Search NASA⌕ Search

SEARCH · Search NASA

Results for “structural stability”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 793 records · Page 44

LiNi 0.8 Fe 0.1 Al 0.1 O 2 as a Cobalt-Free Cathode Material with High Capacity and High Capability for Lithium-Ion Batteries

Obtaining cathode materials with high capacity and cycle stability is one of the main challenges regarding the success of electric vehicle technologies. However, most of the widely used materials with these properties involve the use of toxic and expensive cobalt as the active material. To overcome this challenge, this work proposes a novel cobalt-free cathode material, synthesized for the first time using a solid-state reaction, whose general formula is LiNi 0.8 Fe 0.1 Al 0.1 O 2 (NFA). This class of materials offers high capacity and reduces the battery costs by removing cobalt, without jeopardizing the structural stability and safety of the NFAs. The morphology and the structural properties of the obtained NFA cathode material were characterized using different techniques, e.g., scanning electronic microscopy, X-ray diffraction, X-ray fluorescence, and infrared and Raman spectroscopies. The electrochemical activity and diffusivity of the Li-ion during lithium removal and its insertion into the bulk of the NFA cathode demonstrated high-yield specific capacities of ≈180 mAh g –1 at 0.1C, along with a reasonable rate capability and cycling stability, with a capacity retention of ≈99.6% after 100 charge/discharge cycles at a rate of C/2, and whose operando X-ray diffraction experiments have been used to study the crystallographic transitions during the lithiation–delithiation reaction.

25 ENERGY STORAGE↗

Weldability, strength, and high temperature stability of chemically vapor deposited tungsten

Three types of CVD tungsten (fluoride-produced, chloride-produced and the combination of the two which is termed duplex) were evaluated to determine their weldability, high temperature strength and structural stability during 5000 hour exposure to temperatures of 1540 C and 1700 C. Each type of CVD tungsten could be successfully electron beam welded but the results for the chloride product were not as satisfactory as those of the other two materials. The high temperature strength behavior of the three materials did not differ greatly. However a large difference was noted for the grain growth behavior of the two basic CVD tungsten materials. Fluoride tungsten was found to be relatively stable while for the most part the grain size of chloride tungsten increased appreciably. The examination of freshly fractured surfaces with a scanning electron microscope revealed numerous bubbles in the fluoride material following its exposure to 1700 C for 5000 hours. Less severe thermal treatments produced relatively few bubbles in this material. Only at certain locations within the chloride material associated with the interruption of tungsten were bubbles noted.

Bryant, W. A.↗

Low temperature structural transformation in T[Ni(CN){sub 4}].xpyz with x=1,2; T=Mn,Co,Ni,Zn,Cd; pyz=pyrazine

The materials under study are pillared solids T[Ni(CN){sub 4}].xpyz with one and two (x=1,2) pyrazine (pyz) molecules and where T=Mn, Co, Ni, Zn, Cd. Stimulated by their structural features and potential role as prototype of porous solids for hydrogen storage, the structural stability under cryogenic conditions for this series of pillared solids was studied. At low temperature, in the 100-200 K range, the occurrence of a reversible structural transformation was found. For T=Mn, Co, Zn, Cd, with x=2, the structural transformation was observed to occur around 185 K, and the low temperature phase crystallizes with a monoclinic unit cell (space group Pc). This structure change results from certain charge redistribution on cooling within the involved ligands. For T=Ni with x=1, both the low and high temperature phases crystallize with unit cells of tetragonal symmetry, within the same space group but with a different unit cell volume. In this case the structure change is observed around 120 K. Above that temperature the rotational states for the pyrazine molecule are thermally excited and all the pyrazine molecules in the structure become equivalent. Under this condition the material structure is described using a smaller structural unit. The structural study using X-ray powder diffraction data was complemented with calorimetric and Raman spectroscopy measurements. For the low temperature phases the crystal structures were solved from Patterson methods and then refined using the Rietveld method. - Graphical abstract: Low temperature ordered structure for pyrazine in T[Ni(CN){sub 4}].pyz.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Cation, Anion, and Radical Isomers of C4H4N: Computational Characterization and Implications for Astrophysical and Planetary Environments

