Search NASA⌕ Search

SEARCH · Search NASA

Results for “ion etching”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 91 records · Page 5

Deep potential molecular dynamics simulations of ion-enhanced etching of silicon by atomic chlorine

The continued development of plasma-assisted processing techniques requires a fundamental understanding of plasma-surface interactions. Molecular dynamics (MD) simulations have been employed to complement experimental studies and better understand the properties of such systems. Recently, machine learning (ML) methods have enabled the development of ab initio-based interatomic potentials, which can be generalized to complex combinations of multiple atom types. In this work, we use ML potentials developed using the Deep Potential Molecular Dynamics (DeepMD) framework to provide a model of ion-enhanced etching of Si by Cl atoms. We demonstrate the importance of proper selection of the training data set to the accuracy of the DeepMD model and compare our results to MD results using empirical potentials, as well as to experimental measurements. Exposure of undoped Si at 300 K to thermal Cl atoms yields a steady-state Cl coverage of 1.25 monolayers, which is slightly lower than the value obtained in previous experimental studies. Predictions of Si etch yields by simultaneous Cl atom and Ar + ion impacts as a function of ion energy, neutral to ion flux ratio, and angle of incidence of the ions are in reasonably good agreement with classical MD results and experimental measurements. Finally, etch yields and SiCl x mixed layer thicknesses during simultaneous bombardment of the Si(100) surface by Cl atoms and Cl + ions are in good agreement with experimental data. In conclusion, the present work is a necessary condition for the extension of the DeepMD procedure to more complex systems of interest in plasma-surface interactions.

Artificial neural networks↗

Ion beam etching dependence of spin-orbit torque memory devices with switching current densities reduced by Hf interlayers

We report on the fabrication of nanoscale, three-terminal in-plane spin–orbit torque switching devices with low switching current densities. Critical parameters in the fabrication process, including the ion beam etching angle and time, were optimized to avoid fabrication defects and improve device yield. Measurements of the magnetic field and current-induced switching behavior of the tunnel junctions demonstrate a sensitivity to the nanopillar aspect ratio, which dictates the nanopillars’ anisotropy and thermal stability. Additionally, we show that the current density required for switching can be reduced and the device thermal stability increased by inserting Hf interlayers into the heterostructure. Micromagnetic simulations are generally consistent with the experimentally observed switching behavior, suggesting an increase in the interfacial perpendicular anisotropy at the CoFeB/MgO interface and the reduction in the Dzyaloshinskii–Moriya interaction at the W/CoFeB interface by the Hf interlayers.

36 MATERIALS SCIENCE↗

XeF2 vapor phase silicon etch used in the fabrication of movable SOI structures.

Vapor phase XeF{sub 2} has been used in the fabrication of various types of devices including MEMS, resonators, RF switches, and micro-fluidics, and for wafer level packaging. In this presentation we demonstrate the use of XeF{sub 2} Si etch in conjunction with deep reactive ion etch (DRIE) to release single crystal Si structures on Silicon On Insulator (SOI) wafers. XeF{sub 2} vapor phase etching is conducive to the release of movable SOI structures due to the isotropy of the etch, the high etch selectivity to silicon dioxide (SiO{sub 2}) and fluorocarbon (FC) polymer etch masks, and the ability to undercut large structures at high rates. Also, since XeF{sub 2} etching is a vapor phase process, stiction problems often associated with wet chemical release processes are avoided. Monolithic single crystal Si features were fabricated by etching continuous trenches in the device layer of an SOI wafer using a DRIE process optimized to stop on the buried SiO{sub 2}. The buried SiO{sub 2} was then etched to handle Si using an anisotropic plasma etch process. The sidewalls of the device Si features were then protected with a conformal passivation layer of either FC polymer or SiO{sub 2}. FC polymer was deposited from C4F8 gas precursor in an inductively coupled plasma reactor, and SiO{sub 2} was deposited by plasma enhanced chemical vapor deposition (PECVD). A relatively high ion energy, directional reactive ion etch (RIE) plasma was used to remove the passivation film on surfaces normal to the direction of the ions while leaving the sidewall passivation intact. After the bottom of the trench was cleared to the underlying Si handle wafer, XeF{sub 2} was used to isotropically etch the handle Si, thus undercutting and releasing the features patterned in the device Si layer. The released device Si structures were not etched by the XeF{sub 2} due to protection from the top SiO{sub 2} mask, sidewall passivation, and the buried SiO{sub 2} layer. Optimization of the XeF{sub 2} process and the sidewall passivation layers will be discussed. The advantages of releasing SOI devices with XeF{sub 2} include avoiding stiction, maintaining the integrity of the buried SiO{sub 2}, and simplifying the fabrication flow for thermally actuated devices.

