At least 91 records · Page 5

Pulsed laser induced atomic layer etching of silicon

Here, we demonstrate the laser mediated atomic layer etching (ALEt) of silicon. Using a nanosecond pulsed 266 nm laser focused loosely over and in a parallel configuration to the surface of the silicon, we dissociate Cl 2 gas to induce chlorination. Then, we use pulsed picosecond irradiation to remove the chlorinated layer. Subsequently, we perform continuous wave (CW) laser annealing to eliminate amorphization caused by the picosecond laser etching. Based on atomic force microscopy (AFM) and X-ray photoelectron spectroscopy (XPS), we observed strong evidence of chlorination and digital etching at 0.85 nm etching per cycle with good uniformity.

42 ENGINEERING↗

Bias-pulsed atomic layer etching of 4H-silicon carbide producing subangstrom surface roughness

A new approach to atomic layer etching (ALE) has been demonstrated, and its application to 4H-SiC is reported here. By pulsing only the DC bias for an Ar/Cl2 inductively coupled plasma-reactive ion etching system, the etch cycle duration is reduced by more than an order of magnitude relative to conventional ALE processes. Gas flows are not changed throughout the ALE process. With this process protocol, we achieved an etch rate of 2.48±0.09 Å/cycle with 6 s cycles, an RMS surface roughness (Rq) of 0.83±0.08 Å, and an ALE synergy value of S = 99%. The parameters explored within this ALE process demonstrate effective subangstrom smoothening of 4H-SiC surfaces and is well-suited for a variety of classical and quantum device nanofabrication.

42 ENGINEERING↗

High-Quality Dry Etching of LiNbO3 Assisted by Proton Substitution through H2-Plasma Surface Treatment

The exceptional material properties of Lithium Niobate (LiNbO3) make it an excellent material platform for a wide range of RF, MEMS, phononic and photonic applications; however, nano-micro scale device concepts require high fidelity processing of LN films. Here, we reported a highly optimized processing methodology that achieves a deep etch with nearly vertical and smooth sidewalls. We demonstrated that Ti/Al/Cr stack works perfectly as a hard mask material during long plasma dry etching, where periodically pausing the etching and chemical cleaning between cycles were leveraged to avoid thermal effects and byproduct redeposition. To improve mask quality on X- and Y-cut substrates, a H2-plasma treatment was implemented to relieve surface tension by modifying the top surface atoms. Structures with etch depths as deep as 3.4 µm were obtained in our process across a range of crystallographic orientations with a smooth sidewall and perfect verticality on several crystallographic facets.

36 MATERIALS SCIENCE↗

Multimodal analysis and characterization of the boehmite layer formed on AA6061 before and after alkaline etching

Low-enriched uranium (LEU) alloyed with 10% Mo (U-10Mo) is being considered as a promising alternative to oxide-based dispersion fuel with high-enriched uranium for use in research reactors. The configuration of this proposed LEU monolithic LEU fuel plate consists of a U-10Mo plate-type fuel foil with a 25 µm zirconium interlayer barrier clad with an aluminum alloy (AA6061). In certain research reactors, the clad AA6061 is coated with a boehmite layer to prevent corrosion. The boehmite layer has a high-pH passivation range, which makes it resistant to oxidation. Boehmite is usually formed on the AA6061 surface by autoclave processing. Before the boehmite layer is added, the surface of the AA6061 is cleaned using techniques such as polishing and wet etching. In this study, we use multimodal analysis to examine how pretreatment of AA6061 using polishing followed by alkaline etching affects the chemical composition of the boehmite layer. X-ray photoelectron microscopy (XPS), transmission electron microscopy (TEM), and x-ray diffraction (XRD) were used to study the chemical changes in the boehmite layer caused by alkaline etching pretreatment. XPS provides quantitative analysis for the Al:O ratio as well as oxidation states present on the surface, which suggests slight oxidation of the boehmite surface after alkaline etching of the AA6061 surface. We further explored this suggested oxidation of the boehmite surface using high-resolution transmission electron microscopy with selected area electron diffraction (SAED) and grazing incidence x-ray diffraction (GI-XRD), which suggested only a small amount of aluminum oxide at the surface. The multimodal analysis and imaging yielded new insights for optimizing boehmite growth on AA6061 for research reactors.

