At least 109 records · Page 6

Origin of micrometer-scale dislocation motion during hydrogen desorption

Hydrogen, while being a potential energy solution, creates arguably the most important embrittlement problem in high-strength metals. However, the underlying hydrogen-defect interactions leading to embrittlement are challenging to unravel. Here, we investigate an intriguing hydrogen effect to shed more light on these interactions. By designing an in situ electron channeling contrast imaging experiment of samples under no external stresses, we show that dislocations (atomic-scale line defects) can move distances reaching 1.5 μm during hydrogen desorption. Combining molecular dynamics and grand canonical Monte Carlo simulations, we reveal that grain boundary hydrogen segregation can cause the required long-range resolved shear stresses, as well as short-range atomic stress fluctuations. Thus, such segregation effects should be considered widely in hydrogen research.

36 MATERIALS SCIENCE↗

Thermocouple Testing in Support of the AGR-5/6/7 Experiment

This report documents thermocouple testing performed in IRC Lab C-15 over a period of seven years. This testing supported selection and characterization of the thermocouple set used in the AGR-5/6/7 experiment. The following summary was taken directly from the report. Temperature measurement is a challenging aspect of very high temperature irradiation experiments because commonly used high-temperature commercial thermocouples such as platinum-rhodium (Types S, R, and B) and tungsten-rhenium (Type C), suffer dramatic drift because of neutron-induced transmutation. As a result, these types of thermocouples, which are used routinely for industrial temperature measurements outside of reactors, are used only in very special circumstances for reactor experiments. Conversely, because of their low neutron cross-sections, Type N thermocouples are affected to only a limited extent by neutron irradiation. However, the use of these nickel-based thermocouples is limited when the temperature exceeds 1050°C due to drift arising from minor alloying elements migrating from the thermocouple's metal sheath to the thermoelements. This change in the composition of the thermo-elements results in significant decalibration of the signal. The issues described above were recognized during the early planning stages of the final AGR experiment (designated AGR-5/6/7), and a thermocouple furnace testing program was performed over a seven-year period (2014-2019, 2021) to first select and then characterize the best thermocouple set for the high temperature regions of the AGR-5/6/7 irradiation experiment. The calculated temperature range of the AGR-5/6/7 experiment was 600–1500°C. For temperatures below 1000°C standard Type N thermocouples were deemed adequate. The furnace testing campaign identified two thermocouple types suitable for measuring temperatures above 1000°C, a Mo/Nb thermocouple developed at INL called HTIR-TC, and a Type N thermocouple developed by Cambridge University (called herein Cambridge Type N), which featured a custom high nickel alloy sheath. One of the original goals of the furnace testing program was to identify a thermocouple capable of low drift operation near the peak temperature expected in AGR-5/6/7, i.e., about 1400°C. The HTIR-TC design appeared promising in this regard, however a manufacturing difficulty proved to be a barrier and instead the furnace testing focused on drift performance at 1250°C. The manufacturing difficulty was that the Nb sheaths of the HTIR-TCs experienced extreme embrittlement when heat treated at 1600°C or greater. Heat treatment is needed to stabilize the emf output of this TC type, and the higher the heat treatment temperature the higher the peak temperature of stable operation. Because of the sheath embrittlement the heat treatment temperature had to be lowered to 1450°C resulting in a stable operating temperature of about 1250°C. One of the successes of the furnace testing program was identification of a shortcoming in the heat treatment procedure that had been traditionally used in the production of HTIR-TCs. The shortcoming was that the entire heated length of the HTIR-TC sensor was not being heat treated, but rather only the part of the sensor expected to experience temperatures above 1000°C. The problem manifested itself when the thermocouples were removed from the heat treat furnace and placed in another furnace with a different geometry, their indicated temperatures would be widely scattered, but mostly in the negative direction. The solution was to heat treat the entire heated length of the sensor. Since the deepest immersion depth in the AGR-5/6/7 experiment was about 40 inches, a heat treatment length of 48 inches was used. After this change was implemented, thermocouples which were moved into a new environment with a different temperature profile (i.e., a different furnace), produced accurate temperature measurements. Although assembly of the AGR-5/6/7 experiment was completed in September of 2017 (and irradiation begun in 2018), furnace testing of thermocouples continued in 2018 and 2019. The main purpose of this testing was to establish very long-term drift characteristics of the HTIR and Cambridge Type N thermocouples installed in the experiment. Representative thermocouples from the same lots as those installed in the AGR-5/6/7 experiment were used. Additionally, thermocouples of different designs, (particularly variations on the HTIR-TC design) were "piggy-backed" on this testing program to provide insights for instrumenting future very high temperature irradiation experiments. This two-year testing program demonstrated that HTIR-TCs and Cambridge Type N TCs could operate at 1250°C for up to 10,000 hrs (and in some cases longer) while experiencing negative drifts on the order of 2-4°C/1000 hrs. This performance was considered acceptable given the extreme operating environment the sensors faced.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Cracking Behavior of Irradiated Ex-Plant Materials

