Search NASA⌕ Search

SEARCH · Search NASA

Results for “PDMS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 91 records · Page 5

Synthesis of Bio-Based Repairable Polyimines with Tailored Properties by Lignin Fractionation

Developing sustainable polymers with low-value lignin remains a challenge. Herein, lignin-containing repairable polyimines were synthesized with tailored properties using lignin fractionation. First, softwood Kraft lignin is fractionated into a more homogeneous fraction with a lower molecular weight and a higher OH content. Next, Kraft lignin and its fraction are esterified by levulinic acid to introduce active ketone groups and subsequently condensed with oleylamine (OAm) and bis(3-aminopropyl)-terminated polydimethylsiloxane (PDMS) via a catalyst-free Schiff-base reaction to form grafted lignin-OAm copolymers and cross-linked lignin-PDMS polymer networks (MKL-P and MFL-P), respectively. Results show that lignin-OAm polyimines can be self-repaired and hot reprocessed under pressure, while lignin-PDMS polyimines can be repaired with the assistance of a healing agent, heat, and pressure. Dynamic mechanical analyses demonstrate that the stress–relaxation behaviors of the polyimines follow the Arrhenius law under thermal-stress activation, indicating the occurrence of transimination. Moreover, compared with Kraft lignin, the lignin fraction ameliorates the grafting density of ketones and enhances the cross-linking density of lignin-PDMS polyimine networks. The higher cross-linking density of MFL-P leads to superior stress–relaxation activation energy, thermal stability, hydrophobicity, and light-shielding ability but inferior repairability and translucency. Finally, this work provides insights into the polymerization of lignin-based polymer networks and the potential application of lignin-PDMS polyimines for repairable, translucent, anti-UV, and hydrophobic coatings.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Continuity of monolayer-bilayer junctions for localization of lipid raft microdomains in model membranes

We show that the selective localization of cholesterol-rich domains and associated ganglioside receptors prefer to occur in the monolayer across continuous monolayer-bilayer junctions (MBJs) in supported lipid membranes. For the MBJs, glass substrates were patterned with poly(dimethylsiloxane) (PDMS) oligomers by thermally-assisted contact printing, leaving behind 3 nm-thick PDMS patterns. The hydrophobicity of the transferred PDMS patterns was precisely tuned by the stamping temperature. Lipid monolayers were formed on the PDMS patterned surface while lipid bilayers were on the bare glass surface. Due to the continuity of the lipid membranes over the MBJs, essentially free diffusion of lipids was allowed between the monolayer on the PDMS surface and the upper leaflet of the bilayer on the glass substrate. The preferential localization of sphingomyelin, ganglioside GM1 and cholesterol in the monolayer region enabled to develop raft microdomains through coarsening of nanorafts. Furthermore, our methodology provides a simple and effective scheme of non-disruptive manipulation of the chemical landscape associated with lipid phase separations, which leads to more sophisticated applications in biosensors and as cell culture substrates.

59 BASIC BIOLOGICAL SCIENCES↗

Some aspects of the orientational order distribution of flexible chains in a diblock mesophase

The segmental motions of flexible chains in the lamellar structure of a strongly segregated poly(styrene)-poly(dimethylsiloxane) (PS-PDMS) diblock were investigated over a time scale of a few tens of microseconds. {sup 2}H NMR experiments were performed on the PDMS block, selectively perdeuterated. Transverse relaxation measurements show that the main part of the PDMS repeat units display anisotropic reorientational motions within the diblock lamellae and such a segmental ordering essentially results from interchain steric repulsions. {sup 2}H double quantum-based experiments evidenced a non-uniform local stretching of PDMS chains and enabled the underlying distribution of the orientational order parameter to be determined quantitatively. Besides, a fraction of the PDMS chain segments, about 14%, were found to display isotropic – or nearly isotropic – reorientations, which could be assigned to repeat units located within a thin sublayer (about 1–2 nm) at the lamellae midplane, but also deeper in the lamellae, close to folded parts of the chains. These experimental results were confronted to theoretical descriptions of opposing polymer brushes and, in particular, to the strong-stretching theory (SST) including the entropic contribution of free chain ends.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Infrared dielectric function of polydimethylsiloxane and selective emission behavior

