Search NASA⌕ Search

SEARCH · Search NASA

Results for “Doping”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 883 records · Page 49

Synthesis and Characterization of Er-Doped Nano ZnO Samples

Pure and erbium-doped ZnO nanoparticles (Zn{sub 1−x}Er{sub x}O), (0.00 ≤ x ≤ 0.10), were synthesized by wet chemical co-precipitation method. The structural, optical, and magnetic properties of the prepared samples were investigated using x-ray powder diffraction (XRD), transmission electron microscopy (TEM), ultraviolet-visible spectroscopy (UV), Fourier transform infrared spectroscopy (FTIR), M-H magnetic hysteresis, and electron paramagnetic resonance (EPR). XRD studies exhibit the presence of a single ZnO wurtzite hexagonal crystal structure for 0.00 ≤ x ≤ 0.06. A secondary phase of Er{sub 2}O{sub 3} appears for x > 0.06. This means that the solubility limit for doping Zn{sup 2+} ions by Er{sup 3+} ions is about x = 0.06 under our preparations condition. The lattice parameter a is not affected by the Erbium doping. On the other hand, the lattice parameter c and the unit cell volume V increase with the increase of x up to x = 0.06. This is attributed to the larger ionic size of Er{sup 3+} ions (0.88 Å) compared to Zn{sup 2+} ions (0.74 Å). Both c and V decrease for x > 0.06. TEM micrographs indicate that the shape and the size of the ZnO nanoparticles are modified by changing the doping level of Er. The UV measurements point out that band gap energy E{sub g} decreases with the increase of x up to x = 0.06. Then, it increases for both x = 0.08 and 0.10. FTIR spectra confirm the presence of O–H and Zn–O stretching modes at 3451.963 and 428.901 cm{sup − 1}, respectively, in pure and doped ZnO samples. The Zn–O stretching mode shifts toward a lower wavenumber for x = 0.06 and toward a higher wavenumber for x = 0.10. M-H hysteresis analysis, at room temperature, reveals that the pure ZnO has a ferromagnetic signal combined with diamagnetic and paramagnetic contributions. This ferromagnetism is reduced for the doped samples up to x = 0.02, and an antiferromagnetic alignment appears for 0.04 ≤ x ≤ 0.10. The saturation magnetization (M{sub s}), the coercivity (H{sub c}), the retentivity (M{sub r}), the anisotropy constant (K{sub a}), and the magnetic moment (μ{sub m}) were estimated and discussed in terms of erbium doping for the different samples. EPR spectra for Zn{sub 1−x}Er{sub x}O were measured at room temperature in order to study the effect of Er substitution on the g value, resonance field (H{sub r}), peak to peak line width (ΔH{sub pp}) and spin–spin relaxation time constant (T{sub 2}).

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Magnetic Properties of La-Doped ZnO(0001)–Zn Polar Surface with and without Vacancies: a First-Principle Study

The effects of La doping with and without vacancies on the magnetism of a ZnO(0001)–Zn polar surface were studied using the generalized gradient approximation + U (GGA + U) method of density functional theory to determine the magnetism source of La-doped ZnO. Results revealed that La doping with O vacancy did not cause ZnO ferromagnetism, but La-doped ZnO with Zn vacancy was ferromagnetic. The net magnetic moment was primarily related to the unpaired electron amount of the O 2p state and slightly modified by orbital and anomalous magnetic moments. The anomalous magnetic moment originated from the radiating magnetism moment via quantum electrodynamics and was confirmed to exist via theoretical calculations of magnetism. Formation energy showed that La doping easily generated Zn vacancies in ZnO, but magnetic quenching occurred when the ratio of La ions to Zn vacancies was 2:1. The unpaired O 2p electrons induced by Zn vacancies were the magnetism source of La-doped ZnO. Moreover, the Curie temperature of La-doped ZnO with Zn vacancy reached room temperature. Results showed that the ZnO(0001)–Zn polar surface can be utilized as the surface of ZnO-based diluted magnetic semiconductors because of its unipolarity.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effects of Ag Doping and Point Defect on the Magnetism of ZnO

