Search NASA⌕ Search

SEARCH · Search NASA

Results for “CORROSIVE”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 811 records · Page 45

Corrosion of high temperature alloys in solar salt at 400, 500, and 680ÀC.

Corrosion tests at 400, 500, and 680ÀC were performed using four high temperature alloys; 347SS, 321SS In625, and HA230. Molten salt chemistry was monitored over time through analysis of nitrite, carbonate, and dissolved metals. Metallography was performed on alloys at 500 and 680ÀC, due to the relatively thin oxide scale observed at 400ÀC. At 500ÀC, corrosion of iron based alloys took the form of chromium depletion and iron oxides, while nickel based alloys also had chromium depletion and formation of NiO. Chromium was detected in relatively low concentrations at this temperature. At 680ÀC, significant surface corrosion occurred with metal losses greater than 450microns/year after 1025hours of exposure. Iron based alloys formed complex iron, sodium, and chromium oxides. Some data suggests grain boundary chromium depletion of 321SS. Nickel alloys formed NiO and metallic nickel corrosion morphologies, with HA230 displaying significant internal oxidation in the form of chromia. Nickel alloys both exhibited worse corrosion than iron based alloys likely due to preferential dissolution of chromium, molybdenum, and tungsten.

Kruizenga, Alan Michael↗

Micro-Continuum Modeling of Nuclear Waste Glass Corrosion

The purpose of this contribution is to report on preliminary nano-continuum scale modeling of nuclear waste glass corrosion. The focus of the modeling is an experiment involving a French glass SON68 specimen leached for 25 years in a granitic environment (Guittonneau et al., 2011; Gin et al., 2011; Gin et al., 2013). The 25 year experiment carried out by French scientists offers a unique opportunity to examine the controls on the rate of nuclear glass corrosion under controlled experimental conditions using a borosilicate glass of the kind widely considered for nuclear waste storage. The long term experiment makes it possible to move beyond the initial rate stage, with direct measurements of the longer term, residual rates of corrosion. Important in this regard is whether the rate of corrosion shows a parabolic dependence on time, as would be expected from a conventional diffusion model in which the reaction products (amorphous silica-rich gel) create a diffusion barrier that grows in width over time, or whether the time dependence is linear (Guittonneau et al., 2011). A linear dependence on time would call into question the model of a Passive Reactive Interface (PRI) presented by Cailleteau et al. (2008), although it does not entirely preclude such a model if the interface maintains a constant width over time (forming at the leading edge next to the pristine glass and dissolving at the trailing edge). The leachate concentration measurements collected every 56 days over 25 years by Guittonneau et al. (2011) provide data to constrain the long term corrosion rate and its time dependence.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Inorganic Corrosion-Inhibitive Pigments for High-Temperature Alkali-activated Well Casing Foam Cement

This study evaluates inorganic pigments for improving carbon steel (CS) brine-corrosion protection by the sodium metasilicate-activated calcium aluminate cement/Fly Ash blend at 300 °C. Calcium borosilicate (CBS) and zinc phosphate, significantly improved CS corrosion-protection by decreasing cement’s permeability for corrosive ions and inhibiting anodic corrosion. An amorphous Na 2 O-Al 2 O 3 -SiO 2 -H 2 O phase tightly attached to CS surface formed at 300 °C in CBS-modified cement pore solution. The corrosion rate of the CS covered with this phase was nearly 4-fold lower than in the case of nonmodified cement pore solution where the major phase formed on the surface of CS was crystalline analcime.

15 GEOTHERMAL ENERGY↗

Inorganic Corrosion-Inhibitive Pigments for High-Temperature Alkali-activated Well Casing Foam Cement

This study evaluates inorganic pigments for improving carbon steel (CS) brine-corrosion protection by the sodium metasilicate-activated calcium aluminate cement/Fly Ash blend at 300°C. Calcium borosilicate (CBS) and zinc phosphate, significantly improved CS corrosion-protection by decreasing cement’s permeability for corrosive ions and inhibiting anodic corrosion. An amorphous Na 2 O-Al 2 O 3 -SiO 2 -H 2 O phase tightly attached to CS surface formed at 300oC in CBS-modified cement pore solution. The corrosion rate of the CS covered with this phase was nearly 4-fold lower than in the case of nonmodified cement pore solution where the major phase formed on the surface of CS was crystalline analcime.

