Search NASA⌕ Search

SEARCH · Search NASA

Results for “electron backscattered diffraction”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 109 records · Page 6

Dynamic recrystallization in friction surfaced austenitic stainless steel coatings

Friction surfacing involves complex thermo-mechanical phenomena. In this study, the nature of dynamic recrystallization in friction surfaced austenitic stainless steel AISI 316L coatings was investigated using electron backscattered diffraction and transmission electron microscopy. The results show that the alloy 316L undergoes discontinuous dynamic recrystallization under conditions of moderate Zener-Hollomon parameter during friction surfacing. - Highlights: Black-Right-Pointing-Pointer Dynamic recrystallization in alloy 316L friction surfaced coatings is examined. Black-Right-Pointing-Pointer Friction surfacing leads to discontinuous dynamic recrystallization in alloy 316L. Black-Right-Pointing-Pointer Strain rates in friction surfacing exceed 400 s{sup -1}. Black-Right-Pointing-Pointer Estimated grain size matches well with experimental observations in 316L coatings.

36 MATERIALS SCIENCE↗

Importance of Martensite Spatial Distribution at Large Volume Fractions in Imparting Ductility in High-Strength Dual-Phase Steel

Controlled austenite decomposition in a cold-rolled steel was carried out in a hot-dip process simulator with different inter-critical annealing process parameters to produce dual-phase steel consisting of martensite phase fraction above 50%. The evolving microstructure was characterized by using scanning electron microscope and electron backscattered diffraction techniques. Macro- and micro-texture was characterized by using x-ray diffraction and electron backscattered diffraction techniques, respectively. Uniaxial tensile deformation showed a very good combination of ultra-high strength above 900 MPa with uniform elongation of above 7%. An anomalous increase in ductility was observed for steel with high martensite volume fraction of 62.2% compared to that of lower fraction of 52.3%, indicating the influence of size and spatial distribution arrangement of ferrite and martensite phases. The enhancement in the ductility with high strength was attributed to the improved plastic deformability of hard fine martensite phase along with fine ferrite surrounding it. The nature of micro- and macro-texture was also found to affect strain partitioning compatibility between ferrite and martensite in this study.

36 MATERIALS SCIENCE↗

Characterization of the carbides and the martensite phase in powder-metallurgy high-speed steel

A microstructural characterization of the powder-metallurgy high-speed-steel S390 Microclean was performed based on an elemental distribution of the carbide phase as well as crystallographic analyses. The results showed that there were two types of carbides present: vanadium-rich carbides, which were not chemically homogeneous and exhibited a tungsten-enriched or tungsten-depleted central area; and chemically homogeneous tungsten-rich M{sub 6}C-type carbides. Despite the possibility of chemical inhomogenities, the crystallographic orientation of each of the carbides was shown to be uniform. Using electron backscatter diffraction the vanadium-rich carbides were determined to be either cubic VC or hexagonal V{sub 6}C{sub 5}, while the tungsten-rich carbides were M{sub 6}C. The electron backscatter diffraction results were also verified using X-ray diffraction. Several electron backscatter diffraction pattern maps were acquired in order to define the fraction of each carbide phase as well as the amount of martensite phase. The fraction of martensite was estimated using band-contrast images, while the fraction of carbides was calculated using the crystallographic data.

36 MATERIALS SCIENCE↗

Intrinsic magnetic properties of L1{sub 0} FeNi obtained from meteorite NWA 6259

FeNi having the tetragonal L1{sub 0} crystal structure is a promising new rare-earth-free permanent magnet material. Laboratory synthesis is challenging, however, tetragonal L1{sub 0} FeNi—the mineral “tetrataenite”—has been characterized using specimens found in nickel-iron meteorites. Most notably, the meteorite NWA 6259 recovered from Northwest Africa is 95 vol. % tetrataenite with a composition of 43 at. % Ni. Hysteresis loops were measured as a function of sample orientation on a specimen cut from NWA 6259 in order to rigorously deduce the intrinsic hard magnetic properties of its L1{sub 0} phase. Electron backscatter diffraction showed that NWA 6259 is strongly textured, containing L1{sub 0} grains oriented along any one of the three equivalent cubic directions of the parent fcc structure. The magnetic structure was modeled as a superposition of the three orthonormal uniaxial variants. By simultaneously fitting first-quadrant magnetization data for 13 different orientations of the sample with respect to the applied field direction, the intrinsic magnetic properties were estimated to be saturation magnetization 4πM{sub s} = 14.7 kG and anisotropy field H{sub a} = 14.4 kOe. The anisotropy constant K = 0.84 MJ/m{sup 3} is somewhat smaller than the value K = 1.3 MJ/m{sup 3} obtained by earlier researchers from nominally equiatomic FeNi prepared by neutron irradiation accompanied by annealing in a magnetic field, suggesting that higher Ni content (fewer Fe antisite defects) may improve the anisotropy. The fit also indicated that NWA 6259 contains one dominant variant (62% by volume), the remainder of the sample being a second variant, and the third variant being absent altogether.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

