Search NASA⌕ Search

SEARCH · Search NASA

Results for “Cladding”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,153 records · Page 64

Multi-Functional Zirconium-Silicide Coatings on Zirconium-alloy for Improved Accident Tolerance

Recently, development of protective coatings on zirconium-alloy (Zr-alloy) fuel cladding in light water reactors has been extensively investigated to enhance safety margins in accident scenarios. One accident scenario is degradation of the reactor core under a coolant-limited condition, where a large amount of Zr-alloy claddings would react with high temperature steam, leading to oxidation, hydrogen production, and loss of intrinsic mechanical properties of the fuel cladding. Although, total replacement of Zr-alloy with SiC-SiCf composites or FeCrAl is being considered for the long-term, application of oxidation resistant coatings on zirconium-alloy is being investigated as a near-term solution to mitigate oxidation of Zr-alloy and increase the accident coping time. Coatings, such as chromium, Ti{sub 2}AlC, SiC, and Cr{sub 3}C{sub 2}- NiCr, deposited by various deposition techniques have been investigated. In addition, recent studies on modified heating surface for heat transfer enhancement provides basis on the optimal design of coated Zr-alloy claddings so that the new cladding can be achieve accident tolerance and heat transfer efficiency for both accident and normal operation conditions. Therefore, boiling heat transfer from the coated surface to water environment must be evaluated in parallel. In heat transfer performance, boiling heat transfer is characterized by nucleate boiling, critical heat flux (CHF), transition boiling, minimum film boiling temperature (T{sub min}), and film boiling. Zirconium-silicide (ZrSi{sub 2}) is a potentially attractive protective coating material for cladding applications. Although this material has not been studied extensively, it appears to be a promising candidate because of the high melting points, and the low neutron penalty, and the generally good oxidation resistance to transition metal silicides. It has been reported that oxidation of ZrSi{sub 2} powder in a flowing air environment at elevated temperatures produced ZrO{sub 2}, SiO{sub 2}, and ZrSiO{sub 4}, pointing to the possibility of achieving highly protective surface layers of SiO{sub 2} and ZrSiO{sub 4} that would protect the material from further oxidation. In this study, magnetron sputter deposition of ZrSi{sub 2} on zirconium-alloy flats and cylindrical rods was performed. The coated samples were oxidized in high temperature air (700 deg. C, 1000 deg. C and 1200 deg. C) to evaluate their oxidation resistance. The coated cylindrical rods were quenched in saturated water to observe transition boiling, T{sub min}, film boiling regime, while the coated flats were tested in pool boiling facility to investigate nucleation boiling and CHF.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

INL_intern_poster_RashedA

Advanced nuclear reactors often operate at elevated temperatures, novel fuel with different chemical and thermal properties that may interact differently with cladding, new coolants (e.g., molten salt, liquid metal, or sodium) that are chemically aggressive, requires cladding materials with superior oxidation, corrosion, and creep resistance. Developing fuel cladding for advanced reactors is essential, as the cladding plays a critical role in reactor safety, performance, and longevity. In this study, innovative Non-Concentrated Alloys (NCAs) were developed as novel fuel cladding materials for advanced nuclear reactors. Multiple elements were chosen for the alloys. NCAs were manufactured and tested mechanically, showing promise with the arc-melting method, and setting a clear path for the next step of NCAs' development as a fuel cladding for advanced nuclear reactors.

36 - MATERIALS SCIENCE↗

Effect of spacer grids on high-burnup fuel fragmentation, relocation, and dispersal