The cracking behavior of reactor core internal materials is a key factor for the long-term safety and availability of light water reactors. Subject to high-temperature coolant, thermal and mechanical loading, and neutron irradiation, reactor core internal materials are susceptible to several degradation mechanisms during power operation. To understand the long-term effects of neutron irradiation, irradiated materials harvested from a decommissioned reactor were studied for their cracking susceptibility and fracture resistance. Small compact-tension specimens were machined from different locations on the baffle plates with irradiation doses ranging from 0.06 to 48.5 dpa. Crack growth rate and fracture toughness J-resistance (J-R) curve tests were performed on these specimens in a simulated light water reactor environment, and the fracture morphologies of the tested samples were examined with a scanning electron microscope. All samples behaved similarly under cyclic loading, and no deteriorated corrosion-fatigue behavior was observed in the test environments. Under constant load, no elevated cracking susceptibility was observed either in these samples at low stress intensity factors. However, a rapid cracking behavior featuring very high crack growth rates was observed in several high-dose samples. This rapid crack growth behavior was activated when the applied stress intensity factor, K, was sufficiently high. Once activated, the rapid crack growth remained steady even when the K was lowered to the pre-activation level and stopped only when the K was reduced drastically. Yet, the rapid crack growth could be re-activated repeatedly in these samples by raising the K above the initial activation level. This rapid cracking response may be related to the severe irradiation embrittlement experienced by these samples. The J-R curve tests performed with these samples showed a significant decline in fracture toughness with increasing neutron irradiation. Local cracking at the crack tip facilitated by the severe irradiation embrittlement of this material may be responsible for the rapid crack growth behavior demonstrated by this decommissioned material.

36 MATERIALS SCIENCE↗

Report on Retrieval of the Reactor Pressure Vessel A-60 Surveillance Capsule from Palisades Nuclear Generating Station

Located on the shores of Lake Michigan, the Palisades Nuclear Generating Station (PNGS) was a nuclear power plant that operated in Covert Township, Michigan. The plant had a single pressurized water reactor that produced electricity for the region. The PNGS was shut down in 2022 after more than four decades of service. The PNGS included in its surveillance program a surveillance capsule, designated A-60, containing specimens of a weld metal with nickel content of about 1.36 wt% and copper content of about 0.20 wt%. The capsule was removed from its surveillance position in the early 1995 and has been resident in the spent fuel pool since that time. This capsule was irradiated to a fluence of 1.87×10 20 n/cm 2 (E> 1MeV) that is equivalent for more than 120 effective full power year (EFPY) for the US reactor pressure vessel (RPV) fleet. The material is also of special interest because of its very high nickel content and potential for development of NiMnSi (nickel-manganese-silicon) precipitates. Combination of very high fluence and very high Ni and Cu content makes the material in this capsule of the great interest as benchmark for currently developing embrittlement trend curves (ETC) aiming to predict embrittlement at high fluences. Thus, several years ago the Light Water Reactor Sustainability Program (LWRSP) initiated negotiations with Entergy to harvest this high fluence capsule since it did not present any regulatory interest for PNGS but could play a very important role for LWRSP efforts for developing ETC for very long-term operation. The negotiations resumed once PNGS ownership moved to the Holtec International in June 2022 which was very supportive to the LWRSP efforts to harvest the A-60 capsule from the spent fuel pool. As a result, the contract was placed with the Westinghouse Electric Company (WEC) to come to PNGS site, retrieve the A-60 capsule, bring it to WEC Churchill hot cell facility, open the capsule and send all surveillance specimens in the capsule to ORNL for future characterization. These specimens from the PNGS A-60 capsule have arrived to ORNL in July 2023 and this report summarizes activities to retrieve and deliver specimens to ORNL site for future evaluation.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Towards High-Throughput Computation of Phase-and Defect Diagrams

The past decade has seen immense advances in our understanding of defect thermodynamics, and the use of machine learning and data science approaches has played a critical role in these advances [1–14]. In the area of grain boundaries (GBs), a particular focus has been placed on the effects of alloying – namely, GB solute segregation or more broadly, GB alloying [15–25], which has been observed and catalogued across a vast range of systems [26–50]. The impacts of solute segregation to GBs are numerous, and can range from negative effects such as embrittlement – for example, due to impurities [51–53], during irradiation [54–61], or during heat treatment [62–65] – to positive effects such as the stabilization against grain growth [66–69], thus enabling the design of nanocrystalline alloys with access to an enhanced range of functional and mechanical properties, and the reduction of embrittlement through the segregation of GB strengthening solutes [49,70–79].