In-situ observation of recrystallization in an AlMgScZr alloy using confocal laser scanning microscopy

In this work we present a novel in-situ approach to study the recrystallization behavior of age hardening alloys. We use confocal laser scanning microscopy (CLSM) at 400 °C to investigate the static recrystallization of an AlMg4Sc0.4Zr0.12 alloy in-situ. The results are combined with electron backscatter diffraction (EBSD) and transmission electron microscopy (TEM) analyses. It was found that CLSM is a powerful tool to visualize both the local initiation and temporal sequence of recrystallization. After fast nucleation and initial growth, the grain growth rate decreases and the grain boundary migration stops after some minutes due to Zener pinning from Al{sub 3}(Sc,Zr) precipitates produced during the heat treatment. EBSD and TEM analyses confirm both the boundary movements and the particle-boundary interactions. - Highlights: • First time that CLSM is used to study recrystallization in-situ. • The start and end of recrystallization can be directly observed. • The procedure is easy to apply and requires only simple data interpretation. • In-situ observations on the surface correlate to modifications inside the bulk. • In-situ observations correlate to EBSD and EFTEM analyses.

36 MATERIALS SCIENCE↗

Mechanisms of ultrafine-grained austenite formation under different isochronal conditions in a cold-rolled metastable stainless steel

The primary objective of this work is to obtain fundamental insights on phase transformations, with focus on the reaustenitization process (α′→γ transformation), of a cold-rolled (CR) semi-austenitic metastable stainless steel upon different isochronal conditions (0.1, 1, 10 and 100 °C/s). For this purpose, an exhaustive microstructural characterization has been performed by using complementary experimental such as scanning and transmission electron microscopy (SEM and TEM), electron backscattered diffraction (EBSD), electron probe microanalysis (EPMA), micro-hardness Vickers and magnetization measurements. It has been detected that all microstructural changes shift to higher temperatures as the heating rate increases. The reaustenitization occurs in two-steps for all heating rates, which is attributed to the chemical banding present in the CR state. The α′→γ transformation is controlled by the migration of substitutional alloying elements across the austenite/martensite (γ/α′) interface, which finally leads to ultrafine-grained reaustenitized microstructures (440–280 nm). The morphology of the martensite phase in the CR state has been found to be the responsible for such a grain refinement, along with the presence of χ-phase and nanometric Ni{sub 3}(Ti,Al) precipitates that pin the austenite grain growth, especially upon slowly heating at 0.1 °C/s. - Highlights: •Ultrafine-grained austenite structures are obtained isochronally at 0.1–100 °C/s •The α′→γ transformation occurs in two steps due to the initial chemical banding •A diffusional mechanism governs the α′→γ transformation for all heating rates •The dislocation-cell-type of martensite promotes a diffusional mechanism •Precipitates located at α′/γ interfaces hinder the austenite growth.

36 MATERIALS SCIENCE↗

Effect of Local Postweld Heat Treatments on Metal Inert Gas-Welded A7N01S-T5 Joints

T6, T7, and retrogression and reaging (RRA) postweld heat treatments (PWHTs) were redefined and deployed to restore MIG-welded A7N01-T5 aluminum alloy joints in train-body structures using an inductive heating device. After the PWHT, the microstructures and mechanical properties of the joints were studied by x-ray diffraction (XRD), electron backscattered diffraction (EBSD), and scanning electron microscopy (SEM). The results showed that the hardness and strength of the joints were improved by the T6 treatment, and the tensile strength of the joints reached 87.39% of the base metal. However, an improvement in the corrosion resistance was not observed. The T7-treated joints enhanced the toughness of the welded joints and improved their corrosion resistance. The RRA-treated joints improved the toughness and corrosion resistance and increased the strength and hardness. The RRA treatment had a more comprehensive effect on the improvement of the welded joint structure and performance and is more suitable for postweld heat treatment of the aluminum alloy welded joints in the body of high-speed trains.

36 MATERIALS SCIENCE↗

Structure of bismuth films obtained using an array of identically oriented single-crystal bismuth islands preliminarily grown on a substrate

An array of identically oriented single-crystal bismuth islands formed on mica plates is used as a substrate to improve the structure of bismuth thin films grown by vacuum thermal evaporation. The array of islands is formed by the chemical etching of a single-crystal bismuth film 1 μm thick grown by floating-zone recrystallization under a coating. The structure of the obtained films is studied by X-ray diffraction, atomicforce microscopy, and electron backscatter diffraction scanning electron microscopy.

