In situ diode laser cladding of erosion resistant alloys for repair of light water reactor systems and components
Explore the source record for details and available documents.
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Explore the source record for details and available documents.
A probabilistic assessment was performed on pinching failure of PWR SNF rod cladding under accidental SNF cask transport conditions. a set of 3,000 rod pinching scenarios was analyzed, with different geometrical, material, and loading parameters, using a Latin Hypercube Sampling (LHS). The investigated accidents include train derailments leading to cask collisions or cask drops. Pinching failure was related to cladding offset strain, defined as the plastic deformation interval in radial cladding direction normalized with respect to the outer cladding diameter. Finite element (FE) models were used to compute SNF rod deformations and the offset strain demand OSD in each of the assessed pinching scenarios. The numerical models account for the contribution of the degraded fuel pellets to rod pinching stiffness. The offset strain capacity OSC was computed using regression and interpolation models based on ring compression (RCT) test results, and account for hydride-related effects on cladding ductility. The results show a low probability of pinching failure. Hydride-related cladding embrittlement affects the structural integrity of PWR SNF rods after long-term dry storage of up to 300 years. Radial hydride patterns or large amounts of circumferentially oriented hydrides reduce the cladding ductile deformation capability when pinched at low material temperatures. The probability of hydride-related pinching failure of PWR cladding is estimated after long-term dry storage to address: How do PWR SNF rod conditions like hydrogen content, vacuum drying peak cladding hoop stress σ{sub θ}, and cladding material temperature affect cladding ductility? Is hydride-related cladding embrittlement a material degradation mechanism that affects the structural integrity of PWR SNF rods under pinching loading? What are the controlling parameters for deformation demands in PWR SNF rods under pinching loading? Is the pinching load amplitude an important parameter that controls the probability of pinching failure? How do parameters like pellet-cladding gap or fuel pellet degradation affect the pinching loading capacity of PWR SNF rods? Statistical modelling of PWR SNF rod conditions in U.S. inventory: A pseudo rod database was generated based on EIA database. Analysis of train accident scenarios: a probability density function (pdf) of a pinching load distribution P{sub 9m} of a 9-m cask drop is linearly scaled to generate a more representative: distribution P{sub AS}. The new distribution considers train collision velocities, cask drops for on- and off-bridge accidents, and cask impact orientation. LHS generates 3,000 rod pinching scenarios based on nine independent geometrical, material, and loading parameters. Probabilistic FE Analysis: The LHS realizations are used to generate 3,000 FE models. The FE analysis is conducted for P{sub 9m}, and P{sub AS}. The workflow is automatized. The OSC is computed with regression and interpolation models, as a function of the hydrogen content C{sub H}, vacuum drying peak σ{sub θ}, and SNF temperature T{sub FR}: The regression data was obtained in RCTs on PWR cladding. The OSD is derived from the cladding deformations in the FE models. Cladding failure was identified via a comparison of OSC and OSD. A 300 and a 30 years-of-dry-storage duration is investigated: The dry-storage period affects the expected SNF temperature and consequently, the OSC and the OSD. The material temperature LHS population is adapted to account for a SNF temperature variation. The probability of hydride-related, ductile cladding failure during a severe transportation accident is not significantly affected by the pinching load amplitude: The probability is slightly reduced from a range of less than 0.0333% to 0.1667% for P{sub 9m}, to a range of less than 0.0333% to 0.1333% for P{sub AS}, depending on the vacuum drying peak cladding hoop stress modelling assumptions. Further, the SNF dry-storage duration does not significantly affect the probability of ductile pinching failure. Based on available train accidents data, the pinching failure probability for a 5,000 km long transportation route ranges from less than 1.62 E-7 to a value of 6.47 E-7, depending on the vacuum drying peak cladding hoop stress modelling assumptions. The pinching load amplitude is not a controlling parameter for the probability of ductile cladding pinching failure, and does not control the cladding deformations once pellet-cladding contact is established, The pellet-cladding gap width, however, plays a key role. Fuel pellet degradation only affects the deformation capacity, if the pellet stiffness is significantly reduced (more than 90%). Only highly embrittled cladding is likely to fail. The deformation demands on the cladding under pinching loading are small.
Current structural alloys, code certified for the MSRs temperature ranges, contain high levels of chromium, making them highly susceptible to molten halide salt corrosion. One potential solution to circumvent the need for code certification of novel alloys, which is expensive and time consuming, is to design claddings that will protect the underlying code certified materials from corrosion damage during operation. In this work, we examined the corrosion of Ni and Cu electroplated, Ni and CuNi weld overlay, Mo-laser clad, and carburized claddings on SS316H for use in molten salt reactor environments. After characterization of the cladded materials (Task 1), static corrosion tests were used to assess corrosion resistance of the claddings in typical molten fluoride salts (Task 2). The corrosion tests were performed in molten FLiNaK at 700°C up to 1000 hours. Pre- and post-corrosion Scanning Electron Microscopy (SEM), energy-dispersive-spectroscopy (EDS), Transmission Electron Microscopy (TEM), X-ray Diffraction (XRD) and glow-discharge-optical-emission-spectroscopy (GDOES) were performed on cladding cross-sections and surfaces to evaluate degradation. The Cu and Ni electroplated samples, as well as the carburized samples, showed excellent corrosion resistance relative to the bare SS316H. To assess high temperature cladding stability, ageing experiments were performed at temperatures up to 900 C in inert atmosphere for the electroplated and carburized samples and a diffusion model was developed to predict long term cladding behavior (Task 3). It was found that the Cu cladding was basically insensitive to the high temperature ageing, except for small secondary phases forming at the interface. On the other hand, the Ni electroplated cladding experienced significant interdiffusion. Nevertheless, the gain in corrosion resistance for a 100μm Ni electroplated cladding is phenomenal, with more than 50% reduction in chromium dissolution from the substrate material for the first 15 years of salt exposure at 700°C. To assess radiation resistance and phase stability, high-temperature 4MeV Ni heavy ion irradiation was performed across the cladding/substrate interface up to 50 displacement-per-atom (DPA) at 500°C and 700°C to assess the phase stability and irradiation behaviors of the electroplated systems (Task 4). The Ni and Cu electroplated systems did not experience void swelling at the contrary to the SS316H substrate due to their nanocrystalline nature. Some level of recrystallization was observed in the cladding, as well as radiation induced segregation and enhanced diffusion. The interface acted as a potent sink for point defects with the presence of a void denuded zone. The mechanical properties of the claddings were assessed using thermal shock, micro-indentation, nano-indentation, and four-point bend testing experiments (Task 5). These experiments were performed on the claddings in as-received, corroded, irradiated, and thermally aged states to determine the effects of typical molten salt reactor environments on cladding integrity. No significant mass loss was observed after repeated thermal shocks. While the electroplated samples softened after high-temperature ageing, irradiation hardening compensate this effect, such that there is little different with the as-received materials. The results of these experiments suggest that the electroplated (copper/nickel) show the greatest promise for application in molten salt reactor development. These claddings prevented any chromium dissolution from occurring during the static corrosion experiments. Additionally, they demonstrated favorable properties for high temperature diffusion, phase stability, interfacial mechanical properties, and irradiation resistance. Weld-overlay cladding are also of great interest and could reach properties similar to the electroplated samples upon optimization (especially with multiple weld passes). The carburized SS316H showed excellent behavior as well, but more work needs to be done to assess their long-term stability. Finally, the Mo-laser clad system was not pursued further due to the manufacturing challenges. It is also worth noting that the Ni cladding systems should behave relatively well in terms of weldability since the Ni-weld overlay microstructure and associated corrosion rate are sound. While the NiCu weld-overlay has even lower corrosion rates than the Ni-weld overlay, more studies on welding of Cu-electroplated systems are necessary since Cu clusters are known to embrittle steels.