36 MATERIALS SCIENCE↗

Si–Cl 2 –Ar + Atomic Layer Etching Window: A Fundamental Study Using Molecular Dynamics Simulations and a Reduced Order Model

Silicon (Si) atomic layer etching (ALE) by alternating exposure to chlorine gas (Cl 2 ) and argon ions (Ar + ) is studied by using molecular dynamics (MD) simulations and a reduced order model (ROM). Here, the purpose of this study is to elucidate the properties of the ALE window, a range of ion energies where the amount of Si etched over a series of cycles is nonzero and nearly independent of ion energy. Experimental studies of the Si–Cl 2 –Ar + ALE system report contradictory results related to the ALE window’s ion energy range. Both MD simulations and the ROM show that there is an ALE window present from approximately 15 to 20 eV for normal incidence argon ions. The Si–Cl 2 –Ar + system, therefore, exhibits a narrow ALE window. The amount of Si etched per cycle is less than one atomic layer because of the higher etch yield of Cl atoms relative to atomic Si and silicon chlorides. A modified version of the ROM with an artificially increased Si physical sputtering threshold energy expands the ALE window, illustrating the importance of the difference in chemical and physical sputtering threshold energies in the ALE window energy range. The ROM is also used to examine the dependence of the EPC on the Ar + ion fluence.

energy↗

Enhanced superconducting qubit performance through ammonium fluoride etch

The performance of superconducting qubits is often limited by dissipation and two-level systems (TLS) losses. The dominant sources of these losses are believed to originate from amorphous materials and defects at interfaces and surfaces, likely as a result of fabrication processes or ambient exposure. Here, we explore a novel wet chemical surface treatment at the Josephson junction-substrate and the substrate-air interfaces by replacing a buffered oxide etch (BOE) cleaning process with one that uses hydrofluoric acid followed by aqueous ammonium fluoride. We show that the ammonium fluoride etch process results in a statistically significant improvement in median $\text{T}_1$ by $\sim22\%$ (p = 0.002), and a reduction in the number of strongly-coupled TLS in the tunable frequency range. Microwave resonator measurements on samples treated with the ammonium fluoride etch after niobium deposition and etching also show $\sim33\%$ lower TLS-induced loss tangent compared to the BOE treated samples. As the chemical treatment primarily modifies the Josephson junction-substrate interface and substrate-air interface, we perform targeted chemical and structural characterizations to examine materials differences at these interfaces and identify multiple microscopic changes that could contribute to decreased TLS losses.

36 MATERIALS SCIENCE↗

Carrier Diffusion Lengths in Continuously Grown and Etched-and-Regrown GaN Pin Diodes

Advanced GaN power devices are promising for many applications in high power electronics but performance limitations due to material quality in etched-and-regrown junctions prevent their widespread use. Carrier diffusion length is a critical parameter that not only determines device performance but is also a diagnostic of material quality. Here we present the use of electron-beam induced current to measure carrier diffusion lengths in continuously grown and etched-and-regrown GaN pin diodes as models for interfaces in more complex devices. Variations in the quality of the etched-and-regrown junctions are observed and shown to be due to the degradation of the n-type material. Finally, we observe an etched-and-regrown junction with properties comparable to a continuously grown junction.

