Search NASA⌕ Search

SEARCH · Search NASA

Results for “Hydrogen Degradation”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 145 records · Page 8

Effects of Surface Treatments on Secondary Electron Emission from CVD Diamond Films

Secondary electron emission (SEE) properties of polycrystalline diamond films grown by chemical vapor deposition (CVD) were measured. The total secondary yield (sigma) from as-grown samples was observed to be as high as 20 at room temperature and 48 while heating at 700 K in vacuum. Electron-beam-activated, alkali-terminated diamond films have shown stable values of sigma as high as 60 when coated with CsI and similarly high values when coated with other alkali halides. Diamond coated with BaF2 had a stable sigma of 6, but no enhancement of the SEE properties was observed with coatings of Ti or Au. Hydrogen was identified to give rise to this effect in as-grown films. However, electron beam exposure led to a reduction in sigma values as low as 2. Exposure to a molecular hydrogen environment restored sigma to its original value after degradation, and enabled stable secondary emission during electron beam exposure. Atomic hydrogen and hydrogen plasma treatments were performed on diamond/Mo samples in an attempt to increase the near-surface hydrogen concentration which might lead to increased stability in the secondary emission. Raman scattering analysis, scanning electron microscopy, and Auger electron spectroscopy (AES) confirmed that hydrogen plasma and atomic hydrogen treatments improved the quality of the CVD diamond significantly. Elastic recoil detection (ERD) showed that heating as-grown diamond targets to 7OO K, which was correlated with an increase in sigma, removed contaminants from the surface but did not drive hydrogen from the diamond bulk. ERD showed that the hydrogen plasma treatment produced an increase in the hydrogen concentration in the near-surface region which did not decrease while heating in vacuum at 700 K, but no improvement in the SEE properties was observed.

Mearini, G. T.↗

Hydrogenolysis of Poly(Ethylene–co–Vinyl Alcohol) and Related Polymer Blends over Ruthenium Heterogeneous Catalysts

The hydrogenolysis of polymers is emerging as a promising approach to deconstruct plastic waste into valuable chemicals. Yet, the complexity of plastic waste, including multilayer packaging, is a significant barrier to handling realistic waste streams. Herein, we reveal fundamental insights into a new chemical route for transforming a previously unaddressed fraction of plastic waste – poly(ethylene–co­­–vinyl alcohol) (EVOH) and related polymer blends – into alkane products. Additionally, we report that Ru/ZrO2 is active for the concurrent hydrogenolysis, hydrogenation, and hydrodeoxygenation of EVOH and its thermal degradation products into alkanes (C1–C35) and water. Detailed reaction data, product analysis, and catalyst characterization reveal that the in–situ thermal degradation of EVOH forms aromatic intermediates that are detrimental to catalytic activity. Increased hydrogen pressure promotes hydrogenation of these aromatics, preventing catalyst deactivation and improving alkane product yields. Calculated apparent rates of C–C scission reveal that the hydrogenolysis of EVOH is slower than low–density polyethylene. We apply these findings to achieve hydrogenolysis of EVOH/polyethylene blends and elucidate the sensitivity of hydrogenolysis catalysts to such blends. Overall, we demonstrate progress towards efficient catalytic processes for the hydroconversion of waste multilayer film plastic packaging into valuable products.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Performance of 3rd electrode cells in OAO.

The OAO 2 satellite employed nickel-cadmium batteries with auxiliary (signal) electrodes for overcharge control. During the early life of the satellite, these third-electrode signals provided an orbit-by-orbit indication of the overcharge received by the batteries. By ground command, the battery charger was adjusted on a need basis to provide optimum recharge conditions as indicated by the third-electrode signals during all phases of spacecraft operation and orientation. After more than two years, an unusual degradation in third-electrode signals was observed, providing the first indication of battery degradation. The present paper examines the operation of the battery system and analyzes the battery degradation mechanism. The abnormal performance of the third electrode is related to cell-voltage divergence during periods of overcharge. Cells that had a higher cell voltage showed signs (third-electrode degradation) of small amounts of hydrogen gas generation.