The Westinghouse Electric Company LLC (Westinghouse) accident tolerant fuel (ATF) program funded by Westinghouse and the US Department of Energy (DOE) utilized chromium (Cr) coated zirconium alloy cladding with doped UO 2 (ADOPT(TM)) and uranium silicide (U 3 Si 2 ) high density/high thermal conductivity fuel for its lead test rod (LTR) program with irradiation beginning in 2019. ADOPT is a Cr 2 O 3 +Al 2 O 3 doped UO 2 pellet with increased oxidation resistance and density, and increased resistance to fission gas release. Due to the issues with U 3 Si 2 fuel reaction in pressurized water reactor (PWR) environments, uranium nitride (U 15 N) has been substituted for U 3 Si 2 as a long-term fuel option. Cr coated cladding with ADOPT fuel is the near-term Westinghouse EnCore fuel product. The long-term EnCore ® fuel product is SiGA ® SiC/SiC composite cladding with high density/high thermal conductivity UN fuel. In 2020, the higher burnup and higher enriched and (HBHE) program was integrated into the ATF program. The objective of this expanded program is to extend ATF burnups to at least 75 MWd/kgU to economically facilitate 24-month cycles in PWRs. The ATF program now includes ADOPT fuel with enrichments >5% 235 U. Over the past several years, Westinghouse has tested the Cr coated zirconium (Zr) and silicon carbide (SiC) claddings in Westinghouse Churchill autoclaves and the Massachusetts Institute of Technology (MIT) reactor. Additionally, the Cr coated cladding has been tested in the Advanced Test Reactor (ATR) at Idaho National Laboratory (INL) and in LTR programs at the Doel 4 and Bryon 2 commercial reactors. High temperature tests at the state-of-the-art Westinghouse facilities in Churchill, PA and at Karlsruhe Institute of Technology (KIT) have been carried out to determine the time and temperature limits for the Cr coated zirconium claddings. These tests indicate that Cr coated Zr cladding can take temperatures up to about 1500°C for short periods of time without becoming totally oxidized. The main issue is the formation of the Cr-Zr eutectic at 1333°C resulting in the migration of this eutectic inward with the formation of ZrCr 2 which rapidly oxidizes to ZrO 2 on the outside of the tube. The Cr coated Zr cladding also delays the bursting of the tube, reduces the burst area, and reduces hydriding and embrittlement of the Zr which is a major benefit for reducing fuel fragmentation, redistribution, and dispersal (FFRD), the major licensing issue faced by HBHE. The manufacturing parameters for the SiC have been found to have a significant effect on the corrosion rate of the SiC in light water reactor (LWR) conditions and significant improvements have been made in the yield, quality, and oxidation resistance of the SiC cladding by identifying and tightening manufacturing process parameters. Current autoclave results for SiC composite claddings indicate that a corrosion rate of fewer than 2 micrometers per year can be achieved which meets corrosion requirements under normal operating conditions. High temperature steam oxidation tests at the state-of-the-art Westinghouse facilities in Churchill, PA and at Karlsruhe Institute of Technology (KIT) have been carried and determined that SiC cladding can withstand temperatures up to about 1800°C to 1900°C before excessive corrosion reactions begin, and that the SiC will not balloon and burst. ADOPT fuel pellets were incorporated into the Westinghouse ATF program because of their increased density and oxidation resistance. A topical report supporting the use of ADOPT pellets has been submitted to the NRC and will be approved shortly. ADOPT pellets have been a product in Europe for over 15 years. The additives work to make larger grain sizes which appear to reduce fission gas release during transients as well as increase the density of the pellet. Fuel rod and assembly design in preparation for the lead test rod (LTR) and lead test assembly (LTA) programs is underway as well as licensing efforts with the Nuclear Regulatory Commission (NRC). Finally, accident analyses coupled with economic evaluations for both operating savings as well as fuel savings have been initiated. Modular Accident Analysis Program 5 (MAAP5) calculations indicate that both Cr coated cladding and SiC composite cladding can increase the time to fuel rod loss of geometry for up to two hours longer than current Zr based cladding in a station blackout scenario. This additional time is due to the much higher oxidation resistance of the SiC and Cr coated cladding. These two hours can be used to implement additional response options instituted through the Diverse and Flexible Mitigation Capability (FLEX) program by reactor operators. Both ATF cladding options also reduce hydrogen production which dramatically reduces primary system and containment pressure and the risk of fission product release beyond containment in the unlikely event of an accident. The lower pressure in the system allows more time to feed cooling water to the core, resulting in the avoidance of fuel melting. The coping time is extended indefinitely if the modest water flow provided by FLEX continues. Experimental work on methods to rapidly fabricate SiC composite structures with high density and reduce the fabrication price of SiC fibers while maintaining a high level of performance is needed. Methods for mitigating or stopping the Cr-Zr eutectic are also needed to further improve the oxidation resistance of Cr coated Zr. Minimal (<1%) swelling of U 3 Si 2 and subsequent fission gas release has been demonstrated up to 20 MWd/kgU. Irradiation experiments with U 3 Si 2 fuel in ATR to determine these properties at 40 MWd/kgU were completed but post irradiation examinations were not done since U 3 Si 2 has been replaced by UN. UN has three issues that are being addressed. The first is increasing the oxidation resistance so that there is not excessive reaction up to ~1500°C. While UN increases the pellet density and additives to the UN postponed the temperature at which rapid oxidation occurred by ~100°C to 200°C, this is not enough, and pellet coating options are now being pursued. The second is developing a method to manufacture that does not require the multi-step process of UF 6 to UO 2 to UC to UN. Efforts are underway looking at UF 6 to UN 2 to UN and UF 6 to UF 4 to UN 2 to UN reactions. Finally, an economically acceptable process for potentially enriching the 15 N content of the nitrogen used to make UN to >95% 15N was identified though not experimentally validated. In addition to the work supported by the DOE, research and testing activities are being carried on in a world-wide effort funded by many countries such as Sweden, United Kingdom, Belgium, Netherlands, Spain, Germany, Japan, and France. This work is being facilitated through the Westinghouse led Collaboration for Advanced Research on Accident Tolerant Fuel (CARAT) program. Annual meetings were organized in 2018 and 2019 by Westinghouse as a venue for presentation of this work and to provide for the cross-fertilization of ideas among the many outstanding researchers in the ATF area. No meetings were held in 2020 and 2021 due to the COVID-19 related restrictions on traveling and gatherings. Since SiC, coated cladding, and high-density fuel options are not currently used in the nuclear industry; support from the government and industry members is needed to further the significant effort of setting new standards. The same is true for the Nuclear Regulatory Commission (NRC) which must review and approve the commercial use of these new fuels since all current regulations are oriented toward Zr/UO 2 fuel. Several meetings have been held with the NRC to generate a fast-track approach to licensing ATF using a combination of atomic modeling, in-rod sensors, and in-reactor testing. This approach was memorialized in an “Accelerated Fuel Qualification White Paper” prepared by the Accelerated Fuel Qualification Working Group lead by General Atomics.