36 MATERIALS SCIENCE↗

A New Process for Fabricating Random Silicon Nanotips

An improved process for the fabrication of random arrays of silicon nanotips has been demonstrated to be feasible. Relative to other such processes, this process offers advantages of low cost and simplicity. Moreover, this process can readily be combined with other processes used to fabricate integrated circuits and other monolithic silicon structures. Arrays of silicon nanotips are subjects of research and development efforts directed toward utilizing them as field emitters in flat-panel displays, vacuum microelectronics, and microwave devices. Other silicon-nanotip-fabrication processes developed thus far predominantly include lithography, etching, and/or elaborate deposition steps followed by oxide sharpening steps and are both process intensive as well as expensive. In addition to being cheaper and simpler, the present process can efficiently produce silicon nanotips that range in height from a few microns to several tens of microns and are distributed over large areas. The process mentioned here can be summarized as consisting of (1) the growth of micro-etch masks on a silicon substrate, followed by (2) etching away of the masks, along with some of the substrate, to make an array of sharp tips. In the first step of the process, a cleaned silicon substrate is subjected to reactive ion etching (RIE) in a certain mixture of oxygen and carbon tetrafluoride under radio-frequency excitation. This process step results in the growth of fluorine based compounds in the form of stumps randomly distributed on the substrate. These stumps are known in the art as polymer RIE grass. The dimensions of these stumps are of the order of hundreds of nanometers, the exact values depending on process time and gas composition. The areal density of the stumps decreases with increasing process time as they grow and merge with neighboring stumps. These stumps constitute the micro-etch masks for the next step of the process. In the second step of the process, the substrate covered with the microetch masks is subjected to deep reactive ion etching (DRIE) process, which consists of cycles of reactive ion etching alternating with passivation (the Bosch process). The gas used in the etching substeps is sulfur hexafluoride (SF6); the gas used in the passivation substeps is octafluorocyclobutane (C4F8). The portions of the substrate directly under the RIE grass stubs are etched more slowly than are the portions between the stubs. Hence, what remains at the end of the process, after the stubs and parts of the substrate have been etched away, are silicon spikes where the stubs were (see figure). In a variation of the process, one starts with a silicon or silicon-on-insulator substrate with the intent to etch through the full thickness of the substrate. That is to say, one chooses the thickness so that the DRIE step releases individual nanotips. Such individual silicon nanotips may have utility as microscopic probes in biomedical applications.

Manohara, Harish↗

Effects of type of reactor, crystallinity of SiC, and NF{sub 3} gas pressure on etching rate and smoothness of SiC surface using NF{sub 3} gas plasma

Polycrystalline {beta}-SiC and single-crystalline 4H-SiC surfaces were etched by reactive ion etching (RIE) using NF{sub 3} gas plasma. A smooth surface was obtained on the polycrystalline SiC after RIE at NF{sub 3} gas pressures of 2 and 10 Pa for 10 min, and neither spikes nor pillars were formed on it. On the other hand, some pillars were formed on the single-crystalline SiC surface by RIE at NF{sub 3} gas pressures of 2 and 10 Pa. Though the absence of carbon-rich regions and SiO{sub x} on the outermost surface before etching was confirmed by x-ray photoelectron spectroscopy and Raman analysis, x-ray diffraction analysis revealed that graphite crystallites were present in the single-crystalline SiC bulk. It was concluded that the graphite crystallites acted as masks and the pillars grew up from the graphite crystallites in the single crystalline SiC during RIE.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Simulation of MEMS for the Next Generation Space Telescope

The NASA Goddard Space Flight Center (GSFC) is developing optical micro-electromechanical system (MEMS) components for potential application in Next Generation Space Telescope (NGST) science instruments. In this work, we present an overview of the electro-mechanical simulation of three MEMS components for NGST, which include a reflective micro-mirror array and transmissive microshutter array for aperture control for a near infrared (NIR) multi-object spectrometer and a large aperture MEMS Fabry-Perot tunable filter for a NIR wide field camera. In all cases the device must operate at cryogenic temperatures with low power consumption and low, complementary metal oxide semiconductor (CMOS) compatible, voltages. The goal of our simulation efforts is to adequately predict both the performance and the reliability of the devices during ground handling, launch, and operation to prevent failures late in the development process and during flight. This goal requires detailed modeling and validation of complex electro-thermal-mechanical interactions and very large non-linear deformations, often involving surface contact. Various parameters such as spatial dimensions and device response are often difficult to measure reliably at these small scales. In addition, these devices are fabricated from a wide variety of materials including surface micro-machined aluminum, reactive ion etched (RIE) silicon nitride, and deep reactive ion etched (DRIE) bulk single crystal silicon. The above broad set of conditions combine to be a formidable challenge for space flight qualification analysis. These simulations represent NASA/GSFC's first attempts at implementing a comprehensive strategy to address complex MEMS structures.

