At least 127 records · Page 7

An overview of various critical aspects of low-cobalt/cobalt-free Li-ion battery cathodes

Cathodes of lithium-ion batteries (LIBs) significantly impact the environmental footprint, cost, and energy performance of the battery-pack. Hence, sustainable production of Li-ion battery cathodes is critically required for ensuring cost-effectiveness, environmental benignity, consumer friendliness, and social justice. Battery chemistry largely determines individual cell performance as well as the battery pack cost and life cycle greenhouse gas emission. Continuous manufacturing platforms improve production efficiency in terms of product yield, quality and cost. Spent-battery recycling ensures the circular economy of critical elements that are required for cathode production. Innovations in fast-charging LIBs are particularly promising for sustainable e-mobility with a reduced carbon footprint. This article provides an overview of these research directions, emphasizing strategies for low-cobalt cathode development, recycling processes, continuous production and improvement in fast-charging capability.

25 ENERGY STORAGE↗

Iridium-cobalt oxide synthesized via surfactant-assisted Adams fusion for efficient oxygen evolution in acidic and alkaline media

A series of iridium-cobalt (Ir-Co) oxide catalysts were synthesized using a modified surfactant-assisted Adams fusion method and evaluated for the oxygen evolution reaction (OER) in both acidic and alkaline media. The effect of varying the Ir/Co ratio was systematically studied and compared with commercial Ir black and pure IrO 2 samples. The actual elemental ratios were quantified using X-ray photoelectron spectroscopy (XPS), energy-dispersive X-ray spectroscopy (EDS), and inductively coupled plasma-mass spectrometry (ICP-MS). Among the synthesized samples, the Ir 6 Co 4 catalyst exhibited the best performance in acidic media, achieving an iR-corrected overpotential of 292 mV. In alkaline conditions, it demonstrated comparable activity to Ir black, with an iR-corrected overpotential of 263 mV. XPS and electron energy loss spectroscopy analyses revealed that increasing Co content led to a higher fraction of metallic Ir (Ir 0 ) in the catalyst. In addition, the role of Ir 3+ in enhancing OER activity was explored. A strong correlation was observed between higher Ir 3+ content and improved OER performance in acidic conditions.

Adams fusion↗

Cobalt-free and high-rate stable 5V lithium nickel manganese oxide spinel cathodes enabled via surface oxygen vacancies

Spinel LiNi 0.5 Mn 1.5 O 4 offers both the high-rate, low-cost and safety advantages of LiFePO 4 and the high energy density of LiNiₓMnᵧCo₁₋ₓ₋ᵧO₂ and LiNiₓCoᵧAlzO₂ cathodes. However, the large operating voltage of these materials induces electrolyte oxidation, which degrades the interface and drives Mn dissolution. These reactions are further exacerbated at high rates due to temperature rise. In this study, we discover that ammoniacal treatment followed by annealing introduces a high density of oxygen vacancies in the “near-surface region” of LiNi 0.5 Mn 1.5 O 4 particles. These vacancies release electrons changing the oxidation state of Mn and suppressing its tendency to oxidize the electrolyte. Further, these vacancies enhance the electrode’s electronic conductivity (by ∼3-fold) and Li + diffusivity (by ∼2-fold) greatly improving charge transport, especially when operated at high rates. This results in an across-the-board improvement in self-discharge, specific capacity, energy density, rate capability, coulombic efficiency and cycling stability. When cycled at ∼200 mA g −1 , the capacity fade averaged over 3000 cycles for the surface vacancy-enriched material is ∼0.0167% per cycle compared to an order of magnitude higher fade rate for the baseline material. In conclusion, these findings reveal the potential of targeted surface oxygen vacancy doping to develop cobalt-free and high energy density cathodes that tolerate fast charging and deliver improved cycle life.