The Westinghouse Electric Company LLC (Westinghouse) accident tolerant fuel (ATF) program funded by Westinghouse and the US Department of Energy (DOE) utilized chromium (Cr) coated zirconium alloy cladding with doped UO 2 (ADOPT(TM)) and uranium silicide (U 3 Si 2 ) high density/high thermal conductivity fuel for its lead test rod (LTR) program with irradiation beginning in 2019. ADOPT is a Cr 2 O 3 +Al 2 O 3 doped UO 2 pellet with increased oxidation resistance and density, and increased resistance to fission gas release. Due to the issues with U 3 Si 2 fuel reaction in pressurized water reactor (PWR) environments, uranium nitride (U 15 N) has been substituted for U 3 Si 2 as a long-term fuel option. Cr coated cladding with ADOPT fuel is the near-term Westinghouse EnCore ® fuel product. The long-term EnCore fuel product is SiGA ® SiC/SiC composite cladding with high density/high thermal conductivity UN fuel. In 2020, the higher burnup and higher enriched and (HBHE) program was integrated into the ATF program. The objective of this expanded program is to extend ATF burnups to at least 75 MWd/kgU to economically facilitate 24-month cycles in PWRs. The ATF program now includes ADOPT fuel with enrichments >5% 235 U. Over the past several years, Westinghouse has tested the Cr coated zirconium (Zr) and silicon carbide (SiC) claddings in Westinghouse Churchill autoclaves and the Massachusetts Institute of Technology (MIT) reactor. Additionally, the Cr coated cladding has been tested in the Advanced Test Reactor (ATR) at Idaho National Laboratory (INL) and in LTR programs at the Doel 4 and Bryon 2 commercial reactors. High temperature tests at the state-of-the-art Westinghouse facilities in Churchill, PA and at Karlsruhe Institute of Technology (KIT) have been carried out to determine the time and temperature limits for the Cr coated zirconium claddings. These tests indicate that Cr coated Zr cladding can take temperatures up to about 1500°C for short periods of time without becoming totally oxidized. The main issue is the formation of the Cr-Zr eutectic at 1333°C resulting in the migration of this eutectic inward with the formation of ZrCr 2 which rapidly oxidizes to ZrO 2 on the outside of the tube. The Cr coated Zr cladding also delays the bursting of the tube, reduces the burst area, and reduces hydriding and embrittlement of the Zr which is a major benefit for reducing fuel fragmentation, redistribution, and dispersal (FFRD), the major licensing issue faced by HBHE. The manufacturing parameters for the SiC have been found to have a significant effect on the corrosion rate of the SiC in light water reactor (LWR) conditions and significant improvements have been made in the yield, quality, and oxidation resistance of the SiC cladding by identifying and tightening manufacturing process parameters. Current autoclave results for SiC composite claddings indicate that a corrosion rate of fewer than 2 micrometers per year can be achieved which meets corrosion requirements under normal operating conditions. High temperature steam oxidation tests at the state-of-the-art Westinghouse facilities in Churchill, PA and at Karlsruhe Institute of Technology (KIT) have been carried and determined that SiC cladding can withstand temperatures up to about 1800°C to 1900°C before excessive corrosion reactions begin, and that the SiC will not balloon and burst. ADOPT fuel pellets were incorporated into the Westinghouse ATF program because of their increased density and oxidation resistance. A topical report supporting the use of ADOPT pellets has been submitted to the NRC and will be approved shortly. ADOPT pellets have been a product in Europe for over 15 years. The additives work to make larger grain sizes which appear to reduce fission gas release during transients as well as increase the density of the pellet. Fuel rod and assembly design in preparation for the lead test rod (LTR) and lead test assembly (LTA) programs is underway as well as licensing efforts with the Nuclear Regulatory Commission (NRC). Finally, accident analyses coupled with economic evaluations for both operating savings as well as fuel savings have been initiated. Modular Accident Analysis Program 5 (MAAP5) calculations indicate that both Cr coated cladding and SiC composite cladding can increase the time to fuel rod loss of geometry for up to two hours longer than current Zr based cladding in a station blackout scenario. This additional time is due to the much higher oxidation resistance of the SiC and Cr coated cladding. These two hours can be used to implement additional response options instituted through the Diverse and Flexible Mitigation Capability (FLEX) program by reactor operators. Both ATF cladding options also reduce hydrogen production which dramatically reduces primary system and containment pressure and the risk of fission product release beyond containment in the unlikely event of an accident. The lower pressure in the system allows more time to feed cooling water to the core, resulting in the avoidance of fuel melting. The coping time is extended indefinitely if the modest water flow provided by FLEX continues. Experimental work on methods to rapidly fabricate SiC composite structures with high density and reduce the fabrication price of SiC fibers while maintaining a high level of performance is needed. Methods for mitigating or stopping the Cr-Zr eutectic are also needed to further improve the oxidation resistance of Cr coated Zr. Minimal (<1%) swelling of U 3 Si 2 and subsequent fission gas release has been demonstrated up to 20 MWd/kgU. Irradiation experiments with U 3 Si 2 fuel in ATR to determine these properties at 40 MWd/kgU were completed but post irradiation examinations were not done since U 3 Si 2 has been replaced by UN. UN has three issues that are being addressed. The first is increasing the oxidation resistance so that there is not excessive reaction up to ~1500°C. While UN increases the pellet density and additives to the UN postponed the temperature at which rapid oxidation occurred by ~100°C to 200°C, this is not enough, and pellet coating options are now being pursued. The second is developing a method to manufacture that does not require the multi-step process of UF 6 to UO 2 to UC to UN. Efforts are underway looking at UF 6 to UN 2 to UN and UF 6 to UF 4 to UN 2 to UN reactions. Finally, an economically acceptable process for potentially enriching the 15 N content of the nitrogen used to make UN to >95% 15 N was