Rubber insulators.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Degradation in Photovoltaic Encapsulant Transmittance: Results of the Second PVQAT TG5 Artificial Weathering Study

The optical degradation of encapsulants from ultraviolet (UV) radiation has historically resulted in a significant loss in performance throughout the life of a photovoltaic (PV) module. IEC test methods have recently been developed to screen for PV encapsulants prone to loss in optical performance. The present study was performed to benchmark polymeric packaging materials relative to IEC 62788-1-4 (covering the measurement of optical transmittance) and IEC 62788-1-7 (on the durability of transmittance), provide feedback toward improvement of the methods, and develop insight regarding optical degradation. Contemporary materials were examined, including: poly(ethylene-co-vinyl acetate) (EVA), thermoplastic polyolefin (TPO), polyolefin elastomer (POE), and polyvinyl butyral (PVB) encapsulants; a poly(ethene-co-tetrafluoroethene)/poly(ethylene terephthalate) (ETFE/PET) transparent backsheet; and a polystyrene (PS) working reference material. The use of silica-, specialty-, and rolled-glass was also compared in laminated coupons. Specimen size was separately examined from 2.5 cm to 12.5 cm. Weathering was performed with a xenon source, using IEC TS 62788-7-2 methods A2, A3, A4, and A5 (chamber temperature of 55 Degrees C, 65 Degrees C, 75 Degrees C, or 85 Degrees C), respectively. Characterizations were made using a UV-VIS-NIR spectrophotometer (transmittance and reflectance, with and without an integrating sphere), a UV-VIS fluorescence spectrophotometer, a camera, and an optical microscope. Performance was analyzed, including solar weighted transmittance, yellowness index, UV cut-off wavelength, and haze (scattering). Separate Arrhenius analyses were performed to assess retention of transmittance and changes in yellowness index. The activation energy for both characteristics was found to range from 15 kJ?mol-1-80 kJ/mol-1, with an average of 48 kJ/mol-1, similar to the average of 45 kJ/mol-1 identified in the previous international PV Quality Assurance Task Force (PVQAT) Task Group 5 (TG5) study of more traditional encapsulants. The separate degradation modes of discoloration and scattering were distinguished in the encapsulants using a comprehensive spectral characterization. Based on these results, the IEC 62788-1-7 pass/fail criteria of 5% change in transmittance was confirmed to identify a known bad encapsulant.

durability↗

Damp Heat Induced Degradation of Silicon Heterojunction Solar Cells With Cu-Plated Contacts

Damp heat exposure is one of the most stringent environments for testing the durability of solar cells in packaged modules. Damp heat stresses and induces a variety of degradation modes in solar cells and modules: for example, moisture-induced corrosion of electrodes and interconnections, deterioration of polymeric materials, and/or thermally activated diffusion processes. To screen for these and other potential degradation modes, we subject one-cell modules containing silicon heterojunction (SHJ) solar cells with Cu-plated contacts to extended damp heat tests at 85 °C/85% relative humidity. SHJ cells were laminated with two common encapsulants: ethylene vinyl acetate (EVA) and polyolefin elastomer (POE), and two constructions: glass-backsheet and glass-glass. We observe degradation in all components of solar cell maximum power (PMP): current, voltage, and fill factor, and find evidence of increased carrier recombination and nonideal diode behavior with increasing stress. For glass-backsheet constructions, EVA samples generally degrade more than POE by a factor of approximately 1.5x PMP, and the different encapsulants produce different degradation patterns. Similar trends are observed in glass-glass modules, but to a lesser degree. In a different experiment, we observe a decrease in effective minority carrier lifetime of nonmetallized SHJ precursors measured after damp heat. This implies that some degradation unrelated to the contacts is to be expected and confirms the observation of increasing recombination.