15 GEOTHERMAL ENERGY↗

FY17 Status Report: Research on Stress Corrosion Cracking of SNF Interim Storage Canisters.

This progress report describes work done in FY17 at Sandia National Laboratories (SNL) to assess the localized corrosion performance of container/cask materials used in the interim storage of spent nuclear fuel (SNF). Of particular concern is stress corrosion cracking (SCC), by which a through-wall crack could potentially form in a canister outer wall over time intervals that are shorter than possible dry storage times. Work in FY17 refined our understanding of the chemical and physical environment on canister surfaces, and evaluated the relationship between chemical and physical environment and the form and extent of corrosion that occurs. The SNL corrosion work focused predominantly on pitting corrosion, a necessary precursor for SCC, and process of pit-to-crack transition; it has been carried out in collaboration with university partners. SNL is collaborating with several university partners to investigate SCC crack growth experimentally, providing guidance for design and interpretation of experiments.

36 MATERIALS SCIENCE↗

Collective Summary of sCO2 Materials Development Part II: High-Temperature Alloy Corrosion Behavior within Compact Heat Exchangers.

Materials compatibility is a major concern for the design and operation of supercritical carbon dioxide (sCO2) power cycles. Two areas were recently identified for which very little prior knowledge was available. These were the behavior of polymer materials in low-temperature sCO2 environments as well as the high-temperature corrosion behavior for alloys that have been fabricated into compact heat exchangers. A critical need exists to increase understanding in both areas. As such, the Sandia sCO2 Materials Development program initiated a series of experiments for both areas in FY19. The progress that has been made in understanding the behavior of polymers in sCO2 was summarized in the Part I report, while this Part II report describes progress in the area of compact heat exchanger corrosion. For the compact heat exchangers being developed for use in supercritical CO2 power cycles, alloy corrosion is important to understand as it may lead to reduced flow path area, reduced heat transfer, and blocked flow channels. The fabrication of these heat exchangers involve thermal processes such as brazing or diffusion bonding, where the influence of these processes on the corrosion behavior of the alloys is unknown. Candidate alloys for these heat exchangers are typically evaluated for corrosion behavior as witness coupons, without being subjected to these thermal processes. To close this gap in understanding, a series of experiments were completed that utilized small heat exchanger samples subjected to flowing CO2 for 500 hours at 750°C. Small sections of the heat exchanger samples were characterized before and after the 500 hour exposure in order to characterize the oxide growth in the channels as well as the hardness of the alloys. Results are compared to witness coupons of the same alloys.

36 MATERIALS SCIENCE↗

Analysis of Microbial Communities as Indicators of Microbially Induced Corrosion Potential in Stainless Steel Piping

The 200 West Area Pump-and-Treat (200W P&T) facility is part of the final remedy decision for the 200 ZP-1 Operable Unit (OU) and is the interim remedial action for 200-UP-1 OU at the Hanford Site. The facility also treats water from other sources across the site, including 200-DV-1 OU perched water, groundwater from the 200-BP-5 OU, and leachate from the Environmental Restoration Disposal Facility. The facility originally operated a biological treatment process for nitrate that resulted in systemic biofouling and loss of injection well capacity, requiring frequent and costly well rehabilitation. Biofouling has also contributed to corrosion of welds and pitting of stainless-steel piping at the facility. The biological treatment for nitrate was suspended at the end of 2019 calendar year to eliminate negative impacts from biological treatments which improve facility operations and treatment of carbon tetrachloride. Evaluation of the 200W P&T facility’s response to operational improvements, specifically the suspension of the biological treatment, provides information on the potential for continued microbially induced corrosion (MIC). To this end, historical data sets (2015-2017) were compared with molecular biological analyses of 200W P&T water samples from 2018-2020 to quantify trends in total microbial biomass and specific microbial indicator species (iron, sulfate, nitrate, and manganese reducing bacteria) known to cause and enhance metal corrosion. Results showed unequivocal reductions (in excess of 90%) in all microbiological indicators measured following the suspension of the biological treatment. Although abundance measurements for all corrosive MIC populations initially declined after removal of the treatment system, nitrate-reducing bacteria (nirK) and sulfate-reducing bacteria remain highly abundant in the system, an order of magnitude higher than the number of cells present prior to the removal of the biological treatment system [5.14e (1.4) cells/L, vs. 1.14e (0.07) cells/L, reported as average (±SD) for n=3]. In addition, there was an unexpected inflection point in 2019 where all microbial indicators increased unexpectedly in abundance in 2020 by as much as two orders of magnitude compared to 2019 samples. Given the limited number of water samples available for this analysis, the cause of the increase in microbial indicators post-biological treatment has not yet been determined. Systematic sampling of the facility for continued monitoring is recommended so that the responses of MIC populations can be evaluated to ensure that further corrosion is avoided, allowing the 200W P&T facility to operate safely and efficiently at design capacity.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Corrosion Analysis of 121103072 (SAVY-4000)