36 MATERIALS SCIENCE↗

Phase identification in boron-containing powder metallurgy steel using EBSD in combination with EPMA

Boron (B) is extensively used to induce liquid phase sintering (LPS) in powder metallurgy (PM) steels and thereby increase the densification. The alloying elements in B-containing PM steels affect the boride phase, stability of the boride, the temperature of liquid formation, and the progress of LPS. However, the boride phase has not been systematically identified yet. The main objective of this study was to clarify the influences of alloying elements, including C, Cr, and Ni, on the boride phases using electron backscatter diffraction (EBSD) in combination with electron probe microanalysis (EPMA). Network structures consisting of ferrite, Fe{sub 2}B boride, and Fe{sub 3}C carbide were extensively observed in the Fe–0.4B–0.5C steel. The portions of Fe{sub 2}B were sufficiently larger than those of Fe{sub 3}C, and Fe{sub 3}C was mostly distributed at the interfaces between ferrite and Fe{sub 2}B. Adding 1.5 wt.% Cr or 1.8 wt.% Ni to Fe–0.4B–0.5C steel completely changes the Fe{sub 2}B and Fe{sub 3}C phases to a M{sub 3}(B,C) phase, where M represents the metallic elements, including Fe, Cr, Mo, and Ni. Furthermore, Cr, Mo, B, and C atoms tend to concentrate on the M{sub 3}(B,C) phase, but Ni atoms do not. - Highlights: • Network structures consisting of ferrite, Fe{sub 2}B boride, and Fe{sub 3}C carbide were extensively observed in the Fe–0.4B–0.5C steel. • Adding 1.5 wt.% Cr or 1.8 wt.% Ni to Fe–0.4B–0.5C steel completely transforms the Fe{sub 2}B and Fe{sub 3}C phases to a M{sub 3}(B,C) phase. • Cr, Mo, B, and C atoms tend to concentrate on the M{sub 3}(B,C) phase, but Ni atoms do not.

36 MATERIALS SCIENCE↗

Crystal structure and chemistry of tricadmium digermanium tetraarsenide, Cd3Ge2As4

A cadmium germanium arsenide compound, i.e., Cd3Ge2As4, was synthesized using a double-containment fused quartz ampoule method within a rocking furnace and a melt-quench technique. The crystal structure was determined from single-crystal X-ray diffraction (XRD), scanning and transmission electron microscopies (i.e., SEM, STEM, TEM), and selected area diffraction (SAD) and confirmed with electron backscatter diffraction (EBSD). The chemistry was verified with electron energy loss spectroscopy (EELS).

Cd3Ge2As4, chalcopyrite↗

The Measurement of Grain Size by Electron Beam Backscattered Diffraction

The method of electron back-scatter diffraction provides an analytic means to identify crystalline phase and the grain size of structural materials. The need to utilize imaging parameters consistent with revealing the contributing microstructural scale is often overlooked through packaged imaging scripts. It is shown that imaging parameters consistent with a post processing assessment of low misorientation angles between boundaries are achievable as using pixel sizes on the order of 10 1 nm.

36 MATERIALS SCIENCE↗

Microstructures of chemical vapor deposited high-purity tungsten achieved by two different precursors

Highlights: • CVD tungsten used as electron emitters of thermionic fuel elements was investigated. • Microstructures were characterized with metallography analysis. • The preferred orientation was determined with XRD and EBSD. • The surface morphology was observed with SEM and WLI. • Tungsten via thermolysis of WCl{sub 6} is better for thermionic fuel elements. - Abstract: Chemical vapor deposited (CVD) high-purity tungsten can be manufactured as electron emitters in thermionic fuel elements. Exposed surface planes of the emitter emit electrons and affect the efficiency and load capacity of the thermionic fuel element. In order to determine the electron emission planes of the emitter, the metallurgic structures, the preferred orientation and the as-deposited surface morphology of CVD tungsten have been investigated. In this work, high-purity (over 99.99%) tungsten was achieved by two different precursors: hydrogen reduction of tungsten hexafluoride (WF{sub 6}) and thermolysis of tungsten hexachloride (WCl{sub 6}). The microstructures of CVD tungsten were characterized by metallography analysis, X-ray diffraction (XRD), electron backscattered diffraction (EBSD), and white light interference (WLI). Tungsten fabricated by hydrogen reduction of WF{sub 6} and thermolysis of WCl{sub 6} has <100>-preferred columnar microstructures. However, the latter exhibits larger columnar grains and preferred <100> less. The preferred orientation is caused by the higher growth rate of the <100> orientation and competition between the <100> orientations of different grains. The as-deposited surface consists of tiny pyramids, with <100> axis and {111} side faces. In contrast to tungsten produced by hydrogen reduction of WF{sub 6}, the pyramid on tungsten synthesized via thermolysis of WCl{sub 6} contains small {110} facets on the four edges. Therefore, tungsten made via thermolysis of WCl{sub 6} is a better candidate for thermionic fuel elements, because the higher work function of {110} planes enables better output efficiency.