Ford, F. E.↗

Thermal performance of gaseous-helium-purged tank-mounted multilayer insulation system during ground-hold and space-hold thermal cycling and exposure to water vapor

An experimental investigation was conducted to determine (1) the ground-hold and space-hold thermal performance of a multilayer insulation (MLI) system mounted on a spherical, liquid-hydrogen propellant tank and (2) the degradation to the space-hold thermal performance of the insulation system that resulted from both thermal cycling and exposure to moisture. The propellant tank had a diameter of 1.39 meters (4.57ft). The MLI consisted of two blankets of insulation; each blanket contained 15 double-aluminized Mylar radiation shields separated by double silk net spacers. Nineteen tests simulating basic cryogenic spacecraft thermal (environmental) conditions were conducted. These tests typically included initial helium purge, liquid-hydrogen fill and ground-hold, ascent, space-hold, and repressurization. No significant degradation of the space-hold thermal performance due to thermal cycling was noted.

Sumner, I. E.↗

NASA Engineering and Safety Center Technical Bulletin No. 21-01: Experimental and Computational Study of Cavitation in Hydrogen Peroxide

Cavitation in liquid propulsion systems can lead to performance degradation and hardware failures. The NESC sponsored an investigation to measure and model cavitation in pressurized hydrogen peroxide fl ow. The experimentally measured and computationally predicted cavitation lengths were compared as a function of cavitation number. The measured and predicted data exhibited close agreement over the range of pressures and temperatures studied, and no calibration of the cavitation model coefficients was needed.

NESC Technical Bulletin No. 21-01↗

On-line Inductively Coupled Plasma Mass Spectrometry Reveals Material Degradation Dynamics of Au and Cu Catalysts during Electrochemical CO 2 Reduction

A significant challenge in commercializing electrochemical CO 2 reduction (CO 2 R) is achieving catalyst durability. Here, in this study, online inductively coupled mass spectrometry (ICP–MS) was used to investigate catalyst degradation via nanoparticle detachment and/or dissolution into metal ions under CO 2 R operating conditions in 0.1 M KHCO 3 . We developed an experimental framework with ex situ characterization to validate the online ICP–MS method for in situ evaluation of degradation from metal foils. By varying the applied potential and microenvironment (CO 2 vs N 2 -saturated electrolyte), we gained insights into the degradation of Au and Cu foils under CO 2 R and hydrogen evolution reaction (HER) conditions. While both Au and Cu foils were observed to be stable to dissolution in these regimes, degradation via nanoparticle detachment from the foil surface at the femtogram scale was observed as a function of reaction conditions, providing new insights into material degradation mechanisms. When applying potential steps at −0.1 and −1.0 V vs the reversible hydrogen electrode (RHE), Au was found to degrade via nanoparticle detachment under CO 2 R operating conditions more than under HER conditions, while Cu was found to degrade via nanoparticle detachment in similar amounts during both reactions. Au lost ∼1.8× more mass and ∼7.5× more nanoparticles than Cu under CO 2 R operating conditions. This study demonstrates the use of online ICP–MS to gain insight into the degradation of Au and Cu, the importance of studying unconventional degradation mechanisms such as nanoparticle detachment, and that online ICP–MS can be further utilized to gain fundamental understanding of catalyst durability for a variety of reaction systems.

Yan, Katherine [Stanford Univ., CA (United States)↗

Coupled diffusion-deformation-damage model for polymers used in hydrogen infrastructure

The soft materials used in the infrastructure of hydrogen storage and distribution systems are vulnerable because exposure to high-pressure hydrogen can lead to mechanical damage and property degradation. Some materials, such as polymers, can undergo mechanical failure due to a phenomenon wherein hydrogen gas diffuses through the polymer chains and occupies preexisting cavities or voids inside the polymer material. If the hydrogen gas pressure is reduced more quickly than hydrogen can diffuse back out of the polymer which is necessary for some applications, the trapped hydrogen gas instead escapes by rupturing the material, causing surface blistering or permanent damage. In this study, a continuum mechanics-based fully coupled diffusion-deformation model with damage is developed to predict the stress distribution and damage propagation while the polymer undergoes rapid decompression failure. The hyperelastic material model, along with the maximum principal strain failure theory, was chosen for this study as it represents the nonlinear material response with brittle failure observed in uniaxial tensile tests perfectly. EPDM polymer was chosen for this study because of its commercial availability and common use in hydrogen storage and distribution system. It has superior mechanical properties, high and low temperature resistance, and certain compounds work well in hydrogen gas. This work is useful for design engineers to alter the parameters while manufacturing polymer composites to increase their performance in a high-pressure hydrogen environment.