42 ENGINEERING↗

Plasma-assisted atomic layer etching of single-crystal diamond

Applications of near-surface nitrogen-vacancy (NV) centers in diamond are often limited by surface defects created during processing. Understanding and controlling plasma-induced surface damage is important for preserving the optical and spin properties of diamond NV centers. We report molecular dynamics simulations of a novel form of plasma-aided atomic layer etching of diamond. In this proposed scheme, the initial surface modification step consists of Ar + ion bombardment. This creates an amorphous layer at the surface, the thickness of which is controlled by the ion energy. Amorphization is known to help smooth the surface, at least locally, and would also serve to sputter clean an initially contaminated surface. A second step impacts the amorphous carbon layer with O + between about 1 and 5 eV. Simulations show that this energy range will remove the amorphous carbon but will not etch the underlying diamond. Though this energy range is not trivial to achieve in a conventional low-temperature plasma, potential methods for creating these low-energy O + ions are discussed. In addition to a-C etching, the O + impacts are predicted to remove any isolated (100) diamond terraces by selectively attacking the edges of the terraces. The proposed atomic layer etching (ALE) approach reverses the conventional ALE sequence in which the surface modification step is usually chemical modification (oxidation in this case), followed by a removal step using Ar + impacts. This plasma ALE procedure is predicted to create a diamond surface that is atomically flat and defect free.

Draney, J. S. [Princeton University, NJ (United St↗

Molecular layer etching

A method of etching an organic or hybrid inorganic/organic material. The method etches molecular layer deposition coatings. An etching cycle comprises a first half reaction exposing the coating to a precursor. A second half reaction exposes a second precursor, removing or etching a portion of the coating.

Young, Matthias John↗

Sapphire advanced mitigation process: wet etch to expose sub-surface damage and increase laser damage resistance and mechanical strength

In this study, a novel, to the best of our knowledge, method of wet chemical etching of sapphire workpieces (such as optics, wafers, windows, and cones), called the sapphire advanced mitigation process (or sapphire AMP), has been developed that exposes sub-surface mechanical damage created during the optical fabrication process and significantly enhances the surface laser damage resistance (> 2×) and mechanical strength (up to ~ 2.6×). Sapphire AMP involves first treating the workpiece with a mixture of sulfuric and phosphoric acid ([H 2 SO 4 ]:[H 3 PO 4 ]= 1 : 3) at 220°C, followed with phosphoric acid at 160°C, then with sodium hydroxide base (NaOH) and surfactant at 40°C, and finally with a high-pressure deionized water spray rinse. Sapphire AMP has been demonstrated on both A- and C-plane sapphire workpieces. The mechanism of this etch process involves the reaction of the sapphire (Al 2 O 3 ) surface with sulfuric acid (H 2 SO 4 ) forming aluminum sulfate [Al2(SO4)3], which has low solubility. The high phosphoric acid content in the first and second steps of sapphire AMP results in the efficient conversion of Al 2 (SO 4 ) 3 to aluminum phosphate (AlPO 4 ), which is very soluble, greatly reducing reaction product redeposition on the workpiece surface. Sapphire AMP is shown to expose sub-surface mechanical damage on the sapphire surface created during the grinding and polishing processes, whose etched morphology has either isotropic or anisotropic evolution depending on the nature of the initial surface damage. Sapphire AMP was also designed to remove the key known surface, laser absorbing precursors (namely, foreign chemical impurities, the fracture surface layer of preexisting sub-surface damage, and reaction product or foreign species redeposition or precipitation). Static and sliding indention induced surface microfractures on sapphire are shown after sapphire AMP to have a significant decrease in the fast photoluminescence intensity (a known metric for measuring the degree of laser damaging absorbing precursors). In addition, the onset of laser damage (at 351 nm 3 ns) on sapphire AMP treated workpieces was shown to increase in fluence from ~ 4 to >9.5J/cm 2 . Finally, biaxial ball-on-ring mechanical tests on sapphire disks showed an increase in the failure stress from 340 MPa (with pre-existing 28 µm flaws) to ~ 900MPa after sapphire AMP, which is attributed to the blunting of the surface microfractures.

