Oxidation behavior of Fe-Cr-2Si alloys in high temperature steam
FeCrSi alloys have been proposed as alternatives to FeCrAl alloys for accident-tolerant fuel cladding in light water reactors. Experiments on the oxidation resistance of three Fe-Cr-2Si alloys in high-temperature steam, with 12, 16, and 20 wt. % Cr, show that ≥16 % Cr is sufficient to form a thin, passivating, binary oxide layer. Additionally, at 1200 °C, only Cr 2 O 3 and SiO 2 form on Fe 16 Cr 2 Si and Fe 20 Cr 2 Si, while additional ternary Fe oxides form on Fe 12 Cr 2 Si. Decohesion and spalling of oxide were observed on Fe-Cr-Si alloys exposed to steam at 900 °C and above. Fe 20 Cr 2 Si exhibits the best oxidation resistance of the three in high-temperature steam.