Increasing the fuel burnup limit in light-water reactors to improve fuel cycle economics requires a strong technical foundation. Experimental observations from the Halden and Studsvik programs have revealed severe fuel fragmentation during loss-of-coolant accident (LOCA) conditions, highlighting the need for additional technical evaluation. Consequently, further LOCA test data are needed to complement existing findings and improve the understanding of fuel fragmentation, relocation, and dispersal (FFRD) behavior. Oak Ridge National Laboratory’s Severe Accident Test Station has played a significant role in advancing the understanding of high-burnup fuel fragmentation, relocation, and dispersal phenomena. One remaining gap in the available experimental database is the effect of fuel assembly structural features on cladding deformation behavior during a LOCA, and more specifically, their impact on the fuel’s ability to fragment, relocate, and disperse. Recent analyses using the BISON fuel performance code suggest that cladding deformation near grid spacers will remain below the 3% threshold that has been reported in the NRC Research Information Letter, indicating that the cladding could remain mechanically constrained during the LOCA event. This paper builds upon the BISON analyses to design and conduct a series of out-of-cell tests aimed at further evaluating cladding deformation in and around grid spacers. In addition, these tests were used to assess local cladding temperature conditions and compare them against analytical predictions in order to better replicate expected in-reactor behavior. Finally, an in-cell high-burnup LOCA test was designed and performed to evaluate the effects of a grid spacer, or cladding restraint, on fuel fragmentation, relocation, and dispersal susceptibility. The high-burnup test results differed from those of historical LOCA experiments, with a recorded rupture temperature of 861°C. Two ballooned regions and corresponding rupture openings were observed, with rupture widths of approximately 0.64 mm for both ruptures and rupture lengths of 4.8 mm and 5.6 mm, respectively.

Capps, Nathan [ORNL]↗

3D modeling of missing pellet surface defects in BWR fuel

One of the important roles of cladding in light water reactor fuel rods is to prevent the release of fission products. To that end, it is essential that the cladding maintain its integrity under a variety of thermal and mechanical loading conditions. Local geometric irregularities in fuel pellets caused by manufacturing defects known as missing pellet surfaces (MPS) can in some circumstances lead to elevated cladding stresses that are sufficiently high to cause cladding failure. Accurate modeling of these defects can help prevent these types of failures. The BISON nuclear fuel performance code developed at Idaho National Laboratory can be used to simulate the global thermo-mechanical fuel rod behavior, as well as the local response of regions of interest, in either 2D or 3D. In either case, a full set of models to represent the thermal and mechanical properties of the fuel, cladding and plenum gas is employed. A procedure for coupling 2D full-length fuel rod models to detailed 3D models of the region of the rod containing a MPS defect is detailed in this paper. The global and local model each contain appropriate physics and behavior models for nuclear fuel. This procedure is demonstrated on a simulation of a boiling water reactor (BWR) fuel rod containing a pellet with an MPS defect, subjected to a variety of transient events, including a control blade withdrawal and a ramp to high power. The importance of modeling the local defect using a 3D model is highlighted by comparing 3D and 2D representations of the defective pellet region. Finally, parametric studies demonstrate the effects of the choice of gaseous swelling model and of the depth and geometry of the MPS defect on the response of the cladding adjacent to the defect.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Factors reducing the efficiency of ytterbium fibre lasers and amplifiers operating near 0.98 μm

We have studied the factors that reduce the efficiency of cladding-pumped ytterbium fibre lasers and amplifiers operating in the spectral range around a wavelength of 0.98 μm. It has been shown that the core of the active fibre being not single-mode leads to accelerated development of amplified spontaneous luminescence around λ = 1.03 μm, which reduces the highest possible amplifier efficiency. We have examined the effect of spontaneous luminescence propagating in the first reflective cladding. It has been shown theoretically that the pump-to-signal conversion efficiency is highest when the ratio of the core and cladding diameters in a multimode active fibre lies in the range 0.7 – 1. We have fabricated and characterised an optical fibre with a core-to-cladding diameter ratio of 0.76 (core and cladding diameters of 95 and 125 μm, respectively), which allowed a pump conversion efficiency of 66 % to be reached, a record level for cladding-pumped ytterbium fibre laser systems emitting near 0.98 μm. (paper)

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

An impedance-based diameter gauge for in-pile fuel deformation measurements

During irradiation, the fuel-cladding interface of a nuclear fuel rod can experience significant mechanical and chemical interaction. In-situ measurement of the radial deformation of the cladding can quantify the extent of this interaction and the state of the cladding. Existing capabilities to perform in-pile diameter measurements are limited by required contact and an intrusive presence of a device near to a specimen. To overcome these limitations, researchers have developed and evaluated an electrical impedance based diameter gauge using a benchtop system. The sensor consists of an electrically conductive concentric ring around the fuel cladding such that the electrical impedance between the ring and cladding is measured. Additionally, the cladding diameter is determined through a measurement of the electrical impedance between the electrodes with a known ring electrode diameter. Analytic and 3-D finite element analyses (FEA) were used to quantify the measurement sensitivity, uncertainty, and off-design conditions. The experimental sensor measured diameters with <20 µm of error, and had a measurement resolution of <1 µm for diameters ranging from 9.5 to 9.6 mm. Lastly, the uncertainty analysis for the experimental setup estimated an uncertainty of 20 µm, consistent with the experimentally measured results.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