The magnetism sources and magnetic mechanism of Ag doping and point defect, which coexist in the presence of ZnO, are frequently controversial. To solve these problems, the effects of Ag doping and Zn or O vacancy on the magnetism of ZnO were investigated using geometry optimization and energy calculation according to the first-principles generalized gradient approximation + U (GGA+U) method of density functional theory. Results revealed that the system which Ag doping and Zn vacancy coexists in ZnO could achieve room-temperature ferromagnetism. This system had an extremely high spin polarization, which was advantageous for the spin electron injection sources applied in dilute magnetic semiconductors. Result also revealed that the magnetism of Zn{sub 14}AgO{sub 16} was caused by the electron hybrid coupling effects among the O-2p, Ag-4d, Ag-5s, and Zn-4s orbits. And these effects were produced by the hole carriers after complexes were formed by the Ag doping and Zn vacancy. With regard to the most stable structure of the ground state, all doping systems which Ag replacing Zn and O vacancy coexisted in ZnO and those which Ag replacing Zn, interstitial Ag, and O vacancy coexisted in ZnO were all non-magnetic. Thus, these doping systems were unsuitable for dilute magnetic semiconductors. By contrast, the doping systems of interstitial Ag and Zn vacancy were magnetic, although the magnetism was relatively weak, thus rendering such systems inapplicable as well.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Magnetic Properties of Carbon Co-Doped (Zn,Mn)O Using LDA and LDA-SIC Approximations

In this paper, we used the ab-initio calculations, based on the Korringa-Kohn-Rostoker (KKR) method combined with the coherent potential approximation (CPA), to simulate the magnetic properties of ZnO, doped and co-doped with manganese and carbon, respectively. For this purpose, we have used two different approximations: the Local Density Approximation (LDA) and the Local Density Approximation-Self-Interaction Correction (LDA-SIC). Numerical results are presented for the compound Zn{sub 1 − 0.06}Mn{sub 0.06}O{sub 1−x}C{sub x} when doping and co-doping is performed with Mn and C as doping elements. Total and partial DOSs are given for different concentrations using the two approximations, LDA and LDA-SIC. It is found that for 6% with doping by Mn the system becomes magnetic. The co-doping with carbon changes the behavior of the system : it becomes also magnetic for 4, 6 and 10% concentrations within both, LDA and LDA-SIC approximations. Furthermore, we have discussed the type of mechanism of exchange interaction and found that the double exchange is responsible for the appearing magnetism in the system, within the LDA and p-d interaction for LDA-SIC approximation. For 10% of carbon, we have found that the critical temperature approaches 280 K in the LDA approximation solely; and is about 305 K in the LDA-SIC approximation.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Benchmark Analysis on Magnetic and Photoluminescence Properties of Selective Metal Ions Doped ZnS Nanoparticles

The creation of diluted magnetic semiconductors (DMSs) at lower dimensions that exhibit room temperature ferromagnetism (RTFM) has been given immense significance for the fabrication of a new class of spintronic devices through utilizing spin degrees of freedom besides charge nature of electrons. In this view, nanocrystals of ZnS doped with 4% concentration of Fe, Co, Ni, Cr, Mn, Sr, Cu, and Ce have been synthesized at room temperature (RT) by chemical co-precipitation method. The samples were examined by various characterization techniques like energy dispersive spectroscopy (EDS), X-ray diffraction (XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM), vibrating sample magnetometer (VSM), and photoluminescence (PL). EDS spectra revealed the existence of parent elements in the prepared samples. XRD characterization disclosed hexagonal structures of nanocrystals, and no secondary phases were observed in all the samples except for Cu and Ni doped ZnS. FTIR data confirmed the proper substitution of dopants in the host lattice as all the graphs have almost same stretchings. The magnetic nature of each sample was evaluated from M-H graphs of VSM, and it corroborated the transition of magnetic properties due to doping. Pristine ZnS showed diamagnetic nature, while Fe and Sr doped ZnS evinced strong ferromagnetic and anti-ferromagnetic properties, respectively. Photoluminescence studies on Ce, Sr and Mn doped ZnS samples revealed strong emission peaks with enhanced luminescence properties compared to bare ZnS. Cu, Cr and Mn doped ZnS exhibited a red shift in emission wavelengths, whereas Co doped ZnS showed emission peak shifted towards the blue region as compared to the host lattice.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Co doping effect on structural and optical properties of nickel oxide (NiO) thin films via spray pyrolysis