Nitrogen-containing ions and molecules in the gas phase have been detected in non-Earth environments such as dark molecular clouds and more recently in the atmosphere of Saturn's moon Titan. These molecules may serve as precursors to larger heterocyclic structures that provide the foundation of complex biological molecules. On Titan, molecules of m/z 66 have been detected by the Cassini mission, and species of the empirical formula C 4 H 4 N may contribute to this signature. We have characterized seven isomers of C 4 H 4 N in anionic, neutral radical, and cationic states using density functional theory. Structures were optimized using the range-separated hybrid ωB97X-V with the cc-pVTZ and aug-cc-pVTZ basis sets. Anionic and radical C4H4N favor cyclic structures with aromatic and quasi-aromatic electron arrangements, respectively. Interestingly, ionization from the radical surface to the cation induces significant changes in structural stability, and the global minimum for positively charged isomers is CH 2 CCHCNH + , a pseudo-linear species reminiscent of cyanoallene. Select formation pathways to these structures from Titan's existing or postulated gas-phase species, reactions that are also relevant for other astrophysical environments, are discussed. By characterizing C 4 H 4 N isomers, we have identified energetically stable anionic, radical, and cationic structures that may be present in Titan's atmosphere and dark molecular clouds.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Three Alkali-Metal-Gold-Gallium Systems. Ternary Tunnel Structures and Some Problems with Poorly Ordered Cations

Six new intermetallic compounds have been characterized in the alkali metal (A = Na, Rb, Cs)–gold–gallium systems. Three isostructural compounds with the general composition A0.55Au2Ga2, two others of AAu3Ga2 (A = Rb, Cs), and the related Na13Au41.2Ga30.3 were synthesized via typical high-temperature reactions and their crystal structures determined by single-crystal X-ray diffraction analysis: Na0.56(9)Au2Ga2 (I, I4/mcm, a = 8.718(1) Å, c = 4.857(1) Å, Z = 4), Rb0.56(1)Au2Ga2 (II, I4/mcm, a = 8.950(1) Å, c = 4.829(1) Å, Z = 4), Cs0.54(2)Au2Ga2 (III, I4/mcm, a = 9.077(1) Å, c = 4.815(1) Å, Z = 4), RbAu3Ga2 (IV, Pnma, a = 13.384(3) Å, b = 5.577(1) Å, c = 7.017(1) Å, Z = 4), CsAu3Ga2 (V, Pnma, a = 13.511(3) Å, b = 5.614(2) Å, c = 7.146(1) Å, Z = 4), Na13Au41.2(1)Ga30.3(1) (VI, P6 mmm, a = 19.550(3) Å, c = 8.990(2) Å, Z = 2). The first three compounds (I–III) are isostructural with tetragonal K0.55Au2Ga2 and likewise contain planar eight-member Au/Ga rings that stack along c to generate tunnels and that contain varying degrees of disordered Na–Cs cations. The cation dispositions are much more clearly and reasonably defined by electron density mapping than through least-squares refinements with conventional anisotropic ellipsoids. Orthorhombic AAu3Ga2 (IV, V) are ordered ternary Rb and Cs derivatives of the SrZn5 type structure, demonstrating structural variability within the AAu3Ga2 family. All attempts to prepare an isotypic “NaAu3Ga2” were not successful, but yielded only a similar composition Na13Au41.2Ga30.3 (NaAu3.17Ga2.33) (VI) in a very different structure with two types of cation sites. Crystal orbital Hamilton population (COHP) analysis obtained from tight-binding electronic structure calculations for idealized I–IV via linear muffin-tin-orbital (LMTO) methods emphasized the major contributions of heteroatomic Au–Ga bonding to the structural stability of these compounds. The relative minima (pseudogaps) in the DOS curves for IV correspond well with the valence electron counts of known representatives of this structure type and, thereby, reveal some magic numbers to guide the search for new isotypic compounds. Theoretical calculation of total energies vs volumes obtained by VASP (Vienna Ab initio Simulation Package) calculations for KAu3Ga2 and RbAu3Ga2 suggest a possible transformation from SrZn5- to BaZn5-types at high pressure.

36 MATERIALS SCIENCE↗

Age related changes in the bone tissue under conditions of hypokinesia

Microroentgenography of nine young people, aged 24-29, before and after hypokinesia (16-37 days strict bed rest), showed that the heel bone density of those with initially high bone density generally decreased and that of those with initially low bone density generally increased. X-ray structural analysis of the femurs of 25 corpses of accidentally killed healthy people, aged 18-70, data are presented and discussed, with the conclusion that the bone hydroxyapatite crystal structure stabilizes by ages 20 to 25, is stable from ages 25 to 60 and decreases in density after age 60. It is concluded that bone tissue structure changes, both with age, and in a comparatively short time in hypokinesia.