Kulkarni, Shank S.↗

The interaction of edge dislocations with hydrogen-helium bubbles in tungsten

In fusion reactors, plasmas-facing components undergo degradation due to displacement damage and injection of gas impurities. Significant amounts of hydrogen (H) and helium (He) impurities can be introduced into materials through plasma exposure and nuclear transmutation, and their synergistic effects lead to the formation of mixed He/H bubbles under irradiation, changing their hardening mechanisms. In this study, molecular dynamics (MD) models were developed to study the interaction between ½<111> edge dislocations with mixed He/H-bubbles in W. The critical resolved shear stress (CRSS) that is required for dislocation breakaway increases with He/H-to-vacancy ratio at 600 K, indicating strong pinning effects of mixed He/H bubbles. However, as the temperature increases up to 1400 K, the mixed He/H bubbles become unstable as the H atoms are increasingly emitted from the mixed He/H bubbles and migrate into W matrix, which lowers bubble pressure and CRSS. Overall, these results highlight the synergistic effects of He and H on dislocation behavior in irradiated W during deformation.

36 - MATERIALS SCIENCE↗

Basic Energy Sciences Roundtable: Foundational Science for Carbon-Neutral Hydrogen Technologies

Basic research to identify and understand the fundamental principles governing hydrogen processes is essential for achieving a carbon-neutral, hydrogen-based energy and chemical infrastructure. In August 2021, the Office of Basic Energy Sciences (BES)—in coordination with the US Department of Energy (DOE) technology Offices of Energy Efficiency and Renewable Energy, Fossil Energy and Carbon Management, and Nuclear Energy—held a roundtable titled, “Foundational Science for Carbon-Neutral Hydrogen Technologies,” to discuss the scientific and technical barriers for carbon-neutral hydrogen production, storage, and utilization. Four priority research opportunities (PROs) were identified to address these scientific and technical challenges and accelerate progress toward the realization of energy-efficient, carbon-neutral cycles for hydrogen processes. The PROs are as follows: Discover and Control Materials and Chemical Processes to Revolutionize Electrolysis Systems; Manipulate Hydrogen Interactions to Harness the Full Potential of Hydrogen as a Fuel; Elucidate the Structure, Evolution, and Chemistry of Complex Interfaces for Energy- and Atom-Efficiency; and Understand and Limit Degradation Processes to Enhance the Durability of Hydrogen Systems.

08 HYDROGEN↗

Material technology

Advanced high pressure O2/H2 propulsion systems as exemplified by the Space Shuttle Main Engine (SSME) create challenging operating environments for materials. Many components operate in either hydrogen or hydrogen-steam environments which may significantly degrade the performance of common alloys. The objective of the materials technology projects is to develop and evaluate candidate materials for application in advanced high pressure O2/H2 propulsion systems. These new and improved materials are to improve the durability or performance of the SSME or derivative engine. The program includes projects on the following topics: (1) Hydrogen Resistant Alloys; (2) High Pressure O2 Ignition and Burning; (3) Improved Turbine Blades; (4) Improved Turbine Disk Material; (5) Impact Reactivity in High Pressure O2; and Fiber Reinforced Superalloys.

Dreshfield, R. L.↗

Dynamic Bubbling Balanced Proactive CO 2 Capture and Reduction on a Triple-Phase Interface Nanoporous Electrocatalyst

The formation and preservation of the active phase of the catalysts at the triple-phase interface during CO 2 capture and reduction is essential for improving the conversion efficiency of CO 2 electroreduction toward value-added chemicals and fuels under operational conditions. Designing such ideal catalysts that can mitigate parasitic hydrogen generation and prevent active phase degradation during the CO 2 reduction reaction (CO 2 RR), however, remains a significant challenge. Herein, we developed an interfacial engineering strategy to build a new SnO x catalyst by invoking multiscale approaches. This catalyst features a hierarchically nanoporous structure coated with an organic F-monolayer that modifies the triple-phase interface in aqueous electrolytes, substantially reducing competing hydrogen generation (less than 5%) and enhancing CO 2 RR selectivity (~90%). This rationally designed triple-phase interface overcomes the issue of limited CO 2 solubility in aqueous electrolytes via proactive CO 2 capture and reduction. Concurrently, we utilized pulsed square-wave potentials to dynamically recover the active phase for the CO 2 RR to regulate the production of C1 products such as formate and carbon monoxide (CO). This protocol ensures profoundly enhanced CO 2 RR selectivity (~90%) compared with constant potential (~70%) applied at -0.8 V (V vs RHE). We further achieved a mechanistic understanding of the CO 2 capture and reduction processes under pulsed square-wave potentials via in situ Raman spectroscopy, thereby observing the potential-dependent intensity of Raman vibrational modes of the active phase and CO 2 RR intermediates. Finally, this work will inspire material design strategies by leveraging triple-phase interface engineering for emerging electrochemical processes, as technology moves toward electrification and decarbonization.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