identified though not experimentally validated. In addition to the work supported by the DOE, research and testing activities are being carried on in a world-wide effort funded by many countries such as Sweden, United Kingdom, Belgium, Netherlands, Spain, Germany, Japan, and France. This work is being facilitated through the Westinghouse led Collaboration for Advanced Research on Accident Tolerant Fuel (CARAT) program. Annual meetings were organized in 2018 and 2019 by Westinghouse as a venue for presentation of this work and to provide for the cross-fertilization of ideas among the many outstanding researchers in the ATF area. No meetings were held in 2020 and 2021 due to the COVID-19 related restrictions on traveling and gatherings. Since SiC, coated cladding, and high-density fuel options are not currently used in the nuclear industry; support from the government and industry members is needed to further the significant effort of setting new standards. The same is true for the Nuclear Regulatory Commission (NRC) which must review and approve the commercial use of these new fuels since all current regulations are oriented toward Zr/UO 2 fuel. Several meetings have been held with the NRC to generate a fast-track approach to licensing ATF using a combination of atomic modeling, in-rod sensors, and in-reactor testing. This approach was memorialized in an “Accelerated Fuel Qualification White Paper” prepared by the Accelerated Fuel Qualification Working Group lead by General Atomics.
Metallographic images generated in the Alpha Gamma Hot Cell Facility (AGHCF) have been used for quantitative and qualitative characterization of irradiated metallic fuel pins. Individual high-magnification images (micrographs) contained in AGHCF file folders and experimental notebooks are in the form of polaroid photographs labeled with AGHCF identification number, magnification, and surface condition (as-polished or etched). Low magnification composite images (photomosaics) are also available for fuel cross sections, for radial strips from the fuel center to the cladding outer diameter, and for circumferential strips of the cladding and outer fuel region. The individual images do not have scale bars. Only a few of the composite images contain scale bars. The purpose of this work is to describe and apply methods for checking the magnification (50X to 500X) of individual images and for determining the magnification (~25X to ~100X) of composite images. The metallographic images used to verify and/or determine magnification were generated during the 1989 to 1993 timeframe for cross sections of U-10Zr/HT9 fuel rods irradiated in EBR-II and for cross sections of irradiated U-10Zr/HT9 fuel-rod samples following elevated-temperature tests conducted in the out-of-pile AGHCF Fuel Behavior Test Apparatus (FBTA). Procedures are documented in the AGHCF Operations Manual for preparation of metallographic samples, for calibration verification, and for constructing composites from individual images. Calibration verification of magnification was performed at least semiannually. One standard used for calibration verification was a glass slide with vertical lines indicating distances of 1 mm, 0.1 mm and 0.01mm. Guidance is provided in the current work for determining magnification from images of the standard. In addition to the periodic calibration verification, consistency checks are recommended to verify the magnification of images taken between the routine calibration verifications. For cladding samples with or without significant fuel-cladding chemical interaction (FCCI), images taken at different magnifications (e.g., 150X and 200X) of the unaffected cladding thickness can be compared. This process is independent of changes in cladding thickness due to swelling and creep. For images taken at only one magnification of cladding regions with no FCCI, the cladding thickness determined from the images may be compared to the nominal as-built cladding thickness (15.0 ± 0.5 mils for examples used in current work)). This procedure works best for cladding that has not experienced significant swelling and/or creep (e.g., ≤2% circumferential strain at the cladding outer surface). Composite images were constructed by pasting together higher magnification images and photographing the composite to generate a negative from which the hard-copy photograph was developed. The primary purpose of the composite images was to identify interesting areas of the fuel and cladding for imaging at higher magnification. However, procedures are recommended in the current work for determining composite magnifications to allow quantitative characterization of the fuel. Composites are not recommended for determining cladding thickness or FCCI depth because magnifications are too low (generally ≤110X) and image contrast is low. Fuel cross-section composites were created by pasting together 50X or 75X images. The nominal magnification for the photographed fuel cross-section composites is 25.4X. A more precise magnification can be determined by comparing the average cladding outer diameter measured from the composite to the average cladding outer diameter measured by profilometry. Radial-strip composites were constructed by pasting together high-magnification (150X or 250X) images. The nominal magnification of radial-strip composites photographs is about 100X. A more precise method for determining the magnification of radial strips is to compare the cladding thick
Recent observations from projects sponsored under the DOE-Nuclear Energy Spent Fuel and Waste Disposition campaign show that residual free water, well above the 0.4 gm-moles that correspond to a 3 torr rebound pressure after a 30-minute hold following prototypic drying, may remain within SNF canisters used for long-term dry storage. Specifically, experimental observations in an Integrated Research Project showed subzero temperatures and a local pocket of frozen water in a mockup fuel assembly subjected to an industry practiced drying process. In gas sampling and analysis from the High Burnup (HBU) Demonstration project, using a fully loaded and dried SNF canister, indicated presence of 100 g of residual water had remained in the canister. The effects of residual water in terms of potential adverse impacts on the condition of the SNF and the canister internals during long-term dry storage has been rigorously evaluated to address inadvertent residual water contents. The impact of residual water on the fuel and canister internals, with a focus on the oxidation of the cladding and of postulated exposed (breached-clad) fuel, were evaluated using an integrated set of time-dependent environmental conditions with semi-empirical materials oxidation models. An 'integration model,' with coupled sub-models, developed and previously used by the Center for Nuclear Waste Regulatory Analysis (CNWRA), was applied and expanded with improved sub-models for water radiolysis, and for cladding and fuel oxidations. Cladding oxidation models for various alloys were developed using the rate constants for various cladding alloys in the dry storage temperature range. A burnup-dependent fuel oxidation model was developed; it accounted for inhibition effect of fission products on fuel