A New Criterion to Improve Operational Drizzle Detection with Ground-Based Remote Sensing

Light shallow precipitation in the form of drizzle is one of the mechanisms for liquid water removal, affecting cloud lifetime and boundary layer dynamics and thermodynamics. The early formation of drizzle drops is of particular interest for quantifying aerosol–cloud–precipitation interactions. In models, drizzle initiation is represented by the autoconversion, that is, the conversion of liquid water from a cloud liquid water category (where particle sedimentation is ignored) into a precipitating liquid water category. Various autoconversion parameterizations have been proposed in recent years, but their evaluation is challenging due to the lack of proper observations of drizzle development in the cloud. This work presents a new algorithm for Classification of Drizzle Stages (CLADS). CLADS is based on the skewness of the Ka-band radar Doppler spectrum. Skewness is sensitive to the drizzle growth in the cloud: the observed Gaussian Doppler spectrum has skewness zero when only cloud droplets are present without any significant fall velocity. Defining downward velocities positive, skewness turns positive when embryonic drizzle forms and becomes negative when drizzle starts to dominate the spectrum. CLADS identifies spatially coherent structures of positive, zero, and negative skewness in space and time corresponding to drizzle seeding, drizzle growth/nondrizzle, and drizzle mature, respectively. We test CLADS on case studies from the Jülich Observatory for Cloud Evolution Core Facility (JOYCE-CF) and the Barbados Cloud Observatory (BCO) to quantitatively estimate the benefits of CLADS compared to the standard Cloudnet target categorization algorithm. We suggest that CLADS can provide additional observational constraints for understanding the processes related to drizzle formation better.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Problem Specification for FY12 Modeling of UNF During Extended Storage

The Nuclear Energy Advanced Modeling and Simulation (NEAMS) program of the Advanced Modeling and Simulation Office (AMSO) of the US Department of Energy, Office of Nuclear Energy (DOE/NE) has invested in the initial extension and application of advanced nuclear simulation tools to address relevant needs in evaluating the performance of used nuclear fuel (UNF) during extended periods of dry storage. There are many significant challenges associated with the prediction of the behavior of used fuel during extended periods of dry storage and subsequent transportation. The initial activities are focused on integrating with the Used Fuel Disposition (UFD) Campaign of the DOE/NE and a demonstration that the Advanced Multi-Physics (AMP) Nuclear Fuel Performance code (AMPFuel) for modeling the mechanical state of the cladding after decades of storage. This initial focus will model the long-term storage of the UNF and account for the effect, and generation, of radially and circumferentially oriented hydride precipitates within the cladding and predict the end of storage (EOS) mechanical state (stress, strain) of the cladding. Predicting the EOS state of the cladding is significant because it (1) provides an estimate of the margin to failure of the cladding during nominal storage operation and it (2) establishes the initial state of the fuel for post-storage transportation. Because there are significant uncertainties associated with the storage conditions, hydride precipitate formation, and the beginning of storage (BOS) condition of the UNF, this will also allow for the development of a rigorous capability to evaluate the relative sensitivities of the uncertainties and can help to guide the experimental and analysis efforts of the UFD Campaign. This document is focused on specifying the problem that will be solved with AMPFuel. An associated report, documents the specifics of the constitutive model that will be developed and implemented in AMPFuel to account for the presence and predict the generation of the hydride precipitates. This report satisfies the deliverable for the DOE Office of Nuclear Energy, Advanced Modeling and Simulation Office, milestone M3MS-12OR0605083, 'Definition of Problem Specification,' which defines the problem to be solved that will satisfy milestone M2MS-12OR0605081, 'Demonstration of the Advanced Multi-Physics (AMP) Nuclear Fuel Performance code for modeling UFD.' This document should provide sufficient detail to model a high burnup pressurized water reactor (PWR) fuel rod to provide an estimate of the end of storage (EOS) mechanical state of the cladding. The fuel rod and irradiation history are based on seven cycles of irradiation in the CP and L H.B. Robinson nuclear reactor, which achieved a discharge burnup of 66.682 MWd/kgU. The fuel has been experimentally examined for storage conditions by Argonne National Laboratory for the NRC. In addition, we have compiled a list of key factors that have been shown to strongly influence the EOS state of the fuel and have identified baseline values and ranges of uncertainties that will be considered. The simulations that will be performed have been described in detail and include the modeling assumptions and boundary conditions.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Fuel Performance Modeling Results for Representative FCRD Irradiation Experiments: Projected Deformation in the Annular AFC-3A U-10Zr Fuel Pins and Comparison to Alternative Designs