The complex refractive index of polydimethylsiloxane (PDMS) is determined in the wavelength range between 2.5 μm and 16.7 μm. The parameters of a Drude-Lorentz oscillator model (with 15 oscillators) are extracted from Fourier transform infrared spectroscopy reflectance measurements made on both bulk PDMS and thin films of PDMS deposited on the gold coated silicon substrates. It is shown that thin films of PDMS atop gold exhibit selective emission in the 8 μm to 13 μm atmospheric transmittance window, which demonstrates that PDMS, especially due to its ease of deposition, may be a viable material for passive radiative cooling applications.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

SU-F-I-61: Assessment and Characterization of the Built-in Internal Photometer of Primary Diagnostic Monitors

Purpose: The conformance of Primary Diagnostic Monitors (PDMs) to the DICOM GSDF is increasingly required by several state and city regulators. Our purpose was to quantitatively characterize the luminance performance of the internal, built in photometer of BARCO monitors against an externally calibrated luminance meter. Methods: Thirty one PDMs (BARCO) were included in our analysis. An externally calibrated photometer (RaySafe Solo Light) was used to measure the luminance and illuminance values. Measured monitors were located at various hospital sites, radiology physicians’ offices and radiology reading rooms. All measured PDMs were equipped with the manufacturer’s built-in photometers and connected to Barco MediCal QA web service for manual and automatic quality control measurements. PDM combinations included 1, 2 and 4 monitors depending on the location. TG-18 and SMPTE test patterns were used to evaluate monitor performance. Results: All the PDMs exceeded the luminance ratio of 250:1, as required by NYC PDM guidelines. One PDM failed the NYC requirement for the minimal luminance level of 350 cd/m2. As compared to the external photometer, the difference in measurement of the maximum luminance with the built-in photometer was found to exceed 5% on 6 of the PDM measured, with a maximum deviation of 10%. The age of the monitors that failed was on average 5 years. All monitors passed the luminance uniformity test, which was 30% from the center of the monitor to the 4 corner locations. Four PDMs failed the Gray Scale Display Function (GSDF) calibration. Conclusion: For the consistent display of medical images and continued conformance with the DICOM GSDF standard, it is essential to compare the performance of the built-in photometer with an externally calibrated photometer for monitors that are older than 5 years.

60 APPLIED LIFE SCIENCES↗

Polymer Filler Aging and Failure Studied by Lateral Force Microscopy

In the present work, we study, via force microscopy, the basic physical interactions of a single bead of silica filler with a PDMS matrix both before and after exposure to gamma radiation. Our goal was to confirm our results from last year, and to explore force microscopy as a means of obtaining particle-scale polymer/filler interactions suitable for use as empirical inputs to a computational model consisting of an ensemble of silica beads embedded in a PDMS matrix. Through careful calibration of a conventional atomic force microscope, we obtained both normal and lateral force data that was fitted to yield adhesion, surface shear modulus, and friction of a 1 {micro}m silica bead in contact with PDMS layers of various thickness. Comparison of these terms before and after gamma exposure indicated that initially, radiation exposure lead to softening of the PDMS, but eventually resulted in stiffening. Simultaneously, adhesion between the polymer and silica decreased. This could indicate a serious failure path for filled PDMS exposed to radiation, whereby stiffening of the bulk polymer leads to loss of compressive elastic behavior, while a decrease in polymer filler adhesion results in an increased likelihood of stress failure under load. In addition to further testing of radiation damaged polymers, we also performed FEA modeling of silica beads in a silicone matrix using the shear modulus and adhesion values isolated from the force microscopy experiments as model inputs. The resulting simulation indicated that as a polymer stiffens due to impinging radiation, it also undergoes weakening of adhesion to the filler. The implication is that radiation induces a compound failure mode in filled polymer systems.