A surveillance feedlist for fiscal year (FY) 2022 was developed with the intent to target containers with contents known to generate corrosive gasses. One SAVY-4000 (hereafter “SAVY”) container with a serial number 121103072 was selected due to the reasonable wattage and known molten salt extraction (MSE) material corrosive behavior. The material was measured at 3.08 W with approximately 200 g of material placed inside of the SAVY for 6.07 years. The inner packaging configuration included a ¼ Qt stainless steel slip top inner container and a sPVC bag-out bag enclosing the inner container. Visual observations of the container during retrieval revealed several concerning features on the exterior of the container, notably on the lid. Fig. 1 shows the container lid along with an inset image further magnifying the features of interest. The corroded tamper indicating device (TID) wire and the corroded radioactive material tag wire indicated that corrosive gas species for steel were produced during storage. Although the TID wire and rad tag wire are not the same composition as the SAVY body and lid, these are often used as an indicator of potential corrosion inside of the SAVY container. The oxide residing inside of the filter holes and significant buildup around one hole provided further evidence supporting the presence of corrosive species inside of the container.

36 MATERIALS SCIENCE↗

Multi-Parameter Optical Fiber for Distributed Sensing of Humidity, CH4, CO2, and Corrosion

This work describes the use of the optical fiber sensor (OFS) for successful monitoring of humidity, CH4, and CO2 based on the strain produced along the single-mode fiber (SMF) sensor. This is enabled by absorption of H2O/gases onto the commercially available polyacrylate coated jacketed portion of the fiber resulting in a change in strain. Under equilibrium, a differential microstrain was observed along the jacketed portion of the SMF with N2, CH4, and CO2 at different relative humidity (RH) conditions. The strain response of the SMF under various mixed gas composition and different RH conditions were also measured and made calibration curves accordingly. Linear regression and principal component analysis of the strain datasets provided deconvolution of the impact of strain from H2O, N2, CH4, and CO2. Additionally, modified OFS comprised of the Fe coated fiber section was employed to monitor corrosion based on the increase in backscattered intensity amplitude of the light being passed once corrosion of Fe occurs. Also, corrosion of Fe was studied under soil by installing the fiber in soil with protective measures which would prevent the sensor being mechanically disturbed or broken during installation. The corrosion rates were studied by monitoring the rate at which the intensity of backscattered light amplitude attains a steady state value when complete corrosion of Fe with a specific coating thickness occurs.

Mainali, Badri↗

Applied Research and Development to Support Open Water Testing at PacWave – Task 5: Development of additively manufactured, functionally graded, corrosion resistant clads for wave energy applications

In this task, we focused on developing corrosion-resistant claddings for wave energy applications. Wave energy systems are exposed to saline conditions, which are corrosive to many metallic structural materials (e.g., carbon steel). Corrosion-resistant (stainless) steels are typically alloyed with >18% chromium (Cr) and >8% nickel (Ni), which dramatically raises material costs and can hinder the development of wave energy systems; thus, coatings are a necessary corrosion protection method for most. Non-metallic coatings (paint, epoxy) have shorter service lives, limited resistance to mechanical stress and wear, plus additional costs of inspection and eventual replacement. Therefore, overlay stainless steel (SS) claddings have a cost-effective use case for protecting components from corrosion, particularly for those that may be subject to mechanical stress / wear and with long service lives.