The objective of the present study was to predict the outcome of the AFC-3A annular U-10Zr fuel irradiation experiment. Specifically, the study attempted to predict whether the annular fuel will swell inward and fill the annulus, or swell outward resulting in an undesirable cladding deformation. It was predicted that both 55% and 75% annular fuels operating at 350 W/cm for 201 days will swell inward and partially fill the annulus which signifies a positive outcome of the experiment. The driving mechanism for such behavior is the fuel creep under the compressive stress exerted on the fuel by the cladding as a result of the fuel cladding mechanical interaction. Comparison with the solid fuel revealed that the annular fuel is expected to swell less early in life due to the mechanical constraint provided by the cladding. Furthermore, mechanical constraint is expected to yield a marked reduction of the axial elongation of the annular fuel as compared to the solid fuel. The prediction is based on the assumption that the annular fuel is not capable of moving axially relative to the cladding after the two come in contact. Post irradiation examination results would be very useful to assess the validity of this assumption. Specifically, underprediction of the axial growth would point to the fact that some slippage of the fuel relative to the cladding occurs after the onset of the FCMI. As fuel creep plays the major role in the deformation of the annular fuel, the contributions from the thermal and irradiation induced creep to the total creep rate of fuel were examined to provide guidance for possible creep testing experiments of the fuel (separate effect tests). It was found that irradiation induced creep dominates deformation of the fresh fuel at low temperatures. At high temperatures, and in the case of porous fuel, the thermal creep of the fuel becomes dominant and irradiation induced creep can be neglected. Fission gas induced porosity seems to accelerate fuel creep drastically. Recognizing the sensitivity of the fuel creep to the porosity, additional studies exploring this phenomenon and verifying published equations either experimentally or through computation may benefit the understanding of the annular fuel behavior.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Parametric and experimentally informed BWR Severe Accident Analysis Utilizing FeCrAl - M3FT-17OR020205041

Iron-chromium-aluminum (FeCrAl) alloys are being considered as advanced fuel cladding concepts with enhanced accident tolerance. At high temperatures, FeCrAl alloys have slower oxidation kinetics and higher strength compared with zirconium-based alloys. FeCrAl could be used for fuel cladding and spacer or mixing vane grids in light water reactors and/or as channel box material in boiling water reactors (BWRs). There is a need to assess the potential gains afforded by the FeCrAl accident-tolerant-fuel (ATF) concept over the existing zirconium-based materials employed today. To accurately assess the response of FeCrAl alloys under severe accident conditions, a number of FeCrAl properties and characteristics are required. These include thermophysical properties as well as burst characteristics, oxidation kinetics, possible eutectic interactions, and failure temperatures. These properties can vary among different FeCrAl alloys. Oak Ridge National Laboratory has pursued refined values for the oxidation kinetics of the B136Y FeCrAl alloy (Fe-13Cr-6Al wt %). This investigation included oxidation tests with varying heating rates and end-point temperatures in a steam environment. The rate constant for the low-temperature oxidation kinetics was found to be higher than that for the commercial APMT FeCrAl alloy (Fe-21Cr-5Al-3Mo wt %). Compared with APMT, a 5 times higher rate constant best predicted the entire dataset (root mean square deviation). Based on tests following heating rates comparable with those the cladding would experience during a station blackout, the transition to higher oxidation kinetics occurs at approximately 1,500°C. A parametric study varying the low-temperature FeCrAl oxidation kinetics was conducted for a BWR plant using FeCrAl fuel cladding and channel boxes using the MELCOR code. A range of station blackout severe accident scenarios were simulated for a BWR/4 reactor with Mark I containment. Increasing the FeCrAl low-temperature oxidation rate constant (3 times and 10 times that of the rate constant for APMT) had a negligible impact on the early stages of the accident and minor impacts on the accident progression after the first relocation of the fuel. At temperatures below 1,500°C, increasing the rate constant for APMT by a factor of 10 still resulted in only minor FeCrAl oxidation. In general, the gains afforded by the FeCrAl enhanced ATF concept with respect to accident sequence timing and combustible gas generation are consistent with previous efforts. Compared with the traditional Zircaloy-based cladding and channel box system, the FeCrAl concept could provide a few extra hours of time for operators to take mitigating actions and/or for evacuations to take place. A coolable core geometry is retained longer, enhancing the ability to stabilize an accident. For example, a station blackout was simulated in which cooling water injection was lost 36 hours after shutdown. The timing to first fuel relocation was delayed by approximately 5 h for the FeCrAl ATF concept compared with that of the traditional Zircaloy-based cladding and channel box system.

