Search NASA⌕ Search

SEARCH · Search NASA

Results for “dislocation density”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 1,387 records · Page 77

Heavy ion irradiation response of an additively manufactured 316LN stainless steel

Additive manufacturing has become an appealing technique to fabricate three-dimensional metallic materials and components for nuclear reactors. However, response of additively manufactured alloys to high-dose heavy ion irradiations at elevated temperatures is still not well understood. Here, an additively manufactured 316LN austenitic stainless steel with high-density solidification cells was irradiated using 3.5 MeV Fe ion to a peak dose of 220 dpa at 450 °C. Microscopy studies show a lower Frank loop density and smaller size in the additively manufactured sample compared with its cold worked counterpart, and the cellular structures may largely suppress the formation of perfect loops and dislocation networks and reduce the magnitude of solute segregations comparing with high angle grain boundaries. In conclusion, the present work advances the understanding on the high-temperature irradiation response of additively manufactured steels for nuclear reactor applications.

36 MATERIALS SCIENCE↗

Influence of a TiO{sub 2} buffer layer on the magnetic properties of anatase Co:TiO{sub 2} thin films

Our study addresses the influence of a TiO{sub 2} buffer layer on the morphological, structural, and magnetic properties of Co:TiO{sub 2} films grown on (001) SrTiO{sub 3} substrates by RF sputtering. We demonstrate that a direct correlation exist between the morphology, the Co heterogeneity, and the magnetic properties measured in the films. Correlated analysis by cross section transmission electron microscopy, energy dispersive x-ray, and x-ray photoemission spectroscopy reveals that the Co is not uniformly distributed in the film but concentrated in the surface clusters. Atomic force microscopy analysis illustrates that the unbuffered films present a large density of surface clusters. These clusters are not metallic Co but Co rich TiO{sub 2} anatase phase and they are accompanied by structural defects in the film: dislocations, small angle grain boundaries. Magnetometry analysis shows that the unbuffered films have a net ferromagnetic behavior, while in the buffered ones the ferromagnetism is quenched. Therefore, we conclude that the magnetism in unbuffered samples is related to the surface clusters and seems to have an extrinsic nature.

36 MATERIALS SCIENCE↗

Semicoherent oxide heterointerfaces: Structure, properties, and implications

In the quest for enhanced functionality of all sorts, nanostructured materials are becoming ever more common. This is particularly true of oxide/oxide heterostructures in which the high density of interfaces has been implicated in enhanced properties and used to engineer strain in oxide composite structures. These interfaces are often characterized by a network of misfit dislocations that relieve the lattice mismatch strain between the two materials, and these dislocations themselves are often suggested as the source of either enhancements or degradation of properties. Despite the importance and pervasiveness of misfit dislocations, however, there is still much that is unknown about their structure and properties, particularly in oxide/oxide heterostructures. Here, we give a perspective on the importance of these dislocation networks and the need to interrogate their impact on functionality.

36 MATERIALS SCIENCE↗

In x Ga 1- x As Nanowires on Silicon: One-Dimensional Heterogeneous Epitaxy, Bandgap Engineering, and Photovoltaics

We report on the one-dimensional (1D) heteroepitaxial growth of In x Ga 1-x As (x = 0.2–1) nanowires (NWs) on silicon (Si) substrates over almost the entire composition range using metalorganic chemical vapor deposition (MOCVD) without catalysts or masks. The epitaxial growth takes place spontaneously producing uniform, nontapered, high aspect ratio NW arrays with a density exceeding 1 × 10 8 /cm 2 . NW diameter (~30–250 nm) is inversely proportional to the lattice mismatch between In x Ga 1-x As and Si (~4–11%), and can be further tuned by MOCVD growth condition. Remarkably, no dislocations have been found in all composition In x Ga 1-x As NWs, even though massive stacking faults and twin planes are present. Indium rich NWs show more zinc-blende and Ga-rich NWs exhibit dominantly wurtzite polytype, as confirmed by scanning transmission electron microscopy (STEM) and photoluminescence spectra. Solar cells fabricated using an n-type In 0.3 Ga 0.7 As NW array on a p-type Si(111) substrate with a ~ 2.2% area coverage, operates at an open circuit voltage, V oc , and a short circuit current density, J sc , of 0.37 V and 12.9 mA/cm 2 , respectively. Furthermore, this work represents the first systematic report on direct 1D heteroepitaxy of ternary In x Ga 1-x As NWs on silicon substrate in a wide composition/bandgap range that can be used for wafer-scale monolithic heterogeneous integration for high performance photovoltaics.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Helium effects on microstructural evolution in tempered martensitic steels: In situ helium implanter studies in HFIR