16 TIDAL AND WAVE POWER↗

Degradation science: Integrating modeling and experiments to predict localized corrosion processes (Annual Progress Report)

Additively manufactured (AM) eutectic high-entropy alloys (EHEAs), such as nano-lamellar AlCoCrFeNi 2.1 , have excellent strength, ductility, and wear resistance even at elevated temperatures, but their corrosion behavior in aggressive acids at different length scales remain poorly understood. This work investigates the corrosion behavior of laser powder bed–fused (L-PBF) AlCoCrFeNi 2.1 as a function of annealing temperatures, probing degradation mechanisms from nanoscopic to macroscopic length scales. The alloy is dual phase consisting of a ductile FCC L1 2 phase and a high-strength BCC B2 phase. Rapid solidification during L-PBF produces a far-from-equilibrium nano-lamellar structure with nearly homogeneous elemental distribution, which tends to evolve upon annealing toward Cr/Co/Fe-enriched FCC and Al/Ni-enriched B2. Three conditions were studied: as-printed, 600 °C/5 h, and 1000 °C/1 h, over which B2 lamellae coarsen, lamellar spacing increases, and elemental segregation becomes more prominent. Microstructure and chemistry were characterized by scanning electron microscopy (SEM) and energy-dispersive spectroscopy (EDS), while in-situ electrochemical atomic force microscopy (EC-AFM) was used to link early (<5 h) local dissolution to microstructure after exposure in sulfuric acid. EC-AFM highlights preferential dissolution of the BCC/B2 phase where the surrounding matrix is Cr-depleted and directly quantifies the dissolution rates within individual phases, tracks the transition from early nano-scale attack to partial repassivation, to correlate height differences with current and impedance responses. To monitor longer-term behavior (up to 96 h), ex-situ AFM, SEM, and confocal imaging were combined with conventional bulk electrochemical tests, bridging nanoscale observations to micro/meso-scale damage morphologies. At the meso-scale, the deepest dissolution channels align with the build-direction lamellae and melt-pool boundaries, indicating that printing directionality guides the propagation of these localized corrosion sites. Annealing modifies corrosion by restructuring BCC/FCC phase fractions, lamellar spacing, and Cr/Al segregation, thereby changing the cathode/anode ratio and passive film stability. The results clarify how as-printed and annealed nano-lamellar architectures differ in their susceptibility to selective dissolution; how elemental segregation competes with residual stresses along the build direction. With these insights, future work will use CALPHAD-guided alloy modification to stabilize higher Cr contents in the B2 phase while retaining a dominant FCC+B2/BCC microstructure, with the goal of designing mechanically robust, corrosion-resistant EHEAs for safety-critical applications to leverage the LLNL’s broader national and global security mission.

36 MATERIALS SCIENCE↗

ZM-21 magnesium alloy corrosion properties and cryogenic to elevated temperature mechanical properties

The mechanical properties of bare ZM-21 magnesium alloy flat tensile specimens were determined for test temperatures of +400 F, +300 F, +200 F, +80 F, 0 F, -100 F, -200 F, and -320 F. The ultimate tensile and yield strengths of the material increased with decreasing temperature with a corresponding reduction in elongation values. Stress corrosion tests performed under: (1) MSFC atmospheric conditions; (2) 95% relative humidity; and (3) submerged in 100 ppm chloride solution for 8 weeks indicated that the alloy is not susceptible to stress corrosion. The corrosion tests indicated that the material is susceptible to attack by crevice corrosion in high humidity and chemical type attack by chloride solution. Atmospheric conditions at MSFC did not produce any adverse effects on the material, probably due to the rapid formation of a protective oxide coating. In both the mechanical properties and the stress corrosion evaluations the test specimens which were cut transverse to the rolling direction had superior properties when compared to the longitudinal properties.

Montana, J. W.↗

Apollo experience report: The problem of stress-corrosion cracking

Stress-corrosion cracking has been the most common cause of structural-material failures in the Apollo Program. The frequency of stress-corrosion cracking has been high and the magnitude of the problem, in terms of hardware lost and time and money expended, has been significant. In this report, the significant Apollo Program experiences with stress-corrosion cracking are discussed. The causes of stress-corrosion cracking and the corrective actions are discussed, in terminology familiar to design engineers and management personnel, to show how stress-corrosion cracking can be prevented.