36 MATERIALS SCIENCE↗

Copoly(Imide Siloxane) Abhesive Materials with Varied Siloxane Oligomer Length

Incorporation of PDMS moieties into a polyimide matrix lowered the surface energy resulting in enhanced adhesive interactions. Polyimide siloxane materials were generated using amine-terminated PDMS oligomers of different lengths to study changes in surface migration behavior, phase segregation, mechanical, thermal, and optical properties. These materials were characterized using contact angle goniometry, tensile testing, and differential scanning calorimetry. The surface migration behavior of the PDMS component depended upon the siloxane molecular weight as indicated by distinct relationships between PDMS chain length and advancing water contact angles. Similar correlations were observed for percent elongation values obtained from tensile testing, while the addition of PDMS reduced the modulus. High fidelity topographical modification via laser ablation patterning further reduced the polyimide siloxane surface energy. Initial particulate adhesion testing experiments demonstrated that polyimide siloxane materials exhibited greater abhesive interactions relative to their respective homopolyimides.

Wohl, Christopher J.↗

Durability of polymeric encapsulation materials in a PMMA/glass concentrator photovoltaic system

We examined the durability of polymeric encapsulation materials using outdoor exposure at the nominal geometric concentration of 500 suns. The results for 36-month cumulative field deployment are presented for materials including: poly(ethylene-co-vinyl acetate), (EVA); polyvinyl butyral (PVB); ionomer; polyethylene/polyoctene copolymer (PO); thermoplastic polyurethane (TPU); poly(dimethylsiloxane) (PDMS); poly(diphenyl dimethyl siloxane) (PDPDMS); and poly(phenyl-methyl siloxane) (PPMS). Measurements of the field conditions including ambient temperature and ultraviolet (UV) dose were recorded at the test site during the experiment. Our measurements for the experiment included optical transmittance (with subsequent analysis of solar-weighted transmittance, UV cut-off wavelength, and yellowness index), mass, visual photography, photoelastic imaging, and fluorescence spectroscopy. While the results to date for EVA are presented and discussed, examination here focuses more on the siloxane materials. A specimen recently observed to fail by thermal decomposition is discussed in terms of the implementation of the experiment as well as its fluorescence signature, which was observed to become more pronounced with age. Modulated thermogravimetry (allowing determination of the activation energy of thermal decomposition) was performed on a subset of the siloxanes to quantify the propensity for decomposition at elevated temperatures. Supplemental, Pt-catalyst- and primer-solutions as well as peroxide-cured PDMS specimens were examined to assess the source of the luminescence. Furthermore, our results, including the change in optical transmittance, observed failure modes, and subsequent analyses of the failure modes are described in the conclusions.

14 SOLAR ENERGY↗

Strongly segregated cubic microdomain morphology consistent with the double gyroid phase in high molecular weight diblock copolymers of polystyrene and poly(dimethylsiloxane)

We report the observation of a cubic phase consistent with the double gyroid structure in strongly segregated diblock copolymers of PS-b-PDMS over a volume fraction ({phi}{sub PDMS}) range of {approx}0.39 to 0.45. The samples have respective molecular weights of 127 kg/mol and 73 kg/mol and degree of segregation N{sub {chi}} equal to 187 and 106, respectively, at annealing temperature of 130 C. It is important to highlight that two out of the total four samples investigated, exhibited hexagonally close packed cylindrical domains of PDMS and alternating lamellae at {phi}{sub PDMS} = 0.39 and 0.45, respectively, indicating the possible narrow range of the DG morphology for the specific diblock copolymers.

36 MATERIALS SCIENCE↗

Morphology Control of Poly(styrene- block -dimethylsiloxane) by Simple Blending with Trimethylsilylated Silicate Nanoparticles

Trimethylsilylated silicate nanoparticle (termed MQ resin, combining M Me 3 SiO 1/2 and Q SiO 4/2 units)/poly(styrene- block -polydimethylsiloxane) (PS–PDMS, 31K–15K, polydispersity PD = 1.15, weight-average molecular weight M w = 45.5K) blends behave similarly to block copolymers with different PS/PDMS ratios. MQ is localized in the PDMS phase virtually extending the volume fraction in the block copolymer. This allows for microdomain morphology control beyond what can be achieved with the starting block copolymer. Synthesizing siloxane-containing block copolymers targeted at certain equilibrium morphologies can be time-consuming and in some cases technically challenging. This work reported here shows that MQ is a robust morphology modifier, not limited by the occurrence of surface segregation and the high diffusion rates typically associated with homopolymer modification, as confirmed by looking at the PDMS/PS–PDMS reference. The convenient and robust structure control MQ nanoparticle modification of PS–PDMS provides could overcome one of the hurdles to adoption of block copolymer lithography.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Better Actuation Through Chemistry: Using Surface Coatings to Create Uniform Director Fields in Nematic Liquid Crystal Elastomers