36 MATERIALS SCIENCE↗

Crack Growth Rate and Fracture Toughness Tests on Irradiated Ex-Plant Materials

The performance of structural materials is critical for the safe and economic operation of light water reactors. Exposed to neutron irradiation during service, the reactor core internal materials can undergo significant microstructural and microchemical changes, leading to irradiation hardening and embrittlement. To ensure the structural integrity and functionality of nuclear reactor components during long-term operation, material degradation and damage mechanisms must be understood and managed adequately. In this work, irradiated materials harvested from the decommissioned Zorita reactor were studied for their cracking susceptibility and fracture resistance as a function of irradiation dose up to 47 displacement per atom (dpa). The material is a Type 304 stainless steel sectioned from the baffle plates of this pressurized water reactor with 38 years of service. Crack growth rate and fracture toughness J-resistance (J-R) curve tests were performed in low-corrosion-potential environments at ~315°C. All samples behaved similarly under cyclic loading, and no deteriorated corrosion-fatigue behavior was observed in the test environments. Under constant stress intensity factors, most samples did not show elevated crack growth rates, suggesting an adequate stress corrosion cracking resistance in the test environments. However, an unstable cracking behavior was observed in a 47-dpa sample, resulting in significantly higher crack growth rates than expected at high stress intensity factors. Crack instability was also observed in a 0.06-dpa sample but did not lead to a sustained high crack growth rate. The impact of neutron irradiation was more evident in the fracture toughness J-R curve tests. As the dose increased, the J-R curve declined considerably and became very shallow at high doses. A fully intergranular fracture morphology was also observed among the high-dose samples ruptured in an air atmosphere at room temperature. This brittle fracture mode in the absence of high temperature water environment confirmed a high degree of embrittlement of this material resulting from its service exposure to neutron irradiation.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Direct Imaging of Hydrogen‐Driven Dislocation and Strain Field Evolution in a Stainless Steel Grain

Hydrogen embrittlement (HE) poses a significant challenge to the durability of materials used in hydrogen production and utilization. Disentangling the competing nanoscale mechanisms driving HE often relies on simulations and electron-transparent sample techniques, limiting experimental insights into hydrogen-induced dislocation behavior in bulk materials. This study employs in situ Bragg coherent X-ray diffraction imaging to track three-dimensional (3D) dislocation and strain field evolution during hydrogen charging in a bulk grain of austenitic 316 stainless steel. Tracking a single dislocation reveals hydrogen-enhanced mobility and relaxation, consistent with dislocation dynamics simulations. Subsequent observations reveal dislocation unpinning and climb processes, likely driven by osmotic forces. Additionally, nanoscale strain analysis around the dislocation core directly measures hydrogen-induced elastic shielding. These findings experimentally validate theoretical predictions and offer mechanistic insights into hydrogen-driven dislocation behavior. The quantified nanoscale phenomena serve as critical inputs for multiscale modeling frameworks to predict bulk material responses and accelerate the development of HE-resistant alloys.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Doping Effects on the Ductility of a Lightweight Refractory High-Entropy Alloy: Grain Boundary and Bulk Lattice Aspects

Doping elements in small amounts often segregate to grain boundaries (GBs) in alloys and can significantly impact mechanical properties and performance. Refractory high-entropy alloys (RHEAs) are known for their poor ductility, especially at low temperatures. Promoting GB cohesion through segregation can be an effective approach to mitigate embrittlement. Here, in this study, first-principles density functional theory (DFT) calculations were performed to examine the effects of important interstitial dopants (O, B, C, and N) and substitutional dopants (Cr, Y, La, and Ce) on the Σ5(310) [001] tilt GB of a lightweight RHEA Nb 32.5 Ti 27.5 Mo 22.5 Ta 12.5 Hf 2.5 Zr 2.5 . The DFT calculations reveal that certain dopants, such as B, C, Cr, N, and Y, exhibit favorable GB strengthening effects by improving bonding interactions with the bulk alloy. The impact of doping on the ductility parameter of the bulk lattice, defined as the ratio of surface energy to unstable stacking fault energy for the {110} <111> slip system, was also studied; and the results show that doping reduces the intrinsic ductility of the alloy, decreasing the D-parameter from 2.90 to 2.55, depending on the specific dopant. The present findings provide a foundational understanding at atomic level of the effect of representative dopants on mechanical properties of RHEAs and can be used to guide future alloy design for improved mechanical properties.