36 MATERIALS SCIENCE↗

Nuclear Energy Advanced Modeling and Simulation (NEAMS) Accident Tolerant Fuels High Impact Problem: FeCrAl Modeling Capabilities

Iron-chromium-aluminum alloys are a potential candidate replacement for zirconium-based claddings in light water reactor fuel rods due to their increased strength (lower creep rates and higher yield stress) and slower oxidation kinetics with steam. Their larger neutron absorption cross-section necessitates thinner claddings and larger fuel pellets to maintain the same as-fabricated fuel-to-clad gap. The aggressive development schedule of the United States Department of Energy's (DOE) Advanced Fuels Campaign (AFC) to have potential accident tolerant fuels (ATF) concepts in lead test rods or assemblies by 2022 has necessitated the need for advanced modeling and simulation techniques to investigate the behavior of these materials under normal operating and accident conditions. This report presents the modeling capabilities for FeCrAl claddings at the engineering (continuum) scale developed as part of the Nuclear Energy Advanced Modeling and Simulation (NEAMS) high impact problem (HIP). Sensitivity studies of select material parameters have been completed to determine their significance in predictions of important fuel performance parameters such as fuel centerline and surface temperatures, cladding stresses and strains, fission gas released, and rod internal pressure. Comparative analyses of FeCrAl and Zircaloy-4 claddings for separate effects conditions are presented.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Axial Relocation Model Extension in Bison

Fuel rods subjected to a Loss of Coolant Accident (LOCA) in a nuclear reactor can undergo a complex process known as fuel fragmentation, relocation, and dispersal (FFRD). The loss of coolant results in a severe degradation of the thermal heat transfer coefficient on the waterside surface of the cladding. This, coupled with the loss of coolant pressure causes the cladding to distend (balloon) outward. If the cladding distention is large enough, fuel fragmented during irradiation, may relocate from upper regions of the rod into the ballooned region. This mass relocation results in increased localized heating due to the presence of more fuel within the balloon resulting in further clad distention leading to potential rupture of the cladding. In the event that cladding rupture occurs the relocated fragmented fuel may disperse outside of the rupture opening if the size of the fuel fragments is small enough. Fuel performance modeling can be used to help understand the behavior of fuel rods during the LOCA transient. Existing models are particularly limited in regards to FFRD. This report briefly describes the existing state of the art for fuel performance modeling of fragmentation and fuel axial relocation. A more in depth description the axial relocation model implemented into the Bison fuel performance code in FY17 is provided. In this report, the extension of this existing model from a layered 1D framework to a 2D framework that allows for the introduction of azimuthal variation in the boundary conditions as experienced during a LOCA is discussed. The 2D framework utilized has been developed by the author of this report as part of his dissertation research ongoing at the University of South Carolina under the direction of Professor Travis W. Knight. The report briefly describes the 2D framework used and highlights in more detail the required developments in Bison to facilitate the extension of the axial relocation model to work within this framework. Finally, a few demonstration cases are provided that illustrate the benefit of using the new extended axial relocation model for the simulation of fuel rods under LOCA conditions.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