36 MATERIALS SCIENCE↗

Study of the scale formed on super 304H boiler tube steels after long-term steam oxidation at high temperatures

Highlights: • Steam oxidation tests were performed on the conventional and shot-peened Super304H boiler tube. • A continuous amorphous SiO{sub 2} layer separated the metal from the scale in shot-peened specimen. • The SiO{sub 2} layer enhanced the formation of dense Cr{sub 2}O{sub 3} and FeCr{sub 2}O{sub 4} layers. • The scale on shot-peened specimens is stable upon steam temperature and time increase. Steam oxidation of a Super 304H boiler tube was performed at steam temperatures of 650 °C and 700 °C for time durations up to 5000 h. The oxidation scale outcomes which formed on as-received untreated and shot-peened (SP) tubes were studied using X-ray diffraction (XRD), scanning electron microscopy (SEM), electron backscatter diffraction (EBSD), and transmission electron microscopy (TEM). γ-Grain nanocrystallization on the surface of the SP specimen generated an abundant fraction of grain boundary that guaranteed the formation of a continuous amorphous SiO{sub 2} layer at the metal-scale interface that enhanced the formation of dense Cr{sub 2}O{sub 3} and FeCr{sub 2}O{sub 4} in the scale. Scale breakaway along defects in the outer layer of the scale was accelerated by the steam temperature in the untreated specimens, whereas the scale that formed on the SP specimens appeared to be stable.

36 MATERIALS SCIENCE↗

Growth behavior and orientation relationships in AISI 304 stainless steel during directional solidification

Highlights: • N–W orientation relationship between the lathy ferrite and austenite was determined. • {103} and <001> of ferrite are parallel to the sample surface and heat flow direction. • Lathy ferrite is elongated in [001], [011], and [123] directions during solidification. - Abstract: The formation mechanism of lathy ferrite in AISI 304 stainless steel during directional solidification was discussed in terms of the orientation relationship between ferrite and austenite. Experimental results show that most of the ferrite laths are arranged parallel and a few ferrite laths with perpendicular morphology can also be observed in the solidified microstructure. Selected-area diffraction patterns by transmission electron microscopy (TEM) and pole figures by electron backscatter diffraction (EBSD) show that Nishiyama–Wassermann orientation relationship between the lathy ferrite and austenite exists in the solidified microstructure. Based on the pole figures of the ferrite, it was found that (103) and [001] of the lathy ferrite are parallel to the sample surface and heat flow direction, respectively, during directional solidification. The elongated directions of the lathy ferrite are found to be [001], [011], and [123], which means that the lathy ferrite grows without preferential direction during directional solidification.

36 MATERIALS SCIENCE↗

Giant secondary grain growth in Cu films on sapphire

Single crystal metal films on insulating substrates are attractive for microelectronics and other applications, but they are difficult to achieve on macroscopic length scales. The conventional approach to obtaining such films is epitaxial growth at high temperature using slow deposition in ultrahigh vacuum conditions. Here we describe a different approach that is both simpler to implement and produces superior results: sputter deposition at modest temperatures followed by annealing to induce secondary grain growth. We show that polycrystalline as-deposited Cu on α-Al{sub 2}O{sub 3}(0001) can be transformed into Cu(111) with centimeter-sized grains. Employing optical microscopy, x-ray diffraction, and electron backscatter diffraction to characterize the films before and after annealing, we find a particular as-deposited grain structure that promotes the growth of giant grains upon annealing. To demonstrate one potential application of such films, we grow graphene by chemical vapor deposition on wafers of annealed Cu and obtain epitaxial graphene grains of 0.2 mm diameter.