PdAu/YSZ composite hydrogen separation membranes with enhanced stability in the presence of CO

The effects of gold composition on the tolerance of palladium-based composite membranes to CO exposure was studied under the presence of high CO concentrations. Membranes with PdAu compositions ranging up to 41% by mass were exposed to binary 50/50 H 2 /CO gas atmospheres and both hydrogen flux and purity were monitored over time. It was observed that the highest gold composition (41%) suffered no degradation in membrane performance in terms of permeate hydrogen purity and hydrogen permeation flux during the 48 h exposure. Furthermore, for lower gold compositions, X-ray diffraction patterns suggested that carbon entered the film and could be removed by exposure to a non-CO containing gas mixture over time. However, removal of the carbon adversely affected purity; interestingly, some of the purity decline could be reversed upon re-exposure to the CO gas mixture. It is hypothesized that carbon loading in the palladium films causes lattice expansion and may even fill pore defects, thus lowering leaks through the Pd films. Furthermore, this study suggests that a membrane exposed to a CO mixture should not be cycled between CO and non-CO environments, but rather run continuously for best performance. Additionally, the choice of Pd-alloy and metal composition should be considered in regard to its carbon solubility to best predict lifetime performance.

08 HYDROGEN↗

Investigation of the Hydrogen Embrittlement of API 5L Natural Gas Pipeline Steels

Hydrogen ions produced during corrosion or through hydrogen blending into natural gas pipelines can lead to the degradation of ductility of metals used in these transmission pipelines. The effect of hydrogen on the mechanical properties of pipeline steels was studied for three grades of API 5L steels: X56, X65, and X100. These steels are either commonly used in or considered for use in natural gas transmission pipelines which are being considered for use in hydrogen blending. These steels were subjected to constant strain rate tensile testing after charging with electrochemically generated hydrogen. This presentation reports on work to extend the life of the natural gas pipeline network via understanding the effect of hydrogen embrittlement induced by corrosion processes.

Teeter, Lucas↗

Predicting and Controlling Corrosion (Abbreviated Final Report)

Corrosion accumulates significant replacement costs in the transportation, utility, manufacturing, and infrastructure sectors. It also underpins several of LLNL’s core missions in stockpile stewardship, defense, and energy security. Whereas most corrosion and aging models are empirically parameterized to describe well-defined conditions late in the reaction, the factors that determine the early stages of corrosion—during which mitigation could be most impactful— are poorly understood. This project addressed the critical need for new approaches to predict the kinetics of corrosion initiation based on firm physical and chemical understanding. The activities encompassed degradation of relevant metals in both hydrogen-rich and environmental corrosion scenarios. The team integrated state-of-the-art multiscale simulation, in situ characterization, and data science within three technical thrusts: hydriding of Ti alloys; aqueous corrosion of Al and Ni-Cr alloys; and degradation of additively manufactured 316L stainless steel. In each case, novel capabilities were developed to identify and track the impacts of key atomistic, compositional, and microstructural features on the metal systems. For hydriding, protocols were developed to tightly integrate multiscale models, advanced multimodal characterization, and machine learning to determine how hydrogen interacts with native passivating surface oxides and nucleates new undesired phases, shedding new light on the critical role of grain boundaries, interfaces, and atomically disordered regions. For aqueous corrosion, the project demonstrated methods to predict dissolution rates of metal surfaces in corrosive solutions, to measure and understand microstructural and grain orientation effects on corrosion susceptibility, and to investigate competing growth and dissolution kinetics of surface oxides. For additively manufactured metals, analysis using state-of-the-art microscopy techniques revealed the role of specific heterogeneities invoked during laser processing, including cellular structure, dislocations, and precipitates, on corrosion susceptibility. In addition to new capabilities and understanding, the project provided an avenue for workforce development, as well as key partnerships with stakeholders in corrosion science.