SCALE Lattice Physics Code Assessments of Accident Tolerant Fuel

This report highlights accident-tolerant fuel (ATF) code assessment activities performed under Project NRCHQ- 60-17-T-0017, Lattice Physics Enhancements and Assessment. ATF covers a broad range of advanced fuel and clad designs for light water reactors (LWRs) to enhance performance under several accident conditions. Several ATF concepts are anticipated to be deployed as lead test rods (LTRs) or lead test assemblies (LTAs) within the next five years. The purpose of this work is to assess the predictive capabilities of NRC neutronics codes that underpin various licensing calculations. ATF designs use different fuel and clad materials compared to standard UO 2 fuel and zirconium-alloy claddings (hereafter UO 2 -Zry). These new materials and geometrical designs need to be assessed to quantify the impact of nuclear data uncertainties on quantities of interest (QOIs) in licensing calculations and the impact of modeling approximations which may be valid for UO 2 -Zry but not for ATF. This report outlines a systematic approach for ATF neutronics code assessment which includes sensitivity and uncertainty (S/U) analysis of nuclear data, identification of experimental benchmark and gaps for code validation, investigation of modeling approximations, and code-to-code comparisons of calculated QOIs against high-fidelity reference continuous energy (CE) Monte Carlo (MC) calculations. This report focuses on the assessment of the SCALE/Polaris lattice physics code for reactor safety analysis. Polaris lattice physics calculations generate few group (FG) cross sections for PARCS full-core calculations. (Full-core analysis, spent fuel analysis, and severe accident analysis will be performed in future work.) The selected ATF concepts for this report include Cr 2 O 3 and Al 2 O 3 -Cr 2 O 3 -doped UO 2 fuel, U 3 Si 2 fuel, FeCrAl cladding, SiC cladding, and Cr-coated cladding.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Demonstration of the Coating Analysis Capabilities in BISON

In order to improve the accident tolerance of light water reactor (LWR) fuel, coated cladding materials have been proposed which exhibit much slower oxidation kinetics in high-temperature steam than Zr-alloys. This behavior should decrease the energy release due to oxidation and allow the cladding to remain integral longer in the presence of high-temperature steam, making accident mitigation more likely. In order to determine how these coating materials will adjust the behavior of the Zr-alloy cladding during normal reactor operation, simulations have been performed using the Bison fuel performance code. This analysis focused on modeling and comparing the integral thermo-mechanical performance of coated and uncoated zircaloy cladding with uranium dioxide fuel under normal operating conditions. This analysis demonstrates the ability to model a discrete meshed coating bonded to the cladding exterior and provides a comparison with an uncoated fuel rod. A generic range of coating material properties are implemented given the differences and unknowns regarding the proprietary coating properties used by the vendors. A main-effects analysis was performed to identify trends and sensitivities in how coating material properties affect key fuel performance metrics. Lastly, because residual stresses are expected to form in the coating, arising from the high temperature coating application process and application techniques, an additional analysis was performed to identify the impact of these stresses on the cladding behavior. Future analysis efforts will target more comprehensive documentation of this main effects analysis by sampling the results at the beginning and middle-of-life in order to capture important behavior before and during the onset of gap closure.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Post-Irradiation Examinations of the ATF Experiments - 2020 Status

This report contains the results of post-irradiation examination (PIE) of both Accident Tolerant Fuels-1 (ATF-1) rodlets and ATF-2 rodlets irradiated in the Advanced Test Reactor (ATR). The experiment is part of the U.S. Department of Energy (DOE) Nuclear Technology Research and Development (NTRD) program’s Advanced Fuels Campaign (AFC). The ATF-1 PIE focused on the continuation of the analyses of five rodlets, one containing U 3 Si 2 fuel, two containing UN-U 3 Si 5 composites, and two with UN-U 3 Si 2 composites. The non-destructive examinations of the U 3 Si 2 rodlet showed results comparable to the previously investigated rodlets. The profilometry of the UN-U 3 Si 2 composites highlighted permanent deformation of the cladding at the pellet-pellet interface, suggesting that hourglassing of the composite pellet occurred during irradiation, causing increased localized stresses on the Zirlo cladding tube due to Pellet-Cladding Mechanical Interaction (PCMI). The UN-U 3 Si 5 rodlets, which were contained in Kanthal cladding, did not show enhanced cladding deformation at the pellet interfaces; however, it is to be noted that the initial gap of these two rodlets was larger than typical light water reactor (LWR) gaps. The larger gap might have been sufficient to accommodate the fuel swelling without having contact between the fuel and cladding, explaining the absence of PCMI. Regarding the fission products, no axial redistribution of the major gamma emitters was observed in any of the composite rodlets. Fission gas measurements on the UN-U 3 Si 5 rodlets also has been performed. The estimated fission gas release, based on the calculated fission product inventory, remains limited, with a higher fission gas release for the rodlet that experienced a higher power.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Status of Eddy Current Developments at INL