oxidation rates. The potential for extension of the initial breach flaw (1 mm hole) was evaluated by two separate mechanics criteria. In the first case, a critical cladding strain criterion was used. In the second case, a critical stress intensity was used to evaluate stability of a planar axial flaw postulate. A failure condition exists when a sufficient amount of fuel oxidation (at the postulated breached-clad location) causes fuel pellet swelling to load the cladding to meet a mechanics criterion for flaw extension. The integration model's results provide the following insights. The radiolysis-generated oxygen is consumed with a partitioning between the cladding and the fuel. The extent of cladding oxidation is no more than 2 μm additional consumption of the cladding metal even with 10 moles of residual water, indicating that changes in cladding conditions due to water are expected to be negligible. The conditions for cladding failure (breach opening size extension) directly correlates with the extent of fuel oxidation. Fuel oxidation significant to extend the breach could occur even with 5.5 moles of residual water. The results indicate that fuel oxidation vis-a-vis cladding oxidation is more likely under a higher radiation field, i.e., when radiolytic decomposition of the residual water occurs in few years compared to several decades, and that the conditions to cause failure are increased with fuel and cladding temperatures approaching the peak storage temperature limit of 400 deg. C. (authors)
The Westinghouse Electric Company LLC (Westinghouse) accident tolerant fuel (ATF) program utilizes chromium (Cr) coated zirconium alloy cladding with uranium silicide (U 3 Si 2 ) high density/high thermal conductivity fuel for its lead test rod (LTR) program with irradiation beginning in 2019. The lead test assembly (LTA) program will use both SiC/SiC composites and Cr coated zirconium alloy claddings with the high density/high thermal conductivity U 3 Si 2 pellet which will begin in 2022. Over the past several years, Westinghouse has tested the Cr coated zirconium (Zr) and silicon carbide (SiC) claddings in autoclaves and in the Massachusetts Institute of Technology (MIT) reactor and the U 3 Si 2 pellets have been tested in the Advanced Test Reactor (ATR) at Idaho National Laboratory (INL). High temperature tests at the state-of-the-art Westinghouse facilities in Churchill, PA have been carried out to determine the time and temperature limits for the SiC and Cr coated zirconium claddings. Fuel rod and assembly design in preparation for the LTR and LTA programs is underway as well as licensing efforts with the Nuclear Regulatory Commission (NRC). Finally, accident analyses coupled with economic evaluations for both operating savings as well as fuel savings have been initiated. Cr coated zirconium alloy claddings showed low corrosion rates in both autoclave and in-reactor tests and will be fabricated using commercial processes for the first LTRs for insertion in 2019. Current autoclave results for SiC composite claddings indicate that a corrosion rate of fewer than 2 micrometers per year which meets corrosion requirements may be achieved under normal operating conditions. Modular Accident Analysis Program 5 (MAAP5) calculations indicate that solid fission products can be contained within SiC cladding for up to two hours longer than current Zr based cladding in a station blackout scenario. This additional time is due to the much higher temperature capability of SiC (~2000°C). These two hours can be used to implement additional response options instituted through the FLEX program by reactor operators. While the Cr coated Zr alloy option offers more modest ATF gains (~200°C higher than bare Zr) in similar situations, the coatings do delay the runaway oxidation encountered by uncoated zirconium cladding. Both ATF cladding options also reduce hydrogen production which dramatically reduces primary system and containment pressure and the risk of fission product release beyond containment in the unlikely event of an accident. The lower pressure in the system allows more time to feed cooling water to the core, resulting in the avoidance of fuel melting. The coping time is extended indefinitely as long as the water flow continues. SiC exhibits the highest accident tolerance of any cladding and significant advances in understanding the design, manufacture and accident behavior of SiC cladding have been made. Department of Energy support is needed to continue the on-going experimental work addressing the interaction between U 3 Si 2 and SiC at temperatures >1200°C, the effect of SiC manufacturing methods and manufacturing variability on physical properties, and the ability to predict the mechanical properties of SiC composites based on the composite design. Additionally, experimental work on methods to rapidly fabricate SiC composite structures with high density and reduce the fabrication price of SiC fibers while maintaining a high level of performance is needed. Minimal (<1%) swelling of U 3 Si 2 and subsequent fission gas release has been demonstrated up to 20 MWd/kgU. Irradiation experiments with U 3 Si 2 fuel in ATR to determine these properties at 40 to 50 MWd/kgU are underway. These experiments will provide the data needed to license fuel rod design codes. Research is continuing on production methods for making U 3 Si 2 from UF 6 without going through the U metal step. Oxidation tests of fuel pellets and powder in steam and synthetic air indicate that U 3 Si 2 has a lower oxidation reaction initiation temperature than UO 2 . Options to reduce the U 3 Si 2 oxidation rate are being explored. A hybrid fuel design using pellets with the weight ratio of 30%/70% U 3 Si 2 /UN is currently undergoing testing in the ATR. This approach is being explored to further increase the positive economics of the U 3 Si 2 fuel. In addition to the work supported by the USDOE, research and testing activities are being carried on in a world-wide effort funded by many countries such as Sweden, United Kingdom, Belgium, Netherlands, Spain, Germany, Japan and France. This work is being facilitated through the Westinghouse led Collaboration for Advanced Research on Accident Tolerant Fuel (CARAT) program. Annual meetings are organized by Westinghouse as a venue for presentation of this work and to provide for the cross-fertilization of ideas among the many outstanding researchers in the ATF area. Since SiC, coated cladding and high density fuel options are not currently used in the nuclear industry, support from the government and industry members is needed to further the significant effort of setting new standards. The same is true for the Nuclear Regulatory Commission (NRC) which must review and approve the commercial use of these new fuels since all current regulations are oriented toward Zr/ UO 2 fuel. There are no showstoppers for accident tolerant fuel technologies when considering supply chain, fabrication, enrichment suppliers, production, and licensing. Due to the cost savings from higher density fuel and the accident tolerance of coated claddings, Exelon has identified potential commercial plants to host the LTRs and LTAs. Planning is underway to implement this schedule.