Podrushnyak, E. P.↗

Materials characterization of phosphoric acid fuel cell system

The component materials used in the fabrication of phosphoric acid fuel cells (PAFC) must have mechanical, chemical, and electrochemical stability to withstand the moderately high temperature (200 C) and pressure (500 kPa) and highly oxidizing nature of phosphoric acid. This study discusses the chemical and structural stability, performance and corrosion data on certain catalysts, catalyst supports, and electrode support materials used in PAFC applications.

Venkatesh, Srinivasan↗

Elevating the Practical Application of Sodium-Ion Batteries through Advanced Characterization Studies on Cathodes

Sodium-ion batteries (SIBs) have emerged as promising alternatives to their lithium-ion counterparts due to the abundance of sodium resources and their potential for cost-effective energy storage solutions. The chemistry for SIBs has been investigated since the 1980s, but it went through a slow research and development process. Recently, there has been an acceleration in technology maturation due to a supply chain crisis originating from unequal resource distribution and sustainability and safety concerns regarding lithium-ion batteries. However, the practical application of SIBs has been hindered primarily by challenges related to cathode materials, specifically, surface and structural stabilities in different conditions. Through the integration of advanced techniques such as in situ spectroscopy, operando diffraction, and high-resolution microscopy, a comprehensive understanding of the cathode’s dynamic behavior and degradation mechanisms can be achieved. The identified structural modifications, phase transitions, and degradation pathways offer critical insights into the design of robust cathode materials with prolonged cycling stability, fast charging capability, high energy density, great low-temperature performance, and safety. This review underscores the pivotal role of cutting-edge characterization techniques in guiding the development of high-performance sodium-ion batteries, thereby fostering the realization of sustainable and efficient energy storage solutions for diverse technological applications.

25 ENERGY STORAGE↗

Alkali cation stabilization of defects in 2D MXenes at ambient and elevated temperatures

Transition metal carbides have been adopted in energy storage, conversion, and extreme environment applications. Advancements in their 2D counterparts, known as MXenes, enable the design of unique structures at the ~1 nm thickness scale. Alkali cations have been essential in MXenes manufacturing processing, storage, and applications, however, exact interactions of these cations with MXenes are not fully understood. In this study, using Ti 3 C 2 T x , Mo 2 TiC 2 T x , and Mo 2 Ti 2 C 3 T x MXenes, we present how transition metal vacancy sites are occupied by alkali cations, and their effect on MXene structure stabilization to control MXene’s phase transition. We examine this behavior using in situ high-temperature x-ray diffraction and scanning transmission electron microscopy, ex situ techniques such as atomic-layer resolution secondary ion mass spectrometry, and density functional theory simulations. In MXenes, this represents an advance in fundamentals of cation interactions on their 2D basal planes for MXenes stabilization and applications. Broadly, this study demonstrates a potential new tool for ideal phase-property relationships of ceramics at the atomic scale.

42 ENGINEERING↗

Resolving amorphous solid-liquid interfaces by atomic force microscopy

Recent advancements in liquid atomic force microscopy make it an ideal technique for probing the structure of solid-liquid interfaces. Here, we present a structural study of a two-dimensional amorphous silica bilayer immersed in an aqueous solution utilizing liquid atomic force microscopy with sub-nanometer resolution. Structures show good agreement with atomically resolved ultra-high vacuum scanning tunneling microscopy images obtained on the same sample system, owing to the structural stability of the silica bilayer and the imaging clarity from the two-dimensional sample system. Pair distance histograms of ring center positions are utilized to develop quantitative metrics for structural comparison, and the physical origin of pair distance histogram peaks is addressed by direct assessment of real space structures.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Stability and bifurcation of quasiparallel Alfven solitons

The inverse scattering transformation (IST) is used to study the one-parameter and two-parameter soliton families of the derivative nonlinear Schroedinger (DNLS) equation. The two-parameter soliton family is determined by the discrete complex eigenvalue spectrum of the Kaup-Newell scattering problem and the one-parameter soliton family corresponds to the discrete real eigenvalue spectrum. The structure of the IST is exploited to discuss the existence of discrete real eigenvalues and to prove their structural stability to perturbations of the initial conditions. Also, though the two-parameter soliton is structurally stable in general, it is shown that a perturbation of the initial conditions may change the two-parameter soliton into a degenerate soliton which, in turn, is structurally unstable. This degenerate, or double pole, soliton may bifurcate due to a perturbation of the initial conditions into a pair of one-parameter solitons. If the initial profile is on compact support, then this pair of one-parameter solitons must be compressive and rarefactive respectively. Finally, the Gelfand-Levitan equations appropriate for the double pole soliton are solved.