Both standard and advanced Light Water Reactor (LWR) fuel systems are composed of fuel pellets enclosed in a metallic cladding. The fuel cladding represents the first containment of the fission products and the first safety barrier. Upon progression of irradiation, the cladding properties deteriorate, mainly due to the pick-up of hydrogen, which causes embrittlement, and the consequence corrosion that reduced the metallic substrate. Those changes in the properties combined with the harsh environment, e.g., fatigue and fretting occurring during operation, might eventually lead to loss of hermeticity. Therefore, it is important to be able to quantify the amount of corrosion taking place and to detect and size structural discontinuity that can promote cladding failure. Eddy current testing is one of the non-destructive methods employed for this purpose. Inspections are carried out using special probes, which are designed and optimized to inspect a tube with well-defined geometrical and physical characteristics, i.e. external diameter, wall thickness, material electric conductivity and magnetic permeability. The inspection goals are mainly twofold: first, the determination of the amount of corrosion by measurement of the external oxide thickness; second, the detection of flaws in the tube wall, ether on the external or the internal surface of the tube. This report summarizes the available capabilities for eddy current testing of LWR fuel claddings, identifies needs and are of developments for testing of ATF claddings.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Fuel Performance Analysis of Fast Flux Test Facility MFF-3 and -5 Fuel Pins Using BISON with Post Irradiation Examination Data

Using the BISON fuel-performance code, simulations were conducted of an automated process to read initial and operating conditions from the Pacific Northwest National Laboratory (PNNL) database and reports, which contain metallic-fuel data from the Fast Flux Test Facility (FFTF) MFF Experiments. This work builds on previous modeling efforts involving 1977 EBR-II metallic fuel pins from experiments. Coupling the FFTF PNNL reports to BISON allowed for all 338 pins from MFF-3 and MFF-5 campaigns to be simulated. Each BISON simulation contains unique power and flux histories, axial power and flux profiles, and coolant-channel flow rates. Fission-gas release (FGR), fuel axial swelling, cladding profilometry, and burnup were all simulated in BISON and compared to available post-irradiation examination (PIE) data. Cladding profilometry, FGR, and fuel axial swelling simulation results for full-length MFF metallic pins were found to be in agreement with PIE measurements using FFTF physics and models used previously for EBR-II simulations. The main two peaks observed within the cladding profilometry were able to be simulated, with fuel-cladding mechanical interaction (FCMI), fuel-cladding chemical interaction (FCCI), and thermal and irradiation-induced creep being the cause. A U-Pu-Zr hot-pressing model was included in this work to allow pore collapse within the fuel matrix. This allowed better agreement between BISON-simulated cladding profilometry and PIE measurements for the peak caused by FCMI. This work shows that metallic fuel models used to accurately represent fuel performance for smaller EBR-II pins may be used for full-length metallic fuel, such as FFTF MFF assemblies and the Versatile Test Reactor (VTR). As new material models and PIE measurements become available, FFTF MFF assessment cases will be reassessed to further BISON model development.

36 MATERIALS SCIENCE↗

SiC MODIFICATIONS TO MELCOR FOR SEVERE ACCIDENT ANALYSIS APPLICATIONS

The Department of Energy (DOE) Office of Nuclear Energy (NE) Light Water Reactor (LWR) Sustainability Program encompasses strategic research focused on improving reactor core economics and safety margins through the development of an advanced fuel cladding system. The Fuels Pathway within this program focuses on fuel system components outside of the fuel pellet, allowing for alteration of the existing zirconium-based clad system through coatings, addition of ceramic sleeves, or complete replacement (e.g. fully ceramic cladding). The DOE-NE Fuel Cycle Research & Development (FCRD) Advanced Fuels Campaign (AFC) is also conducting research on materials for advanced, accident tolerant fuels and cladding for application in operating LWRs. To aide in this assessment, a silicon carbide (SiC) version of the MELCOR code was developed by substituting SiC in place of Zircaloy in MELCOR’s reactor core oxidation and material property routines. The purpose of this development effort is to provide a numerical capability for estimating the safety advantages of replacing Zr-alloy components in LWRs with SiC components. This modified version of the MELCOR code was applied to the Three Mile Island (TMI-2) plant accident. While the results are considered preliminary, SiC cladding showed a dramatic safety advantage over Zircaloy cladding during this accident.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