14 SOLAR ENERGY↗

Rapid, large-volume, thermally controlled 3D printing using a mobile liquid interface

In this paper, we report a stereolithographic three-dimensional printing approach for polymeric components that uses a mobile liquid interface (a fluorinated oil) to reduce the adhesive forces between the interface and the printed object, thereby allowing for a continuous and rapid print process, regardless of polymeric precursor. The bed area is not size-restricted by thermal limitations because the flowing oil enables direct cooling across the entire print area. Continuous vertical print rates exceeding 430 millimeters per hour with a volumetric throughput of 100 liters per hour have been demonstrated, and proof-of-concept structures made from hard plastics, ceramic precursors, and elastomers have been printed.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Digital Light Process 3D Printing of Magnetically Aligned Liquid Crystalline Elastomer Free–forms

Liquid crystalline elastomers (LCEs) are anisotropic soft materials capable of large dimensional changes when subjected to a stimulus. The magnitude and directionality of the stimuli-induced thermomechanical response is associated with the alignment of the LCE. Recent reports detail the preparation of LCEs by additive manufacturing (AM) techniques, predominately using direct ink write printing. Another AM technique, digital light process (DLP) 3D printing, has generated significant interest as it affords LCE free-forms with high fidelity and resolution. However, one challenge of printing LCEs using vat polymerization methods such as DLP is enforcing alignment. Here, we document the preparation of aligned, main-chain LCEs via DLP 3D printing using a 100 mT magnetic field. Systematic examination isolates the contribution of magnetic field strength, alignment time, and build layer thickness on the degree of orientation in 3D printed LCEs. Informed by this fundamental understanding, DLP is used to print complex LCE free-forms with through-thickness variation in both spatial orientations. Further, the hierarchical variation in spatial orientation within LCE free-forms is used to produce objects that exhibit mechanical instabilities upon heating. DLP printing of aligned LCEs opens new opportunities to fabricate stimuli-responsive materials in form factors optimized for functional use in soft robotics and energy absorption.

36 MATERIALS SCIENCE↗

Effect of Microstructure on Chain Flexibility and Glass Transition Temperature of Polybenzofulvene

Polybenzofulvene (PBF) is a polydiene with a very high glass transition temperature (T g ), which makes it a potential candidate for use as the hard block for high-temperature thermoplastic elastomer applications. The T g s of polydienes are known to be related to chain flexibility. However, no studies have been reported that correlate the chain flexibility to the microstructure of PBF. Herein, we present a study of solution properties of linear PBFs with narrow molecular weight dispersity and having 1,2-addition ranging from 23% to 99%. The materials were prepared by living anionic polymerization under different conditions. Specifically, the chain flexibility as defined by the Flory's characteristic ratio, , and dependence of chain flexibility on microstructure by combined measurements of intrinsic viscosity and molecular weight using triple-detector size exclusion chromatography (SEC) is studied. The persistence lengths (l p ) and chain diameters (d B ) were also estimated using the touched-bead wormlike chain model. To the best of our knowledge, the characteristic ratio of PBF is found to be the highest of all polydienes that have been reported so far.

36 MATERIALS SCIENCE↗

Volumetric Additive Manufacturing of Dormant Catalytic Chemistries to Generate Silicone Micro‐ and Millifluidic Devices and Instant Molds

Tomographic volumetric additive manufacturing (T‐VAM) rapidly prints solid objects within minutes, accessing photochemistries that are traditionally challenging for layer‐based additive manufacturing methods. This includes high‐viscosity materials, air‐free chemistries, and solid‐state systems. Catalytic chemistries are appealing as a pathway to engineering advanced materials, including tough thermosets, silicone elastomers, and complex block copolymers. However, photoactivated dormant catalytic chemistries, where the catalyst irreversibly activates upon exposure to light, are incompatible with typical tomographic VAM approaches. To address this limitation, a zero‐dose optimization strategy is devised to preserve dormant catalysts in desired regions by keeping them unexposed to light. VAM printed micro‐ and millifluidic devices and instant molds are successfully produced within minutes in silicones polymerized using photoactivated dormant platinum photohydrosilylation catalysts. The printed channels are programmed to be 500 and 2500 µm for the micro‐ and millifluidic devices, and print fidelity is assessed by X‐ray computed tomography. This work demonstrates the potential of zero‐dose optimization to expand the range of chemistries accessible for VAM, enabling the rapid fabrication of complex devices.