Cobalt-free cathodes↗

Active Sites in the Dealuminated Beta Zeolite-Supported Cobalt Catalyst for Non-Oxidative Ethane Dehydrogenation

Dispersed metal species in siliceous zeolites have been actively studied for non-oxidative dehydrogenation of ethane (NDE). Fundamental insights into the dynamics of metal species in zeolites under reaction conditions have rarely been explored. Herein, we report an atomic level understanding of the dynamics and activity of cobalt (Co) sites in dealuminated Beta zeolite (DeAl-BEA) for NDE during induction and reaction conditions with extensive characterization techniques such as diffuse reflectance UV–vis, solid state nuclear magnetic resonance and X-ray photoelectron, X-ray diffraction along with in situ Fourier transform infrared and X-ray absorption spectroscopy. For a catalyst with 0.5 mass % Co loading, tetrahedral Co 2+ mononuclear sites, di-coordinated to the zeolite framework and with two silanol groups in vicinity (i.e., (≡SiO) 2 Co(HO–Si≡) 2 ), form upon exposure to hydrogen during induction and persist through the NDE reaction. Increasing the Co loading to 3.0 mass % yielded Co sites with similar electronic and coordination structures but slightly elongated Co–O bonds. Upon cooling to room temperature, the Co sites persisted in the same coordination environment, though the disappearance of a feature in the Co K-edge near-edge region revealed changes in the active site’s electronic structure coinciding with modest shifts in bond lengths. The electronic structure and activity of (≡SiO) 2 Co(HO–Si≡) 2 sites were studied comparatively to a few other hypothetical Co 2+ coordination structures, using electronic structure calculations and microkinetic simulations. The simulations showed that NDE is controlled by β-hydride elimination following C–H bond activation and that Co-sites possessing flexibility because of neighboring silanol defects are more active. Interestingly, dinuclear Co–O–Co sites (i.e., (≡SiO)Co(HO–Si≡) 2 –O–(HO–Si≡) 2 Co(≡SiO)) were more active than the mononuclear (≡SiO) 2 Co(HO–Si≡) 2 sites because of favorable hydrogen bonding with the vicinal silanol groups. In conclusion, the present study bridges the gap between the knowledge acquired by ex-situ characterizations and the active sites under the reaction conditions in alkane dehydrogenation chemistry.

36 MATERIALS SCIENCE↗

Voltage and temperature effects on low cobalt lithium-ion battery cathode degradation

Degradation of low cobalt lithium-ion cathodes was tested using a full factorial combination of upper cut-off voltage (4.0 V and 4.3 V vs. Li/Li + ) and operating temperature (25 °C and 60 °C). Half-cell batteries were analyzed with electrochemical and microstructural characterization methods. Electrochemical performance was assessed with galvanostatic cycling, cyclic voltammetry (CV), and electrochemical impedance spectroscopy (EIS) supported by distribution of relaxation times (DRT) analysis. Electrode microstructure was characterized with scanning electron microscopy (SEM), X-ray diffraction (XRD), and X-ray absorption near edge structure (XANES) imaging. Higher cut-off voltage cycling shows presence of NiO x formation, a low diffusivity rock-salt phase, in both CV and XRD data. XRD patterns confirmed that the rock-salt phase was beginning to form at the low cut-off voltage at high temperature, but in much lower intensity than at the high cut-off voltage. Higher temperature accelerates degradation processes at both voltages. Degradation factors at high temperature include NiO x formation, cathode material dissolution, and electrolyte decomposition. SEM analysis suggests that supporting phases may isolate and disconnect active material particles reducing capacity retention and battery life cycle. DRT analysis and XANES imaging show that both high temperature samples revealed a NiO x phase based on an increased diffusive impedance and a visible shift in the XANES spectra. The low cut-off voltage, high temperature sample showed a split peak and shift to lower energies indicating early formation of the NiO x phase. The diffusive impedance, which hinders intercalation and deintercalation, is driven by the formation of the NiO x phase. While primarily driven by cut-off voltage, elevated temperature also contributes to this degradation mechanism.

electrochemical impedance spectroscopy↗