Search NASA⌕ Search

SEARCH · Search NASA

Results for “anode-free batteries”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

76 records · Page 5

Li Stripping Behavior of Anode‐Free Solid‐State Batteries Under Intermittent‐Current Discharge Conditions

Anode‐free manufacturing holds promise to enable high energy densities and lower Lithium (Li)‐metal solid‐state batteries (LMSSBs). Nevertheless, in contrast to thick Li foil (>50 µm), the stripping capacity of in situ‐formed Li (10–30 µm) is limited due to diminished creep flow, resulting in reduced accessible capacity. This study explores the correlation between stripping capacity and surface roughness of garnet Li 7 La 3 Zr 2 O 12 (LLZO) solid electrolyte. The results reveal that stripping capacity can be enhanced through the surface modification of solid electrolytes. Additionally, this study scrutinizes the stripping behavior of in situ Li under intermittent‐current discharge conditions, which are more relevant to the operational conditions of electric vehicles (EVs). It is demonstrated that, when compared to constant‐current stripping, intermittent‐current stripping effectively suppresses void formation and enhances the stripping capacity of in situ Li by 40%. It is considered that the intermittent current inhibits the accumulation of Li vacancies, thereby delaying the void formation. These findings provide valuable insights into the development of high‐performance anode‐free LMSSBs for EVs.

25 ENERGY STORAGE↗

A Reductively Stable Electrolyte Realizes Deep Cycling Behavior in Anode‐free Sodium Batteries

For anode‐free sodium batteries to achieve practical consideration, highly reversible chemistries require exceptional ≥99.95% coulombic efficiencies that maintain over prolonged cycling periods. To do so, consumption of this severely limited sodium inventory must be restricted while metal nucleation processes that comprise the in situ formed metal anode are improved. Herein, we describe a fluorine‐free carborane electrolyte that satisfies these criteria by emphasizing reductive stability and weakly coordinating anion behavior as design principles. We find this approach promotes the development of a thin, robust SEI chemistry rich in both organic speciation and boron. The electrolyte described herein exhibits ideal metal nucleation behavior on one‐micron thin carbonaceous current collector surfaces and achieves a metal deposition/stripping efficiency near parity for 400 cycles. This novel anode chemistry is introduced to anode‐free full cell configurations where 87% of the initial discharge capacity is retained after 1000 cycles at 2.0 C. In conclusion, post‐test characterization of deep‐cycled anode‐free cells reveals suppressed capacity fade in these systems is attributed to the chemical stability of the carborane anion.

anode-free↗

High‐Performance Lithium Metal Batteries Enabled by a Fluorinated Cyclic Ether with a Low Reduction Potential

Abstract Electrolyte engineering is crucial for developing high‐performance lithium metal batteries (LMB). Here, we synthesized two cosolvents methyl bis(fluorosulfonyl)imide (MFSI) and 3,3,4,4‐tetrafluorotetrahydrofuran (TFF) with significantly different reduction potentials and add them into LiFSI‐DME electrolytes. The LiFSI/TFF‐DME electrolyte gave an average Li Coulombic efficiency (CE) of 99.41 % over 200 cycles, while the average Li CEs for MFSI‐based electrolyte is only 98.62 %. Additionally, the TFF‐based electrolytes exhibited a more reversible performance than the state‐of‐the‐art fluorinated 1,4‐dimethoxylbutane electrolyte in both Li||Cu half‐cell and anode‐free Cu||LiNi 0.8 Mn 0.1 Co 0.1 O 2 full cell. More importantly, the decomposition product from bis(fluorosulfonyl)imide anion could react with ether solvent, which destroyed the SEI, thus decreasing cell performance. These key discoveries provide new insights into the rational design of electrolyte solvents and cosolvents for LMB.

25 ENERGY STORAGE↗

Balancing Interfacial Reactions to Achieve Long Cycle Life in High Energy Lithium Metal Batteries

Rechargeable lithium (Li) metal batteries have attracted wide attentions as the next generation energy storage technologies. However, simultaneously achieving high cell-level energy density and long cycle life in realistic batteries is still a great challenge. Here we investigate the cell degradation mechanisms of Li||LiNi0.6Mn0.2Co0.2O2 pouch cells using different, but representative cell configurations to understand the fundamental linkage among Li thickness, electrolyte depletion and the structure evolution of solid electrolyte interphase (SEI) layers. Different cell failure modes were discovered when tuning the anode to cathode capacity (N/P) ratio in compatible electrolyte. With a thick-Li anode (N/P ratio = 2.5), initial stable cycling is obtained because of the abundant Li supply from the anode together with an artificially inflated high Coulombic Efficiency, followed by a premature sudden cell death appears due to the enrichment of “ineffective SEI” which does not participate in the electrochemical reactions but keep increasing cell impedance. The anode-free cell (N/P 0:1) displays a steady capacity decay because cathode Li loss dominates from the beginning to the end of cell cycle life. An optimized thin-Li (N/P 1:1) well balances the Li consumption rate with the impedance buildup by minimizing the growth of ineffective SEI layer, thus decelerates cell polarization increasing and extends cycling. Contrary to conventional wisdoms, long cycle life is observed by using ultra thin-Li (20 µm) in balanced cells. A prototype 350 Wh kg-1 pouch cell (2.0 Ah) achieves over 600 long stable cycles with 76% capacity retention without sudden cell death.

Niu, Chaojiang↗