Additive Manufacturing↗

EFFECTS OF GAMMA IRRADIATION ON EPDM ELASTOMERS

Two formulations of EPDM elastomer, one substituting a UV stabilizer for the normal antioxidant in this polymer, and the other the normal formulation, were synthesized and samples of each were exposed to gamma irradiation in initially pure deuterium gas to compare their radiation stability. Stainless steel containers having rupture disks were designed for this task. After 130 MRad dose of cobalt-60 radiation in the SRNL Gamma Irradiation Facility, a significant amount of gas was created by radiolysis; however the composition indicated by mass spectroscopy indicated an unexpected increase in the total amount deuterium in both formulations. The irradiated samples retained their ductility in a bend test. No change of sample weight, dimensions, or density was observed. No change of the glass transition temperature as measured by dynamic mechanical analysis was observed, and most of the other dynamic mechanical properties remained unchanged. There appeared to be an increase in the storage modulus of the irradiated samples containing the UV stabilizer above the glass transition, which may indicate hardening of the material by radiation damage. Polymeric materials become damaged by exposure over time to ionizing radiation. Despite the limited lifetime, polymers have unique engineering material properties and polymers continue to be used in tritium handling systems. In tritium handling systems, polymers are employed mainly in joining applications such as valve sealing surfaces (eg. Stem tips, valve packing, and O-rings). Because of the continued need to employ polymers in tritium systems, over the past several years, programs at the Savannah River National Laboratory have been studying the effect of tritium on various polymers of interest. In these studies, samples of materials of interest to the SRS Tritium Facilities (ultra-high molecular weight polyethylene (UHMW-PE), polytetrafluoroethylene (PTFE, Teflon{reg_sign}), Vespel{reg_sign} polyimide, and the elastomer ethylene propylene diene monomer (EPDM)) have been exposed in closed containers to tritium gas initially at 1 atmosphere pressure. These studies have demonstrated the degradation of properties when exposed to tritium gas. Also, the radiolytic production of significant amounts of hydrogen has been observed for UHMW-PE and EPDM. The study documented in this report exposes two similar formulations of EPDM elastomer to gamma irradiation in a closed container backfilled with deuterium. Deuterium is chemically identical to protium and tritium, but allows the identification of protium that is radiolytically produced from the samples. The goal of this program is to compare and contrast the response of EPDM exposure to two different types of ionizing radiation in a similar chemical environment.

36 MATERIALS SCIENCE↗

Connecting radiation-driven changes in structural, thermal, and mechanical properties in several medical device polymers

Stemming from security threats and shortages in supply, a recent push has emerged to develop alternatives to radioisotope Cobalt-60 gamma radiation for sterilization of polymeric medical products, including electron beam (e-beam) and X-ray machine-based sources. However, before large-scale implementation, the effects of these non-isotope-based methods must be thoroughly investigated from several perspectives, involving their potential detrimental effects on the structural, thermal, and mechanical properties of polymers in medical devices. This paper investigates such effects in commonly used medical device polymers, including polypropylene homopolymer (PPH), polyolefin elastomer (POE), low-density polyethylene (LDPE), acrylonitrile butadiene styrene (ABS), and chlorobutyl rubber (CIIR). To connect radiation-driven changes in polymer structural and thermal properties and corresponding changes in mechanical properties, several characterization techniques were utilized, including gel permeation chromatography (GPC), Fourier transform infrared spectroscopy (FTIR), dynamic mechanical analysis (DMA) and differential scanning calorimetry (DSC). We found that the tensile strength of X-ray irradiated PPH, as well as X-ray, e-beam, and gamma irradiated CIIR decreases due to chain scission, which is corroborated by GPC and DMA. The GPC results of LDPE suggest chain scission, but interestingly without a corresponding decline in tensile strength. By comparison, POE and ABS appear to undergo further crosslinking with increasing irradiation dose, which generally strengthens them. Importantly, in the vast majority of the cases, there were small to no changes in properties upon changing radiation technologies (at a given dose), i.e., no radiation source dependence. However, in a few specific cases, radiation method dependencies did arise, for instance, in terms of the molecular weight of PPH being significantly increased upon X-ray irradiation, while the melting temperature, glass transition temperature, and elongation at break reduced compared to gamma. Overall, this study provides valuable insight into radiation-driven chemical and structural changes in polymers that produce changes in physical and functional properties.