Undoped and cobalt doped nickel oxide thin films (Co:NiO) at different doping concentrations were deposited on a glass substrate at constant substrate temperature by spray pyrolysis. The doping percentage increased from 0 to 10% and the effects of doping content on structural, morphological and optical properties were explored by X-ray diffraction, atomic force microscopy and UV–visible spectroscopy, respectively. X-ray diffraction configurations proved the NiO thin films were polycrystalline in nature having a cubic crystal structure. The regularly used parameters such as crystallite size, micro-strain, dislocation density and texture coefficient are presented from structural data. The average crystallite size is found between 10 and 14 nm with cobalt doping (Co) concentration. The band gap energies were increased with the effect of Co doping concentration in the range between 2.10 and 2.50 eV. The various optical constants as a function of photon energy are modified with Co doping concentration.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Optical and Electrical Properties of Sn-Doped Zinc Oxide Single Crystals

Here, Sn dopant in ZnO may significantly improve the n-type conductivity of ZnO through a characteristic double effect. However, studies on bulk Sn-doped ZnO are rare, and the effect of Sn doping on the optoelectronic properties of bulk ZnO is not well understood. In this work, the effect of Sn doping on the optical and electrical properties of ZnO bulk single crystals was investigated through optical absorption spectroscopy, Hall-effect measurements, and thermoluminescence (TL) spectroscopy. Undoped and Sn-doped ZnO single crystals were grown by chemical vapor transport method and characterized by x-ray diffraction analysis. The Sn doping level in the crystals was evaluated by inductively coupled plasma mass spectroscopy measurements. Hall-effect measurements revealed an increase in conductivity and carrier concentration with increasing Sn doping, while TL measurements identified a few donor species in the crystals with donor ionization energy ranging from 35 meV to 118 meV. Increasing Sn doping was also associated with a color change of single crystals from colorless to dark blue.

36 MATERIALS SCIENCE↗

Ultra-Shallow Doping B, Mg, Ni, Cu, Mn, Cr and Fe into SiC with Very High Surface Concentrations Based on Plasma Stimulated Room-Temperature Diffusion

Very recently, we reported a novel doping method called plasma doping without any external bias (PDWOEB) for the introduction of some impurities into Si and GaN at room temperature (RT). In this work, the RT doping of some impurities, including B, Mg, Ni, Cu, Mn, Cr and Fe, into SiC with ultra-shallow depths of tens of nanometer and very high surface concentrations, approaching or exceeding 1E20/cm{sup 3}, by using PDWOEB is reported. It has been found for the first time that the doping depths and surface concentrations of these impurities doped into SiC by the PDWOEB increase drastically with increasing doping time and the ferromagnetism of SiC due to Ni doping is demonstrated. Moreover, the approximate diffusivities of B, Mg, Ni, Cu, Mn, Cr and Fe in SiC at RT under plasma stimulation are obtained. The physical mechanism of PDWOEB is further discussed, and some unclear viewpoints are clarified.