Johnson, R. E.↗

Effect of a chromium-containing fuel additive on hot corrosion

Four cast superalloys (one cobalt-base and three nickel-base) were tested at 900 C for 100 h in Mach 0.3 combustion gases. 5 ppm of synthetic sea salt were added to the gases in the combustion chamber. Several types of thermal cycle and washing procedures were employed. Similar tests were made with the addition of 300 ppm of a chromium-containing fuel additive. In both sets of tests the extent of hot corrosion was evaluated by specific weight change and metal recession. In general, the chromium additive in the fuel reduced the extent of hot (salt) corrosion but did not eliminate it. The percentage reduction of hot corrosion attack was similar for all four alloys. As great a reduction of hot corrosion was achieved by reducing the number of thermal cycles during the test from 100 to 5 or 6. The effect of washing the alloys every ten cycles as opposed to the end of the test was erratic; some alloys were attacked slightly more, others somewhat less. A NiCrAlY coating was found to be more effective in reducing hot corrosion than either the fuel additive or the washing schedule.

Lowell, C. E.↗

Chemical processes involved in the initiation of hot corrosion of B-1900 and NASA-TRW VIA

Sodium surface-induced hot corrosion of B-1900 and NASA-TRW VIA alloys at 900 C has been studied, with special attention to the chemical reactions during and immediately after the induction period. Thermogravimetric tests were run and data were obtained by chemical analysis of water soluble metal salts and of residual sulfate. Surface analyses of hot corroded samples were obtained by spectroscopic techniques (ESCA). A chemical mechanism for elucidating Na2SO4-induced hot corrosion is proposed indicating that hot corrosion is initiated by basic fluxing of the protective Al2O3 scale. The sequential, catastrophic corrosion results from molybdenum content. The self-sustaining feature is a consequence of the cyclic nature of the acidic fluxing. It is believed that the mechanism is applicable not only to laboratory results, but also to the practical problem of hot corrosion encountered in gas turbine engines.

Fryburg, G. C.↗

Corrosion of 310 stainless steel in H2-H2O-H2S gas mixtures: Studies at constant temperature and fixed oxygen potential

Corrosion of SAE 310 stainless steel in H2-H2O-H2S gas mixtures was studied at a constant temperature of 1150 K. Reactive gas mixtures were chosen to yield a constant oxygen potential of approximately 6 x 10 to the minus 13th power/cu Nm and sulfur potentials ranging from 0.19 x 10 to the minus 2nd power/cu Nm to 33 x 10 to the minus 2nd power/cu Nm. The kinetics of corrosion were determined using a thermobalance, and the scales were analyzed using metallography, scanning electron microscopy, and energy dispersive X-ray analysis. Two corrosion regimes, which were dependent on sulfur potential, were identified. At high sulfur potentials (p sub S sub 2 less than or equal to 2.7 x 10 to the minus 2nd power/cu Nm) the corrosion rates were high, the kinetics obeyed a linear rate equation, and the scales consisted mainly of sulfide phases similar to those observed from pure sulfication. At low sulfur potentials (P sub S sub 2 less than or equal to 0.19 x 10 to the minus 2nd power/cu Nm) the corrosion rates were low, the kinetics obeyed a parabolic rate equation, and scales consisted mainly of oxide phases.

Rao, D. B.↗

High temperature alkali corrosion in high velocity gases

The effects of potential impurities in coal derived liquids such as Na, K, Mg, Ca and Cl on the accelerated corrosion of IN-100, U-700, IN-792 and Mar-M509 were investigated using a Mach 0.3 burner rig for times to 1000 hours in one hour cycles. These impurities were injected in combination as aqueous solutions into the combustor of the burner rig. The experimental matrix utilized was designed statistically. The extent of corrosion was determined by metal recession. The metal recession data were fitted by linear regression to a polynomial expression which allows both interpolation and extrapolation of the data. As anticipated, corrosion increased rapidly with Na and K, and a marked maximum in the temperature response was noted for many conditions. In contrast, corrosion decreased somewhat as the Ca, Mg and Cl contents increased. Extensive corrosion was observed at concentrations of Na and K as low as 0.1 PPM at long times.

Lowell, C. E.↗