Energy-Saving Melting and Revert Reduction Technology (E-SMARRT), Task 5.3: Casting Porosity-Free Grain Refined Magnesium Alloys
The objective of this project was to identify the root causes for micro-porosity in magnesium alloy castings and recommend remedies that can be implemented in production. Three casting magnesium alloys were used to determine the causes of porosity that is a common problem in the magnesium casting industry. These alloys were AM50A, AM60A, and AZ91D, and all were grain refined with C 2 Cl 6 . Gas porosity was found to have little effect if proper degassing methods and foundry practices were used. It was found that sound gating practice, directional solidification towards the riser and generous risering should always dominate in order to produce sound castings. In sand cast magnesium, thermal gradients were found to be an important indicator of heat transfer in the mold. A minimum thermal gradient was found for each alloy that would produce sound castings. There were 2.02°C/cm for AM50A, 1.99°C/cm for AM60A, and 1.97°C/cm for AZ91D. If these gradients are met or exceeded when an area of the casting reaches 50°C below the liquidus for the alloy, the casting will be free of shrinkage porosity in that area. The cooling rates measured during casting magnesium alloys in a pre-heated step permanent mold ranged from 12°F/min in the three inches thick step to 200o F/min in the one inch step. The effect of the cooling rate on the grain size and the mechanical properties was noticeable but not substantial. Grain refining with C 2 Cl 6 had a marked effect on the grain size of the permanent mold step casting. It reduced it by 10-15% in AM50A and by a factor of six in AZ91E from 300 µm to around 55 µm. The mechanical properties of both permanent mold cast AZ91E and AM50A were improved by grain refinement. The most prominent increase was in the elongation of AM50A that more than doubled from 8% to 17%. Computer simulation of porosity was conducted for a well gated commercial wheel casting. The simulation did not predict significant porosity in the wheel. The mechanical testing of tensile specimens excised from the wheel indeed confirmed good properties, in line with the specifications for this alloy. Evidence of minimal micro-porosity was detected in sections cut from the wheel and investigated under optical microscopy. This finding confirms the key role played by utilizing optimal gating and risering practices in minimizing porosity in magnesium castings.