36 MATERIALS SCIENCE↗

Critical differences between electron beam melted and selective laser melted Ti-6Al-4 V

Effective optimization of the production of Ti-6Al-4 V using AM requires a fundamental understanding of the relative importance of different microstructural features to the deformation and failure mechanisms, particularly features that vary between production methods. In this study, the tensile response and deformation mechanisms of electron beam melted (EBM) AM Ti-6Al-4 V material loaded in different orientations and produced using various powder sizes were compared to those of selective laser melted (SLM) AM Ti-6Al-4 V material. The density and morphology of pores, phase fractions, prior-β grains, and defect microstructures were evaluated using scanning electron microscopy, X-ray computed tomography, electron backscatter diffraction, and transmission electron microscopy before and after deformation. The results were used to evaluate the relative importance of each feature on strengthening, deformation, and failure initiation mechanisms. Results focused primarily on coarse-powder EBM materials indicated that phase distribution and defect density were most influential for determining material yield strength as well as maximum possible strain to failure. Porosity was lower overall in EBM Ti-6Al-4 V than in SLM, allowing for occasional increases in part strain to failure, but remained a limiting factor determining overall part ductility.

36 MATERIALS SCIENCE↗

A high-performance β-solidifying TiAl alloy sheet: Multi-type lamellar microstructure and phase transformation

Highlights: • A high-performance β-solidifying TiAl alloy sheet is fabricated via hot rolling. • Fine multi-type β/γ and α{sub 2}/γ lamellar structures are formed during hot-rolling. • These lamellar structures are induced by the β → γ and α + γ → α{sub 2} + γ/γ{sub T} transformations. • The nano-scaled antiphase domain is induced by α → α{sub 2} disorder-order transformation. • The fine multi-type lamellar structures contribute to the strength enhancement. - Abstract: TiAl alloys are widely used in the aerospace industry and, hence, a thorough understanding of the corresponding microstructural evolution is crucial for providing insight into the fabrication of high-performance TiAl alloy sheets. In this study, a high-performance β-solidifying Ti-43Al-9V-0.2Y alloy sheet with multi-type lamellar structures was obtained via hot-rolling at an initial rolling temperature of 1260 °C. Owing to the temperature drop and reheat associated with multi-pass rolling, relatively fine irregular β/γ and regular α{sub 2}/γ lamellar microstructures (average size: ~25 μm) with nano-scaled antiphase domains (APDs) were generated by the β → γ and α + γ → α{sub 2} + γ/γ{sub T} phase transformations. These two lamellar structures have different formation mechanisms. The results of electron backscatter diffraction and transmission electron microscopy revealed that the nucleation and growth of (i) β/γ and (ii) α{sub 2}/γ lamellar structures are induced mainly by (i) stress and (ii) a combination of the stress and temperature drop during hot-rolling, respectively. Thin γ{sub T} precipitates from the α/α{sub 2} or γ phases. This precipitation is induced by the higher stress and lower temperature associated with the later stage (compared with those occurring in the initial stages) of hot-rolling. Moreover, compared with the corresponding as-forged alloy, the as-rolled TiAl alloy sheet exhibits better performance at both room and elevated temperatures. The improvement in the tensile properties is attributed to the duplex microstructure consisting of fine multi-type lamellar structures with nano-scaled APDs. The interface boundaries of β/γ, α{sub 2}/γ and APDs, which are effective in retarding dislocation motion, contribute mainly to strengthening of the alloy sheet.

36 MATERIALS SCIENCE↗

Evolution of the substructure of a novel 12% Cr steel under creep conditions

In this work we study the microstruture evolution of a newly developed 12% Cr martensitic/ferritic steel in as-received condition and after creep at 650 °C under 130 MPa and 80 MPa. The microstructure is described as consisting of mobile dislocations, dipole dislocations, boundary dislocations, precipitates, lath boundaries, block boundaries, packet boundaries and prior austenitic grain boundaries. The material is characterized employing light optical microscopy (LOM), scanning electron microscopy (SEM), transmission electron microscopy (TEM), X-ray diffraction (XRD) and electron backscatter diffraction (EBSD). TEM is used to characterize the dislocations (mobile + dipole) inside the subgrains and XRD measurements are used to the characterize mobile dislocations. Based on the subgrain boundary misorientations obtained from EBSD measurements, the boundary dislocation density is estimated. The total dislocation density is estimated for the as-received and crept conditions adding the mobile, boundary and dipole dislocation densities. Additionally, the subgrain size is estimated from the EBSD measurements. In this publication we propose the use of three characterization techniques TEM, XRD and EBSD as necessary to characterize all type of dislocations and quantify the total dislocation densty in martensitic/ferritic steels. - Highlights: • Creep properties of a novel 12% Cr steel alloyed with Ta • Experimental characterization of different types of dislocations: mobile, dipole and boundary • Characterization and interpretation of the substructure evolution using unique combination of TEM, XRD and EBSD.

36 MATERIALS SCIENCE↗