Controlling the molecular alignment of liquid crystal monomers (LCMs) within nano- and microstructures is essential in manipulating the actuation behavior of nematic liquid crystal elastomers (NLCEs). In this paper, we study how to induce uniformly vertical alignment of nematic LCMs within a micropillar array to maximize the macroscopic shape change using surface chemistry. Landau–de Gennes numerical modeling suggests that it is difficult to perfectly align LCMs vertically in every pore within a poly(dimethylsiloxane) (PDMS) mold with porous channels during soft lithography. In an untreated PDMS mold that provides homeotropic anchoring of LCMs, a radially escaped configuration of LCMs is observed. Vertically aligned LCMs, a preferred configuration for actuation, are only observed when using a PDMS mold with planar anchoring. Guided by the numerical modeling, we coat the PDMS mold with a thin layer of poly(2-hydroxyethyl methacrylate) (PHEMA), leading to planar anchoring of LCM. Confirmed by polarized optical microscopy, we observe monodomains of vertically aligned LCMs within the mold, in agreement with modeling. Finally, after curing and peeling off the mold, the resulting NLCE micropillars showed a relatively large and reversible radial strain (~30%) when heated above the nematic to isotropic transition temperature.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Henry’s Solubility and Diffusion Coefficients for 29 Volatile Organic Compounds in Polydimethylsiloxane Sylgard 184 at 293 K

Two-dimensional (2D) inverse gas chromatography (IGC) enables simultaneous determination of Henry’s solubility and Fickian diffusion coefficients for volatile organic compounds (VOCs) in polymer films. This technique offers a significant advantage over traditional cylindrical column IGC by providing precise control and measurement of the film thickness (here, 0.064 ± 0.002 mm), which is the critical length scale for accurate diffusivity determination. We apply this methodology to characterize VOC transport in Sylgard 184, a widely used polydimethylsiloxane (PDMS)-based polymer containing substantial silica filler content. At room temperature (20 °C), we measured solubility and diffusion coefficients for 29 common VOCs spanning diverse chemical functionalities, including alkanes, aromatics, chlorinated solvents, ketones, esters, and alcohols. Comparison with literature data for pure PDMS reveals that VOC solubility in Sylgard 184 is generally higher; for most non-hydrogen-bonding compounds it remains within a factor of 2 of pure PDMS, whereas alcohols are enhanced by roughly 1.8 to 3.7 times, which we attribute to favorable interactions with residual silanol groups on the silanized silica filler. Diffusion coefficients range from 1.0 × 10 –6 cm 2 /s (n-undecane) to 8.9 × 10–5 cm 2 /s (acetonitrile) and align well with extrapolated literature values for PDMS. This study provides essential thermodynamic and transport data for predicting VOC permeation in Sylgard 184 while demonstrating the utility of 2D IGC as a robust technique for characterizing rubbery polymer membranes across diverse industrial applications.

organic↗

Hydrophobic Polymeric Solvents for the Selective Absorption of CO 2 from Warm Gas Streams that also Contain H 2 and H 2 O