Following the severe accident in Fukushima Daiichi Nuclear Power Plant in Japan, safety related concerns about the zirconium based claddings used in current light water reactors have increased. High corrosion resistance and low neutron absorption cross section make zirconium a suitable cladding material for normal nuclear plant operational conditions. However, for nuclear accident scenarios when safety functions of the plant are lost, Zr claddings undergo exothermic reaction with steam and exacerbate the accident conditions. The exothermic reaction increases the temperature of the cladding and accelerates core melting in severe accident progression. And the generation of explosive hydrogen gas accumulates and challenges the structural integrity. The accident tolerant fuel (ATF) concept is the fuel and cladding system that gives a longer time margin, compared to standard Zr claddings, to cope with the accident when core cooling systems are lost in a nuclear power plant. The ATF cladding should have slower oxidation kinetics and less hydrogen generation than Zr to alleviate consequences of cladding interaction with steam at high temperatures. The maximum time available to mitigate progression of severe accident is an important measure to evaluate benefits of ATF claddings. For this work, the maximum time available to mitigate progression of severe accident is selected as the time at which cladding melting reaction starts. Melting reaction is selected as an upper limit because of the degradation of coolable geometry. Maintaining the coolable geometry is a regulation criteria for both loss of coolant (LOCA) analyses and outside the LOCA analyses. Once the melting of the cladding starts, it exacerbates the deformation of the fuel assembly and hottest rods within the core cannot be cooled by water reflood and results in fuel melting progression. The aim of this work is to evaluate time margin gain of ATF cladding in a severe accident scenario of LOCA without safety injections and station blackout considering oxidation kinetics only. Also it is assumed that safety injections are recovered before melting of the claddings start and the sensitivity of safety injection actuation time on core recovery is analyzed. The core recovery time is the time when makeup water from safety injections quench the fuel rods and halt the progression of the severe accident. This time is estimated by initiating safety injections at different times and observing the hot rod behavior which represents 1/5. of the core in this work. It is considered that core is not recoverable when 20% of the core is damaged.
HERA is a joint experimental program (JEEP) operating within the Nuclear Energy Agency’s (NEA’s) framework for irradiation experiments (FIDES). HERA is dedicated to the understanding of light water reactor (LWR) fuel performance at high burnup under reactivity-initiated accidents (RIA). During RIAs the fuel cladding can be breached by one of two mechanisms; pellet-cladding mechanical interaction or high temperature balloon and rupture. Pellet-cladding mechanical interaction (PCMI) failure occurs in the early phase of an RIA transient where the fuel pellet expands rapidly into the cladding prior to any meaningful heat transfer from the pellet to the cladding. This results in high stresses in the cladding resulting in crack propagation through the base Zircaloy metal and axially along the cladding tube. Failure by PCMI is a brittle failure mode and occurs at low cladding strains, approximately 2% hoop strain. If the cladding survives the PCMI phase of the transient, it may still fail due to ballooning and rupture induced by extended exposure to high temperature. Thermal transport from the fuel pin to the coolant is significantly reduced if a transition to film boiling on the cladding surface occurs. This result in both a rapid increase in fuel temperature, which drives fission gas release, and a spike in cladding temperature, which results in loss of mechanical strength. If the internal pressure of the fuel rod is greater than the system pressure the cladding can inelastically deform and eventually rupture. Failure by swelling and rupture occurs at larger strains, generally greater than 5% hoop strain. While PCMI failures are generally seen as more limiting, the dominance of one failure mode over the other can be affected by both the cladding material conditions, and the transient evolution.
HERA is a joint experimental program (JEEP) operating within the Nuclear Energy Agency’s (NEA’s) framework for irradiation experiments (FIDES). HERA is dedicated to the understanding of light water reactor (LWR) fuel performance at high burnup under reactivity-initiated accidents (RIA). During RIAs the fuel cladding can be breached by one of two mechanisms; pellet-cladding mechanical interaction or high temperature balloon and rupture. Pellet-cladding mechanical interaction (PCMI) failure occurs in the early phase of an RIA transient where the fuel pellet expands rapidly into the cladding prior to any meaningful heat transfer from the pellet to the cladding. This results in high stresses in the cladding resulting in crack propagation through the base Zircaloy metal and axially along the cladding tube. Failure by PCMI is a brittle failure mode and occurs at low cladding strains, approximately 2% hoop strain. If the cladding survives the PCMI phase of the transient, it may still fail due to ballooning and rupture induced by extended exposure to high temperature. Thermal transport from the fuel pin to the coolant is significantly reduced if a transition to film boiling on the cladding surface occurs. This result in both a rapid increase in fuel temperature, which drives fission gas release, and a spike in cladding temperature, which results in loss of mechanical strength. If the internal pressure of the fuel rod is greater than the system pressure the cladding can inelastically deform and eventually rupture. Failure by swelling and rupture occurs at larger strains, generally greater than 5% hoop strain. While PCMI failures are generally seen as more limiting, the dominance of one failure mode over the other can be affected by both the cladding material conditions, and the transient evolution.
Through the early 2000’s, nuclear fuel cladding failure resulting from pellet-cladding interaction in commercial pressurized water reactor fuel was managed successfully by incorporating power ramp restrictions. Within the past decade, however, cladding failures have again begun to appear, often correlated to missing pellet surface defects, and further aggravated by modern reactor operating strategies demanding higher fuel duty operations. In response, renewed efforts in fuel behavior modeling and simulation are being pursued to improve our understanding of the conditions that can lead to missing pellet surface related cladding failure. This paper describes a methodology used to model pellet-cladding interaction related failures observed in commercial pressurized water reactors using the BISON fuel performance code developed at Idaho National Laboratory. In order to accomplish this goal, a three-step process is followed: 1) A failure-stress threshold is developed by using BISON code to model ramp test with known pellet-clad interaction related failures, 2) BISON analysis is applied to a commercial pressurized water reactor cycle startup with one rod confirmed to contain a missing pellet surface defect, and 3) an missing pellet surface sensitivity study of a cycle startup of the same commercial pressurized water reactor which contained a failed fuel rod of un-identified type. The analysis results described in this paper serve to illustrate the BISON code capabilities for modeling pressurized water reactor fuel subjected to higher duty power events.
