Search NASA⌕ Search

SEARCH · Search NASA

Results for “TENSILE DEFORMATION”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 127 records · Page 7

Understanding the deformation behavior of the γ rich transformative Fe 38.5 Mn 20 Co 20 Cr 15 Si 5 Cu 1.5 complex concentrated alloy using in situ synchrotron diffraction

In situ tensile testing coupled with synchrotron x-ray diffraction was used to study the deformation behavior of metastability-engineered Fe 38.5 Mn 20 Co 20 Cr 15 Si 5 Cu 1.5 complex concentrated alloy. Monitoring the evolution of phase fraction and strain hardening response allowed the determination of true critical stress for the onset of the transformation-induced plasticity (TRIP) to be ∼375 MPa, preceded by slip starting at ∼255 MPa. In situ EBSD was used to validate the critical stress for transformation at the microstructure level and observe slip traces to confirm prior slip activity before the transformation. Further, a modeling framework based on stacking fault energy (SFE) was developed to predict the critical stress for transformation. Modeling suggested the SFE of the alloy to fall nearly 15 mJ/m 2 , which agrees well with SFE values calculated using synchrotron peak shifting (12 mJ/m 2 ) and thermodynamic calculation (11 mJ/m 2 ). As a result of γ-fcc to ε-hcp phase transformation, new {0002} ε planes emerged parallel to unaligned {111} γ planes with the tensile loading following S-N orientation relationship. Such selective emergence of new diffraction rings corresponding to ε phase is understood based on the reorientation of γ crystals with reference to tensile axis. In conclusion, this approach can be extended to effectively design alloys based on critical stress required for activating different deformation mechanisms to further push the limits of the strength-ductility envelope.

Complex concentrated alloy↗

Electric current-induced precipitation hardening in advanced high-strength steel

Effect of electric current on precipitation hardening for advanced high-strength steel is investigated based on mechanical testing and microscopic observation. Complex-phase steel containing nano-sized Nb-bearing carbides was used. By comparing the flow stress between uniaxial tension with applied electric current (pulsed tension) and without electric current (nonpulsed tension) at various elevated temperatures, the influence of electric current on precipitation hardening was confirmed. A higher values of Vickers hardness and full-width-at-half-maximum were obtained in the pulsed tensile specimen compared to the identically heat treated specimen after the same deformation. Small angle neutron scattering analysis showed that the volume fraction and mean diameter of newly formed precipitates in the pulsed tensile specimen were higher and larger than those in the induction heat treated specimen, respectively. In conclusion, it clearly shows that additional precipitation hardening could be induced by the athermal effect of electric current, which is distinct from the thermal effect of Joule heating.

36 MATERIALS SCIENCE↗

Elevated temperature ductility dip in an additively manufactured Al-Cu-Ce alloy

The deformation and failure mechanisms of Al-9Cu-6Ce (wt%) based alloys fabricated with laser powder bed fusion were investigated from room temperature to 400°C. The yield and ultimate tensile strengths decreased monotonically with increase in temperature, but the tensile elongation dipped unexpectedly at elevated temperatures and exhibited a minimum at 300°C. The dip in tensile elongation occurred with a concomitant dip in strain-rate sensitivity (SRS) of deformation. The as-fabricated alloy microstructure was heterogeneous, and the heat affected zone (HAZ) underneath the melt pool boundary was prone to strain localization. At 300 °C, the reduced SRS promoted the progression of strain localization in the HAZ leading to failure initiation and the dip in tensile elongation. Furthermore, a higher SRS or strain-hardening rate at other temperatures improved the tensile elongation by slowing the progression of strain localization in the HAZ such that failure initiated by other mechanisms elsewhere in the microstructure. Notably, the tensile elongation was limited by the defect structure only in a narrow temperature range (150 - 200 °C) while at other temperatures it was limited by the inherent microstructural features. This investigation exemplifies unexpected deformation and failure mechanisms possible in heterogeneous microstructures that result from additive manufacturing.