Mott, Brent↗

Fabricating Ultra-Thin Silicon Carbide Diaphragms

A process for fabricating relatively thin SiC diaphragms may include fast Reactive Ion Etching (RIE) followed by Dopant Selective Reactive Ion Etching (DSRIE). The process may produce silicon carbide (SiC) diaphragms thinner than 10 microns. These thinner, more sensitive diaphragms may then be used to effectively resolve sub-psi pressures in jet engines, for example.

Okojie, Robert S.↗

Point defect distribution in high-mobility conductive SrTiO{sub 3} crystals

We have carried out positron-annihilation spectroscopy to characterize the spatial distribution and the nature of vacancy defects in insulating as-received as well as in reduced SrTiO{sub 3} substrates exhibiting high-mobility conduction. The substrates were reduced either by ion etching the substrate surfaces or by doping with vacancies during thin-film deposition at low pressure and high temperature. We show that Ti vacancies are native defects homogeneously distributed in as-received substrates. In contrast, the dominant vacancy defects are the same both in ion etched crystals and substrates reduced during the film growth, and they consist of nonhomogeneous distributions of cation-oxygen vacancy complexes. Their spatial extension is tuned from a few microns in ion-etched samples to the whole substrate in specimens reduced during film deposition. Our results shed light on the transport mechanisms of conductive SrTiO{sub 3} crystals and on strategies for defect-engineered oxide quantum wells, wires, and dots.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Etching of diamond with argon and oxygen ion beams

The angular dependences of the sputter yield of (100) single crystal diamond under argon and oxygen ion beams were investigated. For argon ion beams a large increase in the sputter yield was observed as the angle of incidence was increased from the normal, with a maximum occurring at approximately 60 deg from the normal. The magnitude of the increase and the angle at which the maximum was observed were dependent on the ion energy and species. The shape of the yield versus angle of incidence curve indicated the presence of a highly damaged surface layer. Large deviations from this curve were observed where ion incidence was along channeling directions. Studies with oxygen ion beams showed almost no angular dependence for 500 eV ions while at an energy of 1000 eV the angular dependence was similar to that for argon ions. At normal incidence the yield for 500 eV oxygen ions was seven times larger than that for 500 eV argon ions. For 1000 eV oxygen and argon ions the corresponding ratio is only 2.5. Implications for mechanisms of inert and reactive ion etching are discussed. Application of the data to ion beam shaping of diamond tips for ultrahigh pressure research is discussed.

Whetten, T. J.↗

Efficiency measurements of reflection gratings in the 100-300-A band

Zero-order and first-order efficiencies of plane diffraction grazings over the 100-300-A band have been measured using the NRL beamline facility at the National Synchrotron Light Source. Measurements were taken at grating angles of 5, 10, and 15 deg, and the incident radiation was polarized primarily in the transverse magnetic mode. Four (three laminar, one blazed) of the gratings were ion etched in high quality quartz blanks, overcoated with 200 A of gold. A fifth (blazed) grating was ruled in gold. The line densities are 1000, 2000, and 3600 grooves/mm for those with laminar profiles. Both blazed gratings have a blaze angle of 8 deg and line densities of 3600 grooves/mm. Measured first-order efficiencies up to 15 percent were obtained for the laminar gratings and up to 8 percent was obtained for the ion-etched blazed grating. Much lower efficiencies (not greater than 2 percent) were measured for the ruled grating. A computer program was written to calculate grating efficiencies using a full electromagnetic model. Measured efficiencies of the ion-etched gratings agree well with predicted values, but the measured first-order efficiency of the ruled grating is much lower than predicted.