In response to the Department of Energy (DOE) funded initiative to develop and deploy lead fuel assemblies (LFAs) of Enhanced Accident Tolerant Fuel (EATF) into a US reactor within 10 years, AREVA put together a team to develop promising technologies for improved fuel performance during off normal operations. This team consisted of the University of Florida (UF) and the University of Wisconsin (UW), Savannah River National Laboratory (SRNL), Duke Energy and Tennessee Valley Authority (TVA). This team brought broad experience and expertise to bear on EATF development. AREVA has been designing; manufacturing and testing nuclear fuel for over 50 years and is one of the 3 large international companies supplying fuel to the nuclear industry. The university and National Laboratory team members brought expertise in nuclear fuel concepts and materials development. Duke and TVA brought practical utility operating experience. This report documents the results from the initial “discovery phase” where the team explored options for EATF concepts that provide enhanced accident tolerance for both Design Basis (DB) and Beyond Design Basis Events (BDB). The main driver for the concepts under development were that they could be implemented in a 10 year time frame and be economically viable and acceptable to the nuclear fuel marketplace. The economics of fuel design make this DOE funded project very important to the nuclear industry. Even incremental changes to an existing fuel design can cost in the range of $100M to implement through to LFAs. If this money is invested evenly over 10 years then it can take the fuel vendor several decades after the start of the project to recover their initial investment and reach a breakeven point on the initial investment. Step or radical changes to a fuel assembly design can cost upwards of $500M and will take even longer for the fuel vendor to recover their investment. With the projected lifetimes of the current generation of nuclear power plants large scale investment by the fuel vendors is difficult to justify. Specific EATF enhancements considered by the AREVA team were; Improved performance in DB and BDB conditions; Reduced release to the environment in a catastrophic accident; Improved performance during normal operating conditions; Improved performance if US reactors start to load follow; Equal or improved economics of the fuel; and Improvements to the fuel behavior to support future transportation and storage of the used nuclear fuel (UNF). In pursuit of the above enhancements, EATF technology concepts that our team considered were; Additives to the fuel pellets which included; Chromia doping to increase fission gas retention. Chromia doping has the potential to improve load following characteristics, improve performance of the fuel pellet during clad failure, and potentially lock up cesium into the fuel matrix; Silicon Carbide (SiC) Fibers to improve thermal heat transfer in normal operating conditions which also improves margin in accident conditions and the potential to lock up iodine into the fuel matrix; Nano-diamond particles to enhance thermal conductivity; Coatings on the fuel cladding; and Nine coatings on the existing Zircaloy cladding to increase coping time and reduce clad oxidation and hydrogen generation during accident conditions, as well as reduce hydrogen pickup and mitigate hydride reorientation in the cladding. To facilitate the development process AREVA adopted a formal “Gate Review Process” (GR) that was used to review results and focus resources onto promising technologies to reduce costs and identify the technologies that would potentially be carried forward to LFAs within a 10 year period. During the initial discovery phase of the project AREVA took the decision to be relatively hands off and allow our university and National Laboratory partners to be free thinking and consider options that would not be constrained by preconceived ideas from the fuel vendor. To counter this and to keep the partners focused, the GR process was utilized. During this GR process each of the team members presented their findings to a board made up of technical experts from utilities, fuel manufacturing experts, fuel technical experts, and fuel research and development (R&D) experts. During the initial 2 years of the project there were several major accomplishments. These accomplishments, along with the implications for successfully implementing EATF, are; The experimental spark plasma sintering process (SPS) process was successfully used to produce fuel pellets containing either 10% SiC whiskers or nano-diamond particles. The ability to use this process enables the thermal margin enhancements of the fuel additives to be realized. Without the SPS process, the conventional process cannot support adding pellet additives in the required quantities; Coatings of Ti2AlC were successfully applied to Zircaloy-4 cladding. Testing of Ti2AlC coatings at Loss of Cooling Accident (LOCA) conditions showed reduced cladding oxidation compared to present un-coated Zircaloy-4 cladding. This achievement allows the presently used cladding system to be retained so that the 10 year schedule can be met. Having to implement a new cladding material will extend the development schedule beyond 10 years; Several documents were produced to support future development, testing, and licensing of EATF, including a design requirements traceability matrix, a draft business plan, a draft test plan, a draft regulatory plan, and the acceptance criteria for lead fuel assembly insertion into a commercial reactor. This preparatory work lays the foundation for ensuring the future development plans address all the areas required to test, license, and manufacture the new EATF; and In addition, the high velocity oxy-fuel and electrophoretic deposition (EPD) coating application processes were dropped from further consideration due to their inability to meet manufacturing criteria. This allows the resources to be focused on the most promising EATF concepts identified. Future development opportunities that were identified during this work include; The use of SiC or diamond requires that a new pellet production technique (Spark Plasma Sintering), be developed. This entails investment in developing, proving and implementing a new commercial pellet production process. Development of the process to apply thinner coatings is required; Coatings cannot be too “thick” or they will displace a significant volume of water in the core resulting in reduced thermal hydraulic characteristics; Application of the coating at high temperature can affect the Zircaloy substrate. This will require the development and implementation of a new cladding coating manufacturing process; and Replace the Cold Spray (CS) cladding coating application with the Physical Vapor Deposition (PVD) process to eliminate duplication of work and provide greater control over coating thicknesses. This can result in a reduction in the final cycle economic penalty of coatings.
The design temperature of high plutonium concentration ZPPR fuel assemblies is 600 degrees C. Cladding integrity of the 304L stainless steel cladding is a significant concern with this fuel since even small holes can lead to substantial fuel degradation. Since the fuel has a higher coefficient of thermal expansion than the cladding, an investigation of the stress induced in the cladding due to the differential thermal expansion of fuel and cladding up to the design temperature was conducted. Small holes in the cladding envelope would be expected to lead to the fuel hydriding and oxidizing into a powder over a long period of time. This is the same type of chemical reaction chain that exists in the degradion of the high uranium concentration ZPPR fuel. Unfortunately, the uranium fuel was designed with vents which allowed this degradation to occur. The Pu cladding is sealed so only fuel with damaged cladding would be subject to this damage. The thermal stresses that can be developed in the fuel cladding have been calculated in in this paper and compared to the ultimate tensile stress of the cladding. The conclusion is drawn that thermal stresses cannot induce holes in the cladding even for the highest storage temperatures predicted in calculations (292°C). In fact, thermal stress can not cause cladding failure as long as the fuel temperatures are below the design limit of 600 degrees C (1,112 degrees F).