Hamilton, R. L.↗

S -Adenosylhomocysteine Analogs Selectively Suppress Pan-Coronavirus Replication by Inhibition of nsp14 Methyltransferase

To address the ongoing threat of SARS-CoV-2 and potential emergence of novel coronaviruses, we employed a comprehensive strategy to identify and synthesize inhibitors of coronavirus methyltransferases with chemical analogs of S-adenosylhomocysteine (SAH). Two analogs, designated 4h and 4p, inhibit both mouse hepatitis virus and SARS-CoV-2 replication. Compound 4p was the most potent with half-maximal inhibition of biochemical activity at 0.2 μM and antiviral activity at ∼20 μM. This compound also has low cytotoxicity and preferentially inhibits nsp14 over nsp16 and human methyltransferases. Furthermore, molecular docking based on a newly determined crystal structure of the apo nsp16−nsp10 complex predicts that 4p occupies both the Sadenosylmethione and Gppp binding pockets of nsp14 and nsp16. Selectivity of 4p for nsp14 is likely due to the enhanced structural stability of the nsp14 binding pocket relative to nsp16. These findings highlight SAH analogs as scaffolds for pan-coronavirus therapeutics and underscore the value of structure-guided design in antiviral drug discovery.

Coronavirus↗

Single-Phase Spinel NiCo 2 O 4 as Highly Active and Stable Electrocatalysts for Urea Oxidation Reaction in Urea Electrolysis

Exploring and designing a stable and active catalyst for the urea electro-oxidation reaction (UOR, CO(NH 2 ) 2 + 6OH – → CO 2 + N 2 + 5H 2 O + 6e – ) is crucial for the long-term sustainability of ecological systems and clean energy production. We found that spinel NiCo 2 O 4 is a stable and active electrocatalyst for UOR at a relatively low anodic potential without triggering the competing oxygen evolution reaction (OER). A urea electrolysis cell (CO(NH 2 )2 + H 2 O → CO 2 + N 2 + 2H 2 ) utilizing a spinel NiCo 2 O 4 anode and a commercial Pt cathode was further characterized through galvanostatic polarization tests, demonstrating excellent structural stability at various current densities. Post-mortem analysis of long-term urea electrolysis measurements suggested that NiCo 2 O 4 electrocatalysts maintained a stable spinel structure. However, redistribution of Ni 3+ to Ni 2+ valence on the catalyst surface was observed, in contrast to the intact Co valence, indicating that (i) Ni sites are active toward urea adsorption and sequential electro-oxidation; (ii) while urea oxidation proceeds primarily through the direct electro-oxidation mechanism, chemical reactions between the Ni 3+ site and urea occur during long-term electrochemical UOR operation. Density functional theory (DFT) simulations were used to calculate the adsorption energies of urea molecules on NiO, Co 3 O 4 , and NiCo 2 O 4 , revealing the importance of regulating the configuration of adsorbed urea molecules on the NiCo 2 O 4 surface.

36 MATERIALS SCIENCE↗

Pressure-induced crystallization of an amorphous martensite alloy

Recently, solid-state amorphization through temperature-induced martensitic transition has been reported. The stability of the amorphous martensite phase, which co-exists with a crystalline counterpart, is intriguing but remains ill-defined. In this work, we studied the structural stability of a Ti 59.1 Zr 37 Cu 2.3 Fe 1.6 amorphous martensite alloy by combining in situ high-pressure synchrotron x-ray diffraction with ex situ transmission electron microscopy. During compression at room temperature, an irreversible pressure-induced crystallization of the amorphous martensite phase into a β-Ti phase is revealed. Qualitative analysis reveals the important role of the local atomic strain in stabilizing/destabilizing amorphous martensite alloys and its high tunability of the local atomic strain under high pressure.