The hydrophobic polymers polydimethyl siloxane (PDMS) and polypropyleneglycol dimethylether (PPGDME) may provide an alternative to physical solvents based on the hydrophilic polymer polyethyleneglycol dimethylether (PEGDME) for the precombustion capture of CO{sub 2} from the warm, high pressure stream that also contains H{ 2 O and H 2 . PPGDME can be made with a linear repeat unit (PPGDMEl, poly(1,3-propanediol) dimethylether) or a branched repeat unit (PPGDMEb, poly(1,2-propanediol) dimethylether). The solubility of CO 2 and H 2 in each of the four solvents of specified average molecular weight (PEGDME 250, PDMS 550, PPGDMEl 678 and PPGDMEb 430) is determined between 25 and 120 °C at pressures to 10 MPa. CO 2 is much more soluble in each solvent than H{sub 2}; however, the solubility of CO{sub 2} decreases as the solubility of H 2 increases with increasing temperature. PPGDMEl 678 and PPGDMEb 430 are comparable CO 2 solvents. PPGDMEl 678 absorbs less H{sub 2} than all the other solvents, while PPGDMEb 430 absorbs significantly more H 2 }. PDMS 550 is a very good CO 2 solvent, absorbing more CO 2 than all of the other solvents at all temperatures except for PEGDME 250 at 25 °C. PDMS 550 absorbs more H 2 than all of the other solvents.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

A comparison study of carbon dioxide adsorption on polydimethylsiloxane, silica gel, and Illinois No. 6 coal using in situ infrared spectroscopy

Adsorption of supercritical carbon dioxide (CO{sub 2}) on polydimethylsiloxane (PDMS), silica gel (SiO{sub 2}), and Illinois No. 6 coal was compared using in situ attenuated total reflectance Fourier transform infrared (ATR-FTIR) spectroscopy at pressures up to 14 MPa and temperatures at 40{sup o}C and 50{sup o}C. Only physical adsorption of CO{sub 2} was recorded for PDMS, SiO{sub 2}, and Illinois no. 6. There was no evidence of the formation of carbonic acid, bicarbonates, carbonates, or any other reaction product between CO{sub 2} and PDMS, SiO{sub 2}, and Illinois No. 6 coal. Carbon dioxide adsorption on PDMS and SiO{sub 2} produced a linear isotherm while a typical Langmuir-like isotherm was observed for Illinois No. 6 coal. Attempts to measure CO{sub 2} induced swelling of the three materials was unsuccessful due to the design of the ATR-FTIR cell. 51 refs., 7 figs., 1 tab.

01 COAL, LIGNITE, AND PEAT↗

On the mechanism of marine fouling-prevention performance of oil-containing silicone elastomers

For many decades, silicone elastomers with oil incorporated have served as fouling-release coating for marine applications. In a comprehensive study involving a series of laboratory-based marine fouling assays and extensive global field studies of up to 2-year duration, we compare polydimethylsiloxane (PDMS) coatings of the same composition loaded with oil via two different methods. One method used a traditional, one-pot pre-cure oil addition approach (o-PDMS) and another method used a newer post-cure infusion approach (i-PDMS). The latter displays a substantial improvement in biofouling prevention performance that exceeds established commercial silicone-based fouling-release coating standards. We interpret the differences in performance between one-pot and infused PDMS by developing a mechanistic model based on the Flory–Rehner theory of swollen polymer networks. Using this model, we propose that the chemical potential of the incorporated oil is a key consideration for the design of future fouling-release coatings, as the improved performance is driven by the formation and stabilization of an anti-adhesion oil overlayer on the polymer surface.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Ultrasensitive Nanoelectrospray Ionization-Mass Spectrometry using Poly(dimethylsiloxane) Microchips with Monolithically Integrated Emitters

Poly(dimethylsiloxane) (PDMS) is the most widely used substrate for microfluidic devices as it enables facile fabrication and has other distinctive properties. However, for applications involving highly sensitive nanoelectrospray ionization mass spectrometry (nanoESI-MS) detection, the use of PDMS microdevices has been hindered by the leaching of uncross-linked oligomers and other contaminants from the substrate that yields a large background of chemical noise in the mass spectra. A more general challenge is that microfluidic devices containing integrated electrospray emitters are frequently unable to operate stably in the nanoflow regime where the best sensitivity is achieved. In this report, we extracted the contaminants from PDMS substrates using a series of solvents, eliminating the background observed when untreated PDMS microchips are used for nanoESI-MS. Optimization of the integrated emitter geometry enabled stable operation at flow rates as low as 10 nL/min. Peptide concentrations of 1 nM were readily detected, representing ~170 zmol of consumed analyte, and an extrapolated detection limit of ~40 zmol; these are the lowest mass and concentration detection limits reported to date for a microchip having an integrated electrospray emitter.