36 MATERIALS SCIENCE↗

Unraveling the advances of trace doping engineering for potassium ion battery anodes via tomography

Doping have been considered as a prominent strategy to stabilize crystal structure of battery materials during the insertion and removal of alkali ions. The instructive knowledge and experience acquired from doping strategies predominate in cathode materials, but doping principle in anodes remains unclear. Here, we demonstrate that trace element doping enables stable conversion-reaction and ensures structural integrity for potassium ion battery (PIB) anodes. With a synergistic combination of X-ray tomography, structural probes, and charge reconfiguration, we encode the physical origins and structural evolution of electro-chemo-mechanical degradation in PIB anodes. By the multiple ion transport pathways created by the orderly hierarchical pores from “surface to bulk” and the homogeneous charge distribution governed in doped nanodomains, the anisotropic expansion can be significantly relieved with trace isoelectronic element doping into the host lattice, maintaining particle mechanical integrity. Our work presents a close relationship between doping chemistry and mechanical reliability, projecting a new pathway to reengineering electrode materials for next-generation energy storage.

25 ENERGY STORAGE↗

Synthesis and characterization of Gd-doped magnetite nanoparticles

There has been rising interest in the synthesis of magnetite nanoparticles due to their importance in biomedical and technological applications. Tunable magnetic properties of magnetite nanoparticles to meet specific requirements will greatly expand the spectrum of applications. Tremendous efforts have been devoted to studying and controlling the size, shape and magnetic properties of magnetite nanoparticles. We investigate gadolinium (Gd) doping to influence the growth process as well as magnetic properties of magnetite nanocrystals via a simple co-precipitation method under mild conditions in aqueous media. Gd doping was found to affect the growth process leading to synthesis of controllable particle sizes under the conditions tested (0–10 at% Gd 3+ ). Typically, undoped and 5 at% Gd-doped magnetite nanoparticles were found to have crystal sizes of about 18 and 44 nm, respectively, supported by X-ray diffraction and transmission electron microscopy. These results showed that Gd-doped nanoparticles retained the magnetite crystal structure, with Gd 3+ randomly incorporated in the crystal lattice, probably in the octahedral sites. The composition of 5 at% Gd-doped magnetite was Fe (3-x) Gd x O 4 (x=0.085±0.002), as determined by inductively coupled plasma mass spectrometry. 5 at% Gd-doped nanoparticles exhibited ferrimagnetic properties with small coercivity (~65 Oe) and slightly decreased magnetization at 260 K in contrast to the undoped, superparamagnetic magnetite nanoparticles. Templation by the bacterial biomineralization protein Mms6 did not appear to affect the growth of the Gd-doped magnetite particles synthesized by this method.

36 MATERIALS SCIENCE↗

Statistical fracture behavior of doped UO 2 using a ball-on-ring equibiaxial flexure test method

Metal oxide dopants, such as titanium and chromium oxides, have garnered considerable attention for their potential to increase grain size (≥ 30 µm) in UO 2 fuel, purportedly enhancing fission gas retention during reactor operation. Fuel performance is significantly impacted by fuel fracture behavior, so it is important to understand the effects of enhanced grain size and dopant content on UO 2 fuel fracture. UO 2 pellets were doped with 0.1 wt% TiO 2 and 0.3 wt% Cr 2 O 3 to alter density and grain size. Inductively coupled plasma mass spectroscopy measured dopant levels pre- and post-sintering. X-ray diffraction revealed lattice changes and microstrain via Rietveld refinement. Field emission scanning electron microscopy determined grain sizes of approximately 30 µm for TiO 2 doping and 7 µm for Cr 2 O 3 doping. Transverse rupture strength tests were performed on over 30 samples per dataset to obtain characteristic strength and Weibull modulus. Results indicate no statistical difference in fracture strength between 0.1 wt% TiO 2 doped UO 2 and undoped UO 2 , while 0.3 wt% Cr 2 O 3 doped UO 2 exhibited a 20% decrease in fracture strength. Doped UO 2 samples also showed reduced Weibull modulus compared to undoped UO 2 , suggesting increased scatter in fracture strength. This study's findings suggest that titanium and chromium oxide doping in UO 2 , regardless of grain size, induce residual stresses, decreasing fracture strength and increasing variability in fracture behavior.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Preparation and magnetic properties of Fe{sup 3+}-Nb{sup 5+} co-doped SnO{sub 2}