Meekins, John F.↗

Seasoning of plasma etching reactors: Ion energy distributions to walls and real-time and run-to-run control strategies

Wafer-to-wafer process reproducibility during plasma etching often depends on the conditioning of the inside surfaces of the reactor. Passivation of reactor surfaces by plasma generated species, often called seasoning, can change the reactive sticking coefficients of radicals, thereby changing the composition of the radical and ion fluxes to the wafer. Ion bombardment of the walls may influence these processes through activation of surface sites or sputtering, and so the spatial variation of ion energies on the walls is important. These seasoning processes may occur during a single etching process or on a wafer-to-wafer basis. The seasoning of plasma etching reactors will be discussed using results from a computational investigation of p-Si etching in chlorine plasmas. The transport of etch products, passivation of walls, and sputtered products from walls are accounted for, as well as differentiating the ion energy distributions to different surfaces. A real-time, closed-loop control of etch rate to counter the effects of seasoning was achieved using the bias voltage as an actuator.

36 MATERIALS SCIENCE↗

Ion-beam etching enhances adhesive bonding

Metals and fluoropolymers exposed to 0.5 to 1.0 keV argon ions at current densities of 0.2 to 1.5 mA/sq cm develop surface texturing that increases tensile and shear strength of epoxy bonds. Bonds are 46 to 100 percent stronger than those of chemically etched surfaces. Metals require 3 to 4 hours of bombardment to become properly textured. Fluoropolymers require 5 seconds to 30 minutes. Ion beam will not texture nickel. Unlike chemical treatments, bonding of fluoropolymers can be done days or months after ion treatment.

Banks, B. A.↗

Enhanced electrochemical etching of ion irradiated silicon by localized amorphization

A tailored distribution of ion induced defects in p-type silicon allows subsequent electrochemical anodization to be modified in various ways. Here we describe how a low level of lattice amorphization induced by ion irradiation influences anodization. First, it superposes a chemical etching effect, which is observable at high fluences as a reduced height of a micromachined component. Second, at lower fluences, it greatly enhances electrochemical anodization by allowing a hole diffusion current to flow to the exposed surface. We present an anodization model, which explains all observed effects produced by light ions such as helium and heavy ions such as cesium over a wide range of fluences and irradiation geometries.

36 MATERIALS SCIENCE↗

Fabrication of large dual-polarized multichroic TES bolometer arrays for CMB measurements with the SPT-3G camera

This paper presents the procedures used by Argonne National Laboratory to fabricate large arrays of multichroic transition-edge sensor (TES) bolometers for cosmic microwave background (CMB) measurements. These detectors will be assembled into the focal plane for the SPT-3G camera, the third generation CMB camera to be installed in the South Pole Telescope. The complete SPT-3G camera will have approximately 2690 pixels, for a total of 16,140 TES bolometric detectors. Each pixel is comprised of a broad-band sinuous antenna coupled to a Nb microstrip line. In-line filters are used to define the different band-passes before the millimeter-wavelength signal is fed to the respective Ti/Au TES bolometers. There are six TES bolometer detectors per pixel, which allow for measurements of three band-passes (95 GHz, 150 GHz and 220 GHz) and two polarizations. The steps involved in the monolithic fabrication of these detector arrays are presented here in detail. Patterns are defined using a combination of stepper and contact lithography. The misalignment between layers is kept below 200 nm. The overall fabrication involves a total of 16 processes, including reactive and magnetron sputtering, reactive ion etching, inductively coupled plasma etching and chemical etching.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Evidence for anti-synergism between ion-assisted etching and in-plasma photoassisted etching of silicon in a high-density chlorine plasma

Etching of p-Si in 60 mTorr 10%Cl2/90%Ar Faraday-shielded inductively coupled high density plasmas was investigated under both ionassisted etching (IAE) and photoassisted etching (PAE) conditions. Real-time etching rates and after-etching Si surface chemical compositions were obtained by laser interferometry and vacuum-transfer x-ray photoelectron spectroscopy (XPS), respectively. Precisely controlled ion energy distributions (IEDs) were generated by applying pulsed negative DC bias on the conductive sample stage. Above a 36 eV threshold at a total flow rate of 250 SCCM, the IAE rate increased with the square root of the ion energy. In contrast to the DC bias, etching under RF bias did not exhibit a threshold ion energy because of the wide IED. XPS spectra revealed that the surface layer under PAE conditions had a significantly lower chlorine content, composed of only SiCl. Under IAE conditions, however, silicon dangling bonds (Si•), SiCl 2 , and SiCl 3 were found on the surface, in addition to SiCl, with a relative abundance of SiCl > SiCl 2 , and SiCl 3 . The absence of higher chlorides and Si• under PAE conditions suggested that vacuum ultraviolet photons and above threshold-energy ions interact with the surface very differently. By varying the duty cycle of the pulsed DC bias, it was found that the IAE rate scaled with the energetic ion dose, but only for low duty cycles. For higher duty cycles, the apparent IAE yield fell off with an increasing Cl coverage on the surface, as the duty cycle went up, which pointed to a negative synergy (antisynergism) between PAE and IAE as the explanation. This antisynergism was further supported by the observed decrease of the total etching rate with an increasing period of the pulsed DC bias. A plausible mechanism is that increasing the pulsing period causes more near-surface damage, creating more recombination centers that lead to a higher loss rate of electron-hole pairs through recombination, thereby reducing the PAE rate.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Influence of Processing Techniques on the Surface Microstructure of V{sub 85}Ni{sub 15} Membrane Alloy