This paper documents the development of failure criteria for both pressurized water reactor (PWR) and boiling water reactor (BWR) fuel rod failure due to pellet cladding mechanical interaction (PCMI) during a reactivity insertion accident (RIA). This study was initiated to use cladding mechanical properties using data from separate effects tests to provide a basis to translate nuclear safety research reactor (NSRR) test data to commercial light water reactor conditions. The approach employed for the revised licensing criteria combined elements of experimental results and analytical evaluations to develop a fundamental understanding of fuel behavior during RIA events. The transient behavior of intermediate and high burnup fuel rods using well characterized RIA simulation tests was established. Cladding mechanical properties using data from separate effects tests was also developed. The Zircaloy cladding mechanical properties database of separate effects tests was used to develop the cladding integrity models. The cladding integrity models were then used in combination with the application of the Falcon fuel behavior code to translate NSRR test data to commercial light water reactor conditions. Because of the complex manner in which burnup influences fuel rod failure, it was not possible to develop a fuel rod failure threshold directly from the experimental data. An alternative approach was required that combined analytical modeling and experimental data to develop the PCMI-related contribution to the failure threshold. The analytical approach computed the radial average peak fuel enthalpy required to cause cladding failure by PCMI as a function of hydrogen content. This was accomplished by applying a critical strain energy density (CSED)-based cladding integrity model using data from total and uniform elongation tests of irradiated low-tin Zircaloy-4, ZIRLO, and Zircaloy-2 cladding materials. The CSED was developed as a function of cladding hydrogen content because hydrogen induced embrittlement is a primary effect of burnup. It was found that the failure threshold decreased with hydrogen content due to the increase in PCMI loading as a result of gap closure effects and by the decrease in cladding ductility with hydrogen accumulation. (authors)
Fuel fragmentation, relocation, and dispersal are some of the largest issues remaining in the nuclear industry before rod-average burnup can be increased beyond 62 GWd/tU. The issue is primarily related to the potential for fuel to be dispersed into the reactor primary system, which may increase public risk. One way to prevent dispersal is to avoid cladding burst. The objective of this work is to support the high burnup safety case by evaluating cladding burst under high-burnup, full-length fuel rods and to identify uncertainties that could improve model predictions. The results of this analysis will evaluate realistic, prototypic loss-of-coolant accident (LOCA) conditions; support future cladding burst test designs; and inform the development of mechanistic material models. Realistic high-burnup operating conditions were implemented in the BISON fuel performance code to simulate steady-state and LOCA transient fuel rod evolution to the point at which cladding burst occurred. Parametric studies are performed to assess code response to changes in rod internal pressures and heating rates. Results were compared with simulated LOCA experiments to identify inconsistencies between commercial fuel rod analysis and experimental validation. The representative full-length fuel rod LOCA simulation results did not agree with cladding burst tests. Cladding burst tests indicated burst occurring well below (100–150 °C) those calculated in the full-length fuel rod LOCA analysis. Further investigation indicated that the cladding burst tests do not appear to be representative for full-length fuel rods. The inconsistency investigated in this work showed that the differences between the BISON simulation and the experiment's cladding burst conditions arise from an incomplete characterization of the cladding surface temperature, detailed rodlet characterization, lack of cladding strain measurements, and uncertainty in the cladding creep and failure models.
This reports complete Milestone M2.2.3 Produce zirconium hydride moderator material. In this milestone, we report the successful fabrication of FeCrAl alloys cladded zirconium hydride moderator. Different types of crucible designs were presented, including the basic design with bar cladding material, basic design with tube cladding material, and crucible design with position holding function. Mo and FeCrAl were used as the trial cladding materials. The welding techniques and procedures were reported and discussed. Totally three welding techniques were adopted in the development of moderator cladding, and they are electron beam welding (EBW), laser welding (LW), and gas tungsten arc welding (GTAW). After welding, all cladded crucibles were evaluated with two kinds of leak testing, the helium leak test for minor leakage and the bubble test for major leakage. Due to the concern of the poor neutronics performance, Mo was not ideal for future moderator cladding application. Therefore, detailed characterization of the Mo cladded zirconium hydride was not pursued. Instead, the characterization of FeCrAl cladded zirconium hydride was performed. We discussed two material conditions (i.e., as machined and pre-oxidized conditions) prior to the cladding process, evaluated thermal stability of cladded zirconium hydride moderator through directly measuring hydrogen release, and characterized the zirconium hydride following the thermal desorption measurement. The results showed pre-oxidized FeCrAl is capable of efficiently preventing hydrogen release from the moderator assembly.
A poro-elasto-plastic material model has been developed to capture the response of oxide fuels inside the nuclear reactors under operating conditions. Behavior of the oxide fuel and variation in void volume fraction under mechanical loading as predicted by the developed model has been reported in this article. The significant effect of void volume fraction on the overall stress distribution of the fuel pellet has also been described. An important oxide fuel issue that can have significant impact on the fuel performance is the mechanical response of oxide fuel pellet and clad system. Specifically, modeling the thermo-mechanical response of the fuel pellet in terms of its thermal expansion, mechanical deformation, swelling due to void formation and evolution, and the eventual contact of the fuel with the clad is of significant interest in understanding the fuel-clad mechanical interaction (FCMI). These phenomena are nonlinear and coupled since reduction in the fuel-clad gap affects thermal conductivity of the gap, which in turn affects temperature distribution within the fuel and the material properties of the fuel. Consequently, in order to accurately capture fuel-clad gap closure, we need to account for fuel swelling due to generation, retention, and evolution of fission gas in addition to the usual thermal expansion and mechanical deformation. Both fuel chemistry and microstructure also have a significant effect on the nucleation and growth of fission gas bubbles. Fuel-clad gap closure leading to eventual contact of the fuel with the clad introduces significant stresses in the clad, which makes thermo-mechanical response of the clad even more relevant. The overall aim of this test problem is to incorporate the above features in order to accurately capture fuel-clad mechanical interaction. Because of the complex nature of the problem, a series of test problems with increasing multi-physics coupling features, modeling accuracy, and complexity are defined with the objective of accurate simulation of fuel-clad mechanical interaction subjected to a wide-range of thermomechanical stimuli.