Fe{sup 3+}-Nb{sup 5+} co-doped SnO{sub 2} was prepared at 1200 deg. C by a simple chemical co-precipitation method. The Sn{sub 1-2x}Fe{sub x}Nb{sub x}O{sub 2} solid solutions kept cassiterite structure in the range of 0<x{<=}0.33, and their cell parameters decrease with increasing x. While x=0.40, a second phase with orthorhombic FeNbO{sub 4} structure co-exists with the cassiterite phase, and the second phase becomes dominant while x{>=}0.45. The magnetic measurements indicated that low doping ratio sample (x=0.03) exhibits paramagnetic behavior. A paramagnetic-to-antiferromagnetic phase transition was observed for the samples with higher doping ratio (x{>=}0.15). - Graphical abstract: Fe{sup 3+}-Nb{sup 5+} co-doped SnO{sub 2} was prepared at 1200 deg. C by a simple chemical co-precipitation method. The solubility of Fe{sup 3+} in SnO{sub 2} was increased to 33% by co-doping with Nb{sup 5+}. The magnetic measurements indicated that low doping ratio sample (x=0.03) exhibited paramagnetic behavior. A paramagnetic-to-antiferromagnetic phase transition was observed for the samples with higher doping ratio (x{>=}0.15)

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Phase transformation and optical properties of Cu-doped ZnS nanorods

ZnS nanorods doped with 0-15 mol% of Cu have been prepared by simple solvothermal process. With gradual increase in the Cu concentration, phase transformation of the doped ZnS nanorods from wurtzite to cubic was observed. Twins and stacking faults were developed due to atomic rearrangement in the heavily doped ZnS nanorods during phase transformation. UV-vis-NIR absorbance spectroscopy ruled out the presence of any impure Cu-S phase. The doped ZnS nanorods showed luminescence over a wide range from UV to near IR with peaks at 370, 492-498, 565 and 730 nm. The UV region peak is due to the near-band-edge transition, whereas, the green peak can be related to emission from elementary sulfur species on the surfaces of the nanorods. The orange emission at 565 nm may be linked to the recombination of electrons at deep defect levels and the Cu(t{sub 2}) states present near the valence band of ZnS. The near IR emission possibly originated from transitions due to deep-level defects. - Graphical abstract: ZnS nanorods doped with 0-15 mol% of Cu has been prepared by simple solvothermal route. Interestingly, phase transformation of the doped ZnS nanorods from wurtzite to cubic was observed with gradual increase in the Cu concentration. Doped ZnS nanorods showed luminescence over a wide range from UV to near IR, which is also a rare observation.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Morphology-controlled synthesis and novel microwave electromagnetic properties of hollow urchin-like chain Fe-doped MnO{sub 2} under 10 T high magnetic field

Fe-doped MnO{sub 2} with a hollow sea urchin-like ball chain shape was first synthesized under a high magnetic field of 10 T. The formation mechanism was investigated and discussed in detail. The synthesized samples were characterized by XRD, SEM, TEM, EMPA, and vector network analysis. By doping MnO{sub 2} with Fe, the relative complex permittivity of MnO{sub 2} and its corresponding loss tangent clearly decreases, but its relative complex permeability and its corresponding loss tangent markedly increases. Moreover, the theoretically calculated values of reflection loss show that with increasing the Fe content, the as-prepared Fe-doped MnO{sub 2} exhibits good microwave absorption capability. -- Graphical Abstract: Fe-doped MnO{sub 2} with a hollow sea urchin-like ball chain shape was first synthesized in a high magnetic field of 10 T via a simple chemical process. Display Omitted Highlights: {yields} Fe-doped MnO{sub 2} with a hollow sea urchin-like ball chain shape was first synthesized. {yields} We investigated formation mechanism and electromagnetic properties of the Fe-doped MnO{sub 2}. {yields} By doping MnO{sub 2} with Fe, the electromagnetic properties are improved obviously.