deformation charge density↗

Characterization of boundary precipitation in a heavy ion irradiated tungsten heavy alloy under the simulated fusion environment

In the concerted effort to identify materials capable of surviving the adverse environment of a fusion reactor interior, tungsten heavy alloys have been put forth as leading candidates. Experimental trials and behavioral studies have yielded positive results for their adoption by taking advantage of the alloy’s unique balance of inherently high fracture toughness and low sputter yields; yet due to their relative novelty in the fusion community, there remains a lack of understanding on the response of these materials to the extended high temperature irradiation environment of the reactor interior. Further, to alleviate this issue and provide the necessary data on the behavior of tungsten heavy alloys to the simulated fusion environment, a 90W-7Ni-3Fe alloy has been subjected to elevated temperature sequential Ni + and He + ion irradiations to mimic the expected displacement damage and gas production expected after five years of service as a plasma facing material component. Atomic-scale structural analyses and nanoscale chemical mapping have identified the formation of two distinct precipitation structures, a surface localized η-carbide and an a-W 2 C type tungsten carbide, both of which appear to originate at the bi-phase interface between W and the ductile phase. This irradiation assisted and induced precipitate formation respectively is anticipated to adversely affect these materials by selective embrittlement at bi-phase interfaces leading to a reduction in the material’s overall fracture toughness during prolonged high temperature irradiation. It is asserted that any potential exposure to C during fusion reactor operational service should be minimized as to prevent the formation of these phases.

36 MATERIALS SCIENCE↗

Hydrogen-enhanced compatibility constraint for intergranular failure in FCC FeNiCoCrMn high-entropy alloy

The fundamental mechanism of hydrogen embrittlement was investigated in the high-entropy alloy FeNiCoCrMn using slow strain rate tensile tests with and without internal hydrogen. Hydrogen induced intergranular failure and reduced the average grain elongation parallel to the tensile axis, but also increased the local plasticity within grains. Here, the influence of hydrogen on plasticity establishes a compatibility constraint across grain boundaries, which results in failure along the hydrogen-weakened grain boundaries. This study is the first to directly confirm the presence of the hydrogen-enhanced compatibility constraint in a high-entropy alloy and highlights the importance of developing a physical understanding of grain-scale interactions.

36 MATERIALS SCIENCE↗

Effects of hydrogen partial pressure on crack initiation and growth rate in vintage X52 steel

There is an increasing interest in ensuring compatibility of existing natural gas infrastructure with conveyance of hydrogen, especially for vintage (pre-1970s) pipeline steels. While hydrogen is known to affect the fatigue and fracture resistance of these materials, there is a lack of data on its effects on crack initiation at low hydrogen partial pressure. To address this gap, the current work presents a series of fatigue tests on vintage API Grade X52 steel in pure nitrogen, air and gaseous hydrogen at partial pressures of 1 and 207 bar. Circumferential notch tension (CNT) specimens with direct current potential difference (DCPD) measurements are used to get S–N curves for crack initiation and failure, and compact tension (CT) tests to assess crack growth rates. Results indicate that air accelerates crack initiation, low hydrogen partial pressure affects the crack growth rate, and higher pressures have the largest impact on both. Surprisingly, crack initiation is faster in air than at 1 bar hydrogen partial pressure. The CNT tests also reveal that the orientation of the banded microstructure has no effect on the crack initiation site, but it influences its growth behavior. Moreover, fractography shows that hydrogen also promotes instances of quasi-cleavage and intergranular fracture, linked to embrittlement of the material. Here, these results demonstrate that, while hydrogen may impact the entirety of the fatigue process, its effects on the early stages of damage accumulation become relevant only at larger pressures. More comprehensive studies of crack initiation in hydrogen atmospheres will be critical to future codes and standards for hydrogen infrastructure.