Vanadium-based alloys with a BCC structure are considered to be an alternative to palladium alloys for hydrogen purification. Since the performance of membranes is influenced by not only their bulk characteristics but also their surface condition, we have investigated the effect of different surface preparation techniques (abrasive grinding and polishing, electrolytic polishing, and ion etching) on the surface microstructure of V{sub 85}Ni{sub 15} membrane alloy using X-ray photoelectron spectroscopy. After electrolytic polishing and ion etching, we observed an increase in the percentages of vanadium and nickel metals in the surface layer of the alloy in comparison with its state after abrasive polishing. Such changes are expected to be favorable for an increase in the rate of hydrogen dissociation and recombination on the surface of the membrane material, eventually improving hydrogen transport efficiency.

36 MATERIALS SCIENCE↗

Germanium Lift-Off Masks for Thin Metal Film Patterning

A technique has been developed for patterning thin metallic films that are, in turn, used to fabricate microelectronics circuitry and thin-film sensors. The technique uses germanium thin films as lift-off masks. This requires development of a technique to strip or undercut the germanium chemically without affecting the deposited metal. Unlike in the case of conventional polymeric lift-off masks, the substrate can be exposed to very high temperatures during processing (sputter deposition). The reason why polymeric liftoff masks cannot be exposed to very high temperatures (greater than 100 C) is because (a) they can become cross linked, making lift-off very difficult if not impossible, and (b) they can outgas nitrogen and oxygen, which then can react with the metal being deposited. Consequently, this innovation is expected to find use in the fabrication of transition edge sensors and microwave kinetic inductance detectors, which use thin superconducting films deposited at high temperature as their sensing elements. Transition edge sensors, microwave kinetic inductance detectors, and their circuitry are comprised of superconducting thin films, for example Nb and TiN. Reactive ion etching can be used to pattern these films; however, reactive ion etching also damages the underlying substrate, which is unwanted in many instances. Polymeric lift-off techniques permit thin-film patterning without any substrate damage, but they are difficult to remove and the polymer can outgas during thin-film deposition. The outgassed material can then react with the film with the consequence of altered and non-reproducible materials properties, which, in turn, is deleterious for sensors and their circuitry. The purpose of this innovation was to fabricate a germanium lift-off mask to be used for patterning thin metal films.

Brown, Ari↗

Physical and Chemical Changes of Polystyrene Nanospheres Irradiated with Laser

It has been reported that polymer resist such as PMMA (Poly(methyl methacrylate) which is a well known and commonly used polymer resist for fabrication of electronic devices can show zwitter characteristic due to over exposure to electron beam radiation. Overexposed PMMA tend to changes their molecular structure to either become negative or positive resist corresponded to electron beam irradiation doses. These characteristic was due to crosslinking and scissors of the PMMA molecular structures, but till now the understanding of crosslinking and scissors of the polymer resist molecular structure due to electron beam exposure were still unknown to researchers. Previously we have over exposed polystyrene nanospheres to various radiation sources, such as electron beam, solar radiation and laser, which is another compound that can act as polymer resist. We investigated the physical and chemical structures of the irradiated polystyrene nanospheres with FTIR analysis. It is found that the physical and chemical changes of the irradiated polystyrene were found to be corresponded with the radiation dosages. Later, combining Laser irradiation and Reactive Ion Etching manipulation, created a facile technique that we called as LARIEA NSL (Laser and Reactive Ion Etching Assisted Nanosphere Lithography) which can be a facile technique to fabricate controllable carbonaceous nanoparticles for applications such as lithographic mask, catalysts and heavy metal absorbers.

77 NANOSCIENCE AND NANOTECHNOLOGY↗