36 MATERIALS SCIENCE↗

Infrared absorptive properties of Al-doped ZnO divided powder

Al-doped ZnO powders were synthesised by a Pechini process in order to obtain visible non-absorbent and near-Infrared absorbent particles. Firstly, it has been shown that synthesis under argon combined with the lowest synthesis temperatures (700 deg. C) allows getting the optimal properties for pure ZnO compounds due to creation of n-type defects segregated on oxide grain surface (Zn/O ratio superior to 1). Nevertheless, the near-Infrared absorption properties of the pure ZnO compounds remain low. The Al{sup 3+} doping of ZnO compounds was then investigated. The Al solubility limit inside ZnO doped compounds decreases drastically with the grain size, i.e. with the synthesis temperature. Then, the Al cations distribution varies inside ZnO grains, Al{sup 3+} segregation at the grain surfaces taking place for high synthesis temperatures. The optimal optical properties (high near-Infrared absorption) are reached combining Al-doping and adequate synthesis conditions: annealing under argon at low temperatures. In these conditions, the highest extrinsic (via Al doping) and intrinsic n-types defects rates are indeed reached. - Graphical abstract: Al-doped ZnO powders synthesised from Pechini routes after annealing under argon at low temperatures exhibit high optical selectivity: large Infrared absorption/high visible transparency. Highlights: > ZnO synthesis route with low T/low pO{sub 2} promotes extrinsic defects. > Highly divided Al-doped ZnO oxides (hdAZO) exhibit high Al solubility limit. > hdAZO are IR absorbent because of their high intrinsic/extrinsic defects concentrations.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Growth and characterization of Cl-doped ZnO hexagonal nanodisks

Cl-doped ZnO nanodisks were grown on a Si(111) substrate using a thermal evaporation method. The prepared nanodisks exhibited a hexagonal shape with an average thickness of 50 nm and average diagonal of 270 nm. In addition, undoped ZnO disks with hexagonal shape were grown under the same conditions, but the sizes of these undoped ZnO disks were on the micrometer order. A possible mechanism was proposed for the growth of the Cl-doped ZnO nanodisks, and it was shown that the Cl{sup 1-} anions play a crucial role in controlling the size. X-ray diffraction and Raman spectroscopy clearly showed an extension in the crystal lattice of ZnO because of the presence of chlorine. In addition, these nanodisks produced a strong photoluminescence emission peak in the ultraviolet (UV) region and a weak peak in the green region of the electromagnetic spectrum. Furthermore, the UV peak of the Cl-doped ZnO nanodisks was blueshifted with respect to that of the undoped ZnO disks. - Graphical abstract: Cl-doped ZnO nanodisks and undoped ZnO microdisks have been grown using a thermal evaporation method. Highlights: > Cl-doped ZnO nanodisks with hexagonal shape are grown using a thermal evaporation method. > It is shown that the Cl{sup 1-} anions play a crucial role in controlling the size of the nanodisks. > XRD and Raman results showed that the Cl-doped ZnO nanodisks structure is under a biaxial stress. > UV peak of the PL spectrum is blueshifted for the Cl-doped ZnO nanodisks.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Low temperature synthesis, photoluminescence, magnetic properties of the transition metal doped wurtzite ZnS nanowires