36 MATERIALS SCIENCE↗

Deformation Behavior of β Phase in a WE54 Magnesium Alloy

Second phases play a significant role in the development of high-performance magnesium alloys with rare earth elements. Here, in situ tensile tests combined with synchrotron radiation were carried out to investigate the deformation behavior of β phases in a WE (Mg–Y–Gd–Nd) alloy. By lattice strain analysis, it was found that micro load continuously transferred from the soft α-Mg matrix to the hard β phases during the whole plastic deformation, while this behavior was much more obvious at the beginning of deformation. Based on diffraction peak broadening, Williamson–Hall (W–H) plotting was used to study the microstrain of β phases. The results showed that the microstrain of β phases increased rapidly within 4% plastic strain and reached the maximum at plastic strain of ~6.5%. Since the β phases acted as hard phases, the microstrain was considered as a sign of the stress concentration near phase interfaces. It was also suggested that the effective release of local stress concentration at the β/α-Mg interface benefited the ductility of the WE alloy by the plastic deformation of β phases and phase interface sliding.

36 MATERIALS SCIENCE↗

Exploring the Microstructure-Property Relationship of Mg-Al-Mn alloys enhanced via Friction Stir Processing

Friction Stir Processing (FSP) is a solid-state thermomechanical processing technique that enables local grain refinement, densification, and homogenization of microstructure in metallic components. Here, FSP is applied to thin sheets of high-pressure die cast AM60 to address the porosity and heterogeneities inherent to the casting process. In this work, microstructure characterization is correlated to improvements in the static mechanical properties of the Mg-Al-Mn alloy system at various FSP processing conditions. Notably, there is a significant increase in the ductility and ultimate tensile stress of system following FSP. The dominant deformation mechanisms for the as-cast material and the FSP material are investigated. Finally, the fatigue life improvement is correlated to microstructure modifications that may lead to distinct behavior in crack initiation and crack propagation for the as-cast and FSP material.

Garcia, David↗

Method for Evaluating Irradiation Effects on Flow Stress in Fe-9%Cr ODS Using TEM In Situ Cantilevers

Transmission electron microscopic (TEM) in situ mechanical testing has become a widely utilized tool for simultaneously measuring mechanical properties and understanding fundamental deformation mechanisms in irradiated and nuclear materials. Although tensile and compression specimen geometries are amongst the most common, opportunities remain for investigating alternative geometries that could provide unique insights into the plasticity of irradiated materials. This research demonstrates a new TEM in situ cantilever beam configuration. Cantilevers are produced from as-received and proton irradiated (1 dpa, 500°C) Fe-9%Cr oxide dispersion strengthened (ODS) steel. Flow stress is measured using a TEM in situ depth-sensing mechanical testing holder. A 200 MPa increase in flow stress is measured due to irradiation. Size effects arise when the intrinsic (i.e. microstructural) size approaches the extrinsic (i.e. external dimensions) size and can be described using a power law relationship as a function of the material microstructure and cantilever dimensions.

36 MATERIALS SCIENCE↗

Effect of thickness on degradation of austenitic 347H steel by direct-fired supercritical CO 2 power cycle environment

Austenitic 347H steel of two thicknesses (2.54 and 0.6 mm) was exposed to a simulated direct-fired supercritical CO 2 (sCO 2 ) power cycle environment at 650°C and 1 atm for 1000 h then tensile stressed at room temperature to study the deformation behavior. The thicker 347H formed a protective chromia scale over most of the surface, which minimized carburization of the underlying steel and resulted in no change in mechanical performance. In stark contrast, the thinner 347H formed non-protective Fe-rich oxides over the entire surface, resulting in extensive carburization of the underlying steel. Finally, this led to increased strength but significantly reduced ductility, resulting in partially brittle failure

36 MATERIALS SCIENCE↗

Process control-enabled mitigation of microstructural and plastic heterogeneities in additively manufactured Grade 91 steel