36 MATERIALS SCIENCE↗

Plasma-Induced Tailoring of Graphene Oxide Surfaces for Electrochemical Applications: Functionalization and Etching

This study investigates the use of radio frequency air plasma as an eco-friendly method to rapidly and reversibly tailor the surface properties of graphene oxide (GO) films. We observed a transition from hydrophilic (contact angle ∼55°) to superhydrophilic (<10°) with short plasma exposure, attributed to a synergistic combination of surface modification and etching. Spectroscopic analyses (FTIR, XPS) revealed early stage formation of carbonyl groups and reduction of hydroxyls, while longer treatments induced atomic-level etching (AFM) and structural changes (XRD). This surface engineering enhanced the dielectric properties of GO films but led to reduced aqueous stability. The elucidated interplay between plasma-induced functionalization and etching provides valuable insights for the controlled modification of GO surfaces for various applications, including advanced dielectrics.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Voltage waveform tailoring for high aspect ratio plasma etching of SiO 2 using Ar/CF 4 /O 2 mixtures: Consequences of low fundamental frequency biases

The use of non-sinusoidal waveforms in low pressure capacitively coupled plasmas intended for microelectronics fabrication has the goal of customizing ion and electron energy and angular distributions to the wafer. One such non-sinusoidal waveform uses the sum of consecutive harmonics of a fundamental sinusoidal frequency, f 0 , having a variable phase offset between the fundamental and even harmonics. In this paper, we discuss results from a computational investigation of the relation between ion energy and DC self-bias when varying the fundamental frequency f 0 for capacitively coupled plasmas sustained in Ar/CF 4 /O 2 and how those trends translate to a high aspect ratio etching of trenches in SiO 2 . The fundamental frequency, f 0 , was varied from 1 to 10 MHz and the relative phase from 0° to 180°. Two distinct regimes were identified. Average ion energy onto the wafer is strongly correlated with the DC self-bias at high f 0 , with there being a maximum at φ = 0° and minimum at φ = 180°. In the low frequency regime, this correlation is weak. Average ion energy onto the wafer is instead dominated by dynamic transients in the applied voltage waveforms, with a maximum at φ = 180° and minimum at φ = 0°. The trends in ion energy translate to etch properties. In both, the high and low frequency regimes, higher ion energies translate to higher etch rates and generally preferable final features, though behaving differently with phase angle.

36 MATERIALS SCIENCE↗

Atomic scale etching of diamond: insights from molecular dynamics simulations

Diamond is a promising material for multiple applications in quantum information processing and sensing as well as applications in microelectronics. However, diamond devices can be limited by surface defects that compromise charge stability and spin coherence, among others. Improved strategies in plasma etching of diamond could play an important role in minimizing or eliminating these defects. In this work, we explore plasma-assisted atomic scale etching of diamond using argon ions (Ar + ), hydrogen ions (H + ) and hydrogen atoms (H). We employ classical molecular dynamics (MD) simulations and test several interatomic potentials based on the Reactive Empirical Bond Order (REBO) form with comparisons to a variety of published experimental results. We performed MD simulations of low-energy hydrogen ($\leqslant$50 eV) and argon ( $\leqslant$200 eV) ion bombardment of diamond surfaces. Ar + bombardment can be used to locally smooth initially rough diamond surfaces via the formation of an amorphous C layer, the thickness of which increases with argon ion energy. Subsequent exposure with hydrogen ions (or fast neutrals) will selectively etch this amorphous C layer, leaving the underlying diamond layer mostly intact if the H energy is maintained below about 10 eV. The simulations suggest that combining Ar + smoothing with selective, near threshold energy H removal of amorphous C can be an effective strategy for diamond surface engineering, leading to more reliable and sensitive diamond color center devices.