In this paper, we synthesized the transition metal ions (Mn, Cu, Fe) doped and co-doped ZnS nanowires (NWs) by a one-step hydrothermal method. The results showed that the solid solubility of the Fe{sup 2+} ions in the ZnS NWs was about two times larger than that of the Mn{sup 2+} or Cu{sup 2+} ions in the ZnS NWs. There was no phase transformation from hexagonal to cubic even in a large quantity transition metal ions introduced for all the samples. The Mn{sup 2+}/Cu{sup 2+}/Fe{sup 2+} related emission peaks can be observed in the Mn{sup 2+},Cu{sup 2+} and Fe{sup 2+} doped ZnS NWs. The ferromagnetic properties of the co-doped samples were investigated at room temperature. - graphical abstract: The stable wurtzite ZnS:TM{sup 2+} (TM=Mn, Cu, Fe) nanowires with room temperature ferromagnetism properties were obtained. The different elongation of unit cell caused by the different doped ions was observed. Highlights: ► The transition metal ions doped wurtzite ZnS nanowires were synthesized at 180 °C. ► There was no phase transformation from hexagonal to cubic even in a large quantity introduced for all the samples. ► The room temperature ferromagnetism properties of the co-doped nanowires were investigated.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

High figure of merit and thermoelectric properties of Bi-doped Mg{sub 2}Si{sub 0.4}Sn{sub 0.6} solid solutions

The study of Mg{sub 2}Si{sub 1−x}Sn{sub x}-based thermoelectric materials has received widespread attention due to a potentially high thermoelectric performance, abundant raw materials, relatively low cost of modules, and non-toxic character of compounds. In this research, Mg{sub 2.16}(Si{sub 0.4}Sn{sub 0.6}){sub 1−y}Bi{sub y} solid solutions with the nominal Bi content of 0≤y≤0.03 are prepared using a two-step solid state reaction followed by spark plasma sintering consolidation. Within this range of Bi concentrations, no evidence of second phase segregation was found. Bi is confirmed to occupy the Si/Sn sites in the crystal lattice and behaves as an efficient n-type dopant in Mg{sub 2}Si{sub 0.4}Sn{sub 0.6}. Similar to the effect of Sb, Bi doping greatly increases the electron density and the power factor, and reduces the lattice thermal conductivity of Mg{sub 2.16}Si{sub 0.4}Sn{sub 0.6} solid solutions. Overall, the thermoelectric figure of merit of Bi-doped Mg{sub 2.16}Si{sub 0.4}Sn{sub 0.6} solid solutions is improved by about 10% in comparison to values obtained with Sb-doped materials of comparable dopant content. This improvement comes chiefly from a marginally higher Seebeck coefficient of Bi-doped solid solutions. The highest ZT∼1.4 is achieved for the y=0.03 composition at 800 K. - Graphical abstract: (a)The relationship between electrical conductivity and power factor for Sb/Bi-doped Mg{sub 2.16}(Si{sub 0.4}Sn{sub 0.6}){sub 1−y}(Sb/Bi){sub y} (0<y≤0.03) solid solutions. (b)The correlation between temperature and the combination of the lattice and the bipolar terms of thermal conductivity of Mg{sub 2.16}(Si{sub 0.4}Sn{sub 0.6}){sub 1−y}Bi{sub y} (0≤y≤0.03) solid solutions. (c)Temperature dependent dimensionless figure of merit ZT of Mg{sub 2.16}(Si{sub 0.4}Sn{sub 0.6}){sub 1−y}Bi{sub y} (0≤y≤0.03) solid solutions. - Highlights: • Bi doped Mg{sub 2.16}Si{sub 0.4}Sn{sub 0.6} showed 15% enhancement in the power factor as compared to Sb doped samples. • Bi doping reduced κ{sub ph} of Mg{sub 2.16}Si{sub 0.4}Sn{sub 0.6} due to stronger point defect scattering. • The highest ZT=1.4 at 800 K was achieved for Mg{sub 2.16}(Si{sub 0.4}Sn{sub 0.6}){sub 0.97}Bi{sub 0.03}.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