Synergizing wire arc-directed energy deposition (WA-DED) additive manufacturing (AM) with particle-strengthened creep strength-enhanced ferritic (CSEF) steels enables fabrication and repair of critical power-plant components. Investigations focused on fusion-welded particle-strengthened CSEF steels, such as Grade 91 steel, have linked microstructurally heterogeneous regions—forming due to heat affected zones (HAZ)—with premature failure during elevated temperature service. Fusion-based AM, including WA-DED, likewise generates microstructurally and plastically heterogeneous regions due to spatiotemporally varying thermokinetics during deposition. However, works investigating such microstructural heterogeneities, their implications for mechanical behavior, and strategies to mitigate their formation remain scarce. This work identifies microstructurally and plastically heterogeneous regions within the WA-DED-processed Grade 91 steel. Spatial microhardness variations in the as-fabricated specimen correlate with the variation in the attributes of grain, martensitic microstructure, and precipitates across the fusion zone and HAZ. Digital image correlation-enabled tensile tests performed at 500 °C revealed pronounced deformation localization and a wave-like strain distribution, with wavelength close to the melt pool depth, indicating susceptibility of the as-fabricated components to premature creep failure. Such heterogeneity in microstructural and mechanical behavior was attributed to recurring solid-state phase transformations. Subsequently, an interlayer temperature control strategy was implemented, wherein maintaining interlayer temperature above the martensitic start temperature mitigated the heterogeneous microstructural and plastic response in the as-fabricated condition. Findings open pathways to achieving deformation-localization- and creep-resistant microstructures in WA-DED fabricated particle-strengthened CSEF steel components, reducing reliance on post-welding heat treatments—conventionally required to enhance creep resistance—and enabling on-demand, short lead-time fabrication of next-generation power-plant components.

Heat affected zones↗

Ductile Glassy Polymer Networks Capable of Large Plastic Deformation and Heat-Induced Elastic Recovery

Many thermoplastic polymers are ductile by combining strength and large deformations. These deformations are irreversible - known as plastic deformation. Elastomers can deform reversibly but have low strength. To this end, we developed glassy and ductile polyamide networks capable of large plastic deformation (>200% strain) and high strength (~50 MPa tensile strength and ~1500 MPa Young’s modulus), similar to those of polyolefins and Nylon-66. We discovered that hydrogen bonding between meta-phthalamide groups was essential to the ductility. Since these polyamide networks are covalently bonded, we demonstrated their unique durability by repeatable elastic recovery at elevated temperatures, exhibiting indifferent tensile properties in each cycle. Furthermore, when we fixed the strain during the elastic recovery, these polyamide networks actuated stresses of 9–18 MPa, among the highest reported in shape-memory polymer actuators. Here, we envision these ductile, glassy polymer networks as promising alternatives to ductile thermoplastics, given the combined benefit of ductility and durability.

36 MATERIALS SCIENCE↗

Prediction of strain, inter-layer interaction and critical current in CORC ® wires under axial strain by T-A modeling

Superconducting conductors on round core (CORC ® ) cables and wires can meet the needs of large high-field magnets, such as particle accelerators and compact nuclear fusion machines, due to their simple cabling process, high current-carrying capacity and reliable operation under high mechanical stresses. Many high-field magnets require CORC ® cables to carry a current of thousands of amperes in a background magnetic field exceeding 20 T. As a result, the large electromagnetic forces will deform the cable in the axial direction due to hoop stress and in the transverse direction by compressive stress. Therefore, it is essential to determine the irreversible deformation limit of the CORC ® cable under axial tensile load and optimize the cabling parameters to potentially extend this limit. Analytical and numerical methods are developed to assess the performance degradation of CORC ® wires under axial tensile load. The strain level, interlayer contact pressure and friction and their impact on the critical current are calculated by combining the mechanical response and the T-A method. Analyzing the results shows that the winding angle of the tape and the Poisson’s ratio of the inner core are key factors affecting the irreversible tensile strain limit of CORC ® wires. The smaller the winding angle and the higher the Poisson’s ratio of the inner core, the higher the irreversible tensile strain limit. For multi-layer CORC ® wires, the initial contact pressure caused by the cabling process must also be considered. The inter-layer interaction is coupled with the tape strain of each layer. The results of this research can serve as a basis for optimizing and designing CORC ® wires with extended irreversible strain limits.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Community Data Contribution to M.E.T.A. with ATF-relevant Hydrided Zr cladding (Coated and Uncoated)