74 ATOMIC AND MOLECULAR PHYSICS↗

Direct matter disassembly via electron beam control: electron-beam-mediated catalytic etching of graphene by nanoparticles

Here, we report electron-beam activated motion of a catalytic nanoparticle along a graphene step edge and associated etching of the edge. The catalytic hydrogenation process was observed to be activated by a combination of elevated temperature and electron beam irradiation. Reduction of beam fluence on the particle was sufficient to stop the process, leading to the ability to switch on and off the etching. Such an approach enables the targeting of individual nanoparticles to induce motion and beam-controlled etching of matter through activated electrocatalytic processes. The applications of electron-beam control as a paradigm for molecular-scale robotics are discussed.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Loss Analysis and Performance Optimization Pathways of 729-mV Voc Si Solar Cells with Poly-Si on Locally-Etched Dielectric Passivating Contacts

In this article, the loss analysis of silicon solar cells with polysilicon on locally-etched dielectric passivating contacts with Voc=729.0 mV and efficiency=22.6% has been presented. Experimentally, nano-pinholes were introduced in SiO x (2.2 nm) and SiO x /SiN y (2.2 nm/8nm) stack using metal-assisted chemical etching (MACE). SunSolve and Quokka3 were used to simulate the experimental solar cell and investigate the optical and electrical power losses. Simulations suggest maximum power loss occurs due to recombination and resistive losses in the bulk (~0.76 mW/cm2) followed by power loss due to rear contact recombination (~0.35 mW/cm2). Recombination at the front surface also contributes to 0.24 mW/cm2. The effect of improving the bulk lifetime and lowering the recombination current density at the rear side on Voc, FF and hence, efficiency has been investigated. Further, advanced structures have been proposed to minimize recombination and parasitic absorption to achieve higher Voc and Jsc of the solar cells with locally-etched dielectric passivating contacts.

contacts↗

Plasma etching of wide bandgap and ultrawide bandgap semiconductors

The precise patterning of front-side mesas, backside vias, and selective removal of ternary alloys are all needed for power device fabrication in the various wide bandgap (AlGaN/GaN, SiC) and ultrawide bandgap (high Al-content alloys, boron nitride, Ga2O3, diamond) semiconductor technologies. The plasma etching conditions used are generally ion-assisted because of the strong bond strengths in these materials, and this creates challenges for the choice of masks in order to have sufficient selectivity over the semiconductor and to avoid mask erosion and micromasking issues. It can also be challenging to achieve practical etch rates without creating excessive damage in the patterned surface. The authors review the optimum choices for plasma chemistries for each of the semiconductors and acknowledge the pioneering work of John Coburn, who first delineated the ion-assisted etch mechanism.

42 ENGINEERING↗

Modification of a force field for molecular dynamics simulations of silicon etching by chlorine atoms

Here, a modified classical molecular dynamics (MD) force field is presented for the interaction between silicon (Si) and chlorine (Cl). The original version of the force field is shown to significantly overestimate the probability of Si etching by thermal Cl atoms. However, the modified force field corrects this problem and results in generally good agreement with experimental data. Further, it is shown that while the modification of the force field improves the prediction of Si spontaneous etching with Cl atoms, it does not degrade predictions of atomic-layer etching of Si with Cl[Formula: see text] molecules.

74 ATOMIC AND MOLECULAR PHYSICS↗

Fabrication of Poly-Si on Locally Etched SiOx as Passivating Contacts for c-Si Solar Cells

Proof-of-concept for polysilicon on locally etched oxide (PLEO) contacts. Room temperature approach (via MACE) to engineer pinholes decouples charge-carrier transport across contact from passivation scheme of choice. 19 and 17% PLEO devices fabricated on double-side textured and saw-damage etched n Cz wafers, respectively. Preliminary work on polysilicon on locally etched nitride/oxide (PLENO) contacts. 0.2 fA/cm2 achieved with p PLENO; contact displays Ohmic behavior but still very resistive due to low pinhole density.

c-Si↗