Circumferential notch tension↗

Influence of stacking fault energy and hydrogen on deformation mechanisms in high Mn austenitic steels during in-situ tensile testing

High Mn austenitic steels are considered an economical alloy system for hydrogen storage and transport applications. This study used stacking fault energy (SFE) as a design parameter to achieve hydrogen embrittlement (HE)-resistant high Mn austenitic alloys. The role of hydrogen on the deformation mechanisms of low (29 mJ/m 2 ) and high SFE (49 mJ/m 2 ) alloys was evaluated through in-situ neutron diffraction during tensile loading. Hydrogen-precharging increased yield strength, partly due to hydrogen-induced lattice distortion (i.e., solute strengthening). Hydrogen accelerated the increase in defect density, including dislocations and stacking faults. The formation of planar deformation structures (twins and stacking faults), relative to dislocations, plays a critical role in promoting hydrogen-assisted fracture. The stacking fault frequency parameter obtained from neutron diffraction quantifies planar deformation tendencies, correlated with HE sensitivity. The higher SFE alloy exhibited greater resistance to HE, associated with the reduced propensity to form stacking faults and twins upon deformation in the hydrogen-precharged condition.

High Mn austenitic steel↗

Interplay between hydrogen, temperature, and character angle on dissociated dislocation energies in Fe–Ni–Cr austenitic stainless steels

Dislocation energy has an important role in the mechanical performance of structural metals. While dislocation energies cannot be fully obtained from continuum theories due to the contribution of the dislocation core, they have been calculated via atomistic simulations in elemental metals. However, constraints on the local atomic environments have prevented the use of such approaches in systems that incorporate alloying or interstitial solutes. In this work, we develop robust molecular dynamics methods to resolve these issues through a geometric construction of dislocation dipoles and the calculation of time-averaged energies. Furthermore, we apply these methods to calculate dislocation energies (including core energies) in an Fe 70 Ni 11 Cr 19 austenitic steel at a variety of character angles, hydrogen concentrations, temperatures, and dipole spacings. The resulting highly converged energies show an excellent agreement with continuum expressions. Overall, hydrogen concentrations up to 1.0 % do not have a significant effect on the elastic parameters and dislocation energy. The methods and insights derived in this work have the potential to facilitate the calculation of dislocation energies in a wide range of systems, and to guide our understanding of hydrogen embrittlement.

Alloyed systems↗

Effects of HFIR neutron irradiation on fracture toughness properties of standard and Ni-doped F82H

F82H is the Japanese reference reduced-activation ferritic-martensitic (RAFM) steel for fusion blanket applications. The harsh environment of a fusion reactor, such as neutron irradiation and He/H damage, can result in significant degradation of F82H fracture toughness. Therefore, understanding the fracture toughness behavior of F82H in the fusion environment is critical to ensure the long-term safe operation of the fusion reactor. Here, we summarize seven irradiation campaigns of the High Flux Isotope Reactor (HFIR) at Oak Ridge National Laboratory (ORNL) covering five variants of F82H steels, including F82H IEA, F82H Mod3, F82H doped with 1.4% natural Ni, F82H doped with 1.4% 58 Ni, and F82H doped with 1.4% 60 Ni. The irradiation temperatures covered the range from 220 °C to 530 °C and the neutron irradiation dose spanned 4 dpa to 70 dpa. The effects of neutron irradiation temperature, dose, materials composition, Ni doping, and He production on F82H fracture toughness are discussed. Our results showed that irradiation embrittlement monotonically decreased with increasing irradiation temperature until 400 °C for F82H IEA and F82H Mod3. F82H Mod3 showed better fracture toughness than F82H IEA both before and after neutron irradiation. We determined that 1.4% Ni alloying can be applied to F82H for simulating He effect in a fission reactor without jeopardizing the fracture toughness of the material. However, more studies are needed to understand the effect of high dose (>20 dpa) and He production on F82H fracture toughness.

36 MATERIALS SCIENCE↗

Small-scale mechanical testing and characterization of fuel cladding chemical interaction between HT9 cladding and advanced U-based metallic fuel alloy