Since the aftermath of the Fukushima Daiichi loss-of-coolant accident, accident-tolerant fuel (ATF) claddings have been developed to improve the coping times in such events. However, the mechanical performance of ATF cladding is crucial in ensuring that it does not negatively impact the mechanical integrity during all other stages of the nuclear fuel cycle, and the validity of the existing safe operating margins must be verified. However, due to the cladding’s tube geometry and textured anisotropy, determination of apparent mechanical properties under certain deformation paths is challenging. In the uniaxial hoop direction, for instance, the measured mechanical stresses include frictional forces caused by loading mandrels or varying deformation paths in the sample during traditional ring tensile testing. This experimental difficulty is exacerbated by the specimen size. However, addressing these challenges enables irradiation separate-effects investigations in which the materials can be inserted in reactors like the High Flux Isotope Reactor, and reducing the material consumption of commercially irradiated material allows for further post-irradiation examinations. Despite the advantages of reduced-scale mechanical testing, any drawbacks from new specimen geometries must be evaluated, and uncertainties from specimen preparation, setup, and analysis methodologies must be understood.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Direct observation of strain-enhanced hydrogen segregation and failure at high-angle grain boundaries in nickel

Understanding the mechanisms underlying hydrogen embrittlement remains difficult, even in single-element metals. Both microstructure and stress state influence hydrogen distribution in metals and alloys, which impacts deformation and failure. Here, in this work, we use in-situ Kelvin probe force microscopy (KPFM) to monitor the hydrogen distribution in pure nickel over time at 1.1 % and 3.5 % strain. The sample strained to 3.5 % results in preferential hydrogen segregation to high-angle grain boundaries whereas the sample strained to 1.1 % does not exhibit preferential hydrogen segregation. Optical digital image correlation (DIC) shows that hydrogen charging results in both localized and reduced strains during tensile testing of a notched sample. Later stages of deformation and failure (e.g. microcracking) are studied by using in-situ transmission X-ray microscopy (TXM). TXM reveals nanoscale structural changes to a propagating crack in a hydrogen environment. Localized void growth and secondary cracking occur at grain boundaries near the primary crack front. Correlative electron backscattering diffraction (EBSD) is used to relate the cracking at grain boundaries to the hydrogen segregation observed in KPFM. These findings are unified in a proposed hydrogen embrittlement mechanism that describes the interaction of hydrogen with grain boundaries, and the role of grain boundaries in hydrogen embrittlement.

Grain boundary fracture↗

In-situ high energy X-ray diffraction study of deformation behavior in Nb nanoparticle-martensitic NiTi composite wire

Here, this study investigated the deformation behavior in Nb nanoparticle-martensitic NiTi composite wire during tensile loading by means of in-situ high-energy X-ray diffraction. Compared to Nb nanowires, the dispersedly distributed Nb nanoparticles have little effect on the transformation and deformation behaviors of NiTi matrix, causing the absence of R phase transformation and the occurrence of deformation twinning in NiTi matrix. Meanwhile, the occurrence of deformation twinning in NiTi matrix can reduce the shape strain to be coordinated by the unfavorable orientated martensite variants, and thus decreases the internal stress among NiTi martensite variants generated during martensite reorientation process. In addition, TEM result proved that Nb nanoparticles can achieve exceptionally large elastic strain in B19'-NiTi matrix (~4%), just as Nb nanowires. However, this large elastic strain (stress) will be released with the occurrence of NiTi deformation twinning.

36 MATERIALS SCIENCE↗

Plastic anisotropy and tension-compression asymmetry in nanotwinned Al–Fe alloys: An in-situ micromechanical investigation

The mechanical strength of commercial Al alloys rarely exceeds 700 MP. Recent studies show that nanotwinned Al alloys and other nanocolumnar metals exhibit superb mechanical behaviors but a discrepancy between tensile and hardness measurements often emerges and their orientation dependent deformation mechanisms remain unclear. Here, we inspect the mechanical response of columnar nanotwinned Al–Fe alloys with emphasis on response of grain boundaries to in-situ tension and compression tests along both in-plane and out-of-plane directions inside a scanning electron microscope. Our studies reveal ultra-high out-of-plane tensile and compressive stress, exceeding 1.8 GPa, and an in-plane tensile and compressive stress of 1.1 and 1.6 GPa, respectively. Post-mortem TEM analyses were performed to elucidate the orientation-dependent plastic anisotropy and tension-compression asymmetry in columnar nanotwinned Al–Fe alloys. This study provides an important forward step towards the understanding of deformation mechanisms in high-strength nanotwinned Al alloys and metals with nanocolumnar or non-equiaxed grains.