Microstructural evolutions in tempered martensitic steels (TMS) under neutron-irradiation, at fusion relevant He/dpa ratios and dpa rates, were characterized using a novel in situ He-implanter technique. F82H-mod3 was irradiated at 500 C in HFIR to a nominal 9 dpa and 190 or 380 appm He in both in the as-tempered (AT) and 20% cold-worked (CW) conditions. In all cases, a high number density of 1-2 nm He-bubbles were observed, along with fewer but larger 10 nm void-like faceted cavities. The He-bubbles form preferentially on dislocations and various interfaces. A slightly larger number of smaller He bubbles were observed in the CW condition. The lower He/dpa ratio produced slightly smaller and fewer He-bubbles. Comparisons of these observations to the results in nano-structured ferritic alloy (NFA) MA957 provide additional evidence that TMS may be susceptible to He-embrittlement as well as void swelling at fusion relevant He concentrations, while NFA are much more resistant to these degradation phenomena.

36 MATERIALS SCIENCE↗

Property Improvement in CZT via Modeling and Processing Innovations . Te-particles in vertical gradient freeze CZT: Size and Spatial Distributions and Constitutional Supercooling

A section of a vertical gradient freeze CZT boule approximately 2100-mm 3 with a planar area of 300-mm 2 was prepared and examined using transmitted IR microscopy at various magnifications to determine the three-dimensional spatial and size distributions of Te-particles over large longitudinal and radial length scales. The boule section was approximately 50-mm wide by 60-mm in length by 7-mm thick and was doubly polished for TIR work. Te-particles were imaged through the thickness using extended focal imaging to locate the particles in thickness planes spaced 15-µm apart and then in plane of the image using xy-coordinates of the particle center of mass so that a true three dimensional particle map was assembled for a 1-mm by 45-mm longitudinal strip and for a 1-mm by 50-mm radial strip. Te-particle density distributions were determined as a function of longitudinal and radial positions in these strips, and treating the particles as vertices of a network created a 3D image of the particle spatial distribution. Te-particles exhibited a multi-modal log-normal size density distribution that indicated a slight preference for increasing size with longitudinal growth time, while showing a pronounced cellular network structure throughout the boule that can be correlated to dislocation network sizes in CZT. Higher magnification images revealed a typical Rayleigh-instability pearl string morphology with large and small satellite droplets. This study includes solidification experiments in small crucibles of 30:70 mixtures of Cd:Te to reduce the melting point below 1273 K (1000°C). These solidification experiments were performed over a wide range of cooling rates and clearly demonstrated a growth instability with Te-particle capture that is suggested to be responsible for one of the peaks in the size distribution using size discrimination visualization. The results are discussed with regard to a manifold Te-particle genesis history as 1) Te-particle direct capture from melt-solid growth instabilities, 2) Te-particle formation from dislocation core diffusion and the formation and breakup of Te-tubes, and 3) Te-particle formation due to classical nucleation and growth as precipitates.

36 MATERIALS SCIENCE↗

Lower Length Scale Characterization and Validation of Formation and Stability of Helium Bubbles in Nano-structured Ferritic Alloys under Irradiation

In order to extend the operating license of current light water reactors (LWRs) in the United States and other countries to as many as 80 years or longer, it is demanding to identify potential materials for many of the internal structural components and fasteners. We proposed that 14YWT iron alloy can be adopted in such applications with its excellent material properties, such as high-temperature strength, low creep rate, and high irradiation resistance. Application with 14YWT would improve the void/helium swelling characteristics of the LWR fuels, extend the burn-up limits with the tolerant temperature up to 800oC and reduce the hydrogen production. One key feature of 14YWT material property enhancement is the ultrafine high density of 2-4nm Y-Ti-O enriched nanoclusters (NCs) within the 14YWT iron matrix. The NCs can effectively pin the ultra-fine grain boundaries and dislocations, which significantly enhance mechanical properties of the alloy. Moreover, these nanoclusters remain stable with no coarsening after a large dose of ion irradiation. After ion irradiation, the helium bubbles are observed extremely uniform in size (1nm) and quite homogeneously distributed within the 14YWT matrix, which indicates that the microstructure of 14YWT remains remarkably tolerance to radiation damage. However, there is a lack of understanding of 14YWT both theoretically and experimentally in order to understand the mechanism behind the material property enhancement and to further develop and design a new generation of advanced structural material for current LWR applications and future fusion applications.