08 HYDROGEN↗

The effect of microstructure on hydrogen embrittlement of the nickel-base superalloy, Udimet 700

Material from a single heat of cast and wrought Udimet 700 was processed and/or heat treated to produce five material conditions with identical chemical compositions but with distinct microstructural variations, and then evaluated for susceptibility to hydrogen embrittlement. Two prealloyed powder conditions exhibited significantly improved resistance to hydrogen embrittlement, as compared to wrought material. No degradation in notch or smooth tensile strengths occurred, and average ductilities of 25 percent reduction of area were determined for 2 hydrogen evaluation procedures. For the most severe hydrogenation procedure, ductility levels were reduced to 15 percent. These improvements were attributed to cleaner grain boundaries and decreases grain size.

Gray, H. R.↗

The effect of microstructure on hydrogen embrittlement of the nickel base superalloy, Udimet 700

Material from a single heat of cast and wrought Udimet 700 was processed and/or heat treated to produce five material conditions with identical chemical compositions but with distinct microstructural variations, and then evaluated for susceptibility to hydrogen embrittlement. Two prealloyed powder conditions exhibited significantly improved resistance to hydrogen embrittlement, as compared to wrought material. No degradation in notch or smooth tensile strengths occurred, and average ductilities of 25 percent reduction of area were determined for 2 hydrogen evaluation procedures. For the most severe hydrogenation procedure, ductility levels were reduced to 15 percent. These improvements were attributed to cleaner grain boundaries and decreased grain size.

Gray, H. R.↗

Measurement of radiolytic hydrogen generation and impact of drying treatments on reactor exposed and surrogate aluminum materials

Technical challenges associated with dry storage of Aluminum-clad Spent Nuclear Fuel (ASNF) include a need to better understand the potential extent of gaseous molecular hydrogen (H 2 ) production through radiolytic degradation of the aluminum (oxy)hydroxide films present on ASNF. The characterization of radiolytic gas generation from ASNF (oxy)hydroxide layers has been identified as a key knowledge gap which poses a technical challenge to the long-term storage of ASNF. Task 2 of the action plan for the extended (>50 years) dry storage of ASNF addresses this gap. Previous radiolysis studies performed under Task 2 established baseline estimates of H 2 generation rates from the attendant hydrated oxides. The results confirmed that net radiolytic H 2 production has a dependency on absorbed gamma dose, as well as relative humidity and cover gas composition (air, nitrogen, and argon). Further experiments revealed that the physisorbed water on the samples may significantly impact the radiolytic H 2 yield. This phenomenon complicates the determination of H 2 generation rates for hydrated oxides, which may lead to inaccurate modeling predictions of the long-term H 2 yields in sealed storage systems containing ASNF, particularly when compared to spent fuel casks which have undergone some drying process intended to remove physically- and chemically-bound water. This report describes the testing methods utilized and the hydrogen generation results obtained in an investigation of the effects of gamma irradiation on aluminum materials for a variety of (oxy)hydroxide surface compositions and drying conditions. The testing methods included small-area aluminum material testing in ampules, and large-area aluminum material testing in steel vessels. Test material preparation, irradiation, and radiolytic H 2 measurement methods are summarized. The measured H 2 concentrations, which reflect the variable initial hydrated inventory and drying treatments, are compared to one another as well as to previously published data, to identify the primary factors affecting radiolytic H 2 generation rates and potential equilibrium H 2 concentrations.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Crack Growth Rate at Oxygen Electrode/Electrolyte Interface in Solid Oxide Electrolysis Cells Predicted by Experiment Coupled Multiphysics Modeling

Solid oxide electrolysis cell (SOEC) is a very efficient hydrogen production technology, but the cell degradation is a serious limiting factor for its long-term implementation. Oxygen electrode (OE) delamination is reported to be the critical degradation mechanism. In this study, we present a methodology to understand the delamination failure of the OE due to chemical stress in a better perspective. Several OE configurations were tested: baseline strontium-doped lanthanum cobalt iron oxide (LSCF) single layer design and tantalum-doped strontium cobalt oxide (SCT) - LSCF bilayer designs with different SCT loadings. An electro-chemo-mechanical model is developed to associate the electrochemical behavior of the cell with solid mechanics for calculating crack growth of the cell during long term test. The bilayer configuration with SCT 20 wt% has better performance as it survived in the long-term life test with the least crack length. This study implies that an additional nano-coating of SCT over the OE have improved the species transport and oxygen evolution with reduced chemical stress. As the operating current density decreases, it takes longer time for the cell to reach the delamination with the same critical crack length of 6.5 μ m (∼93% of the electrode/electrolyte interface length). Finally, it was concluded that chemical stress plays a significant role in interface delamination failure, however it may not be the only source of stresses at the interface.

08 HYDROGEN↗