36 MATERIALS SCIENCE↗

All acrylic-based thermoplastic elastomers with high upper service temperature and superior mechanical properties

All acrylic-based thermoplastic elastomers (TPEs) offer potential alternatives to the widely-used styrenic TPEs. However, the high entanglement molecular weight ( M e ) of polyacrylates, as compared to polydienes, leads to “disappointing” mechanical performance as compared to styrenic TPEs. In this study, triblock copolymers composed of alkyl acrylates with different pendant groups and different glass transition temperatures ( T g s), i.e. 1-adamatyl acrylate (AdA) and tetrahydrofurfuryl acrylate (THFA), were synthesized via reversible addition–fragmentation chain transfer (RAFT) polymerization. Thermal characterization of the resulting polymers was performed using differential scanning calorimetry (DSC), and the T g s of both segments were observed for the block copolymers. This indication of microphase separation behavior was further demonstrated using atomic-force microscopy (AFM) and small angle X-ray scattering (SAXS). Dynamic mechanical analysis (DMA) showed that the softening temperature of the PAdA domains is 123 °C, which is higher than that of both styrenic TPEs and commercial acrylic based TPEs with poly(methyl methacrylate) (PMMA) hard block. Here, the resulting triblock copolymers also exhibited stress–strain behavior superior to that of conventional all acrylic-based TPEs composed of PMMA and poly( n -butyl acrylate) (PBA) made by controlled radical processes, while the tensile strength was lower than for products made by living anionic polymerization.

36 MATERIALS SCIENCE↗

Collective Summary of sCO2 Materials Development (Supercritical Transformational Electric Power Generation (STEP) Level 2 Milestone Report) (Parts I - II)

Polymers such as PTFE (polytetrafluorethylene or Teflon), EPDM (ethylene propylene diene monomer) rubber, FKM fluoroelastomer (Viton), Nylon 11, Nitrile butadiene (NBR) rubber, hydrogenated nitrile rubber (HNBR) and perfluoroelastomers (FF_202) are commonly employed in super critical CO 2 (sCO2) energy conversion systems. O-rings and gaskets made from these polymers face stringent performance conditions such as elevated temperatures, high pressures, pollutants, and corrosive humid environments. In FY 2019, we conducted experiments at high temperatures (100°C and 120°C) under isobaric conditions (20 MPa). Findings showed that elevated temperatures accelerated degradation of polymers in sCO2, and that certain polymer microstructures are more susceptible to degradation over others. In FY 2020, the focus was to understand the effect of sCO2 on polymers at low (10 MPa) and high pressures (40 MPa) under isothermal conditions (100°C). It was clear that the same selectivity was observed in these experiments wherein certain polymeric functionalities showed more propensity to failure over others. Fast diffusion, supported by higher pressures and long exposure times (1000 hours) at the test temperature, caused increased damage in sCO2 environments to even the most robust polymers. We also looked at polymers under compression in sCO2 at 100°C and 20 MPa pressure to imitate actual sealing performance required of these materials in sCO2 systems. Compression worsened the physical damage that resulted from chemical attack of the polymers under these test conditions. In FY 2021, the effect of cycling temperature (from 50°C to 150°C to 50°C) for polymers under a steady sCO2 pressure of 20 MPa was studied. The aim was to understand the influence of cycling temperatures of sCO2 for typical polymers under isobaric (20 MPa) conditions. Thermoplastic polymers (Nylon, and PTFE) and elastomers (EPDM, Viton, Buna N, Neoprene, FF202, and HNBR) were subjected to 20 MPa sCO2 pressure for 50 cycles and 100 cycles in separate experiments. Samples were extracted for ex-situ characterization at 50 cycles and upon the completion of 100 cycles. Each cycle constituted of 175 minutes of cycling from 50°C to 150°C. The polymer samples were examined for physical and chemical changes by Dynamic Mechanical and Thermal Analysis (DMTA), Fourier Transform Infrared (FTIR) spectroscopy, and compression set. Density and mass changes immediately after removal from test were measured for degree of swell comparisons. Optical microscopy techniques and micro computer tomography (micro CT) images were collected on select specimens. Evaluations conducted showed that exposures to super-critical CO2 environments resulted in combinations of physical and/or chemical changes. For each polymer, the dominance of cycling temperatures under sCO2 pressures, were evaluated. Attempts were made to qualitatively link the permanent sCO2 effects to polymer micro- structure, free volume, backbone substitutions, presence of polar groups, and degree of crystallinity differences. This study has established that soft polymeric materials are conducive to failure in sCO2 through mechanisms of failure that are dependent on polymer microstructure and chemistry. Polar pendant groups, large atom substitutions on the backbone are some of the factors that are influential structural factors.

36 MATERIALS SCIENCE↗