36 MATERIALS SCIENCE↗

Cross slip of extended dislocations in face-centered cubic metals through phase-field modeling

Cross slip is a dislocation mechanism that significantly impacts the mechanical behavior of engineering alloys. Here, in this work, we advance a 3D phase-field dislocation dynamics (PFDD) mesoscale technique to simulate cross slip across a broad range of face-centered cubic (FCC) metals. The formulation incorporates elastic anisotropy, an FCC numerical grid, and a high-fidelity representation of the entire γ -surface from density functional theory for eight FCC metals and no adjustable parameters or rules. The relaxed core structures under zero stress for all metals are predicted to extend in plane. The analytical model for stacking fault width agrees well with the PFDD result under the assumption of elastic isotropy but overestimates it under elastic anisotropy, when the degree of anisotropy is large. The dynamic simulations are designed to elucidate the material parameters that influence the propensity for cross slip. Whether cross slip occurs under a non-Schmid stress or to bypass a hard obstacle, the critical stress to cross slip scales strongly with the anisotropic energy coefficient for a screw dislocation.

36 MATERIALS SCIENCE↗

A new self-adaptive reconstruction method to identify defects through Wigner–Seitz approach

A new self-adaptive reconstruction method based on local atomic structure at any given molecular dynamics (MD) step has been developed in this article. The method can be used in Wigner–Seitz defect analysis approach to correctly and efficiently explore the information of both point defects and complex defect clusters (e.g. dislocation loops and voids) formed after a displacement cascade where the cascade interacts with grain boundaries and/or dislocations. The algorithm and validation are provided in detail. Results for identification of radiation defects during and after cascades interacting with a dislocation network show that the new method can well recognize all simple and complex defects and defect clusters. Thus, this new method provides a totally new way to explore the density and size of radiation defects at atomic scale after complex MD evolution processes, providing correct information to understand and predict radiation damage in materials through atomic simulations.

72 PHYSICS OF ELEMENTARY PARTICLES AND FIELDS↗

Atomic-scale mechanisms of helium bubble hardening in iron

Generation of helium due to (n,α) transmutation reactions changes the response of structural materials to neutron irradiation. The whole process of radiation damage evolution is affected by He accumulation and leads to significant changes in the material s properties. A population of nanometric He-filled bubbles affects mechanical properties and the impact can be quite significant because of their high density. Understanding how these basic mechanisms affect mechanical properties is necessary for predicting radiation effects. In this paper we present an extensive study of the interactions between a moving edge dislocation and bubbles using atomic-scale modeling. We focus on the effect of He bubble size and He concentration inside bubbles. Thus, we found that ability of bubbles to act as an obstacle to dislocation motion is close to that of voids when the He-to-vacancy ratio is in the range from 0 to 1. A few simulations made at higher He contents demonstrated that the interaction mechanism is changed for over-pressurized bubbles and they become weaker obstacles. The results are discussed in light of post-irradiation materials testing.

36 MATERIALS SCIENCE↗

Planarization of p -GaN surfaces on MOCVD grown V-defect engineered GaN-based LEDs

The large polarization barriers between the quantum wells and quantum barriers in long-wavelength GaN-based light-emitting diodes (LEDs) inhibit their performance by requiring excess driving voltages to reach standard operating current densities. Lateral injection of carriers directly into quantum wells is required to circumvent this issue. V-defects are naturally occurring inverted hexagonal defects with semipolar {$10\bar{1}1$}-plane sidewalls generated on surface depressions from threading dislocations. LEDs engineered to intentionally generate V-defects below the active region of the LED can achieve lateral carrier injection through the V-defect sidewalls and have already been able to demonstrate world record wall-plug efficiencies for LEDs in the green-red wavelengths. V-defects can be enlarged during kinetically limited growth where the growth rate of the c-plane GaN is faster than that of their sidewalls, leaving them unfilled. We report on the metal organic chemical vapor deposition growth conditions required to fill in V-defects with p-GaN during epitaxial growth of the LED post the active region. Circular transmission length measurements of Pd/Au contacts processed on p-GaN surfaces with various amounts of unfilled V-defects showed no significant difference in their sheet resistance and specific contact resistance. J–V measurements of LEDs grown with varying unfilled V-defect densities showed no significant difference in the forward bias regime. However, in the reverse bias regime, catastrophic breakdown occurred at markedly lower voltages for samples with larger unfilled V-defect densities. This suggests that unfilled V-defects may act as hotspots for device failure, and planarizing LED surfaces may help prevent early degradation of LED devices.