36 MATERIALS SCIENCE↗

Initial Developments in Modeling Graphite Behavior

Graphite is used in High Temperature Reactor designs as a moderator, reflector and core material responsible for protecting the fuel and maintaining structural stability. From a safety perspective, it is imperative to be able to predict how graphite will behave under reactor operating conditions which may compromise the core’s structural integrity or fuel’s safety performance. The following report summarizes recent modeling work undertaken at Idaho National Laboratory which focuses on graphite degradation behavior. One phenomenon which is explored in this report and can cause significant degradation to graphite properties is oxidation. Oxidation behavior in graphite is highly temperature dependent. At low temperatures, oxygen can fully penetrate a component and cause a homogeneous damage profile. At high temperatures, only the graphite near the surface of a component is affected. Understanding and modeling this temperature dependence is essential to predicting graphite behavior. In this report, three graphite models are discussed. The first model is used to investigate strength loss after low temperature oxidation. It does this by generating an approximate graphite microstructure then determining the required load to cause crack propagation. It has been shown that the model reproduces the quasi brittle stress versus strain relationship observed in graphite. Strength loss results from the model are shown to match experimental values. The second model investigates strength loss under high temperature oxidation conditions. This model is more applicable to full scale graphite components where the oxidation damage is often inhomogeneous throughout a component. The third model computes stresses in graphite under reactor conditions. Specifically, the model incorporates the effect of creep, irradiation dose, thermal strains, and oxidation in order to predict internal stresses in a component. All of these models are implemented in the Multiphysics Object-Oriented Simulation Environment (MOOSE), an open source, parallel finite element framework.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Global asymptotic stability of dynamic dissipative compensators for multibody flexible space structures

The stability characteristics of dynamic dissipative compensators are investigated for multibody flexible space structures having nonlinear dynamics. The problem addressed is that of proving asymptotic stability of dynamic dissipative compensators. The stability proof uses the Liapunov approach and exploits the inherent passivity of such systems. For such systems these compensators are shown to be robust to parametric uncertainties and unmodeled dynamics. The results are applicable to a large class of structures such as flexible space structures with articulated flexible appendages.

Kelkar, Atul G.↗

In-service Inspection of Radioactive Waste Tanks at the Savannah River Site – 15410

Liquid radioactive wastes from the Savannah River Site (SRS) separation process are stored in large underground carbon steel tanks. The high level wastes are processed in several of the tanks and then transferred by piping to other site facilities for further processing before they are stabilized in a vitrified or grout waste form. Based on waste removal and processing schedules, many of the tanks will be required to be in service for times exceeding the initial intended life. Until the waste is removed from storage, transferred, and processed, the materials and structures of the tanks must maintain a confinement function by providing a barrier to the environment and by maintaining acceptable structural stability during design basis events, which include loadings from both normal service and abnormal (e.g., earthquake) conditions. A structural integrity program is in place to maintain the structural and leak integrity functions of these waste tanks throughout their intended service life. In-service inspection (ISI) is an essential element of a comprehensive structural integrity program for the waste tanks at the Savannah River Site (SRS). The ISI program was developed to determine the degree of degradation the waste tanks have experienced due to service conditions. As a result of the inspections, an assessment can be made of the effectiveness of corrosion controls for the waste chemistry, which precludes accelerated localized and general corrosion of the waste tanks. Ultrasonic inspections (UT) are performed to detect and quantify the degree of general wall thinning, pitting and cracking as a measure of tank degradation. The results from these inspections through 2013, for the 27 Type III/IIIA tanks, indicate no reportable in-service corrosion degradation in the primary tank (i.e., general, pitting, or cracking). The average wall thickness for all tanks remains above the manufactured nominal thickness minus 0.25 millimeter and the largest pit identified is approximately 1.70 millimeter deep (i.e., less than 10% through-wall). Improvements to the inspection program were recently instituted to provide additional confidence in the degradation rates. Thickness measurements from a single vertical strip along the accessible height of the primary tank have been used as a baseline to compare historical measurements. Changes in wall thickness and pit depths along this vertical strip are utilized to estimate the rate of corrosion degradation. An independent review of the ISI program methodology, results, and path forward was held in August 2009. The review recommended statistical sampling of the tanks to improve the confidence of the single strip inspection program. The statistical sampling plan required that SRS increase the amount of area scanned per tank. Therefore, in addition to the baseline vertical strip that is obtained for historical comparisons, four additional randomly selected vertical strips are inspected. To date, a total of 104 independent vertical strips along the height of the primary tank have been completed. A statistical analysis of the data indicates that at this coverage level there is a 99.5% confidence level that one of the worst 5% of all the vertical strips was inspected. That is, there is a relatively high likelihood that the SRS inspection program has covered one of the most corroded areas of any of the Type III/IIIA waste tanks. These data further support the conclusion that there are no significant indications of wall thinning or pitting. Random sampling will continue to increase the confidence that one of the worst 5% has been inspected. In order to obtain the additional vertical strips, and minimize budget and schedule impacts, data collection speed for the UT system was optimized. Prior to 2009, the system collected data at a rate of 32 square centimeters per minute. The scan rate was increased to 129 - 160 square centimeters per minute by increasing the scanner step and pixel sizes in the data acquisition set-up. Laboratory testing was utilized to optimize the scan index/pixel size such that the requirements for wall thinning and pit detection were still maintained. SRS continues to evaluate improvements to ultrasonic equipment.