Fuel cladding chemical interactions (FCCI) occurred on the interface between the nuclear metal fuel and cladding is the primary cause of cladding wastage, weakening cladding mechanical integrity, and placing fuel and cladding at risk. Although the microstructural and phase information of FCCI has been fairly understood, mechanical properties remain less studied due to limited reaction volume. Here, through a combining of advanced electron microscopy characterizations and small-scale mechanical testing techniques, including indentation and micro-tensile testing, this study investigated the microscale mechanical properties of FCCI between the ferritic/martensitic (F/M) HT9 cladding and an advanced Uranium (U)-based metallic fuel irradiated at the Advanced Test Reactor to 2.2% FIMA with peak inner cladding temperature reached to 650 °C. Mechanical testing results show significant hardening and embrittlement in the FCCI region. The brittle fracture of FCCI specimen is mainly attributed to the formation of nano-crystallized intermetallic σ-FeCr phase. Whereas mechanical softening was revealed in the unreacted HT9 matrix due to irradiation-induced microstructural and microchemical evolution, specifically, the disappearance of martensitic lath structure and the formation of Fe 2 Mo Laves phase precipitation which consumed the solid solution strengthening Mo from the F/M HT9 matrix. Due to the achieved high cladding temperature, this fuel pin is of particular significance for revealing the high-temperature irradiation effect on the mechanical properties of HT9 cladding. Therefore, the outcomes of this study are expected to contribute to the development of multi-scale mechanical behavior modeling of HT9 cladding for Generation IV reactors which requires cladding to run at higher temperature (above 600 ?).

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Deformation Strengthening of Uranium and Dilute Uranium Alloys

The strength and ductility of uranium and dilute uranium alloys can be substantially improved by deformation strengthening. The yield strength of unalloyed uranium can be nearly doubled by rolling in the vicinity of 250°C. The embrittling effect of hydrogen is also overcome, eliminating the need for vacuum outgassing to obtain good ductility. Significant differences in longitudinal versus transverse tensile properties result, in part, from texture introduced by unidirectional rolling. Warm rolling of U-2.3%Nb results in both traditional strain hardening and a significant Bauschinger effect, resulting in differences between tensile and compressive yield strength. A similar combination of strain hardening and Bauschinger effect also occurs in deformation strengthened U-0.75%Ti. Warm rolling of U-0.75%Ti results in significantly better combinations of tensile yield strength and ductility than can be obtained by conventional age hardening. Warm rolling prior to aging also reduces the loss of ductility which typically accompanies conventional age hardening. Here, an approach is developed in which the effects of prior deformation on tensile and compressive yield strengths are analyzed in terms of texture, long-range dislocation, and Bauschinger effects. The Bauschinger effect is shown to vary in sign with the type of deformation, thus providing opportunities to tailor tensile and compressive properties.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

A potential emerging issue concerning repair welding of out-of-core PWR components involving tritium exposure and 3 He retention

This paper identifies a potential but previously unrecognized risk of helium-induced embrittlement and cracking during repair welding of out-of-core pressurized water reactor (PWR) components exposed to tritium-contaminated coolant. While previous weldability concerns centered on 4 He accumulation in neutron-irradiated alloys located within the in-core or near-core regions, new measurements show that 3 He generated by tritium decay can accumulate in out-of-core components. Because hydrogen isotopes readily diffuse to grain boundaries and become trapped there, significant 3 He generation at grain boundaries may lead to cracking during weld repairs. Initial data from far-below-core PWR flux thimble tubes confirm the presence of 3 He levels above known cracking thresholds for repair welds. In conclusion, these findings indicate that out-of-core regions should be considered when defining safe weld repair windows in reactors operating for 60–100 years.

Extended PWR lifetimes↗

High energy X-ray diffraction and small-angle scattering measurements of hydrogen fatigue damage in AISI 4130 steel

Accurate lifetime predictions are critical for repurposing existing pipelines for hydrogen transmission as well as for developing novel steels which are minimally susceptible to lifetime degradation by hydrogen. Ultimately, lifetime prediction models assess the amount of damage a material undergoes during a typical service cycle and the cumulative damage a material can withstand prior to failure. However, not all damage processes are equal, and neither is the manner in which mechanical loading translates to damage the same when materials are in inert environments compared to in hydrogen environments. For example, in the three leading proposed mechanisms of hydrogen embrittlement (Hydrogen-Enhanced Decohesion (HEDE), the Hydrogen-Enhanced Localized Plasticity (HELP), and the Nano-Void Coalescence (NVC)), hydrogen is proposed to enhance the manifestation of grain separation, dislocation generation/movement, and void coalescence, respectively. A full understanding of the damage modes requires a measurement capable of probing all three mechanisms at once. Here we present simultaneous High Energy X-ray Diffraction (HEXRD) and Small-Angle X-ray Scattering (SAXS) during fatiguing of steel in hydrogen. HEXRD measurements probe strain and dislocation density; SAXS measurements probe nano-pore generation and coalescence. We will discuss the differences in damage modes between steels fatigued in air and in hydrogen and the role these difference play in lifetime predictions.

36 MATERIALS SCIENCE↗