Chemical vapor deposition↗

Nanoscale conditions for ductile void nucleation in copper: vacancy condensation and the growth-limited microstructural state

Ductile rupture or tearing usually involves structural degradation from the nucleation and growth of voids and their coalescence into cracks. Although some materials contain preexisting pores, the first step in failure is often the formation of voids. Because this step can govern both the failure strain and the fracture mechanism, it is critical to understand the mechanisms of void nucleation and the enabling microstructural configurations which give rise to nucleation. To understand the role of dislocations during void nucleation, the present study presents ex-situ cross-sectional observations of interrupted deformation experiments revealing incipient, subsurface voids in a copper material containing copper oxide inclusions. The local microstructural state was evaluated using electron backscatter diffraction (EBSD), electron channeling contrast (ECC), transmission electron microscopy (TEM), and transmission kikuchi diffraction (TKD). Surprisingly, before substantial growth and coalescence had occurred, the deformation process had resulted in the nucleation of a high density of nanoscale (≈50 μm) voids in the deeply deformed neck region where strains were on the order of 1.5. Such a proliferation of nucleation sites immediately suggests that the rupture process is limited by void growth, not nucleation. With regard to void growth, analysis of more than 20 microscale voids suggests that dislocation boundaries facilitate the growth process. The present observations call into question prior assumptions on the role of dislocation pile-ups and provide new context for the formulation of revised ductile rupture models. While the focus of this study is on damage accumulation in a highly ductile metal containing small, well-dispersed particles, these results are also applicable to understanding void nucleation in engineering alloys.

36 MATERIALS SCIENCE↗

Heavy boron doping effects on biaxially tensile strained germanium (>1.5%) investigated via structural characterization, effective lifetime assessment and atomistic modeling

Highly tensile strained germanium (ε-Ge) represents an essential material system for emerging electronic and photonics applications. Moreover, adjusting the doping levels to moderate or high concentrations can effectively tailor the properties of ε-Ge for specific applications. This article combines experimental characterization with a theoretical framework to examine the effects of heavy elemental boron (B) doping on pseudomorphic sub-50 nm ε-Ge. High resolution X-ray diffractometry is used to validate tensile strain levels of 1.53% and 1.68% in Ge epilayers, surpassing the indirect-to-direct band gap crossover point at ∼1.5% biaxial tensile strain. Cross-sectional transmission electron microscopy revealed visual evidence of stacking faults and surface roughening in 1.68% ε-Ge, although a coherent and abrupt Ge/III–V heterointerface is observed, devoid of interfacial misfit dislocations. Effective lifetime measurements demonstrated approximately twofold enhancement in 1.53% B-doped ε-Ge (N B ∼7 × 10 19 cm −3 ) compared to its unstrained B-doped counterpart, while no such improvement was observed in 1.68% B-doped ε-Ge. This lack of enhancement is attributed to the presence of stacking faults and surface roughness within the ε-Ge epilayer. Through density functional theory calculations, we independently demonstrate that substitutional B atoms induce local deformation of Ge–Ge bonds in both unstrained Ge and ε-Ge epilayers, resulting in an additive tensile strain. This phenomenon could potentially lead to dynamic reduction and overcoming of the critical layer thickness for the system, facilitating the nucleation and subsequent glide of 90° leading Shockley partial dislocations, thereby generating stacking faults. In essence, these findings establish an upper limit on the B-doping concentration that can be achieved in highly ε-Ge epilayers, and collectively, offer valuable insights into the significance of heavy doping in Ge-based heterostructures. As such, this study delineates a fundamental constraint for integrating heavily doped ε-Ge in high-performance optoelectronic systems, necessitating precise strain-doping co-optimization to avoid performance degradation.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Radiation response of a Fe–20Cr–25Ni austenitic stainless steel under Fe 2+ irradiation at 500 °C

The radiation response of a Fe–20Cr–25Ni austenitic stainless steel under self-ion irradiation at 500 °C was systematically investigated. The steel was irradiated at 500 °C by 3.5 MeV Fe 2+ ions to 10, 50, and 150 peak dpa, respectively. In the 200–400 nm depth region, radiation-induced Frank loops were relatively stable in both size and number density from 10 to 150 peak dpa. Anisotropic distribution of Frank loops was observed in the 50 and 150 peak dpa specimens, possibly due to interaction of Frank loops and network dislocations with preferred orientations. Coarse voids were found only in the 50 and 150 peak dpa specimens in depths less than 750 nm, suggesting that injected interstitials at deeper regions suppressed the void nucleation. The peak swelling was very low (~0.4%) for both 50 and 150 peak dpa irradiation. Radiation also led to the formation of intragranular plate-like Cr-rich carbides. Radiation-induced segregation of Ni and Si was found at various sinks: dislocation loops, void surfaces, and carbide-matrix interfaces. Finally, irradiation hardening was measured by nanoindentation and the results are consistent with microstructure-based calculations using the dispersed barrier hardening model. The major contributor to irradiation hardening changed from Frank loops at the lowest dose to network dislocations at the highest dose.