36 MATERIALS SCIENCE↗

Effect of local structure and stoichiometry on the dynamic behavior of bi-metal interfaces

Molecular dynamics (MD) simulations are performed to investigate the failure behavior of Al/Al, Al/Fe, and Al/AlFe bi-layers under high strain-rate shock loading. Additional simulations are performed to invesigate solely the tensile response of these systems and to isolate the effects of loading history on damage and failure. Specifically, the compression stage of the shock is excluded from the tensile simulations. This study shows that local structure variation, including the introduction of serrations, plays different roles in controlling damage nucleation depending on the specific loading condition. Under shock loading, the stress for void nucleation and the resulting void distribution is insensitive to an interface structure, whereas under pure tensile loading, the opposite is true, even though the strain rate is comparable. The above difference can be explained based on the corresponding change in the total deformation prior to damage nucleation under shock loading, which is missing from the pure tensile loading. Therefore, it is concluded that whether local interface structure matters under high strain-rate loading depends on the specific loading history and the stress state: the local structure variation matters only when it alters the deformation behavior, and subsequently, damage nucleation and evolution.

36 MATERIALS SCIENCE↗

Model for the Softening Factor within Stages of Work Hardening

A formulation for a dimensionless coefficient c b is derived that represents a scale of microstructural softening for alloys which follow Kocks-Mecking (K-M) work hardening behavior. The variation of the true plastic strain ε p between the proportional limit σ y and the strength σ u at the instability is determined using the Considère criterion. Parameterization of the model is limited to variables expressly measured within tensile experiments. Further development is now made for the softening factor c bi through the individual and sequential stages 3 and 4 of plastic deformation during K-M work hardening Q behavior. Application is shown for tensile test results of Ti-6Al-4V made by different additively manufactured (AM) processes. It is found that the variation in plastic strain as a function of c bi produces a continuous curve representative of the alloy system. The results of data analysis indicate that Θ o3 and c b3 increase, while Θ o4 and c b4 decrease, as the total plastic strain ε p increases. Furthermore, formulations derived for K-M stages 3 and 4 enable the evaluation of other material parameters such as the activation volume ν* for the onset of plastic deformation. This activation volume is found to be near constant, at a ν*-value of 0.353±0.036 nm 3 as computed using a strain-rate sensitivity of strength exponent m of 0.014, irrespective of the AM method used to produce the Ti-6Al-4V alloy.

36 MATERIALS SCIENCE↗

Isotropic seismic radiation from rock damage and dilatancy

SUMMARY We present semi-analytical and numerical results on isotropic radiation expected to be generated by seismic sources with damaged dilatant materials that sustain during failure an overall shear deformation. The results are derived for inclusions with different stiffness components, including those responsible for shear-volumetric coupling in dilatant material, and different geometries, in a surrounding elastic solid. The obtained relations indicate that the isotropic seismic potency and seismic moment components are proportional to the shear potency components multiplied by the aspect ratio between the thickness and length of the source zone. For a typical rupture zone with a thin tabular geometry, the expected small aspect ratio explains the general seismological observations of small isotropic radiation. However, isotropic radiation induced by dynamic dilation for short and thick sources is more pronounced and may reach for spherical sources sustaining shear deformation 18 per cent of the shear components. Sources that include also tensile components and explosions can produce larger isotropic radiation. The results provide rigorous relations that can be used to estimate different source properties in numerical simulations, experiments and field studies.

Geochemistry & Geophysics↗

Understanding the asymmetric orientations and stress states in polycrystalline NiTi SMA by in-situ synchrotron-based high-energy X-ray diffraction

The stress-induced martensite transformations (SIMTs) dramatically affect the recoverable strain and mechanical response of polycrystalline NiTi. An in-depth understanding of the propagation manner and orientation preference of SIMTs is therefore crucial. Here, in this work, we present a unique asymmetric anisotropy of SIMTs and lattice strains induced by Lüders-type deformation in polycrystalline NiTi, achieved through a combination of in-situ synchrotron X-ray diffraction and uniaxial tensile loading and unloading experiments. Our experimental findings reveal that in polycrystalline NiTi under uniaxial deformation, the asymmetry of SIMTs is attributed to the inhomogeneous strain field caused by the Lüders-type mechanism. The asymmetrical SIMT starts with the forward Lüder band and disappears along with the backward Lüder band. The austenite with the favored orientation of $\langle$110$\rangle$ A //loading direction (LD) transformed and recovered back at a higher rate compared to other orientations during both loading and unloading.

36 MATERIALS SCIENCE↗