dislocation loops↗

Using electron channeling contrast imaging to inform and improve the growth of high-efficiency GaAs solar cells on nanopatterned GaAs substrates

Patterned substrates provide opportunities for reducing the cost of high-efficiency III-V devices by incorporating mechanically weak layers beneficial for substrate reuse (e.g. by spalling). In this work, the functionality of electron channeling contrast imaging (ECCI) as a tool to efficiently understand and mitigate defect formation is exemplified by developing a process in which high-quality III-V material can be grown on nanopatterned GaAs substrates. Reactive ion etching used in the patterning process was found to damage the GaAs substrate surface, leading to the formation of stacking faults in the epitaxial material as observed by ECCI. Etching the patterned substrates in a 1 NH4OH: 1 H2O2: 50 DI H2O solution for 10 s prior to growth removed the substrate surface damage and stacking faults were no longer present. Growth of solar cell device structures initially produced samples with many macroscale flaws creating shunts in the devices, which complicated the assessment of material quality by device measurements. However, ECCI revealed that the epitaxial material surrounding macroscale flaws was free from any crystallographic defects such as stacking faults and threading dislocations. With this knowledge, we focused on refining the patterning process to eliminate the macroscale flaws. Solar cells were then grown on the improved nanopatterned substrates and exhibited device structures with defect densities less than 5 x 105 cm -2 and average conversion efficiency of 24.8%, nearly identical to devices grown on unpatterned epi-ready substrates (25.0%).

14 SOLAR ENERGY↗

Investigation of GaN-on-GaN vertical p - n diode with regrown p -GaN by metalorganic chemical vapor deposition

Here, to mimic selective-area doping, p -GaN was regrown on an etched GaN surface on GaN substrates by metalorganic chemical vapor deposition. Vertical GaN-on-GaN p - n diodes were fabricated to investigate the effects of the etch-then-regrowth process on device performance. The crystal quality of the sample after each epitaxial step was characterized by X-ray diffraction, where the etch-then-regrowth process led to a very slight increase in edge dislocations. A regrowth interfacial layer was clearly shown by transmission electron microscopy. Strong electroluminescence was observed with three emission peaks at 2.2 eV, 2.8 eV and 3.0 eV, respectively. The forward current density increased slightly with the increasing temperature, while the reverse current density was almost temperature independent indicating tunneling as the reverse transport mechanism. This result is very similar to the reported Zener tunnel diode comprising a high doping profile at the junction interface. High levels of silicon and oxygen concentrations were observed at the regrowth interface with a distribution width of ~100 nm. This work provides valuable information of p -GaN regrowth and regrown GaN p - n diodes, which can serve as an important reference for developing selective doping for advanced GaN power electronics for high voltage and high power applications.

42 ENGINEERING↗

Effective pair potential for random fcc CoCrFeMnNi alloys

The single-phase equiatomic CoCrFeMnNi alloy is a random solid solution of five elements on the face-centered cubic lattice, whose pure constituents crystallize in very different structures and exhibit diverse magnetic properties. Due to the randomness of the alloy, 80% of nearest neighbor bonds are between unlike elements and thus the details of bonding in pure structures are less important. The elastic moduli of this alloy give rise to small Cauchy pressure C 12 - C 44 , which suggests that the dominant part of bonding may be described by a simple pair potential. We test this hypothesis by developing a long-range Lennard-Jones potential in which the equilibrium crystal structures of pure constituents are taken as reference. The standard mixing rules for regular solutions are then adopted to obtain parameters for bonds between unlike elements in the quinary system. The transferability of this potential to quaternary CoCrFeNi, ternary CoCrNi, and binary FeNi alloys is investigated and the predictions compared with experiments and density functional theory calculations. By sampling over a large number of random configurations, we investigate the effect of compositional randomness on misfit volumes, energies of point defects and stacking faults, and the dislocation friction stresses experienced by moving edge and screw dislocations.

Materials Science↗